Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron mobility”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

High Temperature Operation of Al 0.45 Ga 0.55 N/Al 0.30 Ga 0.70 N High Electron Mobility Transistors

AlGaN-channel high electron mobility transistors (HEMTs) are among a class of ultra wide-bandgap transistors that have a bandgap greater than ~3.4 eV, beyond that of GaN and SiC, and are promising candidates for RF and power applications. Long-channel Al x Ga 1-x N HEMTs with x = 0.3 in the channel have been built and evaluated across the -50°C to +200°C temperature range. Room temperature drain current of 70 mA/mm, absent of gate leakage, and with a modest -1.3 V threshold voltage was measured. A very large I on /I off current ratio, greater than 10 8 was demonstrated over the entire temperature range, indicating that off-state leakage is below the measurement limit even at 200°C. Finally, combined with near ideal subthreshold slope factor that is just 1.3× higher than the theoretical limit across the temperature range, the excellent leakage properties are an attractive characteristic for high temperature operation.

36 MATERIALS SCIENCE↗

Effect of buffer structures on AlGaN/GaN high electron mobility transistor reliability

AlGaN/GaN high electron mobility transistors (HEMTs) with three different types of buffer layers, including a GaN/AlGaN composite layer, or 1 or 2 lm GaN thick layers, were fabricated and their reliability compared. The HEMTs with the thick GaN buffer layer showed the lowest critical voltage (Vcri) during off-state drain step-stress, but this was increased by around 50% and 100% for devices with the composite AlGaN/GaN buffer layers or thinner GaN buffers, respectively. The Voff - state for HEMTs with thin GaN and composite buffers were 100 V, however, this degraded to 50 60V for devices with thick GaN buffers due to the difference in peak electric field near the gate edge. A similar trend was observed in the isolation breakdown voltage measurements, with the highest Viso achieved based on thin GaN or composite buffer designs (600 700 V), while a much smaller Viso of 200V was measured on HEMTs with the thick GaN buffer layers. These results demonstrate the strong influence of buffer structure and defect density on AlGaN/GaN HEMT performance and reliability.

Liu, L.↗

High-electron-mobility GaN grown on free-standing GaN templates by ammonia-based molecular beam epitaxy

The dependence of electron mobility on growth conditions and threading dislocation density (TDD) was studied for n{sup −}-GaN layers grown by ammonia-based molecular beam epitaxy. Electron mobility was found to strongly depend on TDD, growth temperature, and Si-doping concentration. Temperature-dependent Hall data were fit to established transport and charge-balance equations. Dislocation scattering was analyzed over a wide range of TDDs (∼2 × 10{sup 6} cm{sup −2} to ∼2 × 10{sup 10} cm{sup −2}) on GaN films grown under similar conditions. A correlation between TDD and fitted acceptor states was observed, corresponding to an acceptor state for almost every c lattice translation along each threading dislocation. Optimized GaN growth on free-standing GaN templates with a low TDD (∼2 × 10{sup 6} cm{sup −2}) resulted in electron mobilities of 1265 cm{sup 2}/Vs at 296 K and 3327 cm{sup 2}/Vs at 113 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Double pulse doped InGaAs/AlGaAs/GaAs pseudomorphic high-electron-mobility transistor heterostructures

Double pulse doped ({delta}-doped) InGaAs/AlGaAs/GaAs pseudomorphic high-electron-mobility transistor (HEMT) heterostructures were grown by molecular-beam epitaxy using a multiwafer technological system. The room-temperature electron mobility was determined by the Hall method as 6550 and 6000 cm{sup 2}/(V s) at sheet electron densities of 3.00 x 10{sup 12} and 3.36 x 10{sup 12} cm{sup -2}, respectively. HEMT heterostructures fabricated in a single process feature high uniformity of structural and electrical characteristics over the entire area of wafers 76.2 mm in diameter and high reproducibility of characteristics from process to process.

36 MATERIALS SCIENCE↗

Features of the Electron Mobility in the n-InSe Layered Semiconductor

The dependences of the Hall electron mobility of n-InSe single crystals grown by the Bridgman method on a sample’s technological history, temperature, electric field, doping, and illumination are experimentally investigated. It is established that at temperatures below room temperature, the dependences of the electron mobility on external factors, initial resistivity, and doping are anomalous, i.e., do not obey the theory of free carrier mobility in quasi-ordered crystalline semiconductors. The observed anomalies are attributed to partial disordering and fluctuation of the potential of free energy bands of the n-InSe single crystals and can be controlled by temperature, electric field, doping, and illumination.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Role of Fe impurity complexes in the degradation of GaN/AlGaN high-electron-mobility transistors

Recent experiments show that GaN/AlGaN high-electron-mobility transistors suffer from significant current collapse, which is caused by an increase in the concentration of traps with energy levels 0.5–0.6 eV below the conduction-band edge. This increase in trap concentration is consistent with thermally activated defect diffusion, but the responsible defect complexes have not been identified. It has been suggested that the defect complex may contain iron because of the proximity of the Fe-doped GaN substrate. Here, we report first-principles density-functional calculations of substitutional iron complexes, investigate their properties, and show that the Fe{sub Ga}-V{sub N} complex has properties that account for the observed degradation.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Electron mobility and free-carrier absorption in GaAs - Determination of the compensation ratio

Theoretical calculations of electron mobility and free-carrier absorption in n-type GaAs at room temperature were carried out taking into consideration all major scattering processes. It was found that satisfactory agreement between theoretical and experimental results on free-carrier absorption is obtained only when the effect of compensation is quantitatively taken into account. In conjunction with experimental studies it is shown that the electron mobility (for n greater than 10 to the 15th per cu cm) and free-carrier absorption (for n greater than 10 to the 16th per cu cm) are sufficiently sensitive to the ionized impurity concentration to provide a reliable means for determining the compensation ratio. Convenient procedures are presented for the determination of the compensation ratio from the free-carrier absorption coefficient and from the computed values of room-temperature electron mobility. Values of the compensation ratio obtained by these two procedures are in good agreement provided the carrier-concentration variations in the material are not appreciably greater than 10%.

Walukiewicz, W.↗

High electron mobility of Al x Ga1− x N evaluated by unfolding the DFT band structure

We calculate the alloy-disorder-limited electron mobility of AlxGa1−xN from first principles. AlxGa1−xN is a technologically important ultra-wide-bandgap alloy with promise in light emitting diodes and high-power transistors. Alloying introduces statistical disorder, which causes electrons to scatter between different crystal-momentum states, leading to a reduction in mobility for intermediate alloy compositions. The corresponding lifetime, which appears as an energy broadening in the band structure, can be evaluated by unfolding the band structure from the supercell basis to the primitive-cell basis. We fit the first-principles band broadening with a model scattering potential and evaluate the low-field electron mobility using the semiclassical Boltzmann transport equation in the relaxation-time approximation. Our calculated mobility is in agreement with experimental values. We also find the lowest alloy-scattering electron mobility (total electron mobility) across the entire composition range to be 186 cm2/V s (136 cm2/V s), which is comparable to the highest electron mobility predicted in the competitor system, β-(AlxGa1−x)2O3. Our results elucidate the intrinsic limits imposed by alloy disorder on electron transport in AlxGa1−xN.

Pant, Nick (ORCID:0000000254506045)↗

Time evolution of off-state degradation of AlGaN/GaN high electron mobility transistors

The evolution of AlGaN/GaN high electron mobility transistors under off-state stress conditions is studied by gate leakage current (I{sub g}) monitoring, electroluminescence (EL), and atomic force microscope (AFM) imaging at room temperature. It is found that the number of off-state failure sites as identified by EL increases over time during stress until it reaches a saturation value. I{sub g} increases accordingly during stress until this saturation number of failure sites is reached. AFM scanning of the device surface stripped of metal contacts and passivation reveals surface pits corresponding to the location of the EL spots. These pits have an elongated shape oriented towards the drain contact whose length is correlated with the distance to the adjacent pits and with the time since their appearance during the stress experiment. A model for the generation and evolution of the off-state stress-related failure sites is proposed consistent with the experimental results, bringing together surface migration of electrochemical species with trap-based leakage mechanisms and resulting in the formation of an exclusion zone around each failure site.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Regiospecific Incorporation of Acetylene Linker in High‐Electron Mobility Dimerized Acceptors for Organic Solar Cells with High Efficiency (18.8%) and Long 1‐Sun Lifetime (> 5000 h)

Abstract The commercialization of organic solar cells (OSCs) requires both high power conversion efficiency (PCE) and long‐term stability. However, the lifetime of the OSCs containing small‐molecule acceptors (SMA) should be significantly enhanced. In this study, a series of planarity‐controlled is developed, high electron mobility dimerized SMAs (DSMAs) and realize OSCs with high‐performance (PCE = 18.8%) and high‐stability ( t 80% lifetime = 5380 h under 1‐Sun illumination). An acetylene linker with a planar triple bond is designed for dimerization of SMA units to afford the high backbone planarity necessary to achieve high crystallinity and electron mobility. To further engineer the molecular conformation and electron mobility of the DSMAs, different regioisomers of a Y‐based SMA are dimerized to yield three regioisomerically distinct DSMAs, denoted as DYA‐I, DYA‐IO, and DYA‐O, respectively. It is found that the crystallinity, electron mobility, and glass transition temperature of the DSMAs gradually increase in the order of DYA‐O, DYA‐IO, and DYA‐I, which, in turn, enhance the PCE and device stability of the resulting OSCs; DYA‐O (PCE = 16.45% and t 80% lifetime = 3337 h) < DYA‐IO (PCE = 17.54% and t 80% lifetime = 4255 h) < DYA‐I (PCE = 18.83% and t 80% lifetime = 5380 h).

Chemistry↗

Enhancing Electron Mobility at the LaAlO 3 /SrTiO 3 Interface by Surface Control

Mobility of electrons confined at the LaAlO 3 /SrTiO 3 interface is significantly enhanced by surface control using surface charges and adsorbates, reaching a low temperature value more than 20 000 cm 2 V -1 s -1 . A uniform trend that mobility increases with decreasing sheet carrier density is observed.

36 MATERIALS SCIENCE↗

Molecular beam epitaxy growth of high electron mobility InAs/AlSb deep quantum well structure

InAs/AlSb deep quantum well (QW) structures with high electron mobility were grown by molecular beam epitaxy (MBE) on semi-insulating GaAs substrates. AlSb and Al{sub 0.75}Ga{sub 0.25}Sb buffer layers were grown to accommodate the lattice mismatch (7%) between the InAs/AlSb QW active region and GaAs substrate. Transmission electron microscopy shows abrupt interface and atomic force microscopy measurements display smooth surface morphology. Growth conditions of AlSb and Al{sub 0.75}Ga{sub 0.25}Sb buffer were optimized. Al{sub 0.75}Ga{sub 0.25}Sb is better than AlSb as a buffer layer as indicated. The sample with optimal Al{sub 0.75}Ga{sub 0.25}Sb buffer layer shows a smooth surface morphology with root-mean-square roughness of 6.67 A. The electron mobility has reached as high as 27 000 cm{sup 2}/Vs with a sheet density of 4.54 Multiplication-Sign 10{sup 11}/cm{sup 2} at room temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The unexpected beneficial effect of the L-valley population on the electron mobility of GaAs nanowires

The impact of the L-valley population on the transport properties of GaAs cylindrical nanowires (NWs) is analyzed by numerically calculating the electron mobility under the momentum relaxation time approximation. In spite of its low contribution to the electron mobility (even for high electron populations in small NWs), it is demonstrated to have a beneficial effect, since it significantly favours the Γ-valley mobility by screening the higher Γ-valley energy subbands.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ultra-low noise high electron mobility transistors for high-impedance and low-frequency deep cryogenic readout electronics

We report on the results obtained from specially designed high electron mobility transistors at 4.2 K: the gate leakage current can be limited lower than 1 aA, and the equivalent input noise-voltage and noise-current at 1 Hz can reach 6.3 nV/Hz{sup 1∕2} and 20 aA/Hz{sup 1∕2}, respectively. These results open the way to realize high performance low-frequency readout electronics under very low-temperature conditions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Improvement of electron mobility in La:BaSnO{sub 3} thin films by insertion of an atomically flat insulating (Sr,Ba)SnO{sub 3} buffer layer

One perovskite oxide, ASnO{sub 3} (A = Sr, Ba), is a candidate for use as a transparent conductive oxide with high electron mobility in single crystalline form. However, the electron mobility of films grown on SrTiO{sub 3} substrates does not reach the bulk value, probably because of dislocation scattering that originates from the large lattice mismatch. This study investigates the effect of insertion of bilayer BaSnO{sub 3} / (Sr,Ba)SnO{sub 3} for buffering this large lattice mismatch between La:BaSnO{sub 3} and SrTiO{sub 3} substrate. The insertion of 200-nm-thick BaSnO{sub 3} on (Sr,Ba)SnO{sub 3} bilayer buffer structures reduces the number of dislocations and improves surface smoothness of the films after annealing as proved respectively by scanning transmission electron microscopy and atomic force microscopy. A systematic investigation of BaSnO{sub 3} buffer layer thickness dependence on Hall mobility of the electron transport in La:BaSnO{sub 3} shows that the highest obtained value of mobility is 78 cm{sup 2}V{sup −1}s{sup −1} because of its fewer dislocations. High electron mobility films based on perovskite BaSnO{sub 3} can provide a good platform for transparent-conducting-oxide electronic devices and for creation of fascinating perovskite heterostructures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of proton irradiation on dc characteristics of InAlN/GaN high electron mobility transistors

The effects of proton irradiation on the dc characteristics of InAlN/GaN high electron mobility transistors were investigated. In this study we used 5 MeV protons with doses varying from 21011 to 21015 cm2. The transfer resistance and contact resistivity suffered more degradation as compared to the sheet resistance. With irradiation at the highest dose of 21015 cm2, both forward- and reverse-bias gate currents were increased after proton irradiation. A negative threshold-shift and reduction of the saturation drain current were also observed as a result of radiation-induced carrier scattering and carrier removal. Devices irradiated with doses of 21011 to 21015 cm2 exhibited minimal degradation of the saturation drain current and extrinsic trans- conductance. These results show that InAlN/GaN high electron mobility transistors are attractive for space-based applications when high-energy proton fluxes are present. VC 2011 American Vacuum Society. [DOI: 10.1116/1.3644480]

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Density dependence of electron mobility in the accumulation mode for fully depleted SOI films

The electron mobility µ{sub eff} in the accumulation mode is investigated for undepleted and fully depleted double-gate n{sup +}–n–n{sup +} silicon-on-insulator (SOI) metal–oxide–semiconductor field-effect transistors (MOSFET). To determine the range of possible values of the mobility and the dominant scattering mechanisms in thin-film structures, it is proposed that the field dependence of the mobility µ{sub eff} be replaced with the dependence on the density N{sub e} of induced charge carriers. It is shown that the dependences µ{sub eff}(N{sub e}) can be approximated by the power functions µ{sub eff}(N{sub e}) ∝ N{sub e}{sup -n}, where the exponent n is determined by the chargecarrier scattering mechanism as in the mobility field dependence. The values of the exponent n in the dependences µ{sub eff}(N{sub e}) are determined when the SOI-film mode near one of its surfaces varies from inversion to accumulation. The obtained results are explained from the viewpoint of the electron-density redistribution over the SOI-film thickness and changes in the scattering mechanisms.

36 MATERIALS SCIENCE↗

InAlN high electron mobility transistor Ti/Al/Ni/Au Ohmic contact optimisation assisted by in-situ high temperature transmission electron microscopy

This paper correlates the micro-structural and electrical characteristics associated with annealing of metallic multi-layers typically used in the formation of Ohmic contacts to InAlN high electron mobility transistors. The multi-layers comprised Ti/Al/Ni/Au and were annealed via rapid thermal processing at temperatures up to 925 °C with electrical current-voltage analysis establishing the onset of Ohmic (linear IV) behaviour at 750–800 °C. In-situ temperature dependent transmission electron microscopy established that metallic diffusion and inter-mixing were initiated near a temperature of 500 °C. Around 800 °C, inter-diffusion of the metal and semiconductor (nitride) was observed, correlating with the onset of Ohmic electrical behaviour. The sheet resistance associated with the InAlN/AlN/GaN interface is highly sensitive to the anneal temperature, with the range depending on the Ti layer thickness. The relationship between contact resistivity and measurement temperature follow that predicted by thermionic field emission for contacts annealed below 850 °C, but deviated above this due to excessive metal-semiconductor inter-diffusion.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗