Search NASA⌕ Search

SEARCH · Search NASA

Results for “STEELS - FRICTION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Tensile and pack compressive tests of some sheets of aluminum alloy, 1025 carbon steel, and chromium-nickel steel

Tensile and compressive stress-strain curves, stress-deviation curves, and secant modulus-stress curves are given for longitudinal and transverse specimens of 17S-T, 24S-T, and 24S-RT aluminum-alloy sheet in thicknesses from 0.032 to 0.081 inch, 1025 carbon steel sheet in thicknesses of 0.054 and 0.120 inch, and chromium-nickel steel sheet in thicknesses form 0.020 to 0.0275 inch. Significant differences were found between the tensile and the compressive stress-strain curves, and also the corresponding corollary curves; similarly, differences were found between the curves for the longitudinal and transverse directions. These differences are of particular importance in considering the compressive strength of aircraft structures made of thin sheet. They are explored further for the case of compression by giving tangent modulus-stress curves in longitudinal and transverse compression and dimensionless curves of the ratio of tangent modulus to Young's modulus and of the ratio of reduced modulus for a rectangular section to Young's modulus, both plotted against the ratio of stress to secant yield strength.

Atchison, C S↗

Evolution of {delta}ferrite in a CF3 cast stainless steel upon neutron irradiation to 3, 5, 10, 20, and 40 dpa

The microstructural evolution of delta ferrite in a CF3 cast stainless steel irradiated to 3, 5, 10, 20, and 40 dpa with two dose rates was studied with atom probe tomography (APT) and transmission electron mi-croscopy. Spinodal decomposition and G-phase precipitates induced by neutron irradiation and thermal aging were quantified systematically. The neutron irradiation significantly enhances the spinodal decom-position in delta ferrite as both the spinodal wavelength (i.e. a characteristic repeat distance) and am-plitude (i.e. magnitude of elemental concentration fluctuation) increase after irradiation. The wavelength only varies slightly when the dose increases from 5 to 40 dpa, while the amplitude increases dramatically from 10 to 20 dpa and starts to saturate before 20 dpa. The dose rate and irradiation temperature also have a notable effect on the spinodal wavelength and amplitude. The study shows that higher dose rate promotes a larger wavelength at given irradiation doses. Regarding the G-phase precipitates, a slightly lower irradiation temperature would result in a smaller mean size of G-phase precipitates, while a lower irradiation dose rate would lead to a larger G-phase precipitates at a given temperature and dose. Over-all, the spinodal decomposition and G-phase precipitates in the delta ferrite continue to evolve with the increasing dose beyond 10 dpa. This study confirms that the formation of G-phase precipitates at the in-terdomain region between alpha and alpha-prime is facilitated by the Si and Mo atoms rejected from Fe rich alpha phase and the Ni and Mn atoms rejected from Cr rich alpha-prime phase. Neutron irradiation plays a dominant role in the ferrite instability, and the effect of prior thermal aging at 400 degrees C for 10,000 hours is negligible as the dose is 3 dpa and above.

duplex stainless steel↗

Enabling Production of Low Carbon Emissions Steel through CO 2 Capture from Blast Furnace Gases at Cleveland Cliffs’ 5 mtpa Steel Plant at Burns Harbor, Indiana

Dastur International Inc. has prepared a DOE-funded Pre-front-end engineering design (Pre-FEED) study to capture up to 2.8 mtpa of CO 2 from the available Blast Furnace (BF) gases at the Burns Harbor steel plant operated by Cleveland Cliffs in Burns Harbor, Indiana. The project consists of an amine solvent based pre-combustion carbon capture system, along with a unique BF gas conditioning process which significantly optimizes the project design and architecture in terms of higher volumes (2.8 mtpa vis-à-vis 1.6 mtpa without conditioning) & concentration (32 vol% in conditioned gas vs. 22% in raw BF gas) of CO 2 , which can be captured using a single train, resulting in reduced size and capital cost of the CO 2 capture island, and improved overall economics on a $\$$/tCO 2 captured basis.

42 ENGINEERING↗

Pitting Corrosion in 316L Stainless Steel Fabricated by Laser Powder Bed Fusion Additive Manufacturing: A Review and Perspective

Abstract 316L stainless steel (316L SS) is a flagship material for structural applications in corrosive environments, having been extensively studied for decades for its favorable balance between mechanical and corrosion properties. More recently, 316L SS has also proven to have excellent printability when parts are produced with additive manufacturing techniques, notably laser powder bed fusion (LPBF). Because of the harsh thermo-mechanical cycles experienced during rapid solidification and cooling, LPBF processing tends to generate unique microstructures. Strong heterogeneities can be found inside grains, including trapped elements, nano-inclusions, and a high density of dislocations that form the so-called cellular structure. Interestingly, LPBF 316L SS not only exhibits better mechanical properties than its conventionally processed counterpart, but it also usually offers much higher resistance to pitting in chloride solutions. Unfortunately, the complexity of the LPBF microstructures, in addition to process-induced defects, such as porosity and surface roughness, have slowed progress toward linking specific microstructural features to corrosion susceptibility and complicated the development of calibrated simulations of pitting phenomena. The first part of this article is dedicated to an in-depth review of the microstructures found in LPBF 316L SS and their potential effects on the corrosion properties, with an emphasis on pitting resistance. The second part offers a perspective of some relevant modeling techniques available to simulate the corrosion of LPBF 316L SS, including current challenges that should be overcome.

Voisin, T. (ORCID:0000000287462659)↗

Microstructural characterization of cold-worked 316 stainless steel flux thimble tubes irradiated up to 100 dpa in a commercial Pressurized Water Reactor

Two flux thimble tubes (FTT) made of 15% cold-worked 316 stainless steel (SS) were harvested from Ringhals Pressurized Water Reactor (PWR) Unit 2, with peak damages of 76 and 100 displacements per atom (dpa) after 29 and 34 years’ service, respectively. Specimens sectioned from parent tubes were comprehensively characterized with nominal damage levels of ~0, ~41, ~74, 76, and 100 dpa at a nominal temperature range of 285-323 °C. Both FTTs contained helium and hydrogen gases as transmutation products. The helium follows a production rate of ~9.8 appm/dpa, while environmental factors complicate hydrogen production obscuring an exact H/dpa ratio. Irradiation-induced dislocation loops, nano-cavities, solute clusters, and microsegregation were all observed. The dislocation loops and nano-cavities indicated saturation at 41 dpa. The solute clusters continued to evolve with Ni-Si clusters formed at 41 dpa, and Ni-Si-Mn-P clusters formed at 74 and 100 dpa, but neither clusters exhibited distinct diffraction patterns at any damage levels. Solute clusters were observed to frequently be co-located with dislocation loops, but fully decorated loops were rarely detected. Significant radiation-induced segregation (RIS) was observed around grain boundaries at all damage levels. The modified inverse Kirkendall (MIK) model captured the RIS behavior of major elements. Large cavities within or around an Mn-S rich region were observed for the first time. Through all the damage levels, void swelling is always below 0.05%, making significant dimensional change unlikely in core internals when used at similar conditions. Meanwhile, the role of overwhelming nanocavities, presumably helium bubbles, should be considered in other potential degradation mechanisms, including irradiation-assisted stress corrosion cracking, embrittlement, and loss of fracture toughness, which remain the concerns for extended operation of nuclear power plants.

Post Irradiation Examination, Isotope Dilution Mas↗

Integrated Reference Electrodes in Anion-Exchange-Membrane Electrolyzers: Impact of Stainless-Steel Gas-Diffusion Layers and Internal Mechanical Pressure

Alkaline-membrane electrolyzers operating in pure water might provide scalable low-cost H 2 production but currently lag in performance and durability compared to commercial technologies. Typically, membrane–electrode assemblies (MEAs) are optimized in electrolyzers by changing one parameter at a time and assessing the resulting system performance via two-electrode polarization and impedance measurements. These approaches are limited in their ability to assign performance changes and durability to specific electrodes or processes. We integrate a reference electrode with the MEA to separate anode and cathode responses in both polarization and impedance measurements. Here we illustrate the power of the approach by showing how the fiber diameter of stainless-steel gas-diffusion layers (GDLs) affects performance solely at the anode, while changing the thickness of the cathode GDL simultaneously affects the performance of the anode and cathode due to changes in internal pressure from mechanical compression. This finding was obscured in conventional two-electrode measurements. The work thus guides both high-performance alkaline-membrane water-electrolyzer development and illustrates a useful strategy to study structure–activity relationships in the MEA.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Residual Stress Modeling and Advanced Diffraction Measurements of 347H Steel Weldments

The 347H stainless steel is a primary high-temperature material for many energy and power generation industries. Stress relief cracking (SRC) has been a particular concern in welding of this material. The residual stress induced by welding and its evolution during post-welding heat treatment (PWHT) and subsequent operating and service conditions is one of the primary factors contributing to SRC. The lifetime of welded structure components is also controlled by the precipitation kinetics that accompanies PWHT, stress relaxation process, and long-term aging and complex synergistic factors. Various theories have been proposed in the past to explain SRC. However, a widely accepted approach to predicting the entire damage evolution and the resulting performance reduction is still lacking. This study is to demonstrate a reliable solution for two critical issues that affect the predictions. First, the residual stress distribution obtained from both simulation and neutron diffraction is compared, which increases the accuracy of mechanical analysis simulation model and therefore builds a solid basis for the lifetime prediction model. Second, the generation, evolution, and annihilation of precipitates are monitored by the synchrotron diffraction experiment. Preliminary results demonstrate the critical importance of precipitation kinetics on the residual stress distribution/redistribution during heat treatments.

Yang, Yi↗

The effect of electrical current on premature failures and microstructural degradation in bearing steel

Premature failures associated with microstructural degradation, i.e. white etching cracks (WECS), are becoming commonplace as applications are requiring tribological components to operate under extreme conditions. Although the specific drivers of WECs are still debated, the failures are often found in applications where cyclic loading is combined with added energy from stressors such as slip, impacts, or stray current. The aim of the current work is to elucidate effect that variable current has on premature failure. Numerous commercially available lubricants were tested, and both lubricant base oil type and additive package were found to have an effect on WEC failure time.

Bearing failure↗