Search NASA⌕ Search

SEARCH · Search NASA

Results for “cobalt-free cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Recent Developments in Lithium-Manganese-Nickel Oxide Electrochemistry: The Alchemy of LiMn 0.5 Ni 0.5 O 2

Efforts have been underway for some time at Argonne National Laboratory to design structurally integrated and stabilized lithium-manganese-nickel-oxide cathode materials. The goal has been to find a cobalt-free, high-capacity cathode for a Li-ion battery that is competitive, both cost- and energy-wise, with lithium-nickel-manganese-cobalt-oxide (NMC) and lithium-iron-phosphate (LFP) products. This brief synopsis highlights the remarkable alchemy of LiMn 0.5 Ni 0.5 O 2 resulting from its well-known, slightly disordered layered structure and the recently discovered lithiated spinel phase and totally disordered rock-salt configurations. All three arrangements share a structurally compatible cubic-close-packed oxygen array. The lithiated spinel and layered components provide an intersecting network of two- and three-dimensional channels that facilitate Li + -ion transport, while a minor amount of an extensively disordered rock-salt component likely serves to enhance the structural and electrochemical stability of the electrode. The synopsis also encompasses the historical development of lithiated spinel electrode materials and structurally integrated systems.

Thackeray, Michael M. [Argonne National Laboratory↗

Maximizing Calendering Effects Through the Mechanical Pulverization of Co-Free Nickel-Rich Cathodes in Lithium-Ion Cells

Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles.

25 ENERGY STORAGE↗

Scale-Up of Lithium Iron & Aluminum Nickelate Advanced Cathode and Fabrication of A Battery Pack Comprising The Same

Global battery manufacturers are increasingly worried about the serious supply chain constraint caused by rapid fluctuations in cobalt prices over the years. We present a novel cobalt-free, nickel-rich layered cathode material called NFA class (LiNixFeyAlzO2) to tackle this challenge. Spherical NFA(OH)2 precursors were successfully synthesized by incorporating Ni, Fe, and Al elements using a co-precipitation reaction in a continuous stirred tank reactor. The LiNFAO2 cathode, composed of LiNi0.85Fe0.05Al0.1O2, was synthesized and analyzed using X-Ray diffraction, Mössbauer spectroscopy, and scanning electron microscopy (SEM). The material's electrochemical behavior was evaluated through various techniques at different lithiation/delithiation states in two voltage ranges. The cobalt-free material exhibits a high capacity of 190 mAh/g at 0.1C within the voltage range of 3V-4.5V, as demonstrated by electrochemical performance evaluations. Rate and cycling evaluations showed good rate capability and cycling stability, with 88% capacity retention after 100 cycles at C/3 within the voltage range of 3V-4.3V. Our research shows the great potential of cobalt-free NFA cathodes as a feasible option for developing cost-effective lithium-ion batteries.

25 ENERGY STORAGE↗

Uncovering the Solvation Structure of LiPF 6 –Based Localized Saturated Electrolytes and Their Effect on LiNiO 2 –Based Lithium–Metal Batteries

Electrolytes play a critical role in stabilizing highly reactive lithium-metal anodes (LMAs) and high-voltage cathodes for rechargeable lithium-metal batteries (LMBs). Localized high concentration electrolytes (LHCEs) have achieved remarkable success in the context of LMBs. However, the state-of-the-art LHCEs are based on LiFSI salt, which is prohibitively expensive. Here, the utility of low-cost LiPF 6 salt in localized saturated electrolytes (LSEs) with a series of solvents and diluents in LMBs with cobalt-free LiNiO 2 cathode is systematically explored. Experimental and theoretical analyses reveal that the unique solvation structure formed not only changes the distribution of solvents and anions but also alters the atom–atom distances within them, leading to different reduction and oxidation stabilities compared to low-concentration electrolytes. In addition, LSEs help form LiF-rich interphase layers on the LMA and LiNiO 2 cathode, protecting the electrodes from degradation during cycling. Different LSEs also lead to differences in lithium plating morphology and impedance buildup during cycling, impacting the performance of LMBs. Finally, the solvent and diluent must be carefully selected for compatibility with a lithium salt when developing LHCEs and LSEs for LMBs.

25 ENERGY STORAGE↗

Enhanced Electrochemical Performance of Disordered Rocksalt Cathodes Enabled by a Graphite Conductive Additive

Cobalt-free cation-disordered rocksalt (DRX) cathodes are a promising class of materials for next-generation Li-ion batteries. Although they have high theoretical specific capacities (>300 mA h/g) and moderate operating voltages (~3.5 V vs Li/Li + ), DRX cathodes typically require a high carbon content (up to 30 wt %) to fully utilize the active material which has a detrimental impact on cell-level energy density. To assess pathways to reduce the electrode’s carbon content, the present study investigates how the carbon’s microstructure and loading (10–20 wt %) influence the performance of DRX cathodes with the nominal composition Li 1.2 Mn 0.5 Ti 0.3 O 1.9 F 0.1 . While electrodes prepared with conventional disordered carbon additives (C65 and ketjenblack) exhibit rapid capacity fade due to an unstable cathode/electrolyte interface, DRX cathodes containing 10 wt % graphite show superior cycling performance (e.g., reversible capacities ~260 mA h/g with 85% capacity retention after 50 cycles) and rate capability (~135 mA h/g at 1000 mA/g). Furthermore, a suite of characterization tools was employed to evaluate the performance differences among these composite electrodes. Overall, these results indicate that the superior performance of the graphite-based cathodes is largely attributed to the: (i) formation of a uniform graphitic coating on DRX particles which protects the surface from parasitic reactions at high states of charge and (ii) homogeneous dispersion of the active material and carbon throughout the composite cathode which provides a robust electronically conductive network that can withstand repeated charge–discharge cycles. Overall, this study provides key scientific insights on how the carbon microstructure and electrode processing influence the performance of DRX cathodes. Based on these results, exploration of alternative routes to apply graphitic coatings is recommended to further optimize the material performance.

25 ENERGY STORAGE↗

Cobalt-free and high-rate stable 5V lithium nickel manganese oxide spinel cathodes enabled via surface oxygen vacancies

Spinel LiNi 0.5 Mn 1.5 O 4 offers both the high-rate, low-cost and safety advantages of LiFePO 4 and the high energy density of LiNiₓMnᵧCo₁₋ₓ₋ᵧO₂ and LiNiₓCoᵧAlzO₂ cathodes. However, the large operating voltage of these materials induces electrolyte oxidation, which degrades the interface and drives Mn dissolution. These reactions are further exacerbated at high rates due to temperature rise. In this study, we discover that ammoniacal treatment followed by annealing introduces a high density of oxygen vacancies in the “near-surface region” of LiNi 0.5 Mn 1.5 O 4 particles. These vacancies release electrons changing the oxidation state of Mn and suppressing its tendency to oxidize the electrolyte. Further, these vacancies enhance the electrode’s electronic conductivity (by ∼3-fold) and Li + diffusivity (by ∼2-fold) greatly improving charge transport, especially when operated at high rates. This results in an across-the-board improvement in self-discharge, specific capacity, energy density, rate capability, coulombic efficiency and cycling stability. When cycled at ∼200 mA g −1 , the capacity fade averaged over 3000 cycles for the surface vacancy-enriched material is ∼0.0167% per cycle compared to an order of magnitude higher fade rate for the baseline material. In conclusion, these findings reveal the potential of targeted surface oxygen vacancy doping to develop cobalt-free and high energy density cathodes that tolerate fast charging and deliver improved cycle life.

Cobalt-free cathodes↗

Degradation Pathways of Cobalt–Free LiNiO 2 Cathode in Lithium Batteries

Electrode-electrolyte reactivity (EER) and particle cracking (PC) are considered two main causes of capacity fade in high-nickel layered oxide cathodes in lithium-based batteries. However, whether EER or PC is more critical remains debatable. Herein, the fundamental correlation between EER and PC is systematically investigated with LiNiO 2 (LNO), the ultimate cobalt-free lithium layered oxide cathode. Specifically, EER is found more critical than secondary particle cracking (SPC) in determining the cycling stability of LNO; EER leads to primary particle cracking, but mitigates SPC due to the inhibition of H2-H3 phase transformation. Two surface degradation pathways are identified for cycled LNO under low and high EERs. A common blocking surface reconstruction layer (SRL) containing electrochemically-inactive Ni 3 O 4 spinel and NiO rock-salt phases is formed on LNO in an electrolyte with a high EER; in contrast, an electrochemically-active SRL featuring regions of electron- and lithium-ion-conductive LiNi 2 O 4 spinel phase is formed on LNO in an electrolyte with a low EER. These findings unveil the intrinsic degradation pathways of LNO cathode and are foreseen to provide new insights into the development of lithium-based batteries with a minimized EER and a maximized service life.

25 ENERGY STORAGE↗

Understanding and Mitigating the Dissolution and Delamination Issues Encountered with High-Voltage LiNi 0.5 Mn 1.5 O 4

In our initial study on the high-voltage 5 V cobalt-free spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode, we discovered a severe delamination issue in the laminates when cycled at a high upper cut-off voltage (UCV) of 4.95 V, especially when a large cell format was used. This delamination problem prompted us to investigate further by studying the transition metal (TM) dissolution mechanism of cobalt-free LNMO cathodes, and as a comparison, some cobalt-containing lithium nickel manganese cobalt oxides (NMC) cathodes, as the leachates from the soaking experiment might be the culprit for the delamination. Unlike other previous reports, we are interested in the intrinsic stability of the cathode in the presence of a baseline Gen2 electrolyte consisting of 1.2 M of LiPF 6 in ethylene carbonate/ethyl methyl carbonate (EC/EMC), similar to a storage condition. The electrode laminates (transition metal oxides, transition metal oxides, TMOs, coated on an Al current collector with a loading level of around 2.5 mAh/cm 2 ) or the TMO powders (pure commercial quality spinel LNMO, NMC, etc.) were stored in the baseline solution, and the transition metal dissolution was studied through nuclear magnetic resonance, such as 1 H NMR, 19 F NMR, scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS) and inductively coupled plasma mass spectrometry (ICP-MS). Significant electrolyte decomposition was observed and could be the cause that leads to the TM dissolution of LNMO. To address this TM dissolution, additives were introduced into the baseline electrolyte, effectively alleviating the issue of TM dissolution. The results suggest that the observed delamination is caused by electrolyte decompositions that lead to etching, and additives such as lithium difluorooxalato borate and p-toluenesulfonyl isocyanate can alleviate this issue by forming a firm cathode electrolyte interface. This study provides a new perspective on cell degradation induced by electrode/electrolyte interactions under storage conditions.

25 ENERGY STORAGE↗

Interphase Stabilization of LiNi 0.5 Mn 1.5 O 4 Cathode for 5 V–Class All–Solid–State Batteries

Employing high voltage cobalt-free spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) as a cathode is promising for high energy density and cost-effectiveness, but it has challenges in all-solid-state batteries (ASSBs). Here, it is revealed that the limitation of lithium argyrodite sulfide solid electrolyte (Li 6 PS 5 Cl) with the LNMO cathode is due to the intrinsic chemical incompatibility and poor oxidative stability. Through a careful analysis of the interphase of LNMO, it is elucidated that even the halide solid electrolyte (Li 3 InCl 6 ) with high oxidative stability can be decomposed to form resistive interphase layers with LNMO in ASSBs. Interestingly, with Fe-doping and a Li 3 PO 4 protective layer coating, LNMO with Li 3 InCl 6 displays stable cycle performance with a stabilized interphase at a high voltage (≈4.7 V) in ASSBs. The enhanced interfacial stability with the extended electrochemical stability window through doping and coating enables high electrochemical stability with LNMO in ASSBs. Furthermore, this work provides guidance for employing high-voltage cathodes in ASSBs and highlights the importance of stable interphases to enable stable cycling in ASSBs.

25 ENERGY STORAGE↗

Thermal dynamics of P2-Na 0.67 Ni 0.33 Mn 0.67 O 2 cathode materials for sodium ion batteries studied by in situ analysis

Cobalt-free layered Na 0.67 Ni 0.33 Mn 0.67 O 2 is an attractive cathode material for sodium ion batteries. The thermal stability of cathode materials is crucial to their practical applications. In the current work, we investigate structural and morphological evolution in P2-type Na 0.67 Ni 0.33 Mn 0.67 O 2 cathode materials during annealing via in situ synchrotron X-ray diffraction and transmission electron microscopy. Insights are obtained from the two complementary in situ characterizations (at different length scales) in term of the thermal stability of P2-Na 0.67 Ni 0.33 Mn 0.67 O 2 cathode materials. Here, the results indicate that the hexagonal P2 phase remains unchanged during the heat treatment process, and thermally driven expansion/contraction of lattice parameters exhibit an anisotropic character in the a and c directions. In addition, interfaces/grain boundaries play an important role in the structural stability, which leads to the distinct morphological evolution between the polycrystalline and single-crystal particles.

25 ENERGY STORAGE↗

Co-Free Cathode Materials and Their Novel Architectures

To enable cobalt-free LiNi 0.5 Mn 1.5 O 4 (LNMO) electrode and novel electrolyte formulation for use in next-generation Li-ion batteries (LIB) capable of high energy density, long cycle life and low cost, several methods were developed throughout this project. To enhance the performance of LNMO, Fe-doping on LNMO, laser treatment and atomic layer deposition (ALD) were adopted. Moreover, dry electrode method has successfully helped to fabricate ultra-high loading LNMO with stable performance. The improvement at anode side includes ALD-coating as well as pre-lithiation of graphite anode. In the novel electrolyte development, it was found that all-fluorinated electrolyte with appropriate additives can effectively extend both cycle and calendar life of LNMO full cells at practical loadings. Additional diagnosis of LNMO full cells showed that different types of carbon and porosity of separator play a critical role in the success of LNMO’s high voltage operation. The combined effort throughout the project pushed forward the understanding and commercialization of LNMO at practical level.

25 ENERGY STORAGE↗

Influence of Electrolyte Additives on Interfacial Stability of Manganese-Rich Lithium-Ion Battery Cathodes

Affordable, long-lasting energy storage has become critical to support increased electricity demand in recent years. Cobalt-free, lithium- and manganese-rich lithium nickel manganese oxide (LMR-NM) cathodes stand to reduce cost and supply-chain concerns associated with traditional cobalt-containing cathodes for lithium-ion batteries by leveraging more earth-abundant materials; however, they have shown issues with long-term cycling stability. Here, we investigate lithium difluoro(oxalate)borate (LiDFOB), tris(trimethylsilyl) phosphite (TMSPi), and vinylene carbonate (VC) electrolyte additives for their ability to improve cycling performance of LMR-NM (0.3 Li 2 MnO 3 + 0.7 LiMn 0.5 Ni 0.5 0 2 ) cells. Cryogenic scanning transmission electron microscopy (cryo-STEM) with electron energy loss spectroscopy enables the construction of a structure–function relationship between cathode electrolyte interphase (CEI) characteristics and the electrochemical performance of cells aged with these additives. We find the combination of 2 wt % TMSPi + 1 wt % LiDFOB performs better than any single additive, achieving a 28% improvement in specific capacity over the baseline electrolyte after long-term cycling. We attribute this to LiDFOB mitigating Mn ion dissolution, with cryo-STEM showing Mn stabilized up to the CEI surface, coupled with improved CEI structure and chemistry enabled by TMSPi, evidenced by a moderately thick (∼7–15 nm) CEI that appears to protect against further electrolyte reactions with the particle. These results, achieved through site-specific nanoscale characterization, directly reveal mechanisms through which electrolyte engineering can improve the performance of earth-abundant cathodes, enabling informed development of more affordable and reliable batteries to meet future energy storage needs.

25 ENERGY STORAGE↗

Achieving High Stability and Performance in P2-Type Mn-Based Layered Oxides with Tetravalent Cations for Sodium-Ion Batteries

We report P2-type sodium-manganese-based layered cathodes, owing to their high capacity from both cationic and anionic redox, are a potential candidate for Na-ion batteries to replace Li-ion technology in certain applications. Still, the structure instability originates from irreversible oxygen redox at high voltage remains a challenge. Here, a high sustainability cobalt-free P2- Na 0.72 Mn 0.75 Li 0.24 X 0.01 O 2 (X= Ti/Si) cathode is developed. The outstanding capacity retention and voltage retention after 150 cycles are obtained in Na half-cells. Our finding shows Ti locates on the surface while Si diffuses to the bulk of the particles. Thus, Ti can act as protective layer that alleviate side reactions in carbonate-based electrolyte. Meanwhile, Si can regulate the local electronic structure and suppress oxygen redox activities. Notably, full-cells with hard carbon (≈300-335 Whkg -1 based on the cathode mass) deliver the capacity retention of 83% for P2- Na 0.72 Mn 0.75 Li 0.24 Si 0.01 O 2 and 66% for P2-Na 0.72 Mn 0.75 Li 0.24 Ti 0.01 O 2 after 500 cycles; this electrochemical stability is the best compared to other reported cathodes based on oxygen redox at present. The superior cycle performance also stems from the ability to inhibit microcracking and planar gliding within the particles. Altogether, this finding offers new composition towards developing high performance low-cost cathodes for Na-ion batteries and highlights the unique role of Ti/Si ions.

25 ENERGY STORAGE↗

Cycling Performance and Structure Evolution of Co-Free Lithium- and Manganese-Rich Layered Oxides in Lithium-Ion Batteries

Lithium- and manganese-rich (LMR) layered oxides are high-capacity cathode materials that are being considered for electric vehicle (EV) lithium-ion batteries (LIBs). Here, we investigate the electrochemical cycling behavior of cells containing a cobalt-free LMR oxide, 0.3Li 2 MnO 3 ·0.7LiMn 0.5 Ni 0.5 O 2 , paired with either Li or graphite anodes. Two- and three-electrode cells are cycled under varying conditions to examine the effects of oxide activation, upper cutoff voltage, separator type, and electrolyte composition. Post-cycling characterization of harvested electrodes, with electrochemical, X-ray absorption spectroscopy, and solid-state 6 Li nuclear magnetic resonance spectroscopy techniques, are used to correlate cell performance changes with redox state evolution in the oxide and Li inventory shifts in the cell. Our results show that capacity fade and impedance rise primarily originate at the graphite anode and LMR cathode, respectively. Notably, while Ni undergoes reversible redox, Mn shows no evidence of bulk redox activity even in highly-aged electrodes: only relithiated LMR electrodes show some reduction of Mn. Graphite electrodes degrade due to particle isolation and SEI growth, exacerbated by Mn dissolution and deposition on graphite anodes. These findings highlight the coupled structural and electrochemical degradation mechanisms in LMR/graphite cells and underscore lithium inventory retention and electrode interfacial stability as critical factors for enhancing long-term performance.

Badami, Pavan P. [Argonne National Laboratory (ANL↗

Critical Barriers to Successful Implementation of Earth-Abundant, Mn-Rich Cathodes for Vehicle Applications and Beyond: A Detailed Study of Low SOC Impedance

We report that earth-abundant, sustainable cathode chemistries based on Mn are increasingly attractive for enabling a broader portfolio of cathode oxides. The well-known class of lithium- and manganese-rich cathodes still represents very viable options. However, despite the important work on understanding the mechanisms of voltage fade, hysteresis, and oxygen activity, relatively little attention has been given to understanding the impedance characteristics of these electrodes. In particular, an anomalous rise in area specific impedance at lower states of charge, as well as overall impedance rise and surface damage due to electrolyte interactions, represent critical barriers to implementation. This work presents a comprehensive study of impedance behavior in cobalt-free, lithium- and manganese-rich electrodes. The use of a robust surface treatment allows for long-term behavior to be probed in the absence of surface damage, capacity loss, and impedance rise due to electrolyte interactions. The anomalous rise in impedance could not be correlated to surface changes, or surface phase formation, but could be directly correlated with the bulk processes of voltage fade and voltage hysteresis. The activated material can be explained as a percolating network of higher-voltage, layered-type sites having facile Li diffusion. Interspersed throughout this network are lower-voltage, disordered sites that represent a significant barrier.

25 ENERGY STORAGE↗

Atomic Structural Features of Stacking Faults and Domain Connections in the Li- and Mn-Rich Cathode

Li- and Mn-rich layered oxides (LMRs), a class of earth-abundant materials for rechargeable Li-ion battery cathodes, crystallize into layered structures of two different symmetries: C2/m represented by Li 2 MnO 3 and R$\overline{3}$m represented by LiMn 0.5 Ni 0.5 O 2 . Fundamental questions about how the C2/m and R$\overline{3}$m domains spatially correlate within the same oxide grain and how the C2/m stacking faults arrange themselves when this happens still remain. Here, by using integrated differential phase contrast imaging in scanning transmission electron microscopy (STEM-iDPC), we probe the structural and compositional details of a prototypical, cobalt-free LMR material, 0.3Li 2 MnO 3 •0.7LiMn 0.5 Ni 0.5 O 2 (Li 1.13 Mn 0.57 Ni 0.3 O 2 ). The connection between the C2/m and R$\overline{3}$m domains is found to be abrupt, facilitated by the small lattice mismatch between the two structures. Stacking faults in the C2/m domains feature atomic plane shifting that accommodates stacking sequence changes, which explains why the stacking faults form in a random manner. Furthermore, a local disordering mechanism was identified to correlate with the C2/m stacking faults. Chemically, it is found that Ni coexists with Mn at the transition metal sites within the nominal Li 2 MnO 3 domain. As a result, this study demonstrates that STEM-iDPC is a very useful tool for capturing all the elements in a single image, revealing atomic details on domain connections and stacking faults in the LMRs.

Li-rich and Mn-rich oxides↗

Defining Electrode-Level Metrics for Enabling Earth-Abundant, Mn-Rich Cathodes: A Technoeconomic Analysis of Experimental Materials

Manganese-rich oxides are attractive options as next-generation, earth-abundant cathodes and significant efforts are being directed toward commercial implementation. We report here an updated techno-economic analysis of the lithium- and manganese-rich (LMR) class of earth-abundant cathodes for electric vehicle applications. BatPaC modeling was used to define the cell-level metrics that must be met for these materials to be cost and energy competitive with the current commercial earth-abundant benchmark, LiFePO 4 , as well as anticipated variations such as LiMn 0.8 Fe 0.2 PO 4 . The model was used to evaluate a high-performance material from the literature and subsequently define R&D targets as the likely limits of practical performance for similar LMR systems. Experimental validation and BatPaC evaluation of an advanced, cobalt-free LMR cell system was also conducted. Results show that the advanced LMR cells come within ∼5% of the defined limits and exceed the energy of LiFe(Mn)PO 4 cells at a similar cost. Excellent cycle-life, low impedance, and low impedance rise were also achieved under the conditions tested and reveal that cobalt is not necessary to achieve high-performance LMR oxides. Although the analysis conducted herein reports on LMR cell systems, the methodology and target values defined for performance metrics easily extend to the evaluation of other systems under consideration as earth-abundant options.

Chen, Jiajun [Argonne National Laboratory (ANL), A↗

The Role and Substitution of Cobalt in the Cobalt‐Lean/Free Nickel‐Based Layered Transition Metal Oxides for Lithium Ion Batteries

Here, the Nickel-based layered transition metal oxide cathode represented by NCM (LiNi x Co y Mn z O 2 , x+y+z=1) and NCA (LiNi x Co y Al z O 2 , x+y+z=1) is widely used in the electric vehicle market due to its specific capacity and high working potential, in which Cobalt (Co) plays a huge role in improving the structural stability during the cycle. However, the limited supply of Co, due to its scarcity and the influence of geopolitics, poses a significant constraint on the further advancement of the Nickel-based layered transition metal oxide cathode in the field of energy storage. In this paper, the mechanism of Co in the Nickel-based layered transition metal oxides is reviewed, including its critical role for structural stability such as the inhibition of cationic mixing and the release of lattice oxygen et al. Subsequently, it outlines various strategies to enhance the performance of Co-lean/free materials, such as ion doping, including single-ion doping and multi-ion co-doping, and various surface coating strategies, so as to eliminate the adverse effects of Co loss on materials. Ultimately, this paper offers a glimpse into the promising future of Cobalt-free strategies for high performance of Nickel-based layered transition metal oxides.

25 ENERGY STORAGE↗