Search NASA⌕ Search

SEARCH · Search NASA

Results for “Welding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

High Strength Steel-Aluminum Components by Vaporizing Foil Actuator Welding

This project aimed to address the challenge of effectively welding dissimilar materials—high-strength steel and high-strength aluminum for creating lightweight, multi-material automotive components. For automotive companies, reducing weight of a vehicle is critical task regulated by the government to solve the issue of greenhouse gas emissions. Production of lightweight cars and trucks can be achieved by substitution of current all-steel structures with multi-material lightweight structures that include high strength-to-weight-ration materials such as high-strength steels, aluminum alloys, magnesium alloys, titanium alloys, coupled with lightweight designs. This requires dissimilar metal welding, which is challenging for state of the art joining processes such as resistance spot welding. The cycle of melting-cooling-freezing during traditional welding that can easily ruin the designed outstanding properties of the advanced base metals, such as aluminum alloys, making the welded area much weaker than the base metals. To weld two different metals with great difference in melting points, such as aluminum and steel, it’s even more difficult or impossible because of the formation of brittle intermetallic compounds at the welded interface. In this project, a novel welding method, developed at OSU, was selected for validation and development. This novel technology enables welding by impact without melting and proves to be robust to join various dissimilar lightweight metals. Termed as vaporizing foil actuator welding or VFAW, the technology uses a thin aluminum foil that is rapidly vaporized by a high current pulse to produce an explosive-like pressure pulse to drive one metallic piece into another at the high speed required for impact welding. This project entailed development of the early-stage welding technology in terms of (a) the consumables, the welding apparatus and the power sources, (b) coupon scale screening of many material combinations including corrosion studies, (c) computational modeling and design of the welded interface as well as of the multi-material prototype component, and (d) mechanical testing for strength and durability at coupon scale and to a certain extent the prototype scale. The all-steel engine cradle of 2016 Chevrolet Cruze was chosen as the baseline prototype component. The target set for the project was to demonstrate a 20% weight reduction at a cost premium of less than $\$ $5/lb saved without compromising on baseline mechanical properties. At project completion, a 12% lighter prototype component was demonstrated with an estimated cost premium of $\$ $9.8/lb saved. Besides prototype level demonstration of the technology, this project also enabled elevation of the technology’s readiness level to where a hydraulically actuated welding head was developed and made ready for deployment at a research and development facility for Tier 1 automotive supplier.

36 MATERIALS SCIENCE↗

The Toughness of High-Strength Steel Weld Metals

Low-temperature phase transformation (LTPT) welding consumables are a new class of welding wires developed to mitigate hydrogen-induced cracking in the welding of high-strength steels without preheating or postweld heat treatment. LTPT weld metals have a high strength, but their toughness needs further investigation. LTPT weld metals predominately contain a martensite microstructure, which is necessary to achieve high strength; however, martensitic weld metals containing oxide inclusions have relatively poor toughness. For this study, three welding processes — gas metal arc welding (GMAW), gas tungsten arc welding (GTAW), and hot wire GTAW — were investigated. Optical microscopy, scanning electron microscopes, and transmission electron microscopes were employed for characterization. The role of the shielding gas in the formation of oxide inclusions in LTPT weld metals was investigated. The formation of oxide inclusions in the weld metals was related to the CO 2 in the shielding gas. When 100% Ar or a pure inert shielding gas mixture was used for all three welding processes, oxide inclusions were greatly reduced, and the weld metal toughness improved considerably, matching the base metal toughness. The mechanism by which inclusions promote fracture propagation in the weld metal was proposed.

36 MATERIALS SCIENCE↗

Microstructural Evolution During a Solid State Tube Pinch Weld of Type 304l Stainless Steel

Microstructure development is examined for a specialized spot weld that is used as a solid-state closure process for austenitic stainless steel tubing, referred to as pinch welding. In order to elucidate the microstructural evolution of the weld, a series of test welds were made at nominal conditions using tubing and production like components. These pinch welds normally terminate after twelve cycles of a 60 Hz AC weld process. In this study, production tubes were welded from one to twelve cycles and the microstructure and weld variables after each individual weld cycle number were characterized using radiography and optical metallography. Two electrochemical etchants were used to highlight different microstructural features. The study revealed that: (1) this type pinch weld is largely complete after about six cycles of 60 Hz AC current, half the weld time utilized; (2) the resistance, deformation, and closure length approach “steady-state” conditions after six cycles; and (3) both oxalic and nitric acid electrolytic etchants are useful for highlighting specific microstructural attributes of type 304 L stainless steel. Finally, two distinct microstructural regions can be identified for these welds: the edge of the weld, which is driven by concentrated deformation, recrystallization, and grain growth, and the center region, which is more typical of forge welding and micro-asperity breakdown followed by diffusion and grain-growth.

36 MATERIALS SCIENCE↗

Analysis of the laser welding keyhole using inline coherent imaging

Laser beam welding is a widely used fusion welding process in many industrial applications such as automotive, aerospace, energy, defense, and medical products. Industry has a fundamental need to model the laser welding process to minimize experimental testing and improve confidence in production welds. However, computational models attempting to predict weld formation are limited by an incomplete understanding of the beam-material interactions. As a consequence, these models do not accurately predict the mechanisms associated with laser weld formation. To improve the current state of prediction capabilities, it is vital to better detect/measure the physical aspects of the weld pool during high energy density welding. In this work, a novel real-time laser weld monitoring device using inline coherent imaging (ICI) was used to provide a fundamental understanding of laser weld formation via vaporization. The objective of this work was to investigate and quantify the relationship relating laser weld parameters and the vapor capillary (keyhole) through a state-of-the-art measurement technique. Bead-on-plate laser beam welds were produced with partial penetration on 304L stainless steel, 2205 duplex stainless steel, and Ti-6Al-4V. Keyhole monitoring was performed using a commercially available ICI system to collect keyhole penetration data in real time. These measurements were reconstructed to generate the vapor capillary shape at different welding parameters. Process parameters significantly influenced the keyhole shape and the keyhole root position relative to the process beam. Finally, the keyhole geometry showed distinct differences between the stainless steel alloys and Ti-6Al-4V.

2205↗

Final Report On Non-Intrusive Load Monitoring Of Welding Processes

The conventional method of weld process monitoring is to monitor the process output electrical power close to the point of welding. Non-Intrusive Load Monitoring (NILM) describes the method of monitoring primary or utility electrical power into a welding process well away from the point of welding. The objective of this project was to determine if there is sufficient information within the welding process input power to understand process output power characteristics, and, if so, determine if there is sufficient resolution within the input electrical characteristics to infer some measures of weld quality. To understand the relationship between process input and output power, both input and output power were monitored for two welding processes (GMAW and GTAW) and two different power source types (inverter and SCR). Welds were made with and without intentional disturbances. The results showed that there is a strong correlation between input and output power and that the influence of process disturbances are evident within the input power. A simple method using input power only was devised and successfully demonstrated to discriminate between a weld made with no intentional disturbance (a nominal weld) from a weld made with an intentional disturbance (off-nominal weld). The primary conclusions of this work is that NILM of process input power is sensitive to process disturbances that could influence weld quality and that the approach warrants additional study.

36 MATERIALS SCIENCE↗

Laser spot welding of additive manufactured 304L stainless steel

Here, the goal of this work is to understand if an additively manufactured 304L stainless steel exhibits similar spot-welding behavior as wrought 304L stainless steel. Due to the many differences between an additively manufactured component and wrought product, it is important to determine how the material interacts with the laser and how it affects the weld bead morphology. In this paper, the laser coupling efficiency, weld size, and solidification of spot welds produced in wrought and additively manufactured 304L stainless steel were investigated. The coupling efficiency of wrought and additively manufactured 304L stainless steel of similar surface condition were approximately the same over a range of applied laser energies. Laser welding of the untreated (rougher) surface of additively manufactured 304L, however, showed improved coupling efficiency ranging between 3.3 and 100%. The rougher surface traps the incoming light and increases the coupling efficiency at lower laser energies, while at higher energy, the absorption efficiency is dominated by intrinsic absorption from the keyhole formation rather than surface roughness. The resulting spot weld microstructures differed from welds made in wrought 304L and additively manufactured 304L. Welds made in wrought 304L were fully austenitic containing what is suspected to be massive austenite, which suggests that these welds solidified as primary ferrite. Welds made in additively manufactured 304L were also fully austenitic and contained both cellular austenite and what is suspected to be massive austenite. These observations mean that welds made in additively manufactured 304L solidified as primary ferrite and primary austenite. The differences in weld microstructures made in wrought and AM 304L can be attributed to differences in the composition and solidification rate.

304L stainless steel↗

Understanding radiation effects in friction stir welded MA956 using ion irradiation and a rate theory model

We report an outstanding challenge in the manufacturing and joining of oxide dispersion strengthened steels is retaining the nanofeatures in the alloy throughout the fabrication and welding process. MA956 was friction stir welded with two different sets of welding parameters, resulting in a medium and high heat input. After welding, 5 MeV Fe ++ ion irradiations were performed at doses ranging from 50 to 200 dpa in the temperature range of 400 to 500°C. Post-irradiation characterization was performed with scanning transmission electron microscopy and energy-dispersive x-ray spectroscopy to investigate the Y-Al-O dispersoids, voids, and dislocations. After welding, the dispersoid microstructure coarsened, resulting in fewer and larger dispersoids regardless of heat input. After irradiation, the dispersoid behavior in the welded material was sensitive to temperature, exhibiting growth behavior attributed to Ostwald coarsening at 500 °C but a mixture of nucleation and more muted growth at 400 and 450 °C, attributed to competing mechanisms of radiation-enhanced diffusion and Ostwald coarsening. Void swelling correlated to heat input; being more prevalent in the welded conditions occurring at lower doses and in higher values relative to the base material. The low values of swelling despite microstructure coarsening caused by welding demonstrate the excellent swelling resistance of MA956, even after welding with the highest swelling values of 0.5% noted in the stir zone high heat input condition at 450 °C, 200 dpa. The dislocation behavior was inconsistent: the strongest trend was that network density was higher for welded versus base material, and an increase in loop diameter with temperature was observed. A rate theory model based on the observed microstructure suggests at high temperature interstitial loss to sinks was more likely to be dominant compared to mutual annihilation via point defect recombination, because of an increase of the radiation diffusion coefficient with temperature regardless of initial welded microstructure.

36 MATERIALS SCIENCE↗

On the quantitative characterization of weld microstructures

Here, a new technique to quantify grain shape and grain boundary curvature in the fusion zone (FZ) and the heat-effected zone (HAZ) of refractory metals and alloys has been developed. The application of this technique to quantify the effect of welding speed on these microstructural characteristics in simulated molybdenum welds is highlighted in this study. A 50% increase in weld speed more than doubles the fraction of grain segments in the fusion zone with orientations between 00 to 300 to the normal to the welding direction, with a corresponding 50% decrease in the fraction of grain segments oriented along the welding direction. This increase in weld speed also results in a reduction in grain size from approximately 120 µm to 84 µm along the WD at the FZ centerline. Grain boundary curvature is negative near the weld centerline and the edge of the fusion zone, indicating that with increasing distance from the weld centerline, the grain segments progressively rotate towards a direction normal to the welding direction at both locations. Presence of regions with relatively straight grain segments indicated by curvatures close to zero were identified in between the weld centerline and the edge of the FZ at all weld speeds.

36 MATERIALS SCIENCE↗

Welding of Haynes 282 to Steels to Enable Modular Rotors for Advanced Ultra Super-Critical Steam Turbines

Steam turbines for an Advanced Ultra Super Critical (AUSC) fossil fired power plant will operate at temperatures well above those of current commercial steam cycles with inlet temperatures more than 760 C , which is beyond the capabilities of alloy steels presently used for steam turbine applications and requires advanced materials. Large components such as steam turbine rotors may be made of nickel based super alloys such as Haynes 282 (H282). However, monolithic forgings of superalloys in the sizes required for large steam turbines rotors can be prohibitively expensive besides many technical challenges. To minimize cost and alleviate the related technical challenges, superalloy use needs to be limited to locations on the steam turbine rotor where strength and temperature requirements cannot be met by conventional steels. This is possible if nickel-based superalloys can be successfully welded to steels and the related technical challenges - machining parts made of dissimilar welded materials, non-destructive examination of such welds for flaw detection; and, material properties of such hybrid components – are sufficiently addressed. In this technology development project, we successfully welded H282 to plates up to ~ 75 mm (~ 3 inches) to a 3.5NiCrMoV steel of similar thickness. Advanced ultrasonic inspection technique called Phased Array Ultrasonic Testing (PAUT) was employed to examine the dissimilar H282-Steel welds, into which flat bottomed side drilled holes (SDH) of various diameters were introduced, to determine the minimum detectable feature sizes; it was shown that with PAUT SDH of dia. down to 0.5 mm could be detected in the base alloys and SDH with dia. down to 2.4 mm could be detected in the weld metal under multiple orientations successfully. An autonomous machining process monitoring system was developed and demonstrated whereby the forces acting on the cutting tool could be actively monitored as the cutting tool transitioned from H282 to Steel across the weld using which the machining parameters can be potentially altered without interruption to extend tool life. This project successfully achieved its objectives of - i. Developing a welding methodology and viable welding geometries, to successfully join H282 to steel 3.5CrMoNiV steel to enable manufacture of modular steam turbine rotors for AUSC applications (conditions of at least 760 °Celsius and 3,100 psia (pounds per square inch absolute pressure) and evaluate the material properties of the welded specimen. ii. Employ the advanced ultrasonic inspection technique to the dissimilar weld metal joint and determine the minimum detectable feature sizes. iii. Develop effective machining techniques to machine such hybrid structures with online tool force monitoring and effect machine state metrics for optimal results.

20 FOSSIL-FUELED POWER PLANTS↗

Study of Mechanical Properties, Microstructure, and Residual Stresses of AISI 304/304L Stainless Steel Submerged Arc Weld for Spent Fuel Dry Storage Systems

The confinement boundaries of spent nuclear fuel (SNF) canisters are typically fusion welded. Welded microstructures, strain hardening, and residual stresses combined with a chemically aggressive, chloride-rich environment led to concerns that the welded canister may be susceptible to chloride-induced stress corrosion cracking (CISCC). A comprehensive understanding of the modification of stainless steel (SS) metallurgical and mechanical properties by fusion welding could accelerate the predictive analysis of CISCC susceptibility. This paper describes a submerged arc welding (SAW) procedure that was developed and qualified on 12.7 mm (0.5 in.) thick AISI 304/304L SS to produce joints in a way similar to actual SNF canister manufacturing. This procedure has the potential to reduce the production cost and weld CISCC susceptibility by using fewer welding passes and lower heat input than current industrial applications. Global and local mechanical behaviors and properties, as well as residual stress distributions on the welded joint, were studied. The results indicate that hardness values in the fusion zone (FZ) and heat-affected zone (HAZ) are slightly higher than that of the base metal. Strain localization was presented in the HAZ before the tensile stress reached its maximum value, and then it shifted to the FZ. The specimen finally broke in the FZ. High tensile residual stresses exhibited in the FZ and the nearby HAZ suggest the highest CISCC-susceptible spots. The maximum tensile residual stresses were along the welding direction, indicating that if cracks occur, they would be perpendicular to the welding direction. This study involved developing and qualifying a SAW procedure for SNF canister production. The new procedure yielded cost savings (SAW working efficiency increased by about 80%), improved mechanical properties, and presented moderate residual stresses. Analysis revealed that the welded joint’s low-stress and high-stress damage assessments may be affected by shifts in the strain localization spot under loading.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Welding investigation of a wrought FeMnAl steel for armor application

A new wrought FeMnAl steel contains high Mn content and high Al content. This steel has high strength. When it is compared to conventional steels with the similar strength, its density is lower. FeMnAl steels can be used in armor vehicle manufacturing, in which welding is a common practice to join the steel plates together. The welding of FeMnAl steels has not been sufficiently studied before. Here, this work studied the weldability and weld microstructure of an FeMnAl steel and provided useful data for the welding practice of FeMnAl steels. The influences of weld filler metals and shielding gases were studied, using single-pass bead-on-plate gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) two processes. The optimal filler metals and shielding gases have been determined to achieve the better weldability. Autogenous GTAW and electron beam welding were also conducted. Cracks were found in the HAZ in the GMAW welds and electron beam welds. Fewer or no cracks were found in the HAZ of GTAW welds. SEM, SEM/EDX, TEM, TEM/EDX, and EBSD were used to analyze the grain boundaries in the HAZ and the cracks. The grain boundaries of FeMnAl base metal are mostly high angle grain boundaries (HAGBs), which attract impurity and solute atoms and cause intergranular cracking. The proposed cracking mechanisms are liquation cracking and ductility-dip cracking. It was found that GTAW provides much better weldability for the FeMnAl steel than GMAW and EBW.

FeMnAl steel↗

Validation Exercise of a Coarse Finite Element Model of Laser Welds

The objective of this project is to validate low-fidelity models of 304L to 304L stainless steel partial-penetration laser welds for thin sheets. Low-fidelity means that the weld is represented by coarsely meshed element blocks. Here, the hexahedral element size is approx imately half the weld penetration depth. The material behavior of the block is represented by a J2 plasticity model with a Voce hardening function. The source of the data used in this work is an extensive experimental study conducted by Sharlotte Kramer (1528) and published in 2015. Figure 1 shows a cross-section of the weld of interest. The nominal thickness of the sheets is 0.063 in. while the target penetration depth of the weld is in the range of 0.028 to 0.032 in., extending about half the sheet thickness. Uniaxial tension tests provided data for calibration of base material and weld models. Results of two validation geometries were also provided. The principal validation geometry is shown in Fig. 2. It consists of a plate specimen with in-plane dimensions 6 in × 2.875 in loaded in tension. A circular plug with a 1.5 in. diameter was cut from the center of the plate and then welded in place. The details of the welding schedule are given. An important assumption is that the welds in the calibration and validation specimens have similar geometric and material properties as those in the validation tests. The task was to first calibrate models for the base material and the welds and then simulate the validation tests until the point of weld first failure.

36 MATERIALS SCIENCE↗

Robust Dissimilar Metal Friction Welded Spool for Enhanced Capability for Steam Power Components (Final Program Report)

This project successfully demonstrated the feasibility and advantages of producing durable, friction-welded dissimilar-metal spools, both with and without transition pieces, as well as the use of advanced oxidation-protective coatings for steam power applications. The work encompassed the optimization and full-scale production of NFA tubing, overcoming manufacturing and processing challenges to achieve enhanced strength, creep, and fatigue properties validated by extensive microstructural characterization. Optimized welding techniques were developed and refined for joining dissimilar materials, resulting in defect-free welds optimized for both low- and high-pressure boiler circuits. Systematic evaluation of welding parameters, coupled with heat treatments, ensured reliable performance and minimized weld defects such as banding and cracking. Comprehensive mechanical and non-destructive testing, including tensile, bend, fatigue, and CT scanning, confirmed the superior integrity and durability of the friction-welded joints under representative service conditions. To address oxidation-related degradation, a range of protective alloy coatings—such as IN625, APMT, Duplex 2507, and FeCrAlY—were selected and evaluated for their ability to counteract oxide notch formation at dissimilar metal interfaces. These coatings demonstrated improved oxidation resistance and long-term stability under thermal cycling, thereby extending weld service life. Thermal cyclic testing and long-term studies captured the phase stability and diffusion behavior of coated and uncoated configurations. Validated models for low-cycle fatigue (LCF), creep, and thermal mechanical fatigue (TMF) were developed to predict component life and failure modes. These models confirmed that friction-welded configurations exhibited significantly enhanced performance compared to conventional gas-tungsten arc welding (GTAW), with up to 7× improvement in creep resistance and at least 2× enhancement in fatigue properties. The introduction of a tailored transition piece further reduced thermally induced strains, enhancing fatigue life. The results demonstrate a robust pathway for retrofitting existing steam fleet components and upgrading future equipment to deliver substantially improved cold-start cycling behavior and reduction of unplanned outages due to premature weld failures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Three-dimensional microstructure of a friction stir welded magnesium/steel interface characterized via high-energy synchrotron X-rays

Here, the three-dimensional (3D) microstructure of a friction stir assisted scribe technique (FaST) weld interface consisting of AZ31 magnesium (Mg) alloy and zinc (Zn)-coated DP590 steel was analyzed via synchrotron micro-computed tomography (μ-CT), correlated to synchrotron x-ray diffraction, and electron microscopy. Diffraction assessment of the AZ31/Zn-coated DP590 steel interface revealed the presence of several complex Mg–Zn intermetallic phases and differences in crystalline orientation of the Mg phase at the weld interface. The 3D characterization of the synchrotron μ-CT images of the weld interface revealed: (1) the presence of AZ31 weld nugget material with iron (Fe)-rich particles; (2) the presence of a weld layer at the joining interface with Fe-rich particles; (3) the formation of a thin non-uniform layer between the weld layer and the interface of the scribed DP590 material; and (4) the presence of an Fe–Al-rich intermetallic layer and Fe-rich particles at the interface of the scribed DP590 material. This study also performed a detailed analysis of lump-like features seen in the Zn coating layer at the weld interface. A detailed 3D particle analysis of the Fe-rich particles in the AZ31 weld nugget and the weld layer at the weld interface revealed the presence of several types of particle morphologies (i.e., spherical and irregular).

36 MATERIALS SCIENCE↗

A review of technologies for welding magnesium alloys to steels

Here we review various state-of-the-art methods for welding magnesium alloys and steels using different joint configurations. Microstructural characterizations indicate that four microstructures may form at the Mg/steel interface after welding: unwelded gap, metal oxides, solid solutions, or intermetallic compounds. Reaction products at the Mg/steel interface vary with different welding methods, alloying elements in base materials, interlayers or coatings applied, and preparations of base material before welding. Regarding mechanical property characterization, (a) lap tensile shear testing for lap-welded and spot-welded joints, (b) tensile testing for butt-welded joints and (c) fatigue properties of lap-welded and spot-welded joints are summarized and compared, separately. Reaction products at the Mg/steel interface are correlated with mechanical properties. Finally, ways to enhance Mg/steel joint strength, such as introducing interlocking features during friction stir lap and butt welding, are discussed.

Wang, Tianhao↗

Advanced Autonomous Welding for Refabrication and Follow-On Testing of Previously Irradiated Nuclear Fuel

The performance of follow-on experiments using irradiated nuclear fuel at any point in its lifecycle is a critical step in understanding phenomena and behavior. Transient experiments with high-burnup fuel can deepen the understanding of fuel fragmentation, relocations, and dispersal under loss-of-coolant accidents. An advanced autonomous welding process to refabricate commercial fuel rods inside a hot cell was created and tested to enable flexible experiment approaches on fuels irradiated in commercial and test reactors. Irradiated light water reactor fuel test pins from experiments performed at the Advanced Test Reactor (ATR) at Idaho National Laboratory were used to demonstrate the refabrication process. The welding process was found to be sensitive to welding parameters but flexible such that multiple passes could be performed on the same location until a hermetic weld was obtained. The refabrication of rodlets and successful welds was also found to be sensitive to the preparation of the irradiated cladding and endcaps. Thorough defueling of the fuel at the weld location and proper sizing of the endcaps and backing material mitigated these issues. The use of strategically located heat sinks in contact with the cladding and endcap materials also increased welding and refabrication success. For this work, the test pins were sectioned to remove the original endcaps and fuel was removed from both ends of each rodlet. The reassembly of the rodlets was then completed in four steps, which included the press fitting of new endcaps, the circumferential welding of rodlet endcaps to the cladding, rodlet pressurization in a pressure chamber, and seal welding the rodlet under pressure. The integrity of the refabricated rodlets was then verified via helium leak checking inside a vacuum chamber. The advanced welding system is capable of refabricating rodlets up to 380 mm in length, and repressurizing them up to 15 500 kPa. The refabricated lengths of the rodlets used in this work ranged from 149 to 165 mm and the refabricated fuel stack heights ranged from 70.4 to 79.8 mm. Here, the rodlets were pressurized with argon to an average pressure of 3617 kPa, and the average leak rate after refabrication was 6.7 • 10 -8 cm 3 • s -1 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Hierarchical Multi-scale Modeling of Laser Weld Failure: An Initial Investigation

The failure of 304L laser welds is of interest to system and component designers due to nuclear safety requirements for abnormal environments. Accurately modeling laser weld behavior in full system and component models has proven especially challenging due to three factors: the large variability observed in laser weld characterization tests; the difficulty in isolating the weld material for material characterization and modeling the weld material behavior; and the disparate scales associated with modeling laser welds in large systems. Recent work has shown that meso-scale geometric features of laser welds such as pores and weld root tortuosity are critical to accurately predicting the structural performance of welds. The challenge with modeling these welds is that the geometric features driving their structural performance are generally on the order of ten to hundreds of microns, but can affect the responses of interest in systems and components on the order of centimeters to meters.

36 MATERIALS SCIENCE↗

Metallurgical Analysis and Forward Modeling of Weld Distortion in SMR Containment Vessels

This work aimed to apply Sandia’s expertise in metallurgy and modeling to enable the use of hybrid laser arc welding for building nuclear reactor containment structures, via a collaboration with Holtec International. Experimental observations were coupled with finite element analysis to resolve microstructure development, mechanical properties, distortion, and residual stress in welds relevant to the production of the Holtec SMR-160. High residual stresses were observed in welds that were not subjected to preheat. Meanwhile, the microstructure of the welds generally exhibited a narrow heat affected zone relative to conventional arc welds. FEA appeared to be effective in simulating the thermal/mechanical conditions that occur during hybrid laser arc welding of simplified and instrumented test welds. Subsequently, FEA was used to perform sensitivity analyses for various weld geometries that would be prohibitively costly to assess with physical experiments. Insights from the study were used to inform Holtec’s welding process, and successful production welds were performed in 2025.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗