Search NASA⌕ Search

SEARCH · Search NASA

Results for “Weibull modulus,”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Size effects in 3D–printed polymer–derived, zirconium diboride–reinforced ceramic composites

Preceramic polymers are of interest for use in many manufacturing techniques such as injection molding, ceramic fiber infiltration, and additive manufacturing. However, off-gassing of low molecular weight oligomers occurs when these polymers cure, potentially leading to porosity in the cured part. Here to study how porosity and strength are affected by the size of the printed part, and the presence of a high surface area nano-scale filler, polycarbosilane (PCS) microrods of varying diameter were fabricated via direct ink writing (DIW), an additive manufacturing technique, with two ink formulations containing either zirconium diboride (ZrB 2 ) alone, or ZrB 2 and fumed alumina (FA). Sets of microrods were printed in a range of sizes by using print nozzles of 450, 634, 979, 1 346, or 1 702 μm in diameter, which were thermally cured, pyrolyzed to form ceramic composite microrods, and tested in 3-pt flexure. Porosity increased with increasing diameter, while failure strength decreased. For a given nozzle size, the microrods containing FA displayed lower porosity and higher strength (up to ~500 MPa) compared to the microrods containing only ZrB 2 . Weibull strength analysis was performed on each group of microrods and shows that the addition of FA increased Weibull modulus from 4.63 ± 1.56 to 9.35 ± 0.601. In conjunction with optical microscopy, this analysis indicates two distinct flaw populations in the printed materials, porosity which arises during the curing step and cracking which arises during pyrolysis of the larger specimens.

36 MATERIALS SCIENCE↗

Strength distributions of laminated FeNi-based metal amorphous nanocomposite ribbons

Metal Amorphous Nanocomposite (MANC) materials offer low losses at high magnetic switching frequency, enabling high power density motors with increased rotational speed. While MANCs have high strength, they are brittle. The use of motor components such as a rotor consisting of brittle material presents a reliability concern. Here, a promising MANC alloy is subjected to tensile tests and failure is observed with high-speed photography. A method is developed to prepare tensile specimens of laminated MANC and epoxy layers, simulating the stacking of an epoxy-impregnated tape-wound core. Tensile tests are conducted for single layer ribbon and for five- and ten-layer stacks of laminated material with thin layers of thermosetting epoxy. Failure distributions are shown to have increasing Weibull modulus with increasing layer count. The composite MANC material system is modeled using chain-of-bundles models. Using a k-failure model, we show that single ribbon strength distribution data can be used to predict well the failure distribution of laminated stacks. The agreement occurs when the assumed ineffective length, over which load is recovered in a failed layer, is comparable to the observed interlaminar separation length.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Effective Size Analysis of the Diametral Compression (Brazil) Test Specimen

This study considers the finite element analysis (FEA) simulation and Weibull effective size analysis for the diametral compression (DC) or Brazil specimen loaded with three different push-rod geometries. Those geometries are a flat push-rod, a push-rod whose radius of curvature is larger than that for the DC specimen, and a push-rod whose radius of curvature matches that of the DC specimen. Such established effective size analysis recognizes that the tensile strength of structural ceramics is typically one to two orders of magnitude less than its compressive strength. Therefore, because fracture is much more apt to result from a tensile stress than a compressive one, this traditional analysis only considers the first principal tensile stress field in the mechanically loaded ceramic component for the effective size analysis. The effective areas and effective volumes were computed as function of Weibull modulus using the CARES/Life code. Particular attention was devoted to the effect of mesh sensitivity and localized stress concentration. The effect of specimen width on the stress state was also investigated. The effects of push-rod geometry, the use of steel versus WC push-rods, and considering a frictionless versus no-slip interface between push-rod and specimen on the maximum stresses, where those stresses are located, and the effective area and effective volume results are described. Of the three push-rod geometries, it is concluded that the push-rod (made from WC rather than steel) whose radius of curvature matches that of the DC specimen is the most apt to cause fracture initiation within the specimen's bulk rather than at the loading interface. Therefore, its geometry is the most likely to produce a valid diametral compression strength test. However, the DC specimen remains inefficient in terms of its area and volume efficiencies; namely, the tensile strength of only a few percent of the specimen's entire area or volume is sampled. Given the high probability that a valid (or invalid) test can be proven by ceramic fractographic practices suggests that this test method and specimen is questionable for use with relatively strong structural ceramics.

36 MATERIALS SCIENCE↗

Additive Manufacturing of C/C-SiC Ceramic Matrix Composites by Automated Fiber Placement of Continuous Fiber Tow in Polymer with Pyrolysis and Reactive Silicon Melt Infiltration

An additive manufacturing process for fabricating ceramic matrix composites has been developed based on the C/C-SiC system. Automated fiber placement of the continuous carbon fibers in a polyether ether ketone matrix was performed to consolidate the carbon fibers into a printed preform. Pyrolysis was performed to convert the polymer matrix to porous carbon, and then Si was introduced by reactive melt infiltration to convert a portion of the carbon matrix to silicon carbide. The densities and microstructures were characterized after each step during the processing, and the mechanical properties were measured. The C/C-SiC composites exhibited a porosity of 10–20%, characteristic flexural strength of 234.91 MPa, and Weibull modulus of 3.21. The composites displayed toughness via a significant displacement to failure.

36 MATERIALS SCIENCE↗

Ceramics for the advanced automotive gas turbine engine: A look at a single shaft design

The results of a preliminary analysis of a single shaft regenerative design with a single stage radial turbine are presented to show the fuel economy that can be achieved at high turbine inlet temperatures, with this particular advanced design, if the turbine tip speed and regenerator inlet temperature are not limited. The engine size was 100 hp for application to a 3500 lb auto. The fuel economy was analyzed by coupling the engine to the auto through a continuously variable speed-ratio transmission and operating the system at constant turbine inlet temperature over the Composite Driving Cycle. The fuel was gasoline and the analysis was for a 85 F day. With a turbine inlet temperature of 2500 F the fuel economy was 26.2 mpg, an improvement of 18 percent over that of 22.3 mpg with a turbine inlet temperature of 1900 F. The turbine tip speed needed for best economy with the 2500 F engine was 2530 ft/sec. The regenerator temperature was approximately 2200 F at idle. Disk stresses were estimated for one single stage radial turbine and two two-stage radial-axial turbines and compared with maximum allowable stress curves estimated for a current ceramic material. Results show a need for higher Weibull Modulus, higher strength ceramics.

Nosek, S. M.↗

Effect of hot isostatic pressing on the properties of sintered alpha silicon carbide

Two lots of alpha silicon carbide were isostatically hot-pressed under 138 MPa for 2 h in Ar at temperatures up to 2200 C. Nearly theoretically dense specimens resulted. Hot isostatic pressing increased both room-temperature strength and 1200 C strength, and resulted in improved reliability. One lot of material which was pressed at 2200 C showed increases of about 20 percent in room-temperature strength and about 50 percent in 1200 C flexural strength; the Weibull modulus improved about 100 percent.

Watson, G. K.↗

The effects of surface finish and grain size on the strength of sintered silicon carbide

The effects of surface treatment and microstructure, especially abnormal grain growth, on the strength of sintered SiC were studied. The surfaces of sintered SiC were treated with 400, 800 and 1200 grit diamond wheels. Grain growth was induced by increasing the sintering times at 2050 C. The beta to alpha transformation occurred during the sintering of beta-phase starting materials and was often accompanied by abnormal grain growth. The overall strength distributions were established using Weibull statistics. The strength of the sintered SiC is limited by extrinsic surface flaws in normal-sintered specimens. The finer the surface finish and grain size, the higher the strength. But the strength of abnormal sintering specimens is limited by the abnormally grown large tabular grains. The Weibull modulus increases with decreasing grain size and decreasing grit size for grinding.

You, Y. H.↗

Improved silicon nitride for advanced heat engines

Silicon nitride is a high temperature material currently under consideration for heat engine and other applications. The objective is to improve the net shape fabrication technology of Si3N4 by injection molding. This is to be accomplished by optimizing the process through a series of statistically designed matrix experiments. To provide input to the matrix experiments, a wide range of alternate materials and processing parameters was investigated throughout the whole program. The improvement in the processing is to be demonstrated by a 20 percent increase in strength and a 100 percent increase in the Weibull modulus over that of the baseline material. A full characterization of the baseline process was completed. Material properties were found to be highly dependent on each step of the process. Several important parameters identified thus far are the starting raw materials, sinter/hot isostatic pressing cycle, powder bed, mixing methods, and sintering aid levels.

Yeh, H. C.↗

Improved processing of alpha-SiC

Dry pressing/sintering, slurry pressing/sintering, and hot isostatic pressing have been investigated with a view to developing an optimum processing technique to produce high-strength SiC for high-temperature structural applications. A baseline strength of 348 MPa was achieved by dry pressing and sintering. When slurry pressing was used to minimize agglomerates in the powder, a baseline strength of 428 MPa was obtained. An additional improvement in strength (655 MPa) was obtained by hot isostatic pressing, which prevented the formation of critical flaws resulting from residual agglomerates in the powder. It is expected that surface finish, such as lapping, polishing, and heat treatment, may further improve the strength and Weibull modulus of hot isostatically pressed alpha-sic.

Dutta, Sunil↗

High-strength silicon carbides by hot isostatic pressing

Silicon carbide has strong potential for heat engine hardware and other high-temperature applications because of its low density, good strength, high oxidation resistance, and good high-temperature creep resistance. Hot isostatic pressing (HIP) was used for producing alpha and beta silicon carbide (SiC) bodies with near-theoretical density, ultrafine grain size, and high strength at processing temperatures of 1900 to 2000 C. The HIPed materials exhibited ultrafine grain size. Furthermore, no phase transformation from beta to alpha was observed in HIPed beta-SiC. Both materials exhibited very high average flexural strength. It was also shown that alpha-SiC bodies without any sintering aids, when HIPed to high final density, can exhibit very high strength. Fracture toughness K (sub C) values were determined to be 3.6 to 4.0 MPa m (sup 1/2) for HIPed alpha-SiC and 3.7 to 4.1 MPa m (sup 1/2) for HIPed beta-SiC. In the HIPed specimens strength-controlling flaws were typically surface related. In spite of improvements in material properties such as strength and fracture toughness by elimination of the larger strength-limiting flaws and by grain size refinement, HIPing has no effect on the Weibull modulus.

Dutta, Sunil↗

Improved silicon carbide for advanced heat engines

Work performed to develop silicon carbide materials of high strength and to form components of complex shape and high reliability is described. A beta-SiC powder and binder system was adapted to the injection molding process and procedures and process parameters developed capable of providing a sintered silicon carbide material with improved properties. The initial effort has been to characterize the baseline precursor materials (beta silicon carbide powder and boron and carbon sintering aids), develop mixing and injection molding procedures for fabricating test bars, and characterize the properties of the sintered materials. Parallel studies of various mixing, dewaxing, and sintering procedures have been carried out in order to distinguish process routes for improving material properties. A total of 276 MOR bars of the baseline material have been molded, and 122 bars have been fully processed to a sinter density of approximately 95 percent. The material has a mean MOR room temperature strength of 43.31 ksi (299 MPa), a Weibull characteristic strength of 45.8 ksi (315 MPa), and a Weibull modulus of 8.0. Mean values of the MOR strengths at 1000, 1200, and 14000 C are 41.4, 43.2, and 47.2 ksi, respectively. Strength controlling flaws in this material were found to consist of regions of high porosity and were attributed to agglomerates originating in the initial mixing procedures. The mean stress rupture lift at 1400 C of five samples tested at 172 MPa (25 ksi) stress was 62 hours and at 207 MPa (30 ksi) stress was 14 hours. New fluid mixing techniques have been developed which significantly reduce flaw size and improve the strength of the material. Initial MOR tests indicate the strength of the fluid-mixed material exceeds the baseline property by more than 33 percent.

Whalen, T. J.↗

Strength distribution in commercial silicon carbide materials

Four-point flexural strength testing has been conducted in order to establish the baseline strength and reliability of four different commercial SiC types, in conjunction with reliable Weibull modulus values. Average strength of the samples ranged from 380 to 482 MPa at room temperature and 307 to 470 MPa at 1370 C. The strength scatter reflects the effect of flaw variability, which must be minimized to improve reliability in sintered SiC.

Dutta, Sunil↗

Effects of various consolidation techniques on microstructure, strength, and reliability of alpha-SiC

The effects of slurry pressing, HIP, and sinter-HIP on the strength, microstructure, and critical processing flaws in alpha-SiC are examined. Also, the feasibility of glass encapsulation is determined. Baseline strength was improved by about 25 percent by using slurry pressing instead of dry pressing. HIP further improved average strength to as high as 655 MPa. Sinter-HIP did not noticeably improve average strength. Although process-related flaws such as shrinkage cracks and large voids were not seen in HIPed alpha-SiC, surface-related flaws were observed. It is suggested that surface finishing by lapping, polishing, and heat treating might reduce the effect of surface-related flaws, improving the Weibull modulus in HIPed alpha-SiC.

Dutta, Sunil↗

Improved silicon carbide for advanced heat engines

This is the second annual technical report entitled, Improved Silicon Carbide for Advanced Heat Engines, and includes work performed during the period February 16, 1986 to February 15, 1987. The program is conducted for NASA under contract NAS3-24384. The objective is the development of high strength, high reliability silicon carbide parts with complex shapes suitable for use in advanced heat engines. The fabrication methods used are to be adaptable for mass production of such parts on an economically sound basis. Injection molding is the forming method selected. This objective is to be accomplished in a two-phase program: (1) to achieve a 20 percent improvement in strength and a 100 percent increase in Weibull modulus of the baseline material; and (2) to produce a complex shaped part, a gas turbine rotor, for example, with the improved mechanical properties attained in the first phase. Eight tasks are included in the first phase covering the characterization of the properties of a baseline material, the improvement of those properties and the fabrication of complex shaped parts. Activities during the first contract year concentrated on two of these areas: fabrication and characterization of the baseline material (Task 1) and improvement of material and processes (Task 7). Activities during the second contract year included an MOR bar matrix study to improve mechanical properties (Task 2), materials and process improvements (Task 7), and a Ford-funded task to mold a turbocharger rotor with an improved material (Task 8).

Whalen, Thomas J.↗

High-strength silicon carbides by hot isostatic pressing

Silicon carbide has strong potential for heat engine hardware and other high-temperature applications because of its low density, good strength, high oxidation resistance, and good high-temperature creep resistance. Hot isostatic pressing (HIP) was used for producing alpha and beta silicon carbide (SiC) bodies with near-theoretical density, ultrafine grain size, and high strength at processing temperatures of 1900 to 2000 C. The HIPed materials exhibited ultrafine grain size. Furthermore, no phase transformation from beta to alpha was observed in HIPed beta-SiC. Both materials exhibited very high average flexural strength. It was also shown that alpha-SiC bodies without any sintering aids, when HIPed to high final density, can exhibit very high strength. Fracture toughness K (sub C) values were determined to be 3.6 to 4.0 MPa m (sup 1/2) for HIPed alpha-SiC and 3.7 to 4.1 MPa m (sup 1/2) for HIPed beta-SiC. In the HIPed specimens strength-controlling flaws were typically surface related. In spite of improvements in material properties such as strength and fracture toughness by elimination of the larger strength-limiting flaws and by grain size refinement, HIPing has no effect on the Weibull modulus.

Dutta, Sunil↗

Tensile adhesion testing methodology for thermally sprayed coatings

The structure of thermally sprayed coatings consists of lamellae which are oriented parallel to the substrate surface. The lamellae separate and fracture by distinctive mechanisms which are reflected in the failure morphology, and these may be described as adhesive (between the coating and substrate), cohesive (within the coating), or mixed mode. There is a large variability in the failure stress for any nominally identical group of coatings. A lower bound for the fracture toughness of alumina coatings can be calculated as 0.2 MNm exp -3/2. The coating strength values may also be treated as belonging to the statistical distribution of the Weibull function. The Weibull modulus of the coating strength varied from 1.4 to 3.8. This analysis infers that the flaw size within coatings is highly variable and that the flaws are nonuniformly dispersed. The present work focuses on the question of whether tensile adhesion tests are an appropriate testing method for thermally sprayed materials.

Berndt, Christopher C.↗

Mechanical behavior and failure phenomenon of an in situ-toughened silicon nitride

The Weibull modulus, fracture toughness and crack growth resistance of an in-situ toughened, silicon nitride material used to manufacture a turbine combustor were determined from room temperature to 1371 C. The material exhibited an elongated grain structure that resulted in improved fracture toughness, nonlinear crack growth resistance, and good elevated temperature strength. However, low temperature strength was limited by grains of excessive length (30 to 100 microns). These excessively long grains were surrounded by regions rich in sintering additives.

Salem, Jonathan A.↗

Evaluation and ranking of candidate ceramic wafer engine seal materials

Modern engineered ceramics offer high temperature capabilities not found in even the best superalloy metals. The high temperature properties of several selected ceramics including aluminum oxide, silicon carbide, and silicon nitride are reviewed as they apply to hypersonic engine seal design. A ranking procedure is employed to objectively differentiate among four different monolithic ceramic materials considered, including: a cold-pressed and sintered aluminum oxide; a sintered alpha-phase silicon carbide; a hot-isostatically pressed silicon nitride; and a cold-pressed and sintered silicon nitride. This procedure is used to narrow the wide range of potential ceramics considered to an acceptable number for future detailed and costly analyses and tests. The materials are numerically scored according to their high temperature flexural strength; high temperature thermal conductivity; resistance to crack growth; resistance to high heating rates; fracture toughness; Weibull modulus; and finally according to their resistance to leakage flow, where materials having coefficients of thermal expansion closely matching the engine panel material resist leakage flow best. The cold-pressed and sintered material (Kyocera SN-251) ranked the highest in the overall ranking especially when implemented in engine panels made of low expansion rate materials being considered for the engine, including Incoloy and titanium alloys.

Steinetz, Bruce M.↗