Stress Relaxation Cracking in 347H Stainless Steel Arc Welds: Susceptibility Evaluation of Heat-Affected Zone

Stress relaxation cracking (SRC) is considered one of the major failure mechanisms for 347H stainless steel welds at elevated service temperatures or during post weld heat treatment (PWHT), especially within the heat-affected zone (HAZ). This work focuses on the characterization of SRC susceptibility within 347H physically simulated arc welded HAZ at elevated temperatures. A four-step SRC thermomechanical test in combination with finite element modeling (FEM) of the welding and testing processes is developed to establish a susceptibility map for HAZ. The test first runs a thermal cycle with three different peak temperatures (1335, 1275, and 1150 °C) to duplicate representative HAZ subzone microstructures, followed by time-to-failure examination under a variety of pre-stress (260–600 MPa) and pre-strain conditions (0.03–0.19) as a function of reheat temperatures between 750 and 1050 °C. With the aid of FEM, SRC susceptibility maps are generated to identify the threshold stress, plastic strain, and creep strain as a function of test temperature. It was found out that HAZ subzone with a lower peak temperature (1150 °C) appears to be slightly less susceptible to SRC than the other two subzones that experienced higher peak temperatures. Generally, time-to-fracture reduces with increasing initially applied stress and strain for all test temperatures. The pre-stress thresholds decrease from about 500 to 330 MPa as the testing temperature increases from 800 to 1050 °C, while the corresponding initial plastic strain thresholds reduces from 0.15 to 0.06. The SRC susceptibility was also evaluated through the Larson–Miller Parameter (LMP) analysis as a function of plastic strain, initial stress and starting stress upon reaching the testing temperature, respectively. The 1050 °C test with a high pre-applied strain (0.1) exhibits an extremely short time to failure (t = 3 s) that lies outside the general trend in LMP analysis. Additionally, it was identified that a plastic strain above 0.07 is identified to significantly reduce the bulk creep strain tolerance to fracture and therefore increases SRC susceptibility. Hardness measurement and fractography analysis indicated that the strain aging of niobium carbonitrides and other potential phases in conjunction with intergranular precipitates contributes to an increase in microhardness and increased intergranular cracking susceptibility.

14 SOLAR ENERGY↗

Strain and distortion monitoring during arc welding by 3D digital image correlation

A novel three-dimensional (3D) digital image correlation (DIC) approach using a stereovision system was developed to measure the evolution of strain and distortion near the fusion zone during the gas tungsten arc welding process. Unlike the previously reported two-dimensional (2D) DIC approach using a single camera, the 3D DIC method was immune to the out-of-plane displacement and was capable of measuring 3D deformation. Both 2D and 3D DIC approaches in welding applications were based on the utilisation of the novel high-temperature speckle and the pulsed laser illumination plus bandpass filters. However, the speckle pattern was partially specular reflective causing issues in subset matching in the 3D approach. A new algorithm and experimental procedure was incorporated to solve this problem.

47 OTHER INSTRUMENTATION↗

Video Game Device Haptic Interface for Robotic Arc Welding

Recent advances in technology for video games have made a broad array of haptic feedback devices available at low cost. This paper presents a bi-manual haptic system to enable an operator to weld remotely using the a commercially available haptic feedback video game device for the user interface. The system showed good performance in initial tests, demonstrating the utility of low cost input devices for remote haptic operations.

99 GENERAL AND MISCELLANEOUS↗

The Effect of SiC Addition on Microstructure and Mechanical Properties of Gas Tungsten Arc-Welded Ti-6Al-4V Alloy

In the present study, SiC powder was added in situ for bead-on-plate weldments and fusion butt joints to modify the microstructure and the corresponding mechanical properties. Cross sections of bead-on-plate welds demonstrated that the SiC addition resulted in significant changes of the titanium microstructure. Specifically, a fine lamellar structure of α-phase with a small amount of intergranular β-titanium within the fusion zone could be established. Moreover, the size of prior β-grains was significantly reduced. After welding, no intermetallic silicides were observed. In the fusion zone of the SiC-enhanced samples, a small increase in hardness resulted, and the samples showed an increase in tensile strength, yield strength and elongation.

36 MATERIALS SCIENCE↗

Quarterly Management Document – FY20, 1st Quarter, Multi-pass Hybrid Laser Arc Welding of Alloy 740H

During the first quarter of FY20, work focused on implementing a subcontract with Penn State University to collaborate on the project. Significant delays prevented the subcontract from being placed until the end of December. As a result only limited progress was made on the project. Required equipment was researched and ordered during the first quarter but will not be delivered until the middle of the second quarter of FY20. Delays are not expected to adversely impact the schedule of the project.

36 MATERIALS SCIENCE↗

FY20, 3rd Quarter, Multi-pass Hybrid Laser Arc Welding of Alloy 740H

Although progress has been slowed by telecommuting restrictions at INL and PSU, progress has been made by PSU on modeling and simulation of deep penetration laser welding. Additionally, both INL and PSU has received critical equipment, in the form of high-powered laser wobble heads, needed to verify the modeling and simulation results. The equipment was installed at INL and preliminary tests, based on a test matrix that was developed in this 3rd quarter, will be made early in the 4th quarter. Similarly, the PSU laser wobble head is expected to be installed early in the 4th quarter and preliminary experiments are expected to commence shortly thereafter. Completion dates on a few milestones have been impacted and new dates proposed.

36 MATERIALS SCIENCE↗

Microstructure Optimization and Cracking Control of Additive Manufactured Bainite Steel by Gas Metal Arc Welding Technology

In this work, bainite steel thin wall was prepared by additive manufacturing (AM) with an in situ isothermal transformation at 300 °C. The microstructures were analyzed by scanning electron microscopy (SEM), x-ray diffraction (XRD) and transmission electron microscopy (TEM). The mechanical properties of the AM samples were measured by microhardness testing and tensile testing. The results show that the bainite steel thin wall is free from cracks and each layer has a good bond with preceding one. The bainite steel thin wall displays consistent mechanical properties. The formation of the bainite microstructure improves the toughness of the thin wall and reduces the embrittlement caused by dendritic segregation.

36 MATERIALS SCIENCE↗

Gas tungsten arc welding and post weld heat treatment effects on microstructure and mechanical property of castable nanostructured alloy steel

Here, this paper details the first study of castable nanostructured alloy (CNA) steel gas tungsten arc weldability and the post-weld heat treatment (PWHT) effects. Effects of welding heat input, thermal cycles, and PWHT on microstructures, microhardness distributions, room temperature tensile properties, and fracture characteristics are discussed. Results show that CNA steel exhibits excellent weldability (i.e., no indication of welding defects and reasonable tensile properties). The welded joint exhibited heterogeneous microstructures with δ-ferrite as well as large microhardness variation and fluctuation. The welded joint yield and ultimate tensile strengths were similar to those of the base metal, but the elongations decreased by 30 %. However, with normalization and tempering PWHT, the δ-ferrite was eliminated, microstructure was modified, hardness was unified, and joint ductility was restored. The study indicated that the CNA reduced-activation ferritic-martensitic steel owns excellent weldability, and PWHT is needed for the industrial application of welded structures.

36 MATERIALS SCIENCE↗

Titanium Wire Arc Additive Manufacturing Inert Enclosure and Material Handling Safety Considerations

Wire arc additive manufacturing (WAAM) via metal inert gas (MIG)/gas metal arc welding (GMAW) is a viable option for fabrication of large-scale titanium parts; however, it introduces new safety hazards associated with both the material and the additional system hardware required for the process. Localized gas shielding of the weld arc via standard GMAW torch is inadequate for titanium due to its affinity for oxygen; thereby requiring the use of an inert enclosure to protect the weld from entraining oxygen. The use of the inert enclosure presents potential safety hazards such as operator asphyxiation and brings up discussion of confined space considerations. In addition, the titanium welding process creates pyrophoric titanium soot residue around the deposit, which can undergo deflagration during part cleaning and part removal. This paper provides an overview of the titanium WAAM process along with safety considerations for the design and operation of the inert enclosure as well as functional solutions for the safe handling of the titanium soot by-product.

Walters, Alex↗

Characterization of Solid State Phase Transformation in Continuously Heated and Cooled Ferritic Weld Metal

Arc welding processes involve cooling rates that vary over a wide range (1-100 K/s). The final microstructire is thus a product of the heating and cooling cycles experienced by the weld in addition to the weld composition. It has been shown that the first phase to form under weld cooling conditions may not be that predicted by equilibrium calculations. The partitioning of different interstitial/substitutional alloying elements at high temperatures can dramatically affect the subsequent phase transformations. In order to understand the effect of alloying on phase transformation temperatures and final microstructures time-resolved X-ray diffraction technique has been successfully used for characterization. The work by Jacot and Rappaz on pearlitic steels provided insight into austenitization of hypoeutectic steels using a finite volume model. However there is very little work done on the effect of heating and cooling rates on the phase transformation paths in bainitic/martensitic steels and weld metals. Previous work on a weld with higher aluminum content, deposited with a FCAW-S process indicated that even at aluminum levels where the primary phase to solidify from liquid should be delta ferrite, non-equilibrium austenite was observed. The presence of inhomogeneity in composition of the parent microstructure has been attributed to differences in transformation modes, temperatures and microstructures in dual-phase, TRIP steels and ferritic welds. The objectives of the work included the identification of the stability regions of different phases during heating and cooling, differences in the effect of weld heating and cooling rates on the phase transformation temperatures, and the variation in phase fractions of austenite and ferrite in the two phase regions as a function of temperature. The base composition used for the present work is a Fe-1%Al-2%Mn-1%Ni-0.04%C weld metal. A pseudo-binary phase diagram shows the expected solidification path under equilibrium conditions. However, the effect of heating and cooling rates on the phase transformation path due to non-equilibrium partitioning of alloying elements cannot be predicted by equilibrium phase diagrams. Also, it is unclear if there is retention of delta ferrite to room temperature due to compositional or thermal effects. This would dramatically affect the austenite to ferrite transformation due to carbon and nitrogen enrichment in the austenite.

36 MATERIALS SCIENCE↗

Optical emission spectroscopy of metal vapor dominated laser-arc hybrid welding plasma

During laser-arc hybrid welding, plasma properties affect the welding process and the weld quality. However, hybrid welding plasmas have not been systematically studied. Here we examine electron temperatures, species densities, and electrical conductivity for laser, arc, and laser-arc hybrid welding using optical emission spectroscopy. The effects of arc currents and heat source separation distances were examined because these parameters significantly affect weld quality. Time-average plasma electron temperatures, electron and ion densities, electrical conductivity, and arc stability decrease with increasing heat source separation distance during hybrid welding. Heat source separation distance affects these properties more significantly than the arc current within the range of currents considered. Improved arc stability and higher electrical conductivity of the hybrid welding plasma result from increased heat flux, electron temperatures, electron density, and metal vapor concentrations relative to arc or laser welding.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Toughness of High-Strength Steel Weld Metals

Low-temperature phase transformation (LTPT) welding consumables are a new class of welding wires developed to mitigate hydrogen-induced cracking in the welding of high-strength steels without preheating or postweld heat treatment. LTPT weld metals have a high strength, but their toughness needs further investigation. LTPT weld metals predominately contain a martensite microstructure, which is necessary to achieve high strength; however, martensitic weld metals containing oxide inclusions have relatively poor toughness. For this study, three welding processes — gas metal arc welding (GMAW), gas tungsten arc welding (GTAW), and hot wire GTAW — were investigated. Optical microscopy, scanning electron microscopes, and transmission electron microscopes were employed for characterization. The role of the shielding gas in the formation of oxide inclusions in LTPT weld metals was investigated. The formation of oxide inclusions in the weld metals was related to the CO 2 in the shielding gas. When 100% Ar or a pure inert shielding gas mixture was used for all three welding processes, oxide inclusions were greatly reduced, and the weld metal toughness improved considerably, matching the base metal toughness. The mechanism by which inclusions promote fracture propagation in the weld metal was proposed.

36 MATERIALS SCIENCE↗