Structure property correlations in wet-spun textile PAN fibers for cost-effective carbon fibers applicable in H 2 storage tank manufacturing

The economic viability of high-strength carbon fibers is pivotal for their integration into Type IV compressed hydrogen storage tanks. Oak Ridge National Laboratory is advancing this objective by developing cost-effective, textile-grade polyacrylonitrile (PAN) precursor fibers through an optimized wet spinning-process to garner more microstructural control over the precursor fibers. Here, this study examines the microstructural characteristics of PAN fibers, particularly the crystalline orientation factor, and their impact on mechanical properties in both precursor and thermally converted carbon fibers (CFs). Three wet-spun PAN fibers, all having diameters of 12-13 µm but varying orientation factors were assessed. Comprehensive characterization using X-ray scattering and microscopy revealed that fibers with higher orientation factors exhibited enhanced crystallinity and optimized crystallite sizes. Mechanical testing demonstrated that the PAN fiber with the highest orientation factor achieved the greatest tensile strength (98 ksi) and modulus (1.60 Msi). Additionally optical and scanning electron microscopy confirmed smooth and defect-free surfaces across all samples. These findings indicate that manipulating spinning parameters to maximize orientation factor is more impactful in achieving high strength and modulus over factors attributed to crystallinity and crystallite sizes. Here, highest performing CFs, thermally processed in lab from textile-grade precursor averaged 558 ksi, a 10% increase over previous results.

36 MATERIALS SCIENCE↗

Effects of fiber, matrix, and interphase on carbon fiber composite compression strength

The major goal of this project was to obtain basic information on compression failure properties of carbon fiber composites. To do this, we investigated fiber effects, matrix effects, and fiber/matrix interface effects. Using each of nine fiber types, we prepared embedded single-fiber specimens, single-ply specimens, and full laminates. From the single-fiber specimens, in addition to the standard fragmentation test analysis, we were able to use the low crack density data to provide information about the distribution of fiber flaws. The single-ply specimens provided evidence of a correlation between the size of kink band zones and the quality of the interface. Results of the laminate compression experiments mostly agreed with the results from single-ply experiments, although the ultimate compression strengths of laminates were higher. Generally, these experiments showed a strong effect of interfacial properties. Matrix effects were examined using laminates subjected to precracking under mixed-mode loading conditions. A large effect of precracking conditions on the mode 1 toughness of the laminates was found. In order to control the properties of the fiber/matrix interface, we prepared composites of carbon fiber and polycarbonate and subjected these to annealing. The changes in interfacial properties directly correlated with changes in compression strength.

Nairn, John A.↗

Effects of Debulking on the Fiber Microstructure and Void Distribution in Carbon Fiber Reinforced Plastics

Carbon Fiber Reinforced Plastics (CFRPs) are widely used due to their high stiffness to weight ratios. A common process manufacturers use to increase the strength to weight ratio is debulking. Debulking is the process of compacting a dry fibrous reinforcement prior to resin infusion. This process is meant to decrease the average inter-fiber distance, effectively increasing the fiber volume fraction of the sample. While this process is widely understood macroscopically its effects on fibrous microstructures have not yet been well characterized. The aim of this work is to compare the microstructures of three CFRP laminates, varying only the debulking step in the manufacturing process. High resolution serial sections of all three laminates were taken for analysis. Using these scans, the fiber positions were reconstructed. Statistical descriptors such as local fiber and void volume fractions, fiber orientation, and void distribution and morphology were then generated for each sample. Fiber clusters present within the material were identified and analyzed for each level of debulking applied. Using these descriptors, the effects of debulking on the morphology and organization of the composite microstructure was evaluated.

carbon fiber↗

Developing a New Polyolefin Precursor for Low-Cost, High-Strength Carbon Fiber

Current high-strength carbon fibers (CFs) are mostly derived from PAN polymer precursor, which are very expensive with limited usage in the high-end products. On the other hand, it has also stimulated research interest to develop new low-cost precursors and manufacturing process. Despite numerous studies, researchers have yet to develop a new polymeric precursor that is less expensive, melt-spinnable, and offers a high C-yield. In this three-year R&D project, we proposed three consecutive research phases, including (i) the development of new polyolefin-based precursors that can be thermally transformed to C material in one heating step under inert atmosphere and achieved a C-yield >80%, which is more than 60% higher than that of current PAN precursor, (ii) With the suitable new polyolefin-based precursor, we can focus on CF manufacturing process, including fiber spinning, stabilization, and carbonization, to form high quality carbon fibers with the desirable polymorphous morphology, and (iii) the investigation of thermal conversion process under tension for converting polyolefin-based precursor fibers to high tensile strength carbon fibers with specific graphite crystallite size, orientation of basal line, order-disorder ratio, fiber diameter, and reduced structural defect (voids). composites.

08 HYDROGEN↗

Electroplated Polymer‐Modified Carbon Fiber for Performance‐Enhancing Composite Interfaces

Carbon fiber composite performance relies on the fiber-matrix interface for effective load transfer. To enhance interfacial properties between the fiber and matrix, often carbon fiber surfaces are oxidatively and covalently modified to incorporate chemical functional groups. By contrast, here, noncovalent electrodeposition of functional polyelectrolyte is applied onto conducting carbon fibers from aqueous solutions. A natural polymer, chitosan (CS), is electro-deposited onto the fiber surface, which undergoes multi-scale physical interactions. The bound CS layer with abundant amine functionalities reacts with epoxy moieties within the matrix to improve the interfacial properties. The scalable and energy-efficient electrodeposition eliminates traditional functionalization and sizing requirements of carbon fiber while delivering significantly higher mechanical performance with enhanced consistency. For continuous fiber reinforced composites, compared to conventional fibers, apparent interlaminar shear strength increases by 27%, reaching ≈86 MPa. The short fiber composites with only 2–11 wt.% fibers exhibit ≈20% increase in tensile strength with a peak performance of 120 MPa. Unlike traditionally treated and sized carbon fiber, this approach delivers coated fibers with long shelf-life and allows recovery of both CS in electrolyte form and carbon fiber by continuous electrochemical processing of the modified fibers with inverse polarity; thus, it promotes overall fiber recyclability.

36 MATERIALS SCIENCE↗

Early development of multifilament polyacrylonitrile-derived structural hollow carbon fibers from a segmented arc spinneret

Carbon fiber is a highly desired material for structural applications requiring high strength and stiffness and low weight but has seen only incremental improvements in properties over the last few decades. Further increases in carbon fiber specific properties, including specific strength and specific modulus, would further propel its unique capabilities. One method to produce high specific property carbon fibers for structural applications is the development of hollow carbon fibers. In this work, we report on the early development of polyacrylonitrile-derived structural hollow carbon fibers. Here, multifilament, continuous tow, polyacrylonitrile-based precursor hollow fibers were successfully produced utilizing a segmented arc spinneret approach. When batch oxidized, the hollow precursor fibers demonstrated evidence of oxidation proceeding from both the interior and exterior of the filament. Further results suggested that reducing the precursor hollow fiber wall thickness would allow for complete, homogeneous oxidation, thereby avoiding the skin-core structure often observed in commercial carbon fiber. Here, hollow carbon fibers were as small as 35 µm outer diameter, 22 µm inner diameter (6.5 µm wall thickness). At these diameters, the hollow carbon effective fiber specific strength was 0.54 N/tex and the effective specific modulus was 120 N/tex, approaching the effective specific modulus of T700S at 136 N/tex.

36 MATERIALS SCIENCE↗

Heat Treated Carbon Fiber Material Selection Database

Carbon fibers are used in a variety high temperature applications and materials. However, one limiting factor in their transition into additional applications is an understanding of their functional properties during component processing and function. The requirements on the fibers are governed by the nature of the materials and the environments in which they will be used. The current carbon fiber vendor literature is geared toward the polymeric composite industry and not the ceramic composite industry. Thus, selection of carbon fibers is difficult, since their properties change as a function of heat treatment, processing or component operational temperature, which ever is greatest. To enable proper decisions to be made, a program was established wherein multiple fibers were selected and heat treated at different temperatures. The fibers were then examined for their physical and mechanical properties which are reported herein.

Effinger, M.↗

Insights into the thermal history of carbon fibers using Raman spectroscopy and a novel kinetic model

Carbon fibers and carbon fiber composites are applied in high-performance applications, but a key consideration for application is their relative sensitivity to oxidative environments. To enable in-situ characterization of carbon fibers exposed to oxidative conditions, the Raman spectral response of T700 carbon fibers that have been exposed to a variety of dwell temperatures is reported herein with dwell times reaching up to 1 month. Here, we evaluate the spectra holistically by using integrated absolute difference analysis. By combining this analysis with straightforward kinetic models, we connect the total Raman spectral response to the temperature-time curve that could yield such a shift in spectral parameters. Our work connects the Raman spectral response of carbon fibers to their thermal history and can easily be extended to other graphitic materials, such as nuclear graphite.

36 MATERIALS SCIENCE↗

Low Cost, High Volume, Carbon Fiber Precursor for Plasma Oxidation

Light weighting with carbon fiber is critical to improving the energy efficiency of wind turbines, airplanes, and automobiles, but the high cost of carbon fiber continues to limit market growth and applications. Half of this cost is in the raw materials. For the carbon fiber market to reach the next level of adoption, the cost of both the raw materials and conversion must be reduced. This project considered the combination of low-cost, textile-grade precursors combined with the increased efficiency of plasma oxidation to greatly reduce the cost of carbon fiber. The primary objective of this project was to make industrial-grade carbon fiber (550 ksi tensile strength, 35 Msi tensile modulus) from textile-grade PAN precursors, something that cannot be achieved with conventional oxidation and to date has not been achieved with any technology. To accomplish this, the project team iteratively optimized the process conditions in the plasma oxidation and carbonization stages to maximize the tensile properties of the resultant carbon fibers. This involved implementing experimental designs for both stages, whereby process conditions (e.g. temperature) were varied and correlated to fiber properties. Samples of oxidized PAN fibers (OPFs) were prepared using a small pilot-scale plasma oxidation oven at 4XTechnologies (4XT). The thermal, chemical, and physical properties of OPF samples were analyzed by the University of Tennessee (UTK) and Oak Ridge National Laboratory (ORNL). The OPF samples were then converted to carbon fiber by subsequent low- and high-temperature carbonization using a lab-scale furnace at ORNL. The resultant carbon fibers were tested for tensile strength also at ORNL, and the results were fed back into the experimental design. Of the hundreds of carbon fiber samples produced over the course of the project, the best sample had an average break strength of 479 ksi and modulus of 33 Msi. While the best tensile properties achieved fell short of the final project targets of 550 ksi for break strength and 35 Msi for modulus, the team demonstrated the potential to produce industrial-grade carbon fiber using textile-grade precursors. The best performing fiber samples had tensile properties that are 87% of the goal for tensile strength and 94% of the goal for tensile modulus. With additional optimization work, it is likely that the targets could be achieved, since only a fraction of the process parameter space was explored during this project. 4XT and its affiliate (4M) have already secured funding through private equity, and there is a CRADA (Cooperative Research and Development Agreement) project currently underway with the Carbon Fiber Technology Center (CFTF) at ORNL to continue this research. Additionally, while not an original goal of the project, the carbon fibers for most samples had diameters >8.5μm. This is considerably larger than commercially available carbon fiber products, which can impart unique properties to the composites (e.g. increased compressive strength) and decrease manufacturing costs even further. Moreover, these fibers were oxidized with plasma oxidation using residence times ranging <60mins, which would be considered fast for normal diameter fibers, but it is as much as 5x faster when factoring in the diameter of the fibers.

36 MATERIALS SCIENCE↗

Carbon fiber classification using raman spectroscopy

Carbon fiber characterization processes are described that include multi-condition Raman spectroscopy-based examination combined with multivariate data analyses. Methods are a nondestructive material characterization approach that can provide predictions as to carbon fiber bulk physical properties, as well as identification of unknown carbon fiber materials for quality control purposes. The framework of the multivariate analysis methods includes a principal component-based identification protocol including comparison of Raman spectral data from an unknown carbon fiber with a data library of multiple principal component spaces.

Houk, Amanda L.↗

Precursor Processing Development for Low Cost, High Strength Carbon Fiber for Composite Overwrapped Pressure Vessel Applications

Carbon fiber (CF) is central to produce lightweight, high pressure, composite overwrapped pressure vessels (COPVs), which are used for on-board storage of hydrogen for fuel cell vehicles. In 2015, carbon fiber cost accounted for 62% of the cost of a hydrogen storage system, as COPVs were manufactured with T700S CF at $\$ $29.40/kg CF. The high cost of hydrogen storage, largely attributed to the carbon fiber cost, limits the application of fuel cells in vehicles. Therefore, our team endeavored to develop fiber processing to demonstrate carbon fiber tensile properties similar to T700S with a production cost potential of $\$ $12.60/kg or less. Here, the overarching goal of the project was the development of low cost, high strength carbon fiber for composite overwrapped pressure vessels. Within the project, our team investigated a new low-cost, high-volume, high quality polyacrylonitrile (PAN)-based precursor terpolymer for the production of carbon fiber precursors, methods for increasing water and energy use efficiency in wash-water/solvent separation, and ultimately developed a multifilament spinning and conversion process for the production of hollow carbon fibers from a segmented arc spinneret utilizing a solution spinning method.

08 HYDROGEN↗

Large-scale carbon fiber tests

A realistic release of carbon fibers was established by burning a minimum of 45 kg of carbon fiber composite aircraft structural components in each of five large scale, outdoor aviation jet fuel fire tests. This release was quantified by several independent assessments with various instruments developed specifically for these tests. The most likely values for the mass of single carbon fibers released ranged from 0.2 percent of the initial mass of carbon fiber for the source tests (zero wind velocity) to a maximum of 0.6 percent of the initial carbon fiber mass for dissemination tests (5 to 6 m/s wind velocity). Mean fiber lengths for fibers greater than 1 mm in length ranged from 2.5 to 3.5 mm. Mean diameters ranged from 3.6 to 5.3 micrometers which was indicative of significant oxidation. Footprints of downwind dissemination of the fire released fibers were measured to 19.1 km from the fire.

Pride, R. A.↗

Filament Formation and Melt Spinning of Coal-Based Mesophase Pitch for Carbon Fiber Production

High-performance carbon fibers excel as high specific strength and modulus materials, and are utilized in composites applications ranging across aerospace, automotive, energy, infrastructure, and sports equipment sectors. Compared to PAN-based carbon fiber, mesophase pitch-based carbon fiber has lower tensile strength but provides a higher modulus, higher thermal conductivity, and a lower cost potential. However, challenges in stable, continuous melt spinning processing are a serious limiting factor. Unlike typical melt spinning of long, linear chain polymers, mesophase pitch is a comprised of relatively shorter polycyclic aromatic hydrocarbons which form a liquid crystal. In its ‘green’ or ‘as-spun’ state, the fibers are very fragile. Moreover, its temperature of processing is quite high, often approaching 400ºC. Complex flow dynamics combined with short length and time scale heat transfer render its melt spinning a formidable processing challenge. Improved understanding of the root causes for nascent filament breakage and spinning instabilities are needed. This work aims to determine fundamental phenomena that govern mesophase pitch filament formation by comparison of required draw force and uninterrupted spinning minutes with applied draw down ratio. The effect of perturbations on spinning stability are analyzed using capillary rheometry, microscopy of elongating filaments, and filtration.

01 COAL, LIGNITE, AND PEAT↗