Search NASA⌕ Search

SEARCH · Search NASA

Results for “deep level transient spectroscopy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Quenched-in defects in flashlamp-annealed silicon

Deep levels introduced in boron-doped silicon by heat-pulse annealing with a tungsten-halogen flashlamp are investigated using deep-level transient spectroscopy. Two majority-carrier trapping levels in the band gap, at Ev + 0.32 eV and at Ev + 0.45 eV, are observed. These results are compared to those obtained by furnace-quenching and laser-annealing studies. Both the position in the gap and the annealing kinetics of the hole trap at Ev + 0.45 eV suggest that this center is due to an interstitial iron impurity in the lattice. The deep levels are not consistently observed in all flashlamp-annealed Si crystals utilized.

Borenstein, J. T.↗

Electronic properties of deep-level defects in proton irradiated AlGaAs-GaAs solar cells

Deep level transient spectroscopy and capacitance voltage techniques as well as analysis of the forward current voltage (I-V) characteristics and SEM-EIC data were carried out for proton irradiated GaAs solar cells over a wide range of proton energies and proton fluences. Defect and recombination parameters such as defect energy levels and density, carrier capture cross sections and lifetimes as well as diffusion lengths in the undoped n-GaAs LPE layers were determined. Good correlation between these defect parameters and solar cell performance parameters was obtained for GaAs solar cells irradiated by 200 and 290 KeV protons. It was found that 200 to 290 KeV protons will produce the most defects and damages to the GaAs solar cell structure used. The influence of the low temperature (200 to 400 C) periodic thermal annealing on the deep level defects and the performance of the 200 KeV proton irradiated cells is discussed.

Li, S. S.↗

DLTS analysis of radiation-induced defects in one-MeV electron irradiated germanium and Alsub0.17Gasub0.83As solar cells

The radiation-induced deep-level defects in one-MeV electron-irradiated germanium and AlxGal-xAs solar cell materials using the deep-level transient spectroscopy (DLTS) and C-V techniques were investigated. Defect and recombination parameters such as defect density and energy levels, capture cross sections and lifetimes for both electron and hole traps were determined. The germanium and AlGaAs p/n junction cells were irradiated by one-MeV electrons. The DLTS, I-V, and C-V measurements were performed on these cells. The results are summarized as follows: (1) for the irradiated germanium samples, the dominant electron trap was due to the E sub - 0.24 eV level with density around 4x10 to the 14th power 1/cu cm, independent of electron fluence, its origin is attributed to the vacancy-donor complex defect formed during the electron irradiation; (2) in the one-MeV electron irradiated Al0.17Ga0.83 as sample, two dominant electron traps with energies of Ec-0.19 and -0.29 eV were observed, the density for both electron traps remained nearly constant, independent of electron fluence. It is shown that one-MeV electron irradiation creates very few or no new deep-level traps in both the germanium and AlxGa1-xAs cells, and are suitable for fabricating the radiation-hard high efficiency multijunction solar cells for space applications.

Li, S. B.↗

Thermal Stability of Schottky Contacts and Rearrangement of Defects in β ‐Ga 2 O 3 Crystals

Abstract The thermal stability of different Schottky contacts (Au, Pt, and Ni) on (100) β ‐Ga 2 O 3 single crystals grown by the Czochralski method is investigated. Besides the examination of the Schottky barrier parameters, contact‐dependent defect levels are investigated by deep‐level transient spectroscopy (DLTS) in a 100–650 K (ramp‐up) and 650–100 K (ramp‐down) temperature cycle. Several defect levels are detected below the conduction band minimum at 0.41, 0.60, 0.77, 0.96, and 1.17 eV. In the temperature ramp‐down DLTS, the 1.17 eV level disappears, and the 0.60 eV level appears for all Schottky contacts. DFT calculations suggest that rearrangement and dissociation of a single hydrogen from a doubly‐hydrogenated Ga─O divacancy complex occurs during the temperature sweep under bias. The trap level at 0.96 eV only appears after the thermal load for the Ni contact, in contrast to Au and Pt, where it is present without a thermal budget. Temperature‐dependent leakage current (at −4 V) measurements indicate oxidation of Ni, and further thermodynamic analysis suggests alloying of Au‐Ga atoms at the Au/ β ‐Ga 2 O 3 interface. These studies provide insight into the behavior induced by these common Schottky contacts and the alteration associated with temperature cycling.

36 MATERIALS SCIENCE↗

Large-Area (Ag,Cu)(In,Ga)Se 2 Thin-Film Solar Cells with Increased Bandgap and Reduced Voltage Losses Realized with Bulk Defect Reduction and Front-Grading of the Absorber Bandgap

The 1.24 eV bandgap, 18.8% power conversion efficiency Ag-alloyed chalcopyrite (Ag,Cu)(In,Ga)Se 2 (ACIGS) solar cells are characterized to relate voltage and efficiency improvements to electro-optical (EO) characteristics. Shockley-Read-Hall recombination center defect density, identified and characterized through deep level transient spectroscopy and time-resolved photoluminescence (TRPL), is reduced through potassium and copper treatment optimization. Concomitantly, longer minority carrier lifetimes are achieved, which increases open-circuit voltage (V OC ). Near-conduction band defects associated in earlier studies with light-induced current instability are also mitigated. Analysis of charge-carrier dynamics after single- and two-photon excitation is used to separate recombination at the front interface and in the absorber bulk. From TRPL decay simulations, the authors estimate ranges of key solar cell material characteristics: bulk carrier lifetime T bulk = 110-210 ns, charge-carrier mobility u = 110-160 cm 2 V -1 s -1 , and front interface recombination velocity S front = 700-1050 cm s -1 . This lowest-reported S front for ACIGS absorbers originates from the notched conduction band grading, which also makes the impact of the back interface recombination negligible. It is suggested in the results that solar cell performance enhancements can be made most readily with two distinct strategies: improving device architecture and reducing semiconductor defect densities. Using these approaches, power conversion efficiency in large-area solar cells is improved by 1.1% absolute.

14 SOLAR ENERGY↗

Spectroscopic Investigation of Shallow Hole Traps in Ga- and B-doped Czochralski Silicon: Insight into Light-Induced Degradation

We report the minority carrier lifetime in B-doped Czochralski (Cz) Si declines upon carrier injection due to light-induced degradation (LID), which is attributed to the formation of a recombination-active boron-oxygen complex. Ga-doped Cz Si does not undergo LID. Previously, we showed that B-doped Cz Si undergoes a transition from paramagnetic to diamagnetic due to LID. Herein, we show that Ga-doped Cz Si remains paramagnetic upon carrier injection. This suggests that either the shallow hole traps that are formed in B-doped Cz Si are absent in Ga-doped Cz Si, or the negative-U centers in Ga-doped Cz Si do not transform into a recombination-active configuration, because the shallow acceptor trap state is shallower than the Ga acceptor level in the forbidden gap. In contrast to B-doped Cz Si, the defect signatures in Ga-doped Cz Si do not change upon light exposure, as detected by both electron paramagnetic resonance and deep-level transient spectroscopy.

14 SOLAR ENERGY↗

An all optical approach for comprehensive in-operando analysis of radiative and nonradiative recombination processes in GaAs double heterostructures

We demonstrate an all optical approach that can surprisingly offer the possibility of yielding much more information than one would expect, pertinent to the carrier recombination dynamics via both radiative and nonradiative processes when only one dominant deep defect level is present in a semiconductor material. By applying a band-defect state coupling model that explicitly treats the inter-band radiative recombination and Shockley–Read–Hall (SRH) recombination via the deep defect states on an equal footing for any defect center occupation fraction, and analyzing photoluminescence (PL) as a function of excitation density over a wide range of the excitation density (e.g., 5–6 orders in magnitude), in conjunction with Raman measurements of the LO-phonon plasmon (LOPP) coupled mode, nearly all of the key parameters relevant to the recombination processes can be obtained. They include internal quantum efficiency (IQE), minority and majority carrier density, inter-band radiative recombination rate (W r ), minority carrier nonradiative recombination rate (W nr ), defect center occupation fraction (f), defect center density (N t ), and minority and majority carrier capture cross-sections (σ t and σ tM ). While some of this information is thought to be obtainable optically, such as IQE and the W r /W nr ratio, most of the other parameters are generally considered to be attainable only through electrical techniques, such as current-voltage (I-V) characteristics and deep level transient spectroscopy (DLTS). Following a procedure developed herein, this approach has been successfully applied to three GaAs double-heterostructures that exhibit two distinctly different nonradiative recombination characteristics. The method greatly enhances the usefulness of the simple PL technique to an unprecedented level, facilitating comprehensive material and device characterization without the need for any device processing.

14 SOLAR ENERGY↗

Experimental and theoretical studies of native deep-level defects in transition metal dichalcogenides

Abstract Transition metal dichalcogenides (TMDs), especially in two-dimensional (2D) form, exhibit many properties desirable for device applications. However, device performance can be hindered by the presence of defects. Here, we combine state of the art experimental and computational approaches to determine formation energies and charge transition levels of defects in bulk and 2D MX 2 (M = Mo or W; X = S, Se, or Te). We perform deep level transient spectroscopy (DLTS) measurements of bulk TMDs. Simultaneously, we calculate formation energies and defect levels of all native point defects, which enable identification of levels observed in DLTS and extend our calculations to vacancies in 2D TMDs, for which DLTS is challenging. We find that reduction of dimensionality of TMDs to 2D has a significant impact on defect properties. This finding may explain differences in optical properties of 2D TMDs synthesized with different methods and lays foundation for future developments of more efficient TMD-based devices.

36 MATERIALS SCIENCE↗

Probing unintentional Fe impurity incorporation in MOCVD homoepitaxy GaN: Toward GaN vertical power devices

Unintentional impurity incorporation in GaN drift layers represents a challenging issue that can limit their potential performance in vertical power devices. In this paper, we focus on studying the origins of Fe impurity incorporation in metal-organic chemical vapor deposition (MOCVD) grown GaN materials. Acting as a compensator in n-type GaN drift layers, Fe impurities can reduce the electron mobility in GaN and limit the lowest controllable doping level. Two sources, the sample cleaning process and growth susceptor, were identified as the main mechanisms of Fe incorporation in the MOCVD GaN growth process. It was found that solvent cleaning of the wafer can introduce significant Fe contamination at the growth interface, which would slowly be incorporated into the GaN epilayer, thus causing background Fe impurity as high as 10 17 cm -3 level. Moreover, the Fe impurity in the coating material on the susceptor can introduce additional Fe impurity during the growth process. Our studies revealed that the Fe impurity level could be significantly suppressed by more than two orders when an alternative cleaning process was used and the susceptor surface was fully covered by substrates. Characterization of the Fe impurity concentrations was performed via secondary ion mass spectrometry. The trap level (E C - 0.57) eV from deep-level transient spectroscopy that had previously been attributed to Fe confirmed the carrier compensation effect from Fe. Room temperature Hall mobility as high as 1007 cm 2 /V s was achieved on the MOCVD grown low-Fe GaN. Results from this work will provide guidance for achieving high purity GaN toward high performance GaN vertical power devices.

42 ENGINEERING↗

Identification of dislocation-related and point-defects in III-As layers for silicon photonics applications

Abstract The aim of this paper is to identify, analyze and compare the defects present in III-As, as a function of dislocation density, and as a function of the presence/absence of quantum dots (QDs). Such materials are of fundamental importance for the development of lasers and photodiodes for silicon photonics. The study is based on an extensive deep-level transient spectroscopy investigation, carried out on GaAs pin diodes grown on Si and on GaAs (that differ in the dislocation density), with and without embedded QDs. The original results described in this paper demonstrate that: (a) we were able to identify four different defects within the device grown on Si (three electron and one hole traps) and one defect (hole trap) in the device on GaAs, common to both samples; (b) all the majority carrier traps identified are located near midgap, i.e. are efficient non-radiative recombination centers; (c) such defects are absent (or non-detectable) in the sample grown on GaAs substrate, having a very low dislocation density; (d) the presence of QDs does not result in additional defects within the semiconductor material; (e) the analysis of the capture kinetics revealed that two of the identified traps are related to point defects, whereas the other two traps can be associated with point defects located near a dislocation; (f) a comparison with previous reports indicate that the detected traps are related to native III-As defects, or to oxygen-related complexes.

Physics↗

Multistability of isolated and hydrogenated Ga–O divacancies in β–Ga 2 O 3

This work systematically explores 19 unique configurations of the close-associate Ga–O divacancies (V Ga V O ) in β–Ga 2 O 3 , including their complexes with H impurities, using hybrid functional calculations. Interestingly, most configurations are found to retain the negative-U behavior of V O , as they exhibit a thermodynamic (–/3–) charge-state transition level energetically located in the upper part of the band gap, where the 3– charge state is associated with the formation of a Ga–Ga dimer. The energy positions of the thermodynamic (–/3–) charge-state transition levels divide the divacancy configurations into three different groups, which can be understood from the three possible Ga–Ga dimerizations resulting from the tetrahedral and octahedral Ga sites. The relative formation energies of the different divacancy configurations, and hence the electrical activity of the divacancies, is found to depend on the Fermi-level position, and the energy barriers for transformation between different divacancy configurations are explored from nudged elastic band calculations. Hydrogenation of the divacancies is found to either passivate their negative-U charge-state transition levels or shift them down in Fermi level position, depending on whether the H resides at V O or forms an O–H bond at V Ga , respectively. Finally, the divacancy is discussed as a potential origin of the so-called E$^{*}_{2}$ center previously observed by deep-level transient spectroscopy.

36 MATERIALS SCIENCE↗

Intrinsic and complex defect engineering of quasi-one-dimensional ribbons Sb 2 S 3 for photovoltaics performance

Sb 2 S 3 has attracted great attention recently as a prospective solar cell absorber material. In this work, intrinsic defects, dopants, and their complexes in Sb 2 S 3 are systematically investigated by using hybrid functional theory. V Sb and V S are dominant native defects and pin the Fermi level near the midgap, which is consistent with the high resistivity observed experimentally. Both V Sb and V S introduce deep levels inside the band gap, which can trap free carriers. Our calculated deep transition levels of V Sb and Sb S are consistent well with the results of the deep-level transient spectroscopy measurement. We further study dopants (including Cu, Ti, Zn, Br, and Cl) in Sb 2 S 3 and find that Zn and Br/Cl are shallow acceptors and donors, respectively, which may be used to control the carrier and trap densities in Sb 2 S 3 . In addition, the defect complexes, i.e., Cu(Zn) Sb +V S and Cl(Br) S +V Sb are also investigated. The interaction between the donor and acceptor defects makes the defect levels of complexes shallower and less detrimental to carrier transport.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High Performance GaAs Solar Cells Grown at High Growth Rates by Atmospheric-Pressure Dynamic Hydride Vapor Phase Epitaxy

We report GaAs solar cells grown at rates exceeding 300 um/h by atmospheric-pressure dynamic hydride vapor phase epitaxy (D-HVPE). The surface morphology of the GaAs layers grown at those rates is smooth, with root mean square surface roughness of < 1.4 nm. We grew GaAs solar cells at rates from 35 - 309 um/h with negligible degradation in open circuit voltages (VOC), which ranged from 1.04 - 1.07 V. We showed the slight decrease in VOC is due to lack of doping optimization at higher growth rates. Deep level transient spectroscopy measurements showed low point defect densities that increases slightly with growth rate from 35 - 309 um/h. The low point defect concentrations and the high VOCs indicate that high material quality can be maintained at these extremely high growth rates, enabling the deposition of high efficiency cells in mere seconds instead of hours.

14 SOLAR ENERGY↗

Stability of Silicon Heterojunction Solar Cells Having Hydrogen Plasma Treated Intrinsic Layer

The open-circuit voltage of Silicon Heterojunction (HJ) cells can be improved by using extrinsic hydrogen plasma treatment (HPT) to reduce the trap states (NT) which we have verified using Deep Level Transient Spectroscopy (DLTS). However, hydrogen has been associated with long-term degradation. We have investigated the stability of HJ cells with and without HPT using accelerated degradation (1-sun illumination, 90 degrees C temperature, argon ambient for 1000 hours). The stability has been studied using DLTS, current-voltage, and Suns-Voc. Our results show HPT cells are stable and maintain their higher Voc and lower NT after accelerated degradation.

degradation↗

Study of electronic properties in proton- and electron-irradiated GaAlAs and GaAs solar cell materials

Diagnostical measurement techniques such as dark I-V, C-V, the thermally insulated capacitance, and the deep level transient spectroscopy methods were employed to study defect properties in the proton-irradiated n-GaAs materials. Defect energy levels, thermal emission rates, and capture cross sections of electrons as well as trap densities were deduced from these measurements and the results are presented. Correlations between the measured defect parameters and the dark I-V characteristics of the n-GaAs Schottky barrier diodes are also discussed. Defect energy levels (i.e., electron traps) determined are also compared with published data in order to identify their physical origins.

Li, S. S.↗

Reverse annealing in radiation-damaged, silicon solar cells

In order to understand the results in terms of properties of the radiation induced defects, a combination of diffusion length measurements and defect data obtained from Deep Level Transient Spectroscopy were used. The results indicate that the defect at E sub v + 0.30 eV is responsible for the observed reversed annealing. The defect was identified as a boron-oxygen vacancy complex. This identification is a guide to processing efforts aimed at increasing the concentration of these radiation induced defects.

Weinberg, I.↗

Radiation damage annealing mechanisms and possible low temperature annealing in silicon solar cells

The defect responsible for reverse annealing in 2 ohm/cm n(+)/p silicon solar cells was identified. This defect, with energy level at e sub v + 0.30 eV was tentatively identified as a boron oxygen-vacancy complex. Results indicate that its removal could result in significant annealing for 2 ohm/cm and lower resistivity cells at temperatures as low as 200 C. These results were obtained by use of an expression derived from the Shockley-Read-Hall recombination theory which relates measured diffusion length ratios to relative defect concentrations and electron capture cross sections. The relative defect concentrations and one of the required capture cross sections are obtained from Deep Level Transient Spectroscopy. Four additional capture cross sections are obtained using diffusion length data and data from temperature dependent lifetime studied. These calculated results are in reasonable agreement with experimental data.

Weinberg, I.↗

Crystal growth of device quality GaAs in space

The apparatus and techniques used in effort to determine the relationships between crystal growth and electronic properties are described with emphasis on electroepitaxy and melt-grown gallium aresenide crystal. Applications of deep level transient spectroscopy, derivative photocapitance spectroscopy, and SEM-cathodoluminescene in characterizing wide bandgap semiconductors; determining photoionization in MOS, Schottky barriers, and p-n junctions; and for identifying inhomogeneities are examined, as well as the compensation of indium phosphide.

Gatos, H. C.↗