Insights from incorporating reference electrodes in symmetric lithium-ion cells with layered oxide or graphite electrodes

Symmetric cells provide complementary means to probe electrochemical processes in lithium-ion batteries. Here, positive and negative electrodes harvested from conventional oxide/graphite cells are cross-paired, and the assembled reference-electrode-bearing symmetric cells are cycled/aged. For graphite symmetric cells, the electrode potentials and impedances remain nearly constant during calendar aging and the parasitic currents are typically small. However, at higher cell voltages when the “positive” graphite potential exceeds 1.0 V vs. Li/Li + , the capacity loss is higher, indicating that even a mild (but prolonged) overdischarge can damage the SEI. For the layered-oxide symmetric cells there are strong parasitic currents and a persistent slide of the electrode potential over time during calendar aging. Significant cell impedance rise, especially at higher hold voltages, is also observed. Curiously, the impedance rise in the “negative” oxide electrode, which experiences potentials below 4.0 V vs. Li/Li + , is greater than in the “positive” oxide electrode that experiences much higher potentials. We postulate that electrolyte oxidation is responsible for the behavior of these oxide symmetric cells, as it supplies electrons (that bind more Li + into the cathode, causing the potential slide) and protons (that contribute to impedance rise). Furthermore, these insights can guide the development of future lithium-ion cell chemistries.

25 ENERGY STORAGE↗

Stable voltage source for Penning trap experiments

A voltage reference has been developed to bias ring electrodes of two Penning traps between -90 and 0 V. For output voltages near -90 V, the Allan deviation of the system's voltage instability is less than 1 part in 10{sup 8} over all time scales shorter than 10{sup 4} s. For averaging times longer than several seconds, the system's stability is determined almost completely by the noise, drift, and aging of the zener diodes in the array of voltage reference integrated circuits. For shorter averaging times, active filters built into the new system significantly reduce the intrinsic noise of the zener diodes. The system makes it possible to continuously adjust the ring voltages for frequency locking the axial motion in the two Penning traps. By keeping electrical noise highly correlated between the two traps, measurement uncertainty should be reduced for precision experiments such as Penning trap mass spectrometry.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Vestibulo-ocular and vestibulospinal function before and after cochlear implant surgery

Vestibular function in cochlear implant candidates varies from normal to total absence of function. In patients with intact vestibular function preoperatively, invasion of the otic capsule places residual vestibular function at risk. Speech-processing strategies that result in large amplitude electrical transients or strategies that employ high amplitude broad frequency carrier signals have the potential for disrupting vestibular function. Five patients were tested with and without electrical stimulation via cochlear electrodes. Two patients experienced subjective vestibular effects that were quickly resolved. No long-term vestibular effects were noted for the two types of second generation cochlear implants evaluated. Histopathological findings from another patient, who had electrically generated vestibular reflex responses to intramodiolar electrodes, indicated that responses elicited were a function of several variables including electrode location, stimulus intensity, stimulus amplitude, and stimulus frequency. Differential auditory, vestibulocolic, and vestibulospinal reflexes were demonstrated from the same electrode as a function of stimulus amplitude, frequency, and duration.

Case Reports↗

Operation status of the electron cyclotron resonance ion source at Gunma University

An ECR ion source of Gunma University Heavy Ion Medical Center, so-called KeiGM [M. Muramatsu, A. Kitagawa, Y. Sakamoto, S. Sato, Y. Sato, H. Ogawa, S. Yamada, H. Ogawa, Y. Yoshida, and A. G. Drentje, Rev. Sci. Instrum. 76, 113304 (2005)], has been operated for cancer therapy and physical/biological experiment since 2010. KeiGM produces typically 230 μA of 10 keV/u C{sup 4+} ions from CH{sub 4} gases. The vacuum pressure is kept between 1.2 × 10{sup −4} and 1.7 × 10{sup −4} Pa so as to suppress the pulse-to-pulse current fluctuation within ±10%. The extraction electrode is cleaned every 6–8 months in order to remove deposited carbon, which increases the leak current and discharge. In order to investigate the possibility of long-term operation without such maintenances, oxygen aging for the cleaning of the extraction electrode has been tested in the test bench. The same-designed ion sources at National Institute of Radiological Sciences and SAGA Heavy Ion Medical Accelerator in Tosu (SAGA-HIMAT) are also operated with stable C{sup 4+} current, which are suitable for the continuous operation for cancer therapy.

43 PARTICLE ACCELERATORS↗

Durability of Pt-Co Alloy Polymer Electrolyte Fuel Cell Cathode Catalysts under Accelerated Stress Tests

The durability of Pt-Co alloy cathode catalysts supported on high surface area carbon is investigated by subjecting them to accelerated stress tests (ASTs). The catalysts had different initial Co contents and nanoparticle morphologies: a “spongy” porous morphology for the high-Co (H) content catalyst, and a fully alloyed crystalline morphology for the medium-Co (M) and low-Co (L) content catalysts. The specific activity of the catalysts depends on their initial Co content, morphology and nanoparticle size, and remained higher than 1000 μA/cm 2 -Pt after 27–50% Co loss. The H-catalyst electrode showed the smallest kinetic overpotentials (η c s ) due to higher initial Pt loading than the other two electrodes, but it had the fastest increase in ηcs with AST cycling due to lower Co retention; the L-catalyst electrode showed higher η c s due to a lower initial Pt loading, but had a smaller increase in η c s with aging due to higher Co retention; the M-catalyst electrode showed a similar increase in η c s with aging, but this increase was due to the combined effects of Co dissolution and electrochemically active surface area (ECSA) loss. In conclusion, the modeled increase in mass transfer overpotentials with aging correlates with the initial Pt loading, ECSA loss and the initial catalyst morphology

25 ENERGY STORAGE↗

Understanding LIB Battery Electrodes Through Classical Electrochemical Interface Theory

Classical models of the electrochemical interface can be applied to complex and dynamic electrodes to understand important mechanisms that are relevant to device-level phenomena like calendar aging or cycle life. Here, we show that negative alloy electrodes with wide electrochemical windows cannot be assumed to have static interfaces throughout all states of charge. Under high states of charge, the interface -including the solid electrolyte interphase - has characteristics that resemble a highly polarized electrode far from the point of zero charge. Under these conditions, the interface can be understood through the Helmholtz model. At lower states of charge, the interface capacitance decreases and the space charge layer length increases. This transformation resembles a metal electrode approaching the point of zero charge which is understood through the Gouy-Chapman-Stern-Grahame model of the electrochemical interface. This transformation happens at both silicon and carbon-coated silicon interfaces. From voltage-limited cycling experiments, in the limit of the diffuse double layer, the silicon electrode impedance rises significantly in the first few cycles. This rise is related to the continuous electrochemical reduction of electrolyte components from an interface that is not electronically screened from the electrolyte. In other words, an electrode interface for batteries should resemble a 'Helmholtz-like' structure.

anode↗

Structural comparison of nickel electrodes and precursor phases

A summary of previous Raman spectroscopic results and a discussion of important structural differences in the various phases of active mass and active mass precurors are presented. Raman spectra provide unique signatures for these phases, and allow one to distinguish each phase, even when the compound is amorphous to X-rays (i.e., does not scatter X-rays because of a lack of order and/or small particle size). The structural changes incurred during formation, charge and discharge, cobalt addition, and aging will be discussed and related to electrode properties. Important structural differences include NiO2 layer stacking, nonstoichiometry (especially cation-deficit nonstoichiometry), disorder, dopant content, and water content. The results indicate that optimal nickel active mass is non-close packed and nonstoichiometric. The formation process transforms precursor phases into this structure. Therefore, the precursor disorder, or lack thereof, influences this final active mass structure and the rate of formation. Aging processes induce structural change which is believed to be detrimental. The role of cobalt addition can be appreciated in terms of structures favored or stabilized by the dopant. In recent work, the in situ Raman technique to characterize the critical structural parameters was developed. An in situ method relates structure, electrochemistry, and preparation. In situ Raman spectra of cells during charge and discharge, either during cyclic voltammetry or under constant current conditions were collected. With the structure-preparation knowledge and the in situ Raman tool, it will be possible to define the structure-property-preparation relations in more detail. This instrumentation has application to a variety of electrode systems.

Cornilsen, Bahne C.↗

Degradation and Modeling of Large-Format Commercial Lithium-Ion Cells as a Function of Chemistry, Design, and Aging Conditions

Demand for large-format (>10 Ah) lithium-ion batteries has increased substantially in recent years, due to the growth of both electric vehicle and stationary energy storage markets. The economics of these applications is sensitive to the lifetime of the batteries, and end-of-life can either be due to energy or power limitations. Despite this, there is little information from cell manufacturers on the sensitivity of cell degradation to environmental conditions or battery use. This work reports accelerated aging test data from four commercial large-format lithium-ion batteries from three manufacturers, with varying design (thickness, casings, ...), chemistry (lithium-iron-phosphate (LFP) or lithium-nickel-manganese-cobalt-oxide positive electrodes (NMC), with graphite (Gr) negative electrodes), and capacity (50 to 250 Amp hours). The tested LFP|Gr cell is found to be relatively insensitive to cycling conditions like temperature or voltage window, while NMC|Gr cells have varying sensitivity. Degradation trends are further investigated by training predictive models: simple polynomial trend lines, a semi-empirical reduced-order model, and an empirical reduced-order model identified using machine-learning based on symbolic regression. Calendar and cycle life are simulated over a variety of conditions to directly compare the various batteries. Cell size and thickness are found to substantially impact sensitivity to temperature during cycle aging, while electrode chemistry impacts depth-of-discharge sensitivity. Real-world battery lifetime is evaluated by simulating residential energy storage and commercial frequency containment reserve systems in several U.S. climate regions. Predicted lifetime across cell types varies from 7 years to 20+ years, though all cells are predicted to have at least 10 year life in certain conditions.

battery lifetime↗

Revealing the aging process of solid electrolyte interphase on SiOx anode

Abstract As one of the most promising alternatives to graphite negative electrodes, silicon oxide (SiO x ) has been hindered by its fast capacity fading. Solid electrolyte interphase (SEI) aging on silicon SiO x has been recognized as the most critical yet least understood facet. Herein, leveraging 3D focused ion beam-scanning electron microscopy (FIB-SEM) tomographic imaging, we reveal an exceptionally characteristic SEI microstructure with an incompact inner region and a dense outer region, which overturns the prevailing belief that SEIs are homogeneous structure and reveals the SEI evolution process. Through combining nanoprobe and electron energy loss spectroscopy (EELS), it is also discovered that the electronic conductivity of thick SEI relies on the percolation network within composed of conductive agents (e.g., carbon black particles), which are embedded into the SEI upon its growth. Therefore, the free growth of SEI will gradually attenuate this electron percolation network, thereby causing capacity decay of SiO x . Based on these findings, a proof-of-concept strategy is adopted to mechanically restrict the SEI growth via applying a confining layer on top of the electrode. Through shedding light on the fundamental understanding of SEI aging for SiO x anodes, this work could potentially inspire viable improving strategies in the future.

25 ENERGY STORAGE↗

Cycling behavior of NCM523/graphite lithium-ion cells in the 3–4.4 V range: Diagnostic studies of full cells and harvested electrodes

Energy density of full cells containing layered-oxide positive electrodes can be increased by raising the upper cutoff voltage above the current 4.2 V limit. In this article we examine aging behavior of cells, containing LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523)-based positive and graphite-based negative electrodes, which underwent up to ~400 cycles in the 3-4.4 V range. Electrochemistry results from electrodes harvested from the cycled cells were obtained to identify causes of cell performance loss; these results were complemented with data from X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS) measurements. Our experiments indicate that the full cell capacity fade increases linearly with cycle number and results from irreversible lithium loss in the negative electrode solid electrolyte interphase (SEI) layer. The accompanying electrode potential shift reduces utilization of active material in both electrodes and causes the positive electrode to cycle at higher states-of-charge. Here, full cell impedance rise on aging arises primarily at the positive electrode and results mainly from changes at the electrode-electrolyte interface; the small growth in negative electrode impedance reflects changes in the SEI layer. Our results indicate that cell performance loss could be mitigated by modifying the electrode-electrolyte interfaces through use of appropriate electrode coatings and/or electrolyte additives.

30 DIRECT ENERGY CONVERSION↗

Battery aging mode identification across NMC compositions and designs using machine learning

A comprehensive understanding of lithium-ion battery (LiB) lifespan is the key to designing durable batteries and optimizing use protocols. Although battery lifetime prediction methods are flourishing, diagnosis of the root causes of aging and degradation have not yet been well developed nor studied for a broad mixture of designs and use cases. Here, we create a machine-learning (ML)-based framework that distinguishes aging modes using multiple electrochemical signatures recorded cycle-by-cycle. The predominant aging behaviors include a combination of loss of active materials in cathode (LAMPE) and a loss of Li inventory (LLI) in Li plating or solid electrolyte interphase (SEI) formation, manifested from 44 batteries representing two cathode chemistries, two electrode loadings, and five charging rates. Here, the aging mode classification accuracy is 86% using features within the first 50 cycles and increases to 88% beyond 225 cycles. The same features can quantify the percentage of end-of-life LAMPE with only 4.3% of error.

25 ENERGY STORAGE↗

Redox-homogeneous, gel electrolyte-embedded high-mass-loading cathodes for high-energy lithium metal batteries

Lithium metal batteries have higher theoretical energy than their Li-ion counterparts, where graphite is used at the anode. However, one of the main stumbling blocks in developing practical Li metal batteries is the lack of cathodes with high-mass-loading capable of delivering highly reversible redox reactions. To overcome this issue, here we report an electrode structure that incorporates a UV-cured non-aqueous gel electrolyte and a cathode where the LiNi 0.8 Co 0.1 Mn 0.1 O 2 active material is contained in an electron-conductive matrix produced via simultaneous electrospinning and electrospraying. This peculiar structure prevents the solvent-drying-triggered non-uniform distribution of electrode components and shortens the time for cell aging while improving the overall redox homogeneity. Moreover, the electron-conductive matrix eliminates the use of the metal current collector. When a cathode with a mass loading of 60 mg cm -2 is coupled with a 100 µm thick Li metal electrode using additional non-aqueous fluorinated electrolyte solution in lab-scale pouch cell configuration, a specific energy and energy density of 321 Wh kg -1 and 772 Wh L -1 (based on the total mass of the cell), respectively, can be delivered in the initial cycle at 0.1 C (i.e., 1.2 mA cm -2 ) and 25 °C.

25 ENERGY STORAGE↗

Coulombic Efficiency and Capacity Retention are Not Universal Descriptors of Cell Aging

Capacity and coulombic efficiency are often used to assess the performance of Li-ion batteries, under the assumption that these quantities can provide direct insights about the rate of electron consumption due to growth of the solid electrolyte interphase (SEI). Here, we show that electrode properties can actually change the amount of information about aging that can be directly retrieved from capacity measurements. During cycling of full-cells, only portions of the voltage profiles of the positive and negative electrodes are accessible, leaving a reservoir of cyclable Li + stored at both electrodes. The size and availability of this reservoir depends on the shape of the voltage profiles and accessing this extra Li + can offset some of the capacity that is consumed by the SEI. Consequently, capacity and efficiency measurements can, at times, severely underestimate the rate of side reactions experienced by the cell. We show, for example, that a same rate of SEI growth would cause faster capacity fade in LiFePO 4 than in NMC cells, and that the perceived effects of aging depend on testing variables such as depth of discharge. Simply measuring capacity may be insufficient to gauge the true extent of aging endured by Li-ion batteries.

25 ENERGY STORAGE↗

Electrical conductivity method to assess static stability of self-consolidating concrete

The objective of this study is to evaluate the applicability of the electrical conductivity method to assess the stability of self-consolidating concrete (SCC) at early age. The method consists in inserting four electrode pairs at different depths of concrete to monitor local change in ionic concentrations with time. Such variations can reflect migration of bleed water along concrete column during the plastic stage. The experimental set-up consisted of a rectangular column measuring 1005 mm in height and 250 x 250 mm in cross section. The variations in ionic concentrations were exploited to derive stability indices with regards to bleeding and homogeneity of concrete. Derived stability indices included bleeding coefficient, segregation coefficient, and homogeneity index. Various SCC mixtures made with a fixed water-to-cementitious materials ratio (w/cm) of 0.42, different aggregate gradations, and slump-flow values of 650 {+-} 10 and 700 {+-} 10 mm were evaluated. Analysis of changes in ionic concentrations along column samples with time provided adequate evaluation of stability of SCC. For example, the increase in the concentration of viscosity-modifying admixture from 1% to 2% was shown to decrease the homogeneity index from 0.36 to 0.27, reflecting better stability. Validation procedure was carried out by correlating stability indices derived from electrical conductivity measurements to physical variations of coarse aggregate concentrations determined on plastic concrete sampled from the tested column elements at the end of electrical conductivity monitoring period. Good correlations between stability indices and aggregate concentrations are established.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Substantial oxygen loss and chemical expansion in lithium-rich layered oxides at moderate delithiation

Delithiation of layered oxide electrodes triggers irreversible oxygen loss, one of the primary degradation modes in lithium-ion batteries. However, the delithiation-dependent mechanisms of oxygen loss remain poorly understood. Here we investigate the oxygen non-stoichiometry in Li 1.18–x Ni 0.21 Mn 0.53 Co 0.08 O 2–δ electrodes as a function of Li content by using cycling protocols with long open-circuit voltage steps at varying states of charge. Surprisingly, we observe substantial oxygen loss even at moderate delithiation, corresponding to 2.5, 4.0 and 7.6 ml O 2 per gram of Li 1.18–x Ni 0.21 Mn 0.53 Co 0.08 O 2–δ after resting at upper capacity cut-offs of 135, 200 and 265 mAh g −1 for 100 h. Our observations suggest an intrinsic oxygen instability consistent with predictions of high oxygen activity at intermediate potentials versus Li/Li + . In addition, we observe a large chemical expansion coefficient with respect to oxygen non-stoichiometry, which is about three times greater than those of classical oxygen-deficient materials such as fluorite and perovskite oxides. Furthermore, our work challenges the conventional wisdom that deep delithiation is a necessary condition for oxygen loss in layered oxide electrodes and highlights the importance of calendar ageing for investigating oxygen stability.

Atomistic models↗

The influence of electrochemical cycling protocols on capacity loss in nickel-rich lithium-ion batteries

The transition towards electric vehicles and more sustainable transportation is dependent on lithium-ion battery (LIB) performance. Ni-rich layered transition metal oxides, such as NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ), are promising cathode candidates for LIBs due to their higher specific capacity and lower cost compared with lower Ni content materials. However, complex degradation mechanisms inhibit their use. In this work, tailored aging protocols are employed to decouple the effect of electrochemical stimuli on the degradation mechanisms in graphite/NMC811 full cells. Using these protocols, impedance measurements, and differential voltage analysis, the primary drivers for capacity fade and impedance rise are shown to be large state of charge changes combined with high upper cut-off voltage. Focused ion beam-scanning electron microscopy highlights that extensive microscale NMC particle cracking, caused by electrode manufacturing and calendering, is present prior to aging and not immediately detrimental to the gravimetric capacity and impedance. Scanning transmission electron microscopy electron energy loss spectroscopy reveals a correlation between impedance rise and the level of transition metal reduction at the surfaces of aged NMC811. The present study provides insight into the leading causes for LIB performance fading, and highlights the defining role played by the evolving properties of the cathode particle surface layer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lithium tetrafluoro oxalato phosphate as electrolyte additive for lithium-ion cells.

Lithium tetrafluoro oxalato phosphate (LTFOP) was investigated as an electrolyte additive to improve the life of mesocarbon microbead (MCMB)/Li{sub 1.1}[Ni{sub 1/3}Co{sub 1/3}Mn{sub 1/3}]{sub 0.9}O{sub 2} (NCM) cells for high power applications. With the addition of 1-3 wt % LTFOP to MCMB/NCM cells, the capacity retention after 200 cycles at 55 C significantly improved. Electrochemical impedance spectroscopy showed that the LTFOP addition in the electrolyte increased the initial impedance but lowered the impedance growth rate during cycling. Aging tests at 55 C indicated that the capacity retention of the negative electrode significantly benefited as a result of the LTFOP addition. Differential scanning calorimetry showed that the safety of the lithiated MCMB is significantly improved with the LTFOP addition.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Surface Studies of High Voltage Lithium Rich Composition: Li1.2Mn0.525Ni0.175Co0.1O2

This article reports the evidence of surface film formation because of the breakdown of electrolyte upon high voltage cycling (4.9 V) of lithium rich cathode having a nominal composition of, Li1.2Mn0.525Ni0.175Co0.1O2. We studied the chemical composition of this passivation film using electrochemical impedance, X-ray Photoelectron and micro-Raman spectroscopy and the results were compared against the pristine electrode. In order to distinguish the changes in the surface films composition induced by prolonged electrochemical cycling versus chemical passivation effect, we also studied the surface composition of cathode powders aged with electrolytes at 60 oC. Our study shows that electrodes cycled beyond 150 cycles showed a rapid drop in capacity due to increase in the surface film resistance resulting in limited capacity utilization.