At least 55 records · Page 3

Passive Mitigation of Cascading Propagation in Multi-Cell Lithium Ion Batteries

The heat generated during a single cell failure within a high energy battery system can force adjacent cells into thermal runaway, creating a cascading propagation effect through the entire system. This work examines the response of modules of stacked pouch cells after thermal runaway is induced in a single cell. The prevention of cascading propagation is explored on cells with reduced states of charge and stacks with metal plates between cells. Reduced states of charge and metal plates both reduce the energy stored relative to the heat capacity, and the results show how cascading propagation may be slowed and mitigated as this varies. These propagation limits are correlated with the stored energy density. Results show significant delays between thermal runaway in adjacent cells, which are analyzed to determine intercell contact resistances and to assess how much heat energy is transmitted to cells before they undergo thermal runaway. A propagating failure of even a small pack may stretch over several minutes including delays as each cell is heated to the point of thermal runaway. This delay is described with two new parameters in the form of gap-crossing and cell-crossing time to grade the propensity of propagation from cell to cell.

25 ENERGY STORAGE↗

Chemical Evolution in Silicon–Graphite Composite Anodes Investigated by Vibrational Spectroscopy

Silicon–graphite composites are under development for the next generation of high-capacity lithium-ion anodes, and vibrational spectroscopy is a powerful tool to identify the different mechanisms that contribute to performance loss. With alloy anodes, the underlying causes of cell failure are significantly different in half-cells with lithium metal counter electrodes compared to full cells with standard cathodes. However, most studies which take advantage of vibrational spectroscopy have only examined half-cells. In this work, a combination of FTIR and Raman spectroscopy describes several factors that lead to degradation in full pouch cells with LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) cathodes. The spectroscopic signatures evolve after longer term cycling compared to the initial formation cycles. Several side-reactions that consume lithium ions have clear FTIR signatures, and comparison to a library of reference compounds facilitates identification. Raman microspectroscopy combined with mapping shows that the composite anodes are not homogeneous but segregate into graphite-rich and silicon-rich phases. Lithiation does not proceed uniformly either. A basis analysis of Raman maps identifies electrochemically inactive regions of the anodes. In conclusion, the spectroscopic results presented here emphasize the importance of improving electrode processing and SEI stability to enable practical composite anodes with high silicon loadings.

25 ENERGY STORAGE↗

Performance storage, safety and disposal of Li/SO2 cells

Cell performance characteristics after storage at room temperature and 71 C as well as some cell failure modes are evaluated. The performance of cells at low temperatures (-30 C) even into voltage reversal is also considered. The correlation of Li/SO2 coulombic ratio with generated free cyanide (CN-) in forced discharged D cells is also included.

Dimasi, G. J.↗

Material Failure Mechanisms of Alkaline Zn Rechargeable Conversion Electrodes

Zinc (Zn) alkaline electrodes hold great importance and promise in the battery technology community, yet their behavior in real-world applications is still poorly understood. Here, we report a study of failure mechanisms and material evolution during cycling of 27 zinc–manganese dioxide (Zn–MnO 2 ) cells wherein the percent utilization of the Zn electroactive material is systematically varied between 1 and 16%. Cell fabrication is kept typical of the prevailing industrial cell design. The cycle life ranges from 2800 to 60, depending inversely on the Zn utilization. In all cases, the Zn material microstructure sheds the polytetrafluoroethylene (PTFE) binder and forms zinc oxide (ZnO) rods, with longer rods formed by lower current per Zn mass. Irreversible side reactions such as the hydrogen evolution reaction (HER), short circuits, or gas crossover cause the Zn anode’s charging efficiency to average 92% (as low as 86%), which in turn causes the baseload of metallic Zn to gradually disappear. Cell failure occurs after the baseload of metallic Zn is exhausted. The total lifetime discharge capacity remains constant near 12 ± 5 Ah/g Zn invariant of Zn utilization, which suggests that the aforementioned processes of Zn microstructural evolution and side-reaction destruction of baseload metallic zinc both progress linearly with cell capacity throughput. Manual reproduction of individual Zn failure mechanisms is performed in 22 fresh cells. Tight packing of the microstructure can lead to poor mass transfer, which causes supersaturation of soluble Zn and finally produces a high overvoltage during discharge. Here, the low charging current density yields poor coulombic efficiency due either to the competitive HER or soft short circuits.

25 ENERGY STORAGE↗

Parrallel Connections Would Improve Array Reliability

Hexagonnally-close-packed round solar cells are interconnected in series strings. Parallel contacts between cells at equipotential in adjacent series strings insure redundant current paths to relieve adverse effects of cell failures and mismatches. Parallel connections carry no current if cells are matched and functioning normally. If cell fails, tabs carry current to bypass inoperative cell.

Crouthamel, M. S.↗

TERRA Battery Thermal Control Anomaly - Simulation and Corrective Actions

The TERRA spacecraft was launched in December 1999 from Vandenberg Air Force Base, becoming the flagship of NASA's Earth Observing System program to gather data on how the planet's processes create climate. Originally planned as a 5 year mission, it still provides valuable science data after nearly 10 years on orbit. On October 13th, 2009 at 16:23z following a routine inclination maneuver, TERRA experienced a battery cell failure and a simultaneous failure of several battery heater control circuits used to maintain cell temperatures and gradients within the battery. With several cells nearing the minimum survival temperature, preventing the electrolyte from freezing was the first priority. After several reset attempts and power cycling of the control electronics failed to reestablish control authority on the primary side of the controller, it was switched to the redundant side, but anomalous performance again prevented full heater control of the battery cells. As the investigation into the cause of the anomaly and corrective action continued, a battery thermal model was developed to be used in determining the control ability remaining and to simulate and assess corrective actions. Although no thermal model or detailed reference data of the battery was available, sufficient information was found to allow a simplified model to be constructed, correlated against pre-anomaly telemetry, and used to simulate the thermal behavior at several points after the anomaly. It was then used to simulate subsequent corrective actions to assess their impact on cell temperatures. This paper describes the rapid development of this thermal model, including correlation to flight data before and after the anomaly., along with a comparative assessment of the analysis results used to interpret the telemetry to determine the extent of damage to the thermal control hardware, with near-term corrective actions and long-term operations plan to overcome the anomaly.

Grob, Eric W.↗

Failure Mechanism of Fast-Charged Lithium Metal Batteries in Liquid Electrolyte

In recent years, lithium anode has re-attracted broad interest because of the necessity of employing lithium metal in the next-generation battery technologies such as lithium sulfur (Li-S) and lithium oxygen (Li-O2) batteries. Fast capacity degradation and safety issue associated with rechargeable lithium metal batteries have been reported, although the fundamental understanding on the failure mechanism of lithium metal at high charge rate is still under debate due to the complicated interfacial chemistry between lithium metal and electrolyte. Herein, we demonstrate that, at high current density, the quick growth of porous solid electrolyte interphase towards bulk lithium, instead of towards the separator, dramatically builds up the cell impedance that directly leads to the cell failure. Understanding the lithium metal failure mechanism is very critical to gauge the various approaches used to address the stability and safety issues associated with lithium metal anode. Otherwise, all cells will fail quickly at high rates before the observation of any positive effects that might be brought from adopting the new strategies to protect lithium.

Environmental Molecular Sciences Laboratory↗

NiCd battery reliability for shuttle serviced spacecraft

Data from life-cycle testing of 22-cell NiCd batteries designed for shuttle-service spacecrafts are analyzed, first by averaging battery cycle lives as a function of temperature and depth of discharge, and then by calculating single cell failure and survival probabilities as a function of temperature, depth of discharge, and number of operating cycles. The single cell data are used to calculate battery survival probabilities. A mathematical failure model which is a function of the quantity of charge through the battery and the temperature is characterized, suggesting a predictive capability for accurate estimation of energy storage subsystem life and performance of accelerated tests. The failure mechanism described is apparently independent of most charge-discharge parameters and common to most cell sizes.

Eliason, J.↗

A life prediction methodology for encapsulated solar cells

This paper presents an approach to the development of a life prediction methodology for encapsulated solar cells which are intended to operate for twenty years or more in a terrestrial environment. Such a methodology, or solar cell life prediction model, requires the development of quantitative intermediate relationships between local environmental stress parameters and the basic chemical mechanisms of encapsulant aging leading to solar cell failures. The use of accelerated/abbreviated testing to develop these intermediate relationships and in revealing failure modes is discussed. Current field and demonstration tests of solar cell arrays and the present laboratory tests to qualify solar module designs provide very little data applicable to predicting the long-term performance of encapsulated solar cells. An approach to enhancing the value of such field tests to provide data for life prediction is described.

Coulbert, C. D.↗

Effect of LEO cycling on 125 Ah advanced design IPV nickel-hydrogen flight cells. An update

Validation testing of the NASA Lewis 125 Ah advanced design individual pressure vessel (IPV) nickel-hydrogen flight cells was conducted. Work consisted of characterization, storage, and cycle life testing. There was no capacity degradation after 52 days of storage with the cells in the discharged state, an open circuit, 0 C, and a hydrogen pressure of 14.5 psia. The catalyzed wall wick cells were cycled for over 11,000 cycles with no cell failures in the continuing test. One of the noncatalyzed wall wick cells failed.

Smithrick, John J.↗

Validation test of 125 Ah advanced design IPV nickel-hydrogen flight cells

An update of validation test results confirming the advanced design nickel-hydrogen cell is presented. An advanced 125 Ah individual pressure vessel (IPV) nickel-hydrogen cell was designed. The primary function of the advanced cell is to store and deliver energy for long-term, Low-Earth-Orbit (LEO) spacecraft missions. The new features of this design, which are not incorporated in state-of-the-art design cells, are: (1) use of 26 percent rather than 31 percent potassium hydroxide (KOH) electrolyte; (2) use of a patented catalyzed wall wick; (3) use of serrated-edge separators to facilitate gaseous oxygen and hydrogen flow within the cell, while still maintaining physical contact with the wall wick for electrolyte management; and (4) use of a floating rather than a fixed stack (state-of-the-art) to accommodate nickel electrode expansion due to charge/discharge cycling. The significant improvements resulting from these innovations are extended cycle life; enhanced thermal, electrolyte, and oxygen management; and accommodation of nickel electrode expansion. Six 125 Ah flight cells based on this design were fabricated by Eagle-Picher. Three of the cells contain all of the advanced features (test cells) and three are the same as the test cells except they do not have catalyst on the wall wick (control cells). All six cells are in the process of being evaluated in a LEO cycle life test at the Naval Weapons Support Center, Crane, IN, under a NASA Lewis Research Center contract. The catalyzed wall wick cells have been cycled for over 19000 cycles with no cell failures in the continuing test. Two of the noncatalyzed wall wick cells failed (cycles 9588 and 13,900).

Smithrick, John J.↗

Validation test of 125 Ah advanced design IPV nickel-hydrogen flight cells

An update of validation test results confirming the advanced design nickel-hydrogen cell is presented. An advanced 125 Ah individual pressure vessel Ni-H cell was designed. The primary function of the advanced cell is to store and deliver energy for long-term LEO spacecraft missions. The new features of this design are: (1) use of 26 percent rather than 31 percent KOH electrolyte; (2) use of a patented catalyzed wall wick; (3) use of serrated-edge separators to facilitate gaseous O and H flow within the cell, while maintaining physical contact with the wall wick for electrolyte management; and (4) use of a floating rather than a fixed stack to accommodate Ni electrode expansion due to charge/discharge cycling. The significant improvements resulting from these innovations are extended cycle life; enhanced thermal, electrolyte, and oxygen management; and accommodation of Ni electrode expansion. Six 125 Ah flight cells based on this design were fabricated; the catalyzed wall wick cells have been cycled for over 19,000 cycles with no cell failures in the continuing test. Two of the noncatalyzed wall wick cells failed (cycles 9588 and 13,900).

Smithrick, John J.↗

Effect of Coal Contaminants on Solid Oxide Fuel System Performance and Service Life

The U.S. Department of Energy’s SECA program envisions the development of high-efficiency, low-emission, CO 2 sequestration-ready, and fuel-flexible technology to produce electricity from fossil fuels. One such technology is the integrated gasification-solid oxide fuel cell (SOFC) that produces electricity from the gas stream of a coal gasifier. SOFCs have high fuel-to-electricity conversion efficiency, environmental compatibility (low NO x production), and modularity. The primary objective of the Phase I study was to determine the sensitivity of the performance of solid oxide fuel cells to trace level contaminants present in a coal-derived gas stream in the temperature range 700° to 900°C. Laboratory-scale tests were performed with 1-inch diameter solid oxide fuel cells procured from InDec B.V., Netherlands. These cells produce 0.15, 0.27, and 0.35 W/cm 2 at 700°, 750°, and 800°C, respectively, in a H 2 anode feed and are expected to be stable within 10% of the original performance over a period of 2000 h. A simulated coal-derived gas containing 30.0% CO, 30.6% H2 11.8% CO2, 27.6% H 2 O was used at a rate of ~100 standard cm 3 /min to determine the effect of contaminants on the electrical performance of the cells. Alumina or zirconia components were used for the gas manifold to prevent loss of contaminants by reaction with the surfaces of the gas manifold Short-term accelerated tests were conducted with several contaminants including As, P, CH 3 Cl, HCl, Hg, Sb, and Zn vapors. In these tests, AsH 3 , PH 3 , Cd vapor and CH 3 Cl identified as the potential contaminants that can affect the electrical performance of SOFCs. The effect of some of these contaminants varied with the operating temperature. Cell failure due to contact break inside the anode chamber occurred when the cell was exposed to 10 ppm arsenic vapor at 800°C. The electrical performance of SOFC samples suffered less than 1% in when exposed to contaminants such as HCl(g), Hg(g), and Zn(g), and SbO(g) at levels of 8 ppm and above. AsH 3 vapor at 0.5 ppm did not affect the electrical performance of an SOFC sample even after 1000 h at 750°C. In Phase II of the program, long-term tests will be performed with multiple contaminants at a temperature range of 750° to 850°C. These tests will be at contaminant levels typical of coal-derived gas streams that have undergone gas cleanup using Selexol technology. The chemical nature of the contaminant species will be identified at the operating temperature of SOFC and compare them with thermodynamic equilibrium calculations. The results of the testing will be used to recommend the sensitivity limits for SOFC operation and to assess the reduction in the service life of the SOFC for trace level contaminants.

20 FOSSIL-FUELED POWER PLANTS↗

Identifying the Cause of Rupture of Li-Ion Batteries during Thermal Runaway

As the energy density of lithium-ion cells and batteries increases, controlling the outcomes of thermal runaway becomes more challenging. If the high rate of gas generation during thermal runaway is not adequately vented, commercial cell designs can rupture and explode, presenting serious safety concerns. Here, ultra-high-speed synchrotron X-ray imaging is used at >20 000 frames per second to characterize the venting processes of six different 18650 cell designs undergoing thermal runaway. For the first time, the mechanisms that lead to the most catastrophic type of cell failure, rupture, and explosion are identified and elucidated in detail. The practical application of the technique is highlighted by evaluating a novel 18650 cell design with a second vent at the base, which is shown to avoid the critical stages that lead to rupture. The insights yielded in this study shed new light on battery failure and are expected to guide the development of safer commercial cell designs.

25 ENERGY STORAGE↗

Cycling of block copolymer composites with lithium-conducting ceramic nanoparticles

Solid polymer and perovskite-type ceramic electrolytes have both shown promise in advancing solid-state lithium metal batteries. Despite their favorable interfacial stability against lithium metal, polymer electrolytes face issues due to their low ionic conductivity and poor mechanical strength. Highly conductive and mechanically robust ceramics, on the other hand, cannot physically remain in contact with redox-active particles that expand and contract during charge-discharge cycles unless excessive pressures are used. To overcome the disadvantages of each material, polymer-ceramic composites can be formed; however, depletion interactions will always lead to aggregation of the ceramic particles if a homopolymer above its melting temperature is used. In this study, we incorporate Li 0.33 La 0.56 TiO 3 (LLTO) nanoparticles into a block copolymer, polystyrene- b -poly (ethylene oxide) (SEO), to develop a polymer-composite electrolyte (SEO-LLTO). TEMs of the same nanoparticles in polyethylene oxide (PEO) show highly aggregated particles whereas a significant fraction of the nanoparticles are dispersed within the PEO-rich lamellae of the SEO-LLTO electrolyte. We use synchrotron hard x-ray microtomography to study the cell failure and interfacial stability of SEO-LLTO in cycled lithium-lithium symmetric cells. Three-dimensional tomograms reveal the formation of large globular lithium structures in the vicinity of the LLTO aggregates. Encasing the SEO-LLTO between layers of SEO to form a “sandwich” electrolyte, we prevent direct contact of LLTO with lithium metal, which allows for the passage of seven-fold higher current densities without signatures of lithium deposition around LLTO. We posit that eliminating particle clustering and direct contact of LLTO and lithium metal through dry processing techniques is crucial to enabling composite electrolytes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical degradation of amorphous-silicon photovoltaic modules

Techniques of module electrochemical corrosion research, developed during reliability studies of crystalline-silicon modules (C-Si), have been applied to this new investigation into amorphous-silicon (a-Si) module reliability. Amorphous-Si cells, encapsulated in the polymers polyvinyl butyral (PVB) and ethylene vinyl acetate (EVA), were exposed for more than 1200 hours in a controlled 85 C/85 percent RH environment, with a constant 500 volts applied between the cells and an aluminum frame. Plotting power output reduction versus charge transferred reveals that about 50 percent a-Si cell failures can be expected with the passage of 0.1 to 1.0 Coulomb/cm of cell-frame edge length; this threshold is somewhat less than that determined for C-Si modules.

Mon, G. R.↗

Preliminary results: Root cause investigation of orbital anomalies and failures in NASA standard 50 ampere-hour nickel-cadmium batteries

Two lots of NASA standard 50 A.H. Ni-Cd battery cells, manufactured by Gates Aerospace Batteries and built into batteries by McDonnell Douglas, have experienced significant performance problems. The two lots were used on the Compton Gamma Ray Observatory and the Upper Atmosphere Research Satellite. Both of these satellites are Low Earth Orbital (LEO) satellites containing batteries on a parallel bus charged to NASA standard V/T curves using a NASA standard power regulator. The following preliminary conclusions were reached: (1) several plate and cell parameters have migrated within their spec limits over the years (in some cases, from one extreme to the other); (2) several parametric relationships, not generally monitored and therefore not under specification control, have also migrated over the years; (3) many of these changes appear to have taken place as a natural consequence of changes in GE/GAB materials and processes; (4) several of these factors may be 'conspiring' to aggravate known cell failure mechanisms (factors such as heavier plate, less teflon and/or less-uniform teflon, and less electrolyte) but all are still in spec (where specs exist); (5) the weight of the evidence collected to characterize the anomalies and to characterize the negative electrode itself, strongly suggests that alterations to the structure, composition, uniformity, and efficiency of the negative electrode are at the heart of the battery performance problems currently being experienced; and (6) further investigation at all levels (plate, cell, battery, and system) continues to be warranted.

Toft, Mark R.↗