Durability Optimization of CO 2 Electrolyzers for Syngas Evolution

Recently, there has been an increased interest in mitigating anthropogenic CO 2 emissions through the electrochemical conversion of CO 2 into fuels and fuel feedstocks, including hydrogen gas (H 2 ), carbon monoxide (CO), and mixtures of the two to yield syngas. Commercial applications of these systems require high catalytic selectivity for the desired products, while exhibiting operational lifetimes exceeding thousands of hours. Advancements in this field have produced systems that display high selectivity of the desired products at faradaic efficiencies exceeding 95%. Despite the advancements made in CO 2 electrolysis, system durability remains a standing challenge in the field. CO 2 electrolyzer lifetimes are often limited by carbonate fouling, catalyst degradation, detrimental flooding of electrode microporous layers and anion exchange membrane (AEM) failures. In this report, a 5 cm 2 membrane electrode assembly (MEA) device is used to investigate potential failure modes and to optimize AEM CO 2 electrolyzer operation. Key findings of this study include the importance of CO 2 flow rate, use of a thin PiperION PTFE-reinforced membrane, optimizing compression to enhance contact under 40 in-lb compression, and the effect of more compressible, commercial iridium oxide anodes on system durability.

Abouremeleh, Mohammed H. [Lawrence Berkeley Nation↗

Pressure-induced phase transition in barium hydride studied with neutron scattering

Barium hydride can undergo a structural phase transition from an orthorhombic phase to a hexagonal phase induced by high temperature or high pressure. This transition causes an immediate increase in the hydrogen diffusion rates by over an order of magnitude, and therefore, understanding the origin and details of such transition is of great interest not only for fundamental reasons but also for improving materials for future applications. In this work, the pressure evolution of the crystal structure was characterized using neutron powder diffraction up to a maximum pressure of 11.3 GPa. The pressure dependence of the unit cell volumes, lattice parameters, atomic sites, and compressibilities were determined for both phases. A structural phase transition occurred over a wide pressure range of P = 1.3 GPa–4.9 GPa. The transition to the higher density hexagonal phase reduced the volume per formula unit of BaD 2 by 13.6%, hence increasing the volumetric storage density. In addition, we investigated the hydrogen diffusion process using high pressure quasi-elastic neutron scattering up to 7.1 GPa. Our results show that the hydrogen mobility increases with pressure in the hexagonal phase. This work sheds light on the structural and dynamical aspects of barium hydride caused by the application of high pressure. Finally, the results may aid in the development of advanced metal hydride systems with increased hydrogen dynamics.

36 MATERIALS SCIENCE↗

Oxygen Electrocatalysis on Mixed-Metal Oxides/Oxyhydroxides: From Fundamentals to Membrane Electrolyzer Technology

Catalyzing the oxygen evolution reaction (OER) is important for key energy-storage technologies, particularly water electrolysis and photoelectrolysis for hydrogen fuel production. Under neutral-to-alkaline conditions, first-row transition-metal oxides/(oxy)hydroxides are the fastest-known OER catalysts and have been the subject of intense study for the past decade. Critical to their high performance is the intentional or accidental addition of Fe to Ni/Co oxides that convert to layered (oxy)hydroxide structures during the OER. Unraveling the role that Fe plays in the catalysis and the molecular identity of the true “active site” has proved challenging, however, due to the dynamics of the host structure and absorbed Fe sites as well as the diversity of local structures in these disordered active phases. In this Account, we highlight our work to understand the role of Fe in Ni/Co (oxy)hydroxide OER catalysts. We first discuss how we characterize the intrinsic activity of the first-row transition-metal (oxy)hydroxide catalysts as thin films by accounting for the contributions of the catalyst-layer thickness (mass loading) and electrical conductivity as well as the underlying substrate’s chemical interactions with the catalyst and the presence of Fe species in the electrolyte. We show how Fe-doped Ni/Co (oxy)hydroxides restructure during catalysis, absorb/desorb Fe, and in some cases degrade or regenerate their activity during electrochemical testing. We highlight the relevant techniques and procedures that allowed us to better understand the role of Fe in activating other first-row transition metals for OER. We find several modes of Fe incorporation in Ni/Co (oxy)hydroxides and show how those modes correlate with activity and durability. We also discuss how this understanding informs the incorporation of earth-abundant transition-metal OER catalysts in anion-exchange-membrane water electrolyzers (AEMWE) that provide a locally basic anode environment but run on pure water and have advantages over the more-developed proton-exchange-membrane water electrolyzers (PEMWE) that use platinum-group-metal (PGM) catalysts. We outline the key issues of introducing Fe-doped Ni/Co (oxy)hydroxide catalysts at the anode of the AEMWE, such as the oxidative processes triggered by Fe species traveling through the polymer membrane, pH-gradient effects on the catalyst stability, and possibly limited catalyst utilization in the compressed stack configuration. We also suggest possible mitigation strategies for these issues. Lastly, we summarize remaining challenges including the long-term stability of Fe-doped Ni/Co (oxy)hydroxides under OER conditions and the lack of accurate models of the dynamic active surface that hinder our understanding of, and thus ability to design, these catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗