Not Available
Quarternary lithium-ion battery electrolyte solutions containing ester co-solvents in mixtures of carbonates have been demonstrated to have high conductivity at low temperatures (<-20 degrees Celcius).
Application of advanced anode and cathode materials in commercial lithium-ion batteries is attracting attention due to their high capacity. Silicon (Si)/graphite anodes and nickel (Ni)-rich lithium nickel manganese cobalt oxide with layered structures have been paired in commercial 18650 high energy density cells (~270 Wh/kg). It is crucial to investigate the cell performance and the aging behavior of this commercial cell. In this study, we present commercial cell degradation mechanisms by comparing fresh and aged electrodes, including changes of crystal structure, morphology, elemental composition, and electrochemical properties. The quantitative analysis was done based on dV/dQ incremental capacity analysis of 18650 cells. To determine the amount of cyclable lithium ions (Li + ) and active material loss, the lithiation and delithiation capacity were compared for fresh and aged electrodes in half coin cells. Results showed that even with 5% (by mass) of Si added in the anode, cracks occurred across the anode leading to contact loss and thickening of the solid electrolyte interphase (SEI) layer. Additionally, the average fluorine (F) ratio of the aged anodes was higher compared to that of the fresh anodes. More severely, the F content on the Si aggregations on aged anodes increased to as high as 5 times that of the fresh anode, indicating SEI growth, especially on Si particles. Solid 7 Li nuclear magnetic resonance results showed no detectable Li metal deposition on the aged anode. On the cathode side, cracks on the primary particle interfaces contributed to cathode material loss, contact loss, and impedance rise. Furthermore, Li + loss into the thickened SEI layer, particle cracking, and impedance rise are the main reasons behind cell degradation.
Solid Electrolyte Interphase (SEI) has been identified as the most important and least understood component in lithium-ion batteries. Despite extensive studies in the past two decades, a few mysteries remain: what is the chemical form of and degree of mobility of Li + in the interphase? What fraction of Li + is permanently immobilized in the SEI, while the rest are still able to participate in the cell reactions via the ion-exchange process with Li + in the electrolyte? This study attempted to answer, in part, these questions by using 6 Li and 7 Li-isotopes to label SEIs and electrolytes, and then quantifying the distribution of permanently immobilized and ion-exchangeable Li + with solid-state NMR and ToF-SIMS. The results showed that the majority of Li + were exchanged after one SEI formation cycle, and a complete exchange after 25 cycles. Ion exchange by diffusion based on concentration gradient in the absence of applied potential also occurred simultaneously. This knowledge will provide a foundation for not only understanding but also designing better SEIs for future battery chemistries.
Vinylene Carbonate (VC) was added to the electrolyte in graphite-lithium half-cells. We report its effect on the coulombic efficiency (as capacity shift) of graphite electrodes under various formation cycling conditions. Cyclic voltammetry on glassy carbon showed that VC passivates the electrode against electrolyte reduction. The dQ/dV plots of the first lithiation of the graphite suggest that VC alters the SEI layer, and that by varying the cell formation rate, the initial ratio of ethylene carbonate to VC in the SEI layer can be controlled. VC was found to decrease first cycle efficiency and reversible capacity (in ongoing cycling) when used to excess. However, experiments with VC additive used with various formation rates did not show any decrease in capacity shift.
Quarternary lithium-ion battery electrolyte solutions containing ester co-solvents in mixtures of carbonates have been demonstrated to have high conductivity at low temperatures (< -20C). However, in some cases the presence of such co-solvents does not directly translate into improved low temperature cell performance, presumably due to the formation of ionically resistive surface films on carbonaceous anodes. In order to understand this behavior, a number of lithium-graphite cells have been studied containing electrolytes with various ester co-solvents, including methyl acetate (MA), ethyl acetate (EA), ethyl propionate (EP), and ethyl butyrate (EB). The charge/discharge characterization of these cells indicates that the higher molecular weight esters result in electrolytes which possess superior low temperature performance in contrast to the lower molecular weight ester-containing solutions, even though these solutions display lower conductivity values.
Graphites MCMB-2810 and OMAC-15 (made by Osaka Gas Inc.), and SNG12 (Hydro Quebec, Inc.) were evaluated (in coin cells with lithium counter electrodes) as anode materials for lithium-ion cells intended for use in hybrid electric vehicles. Though the reversible capacity obtained for SNG was slightly higher than that of OMAC or MCMB, its 1st cycle efficiency was lower. Voltage vs capacity plots of cycling data show that the discharge and charge limits shift to higher capacity values due to continuation of anode side reactions. Varying the cycle charge and discharge limits was found to have no significant effect on fractional capacity shift per cycle.
Charging energy-dense lithium-ion batteries (LIBs) with thick graphite electrodes at high current densities are typically accompanied by poor performance and safety issues. The root cause is the onset of Li plating at the surface of graphite when lithiated to a high capacity within a short time period. Here, we investigated the behavior of graphite electrodes with various particle sizes under fast charge operations. Results from the electrochemical characterization on graphite electrodes exhibit the superiority of smaller particles over bigger particles in terms of suppressing the onset of Li plating and growth of plated Li particles. Observations from scanning electron microscopy also corroborate the presence of plated Li in electrodes with big graphite particles and its absence in graphite electrodes with small particles, when the cells were lithiated to 90% of the state of charge (SOC). Further, the improved performance of cells with the small particles might be associated with the low Li-ion concentration at the surface of graphite and thus reduced overpotential in graphite electrodes. The simulated results revealed that, compared to bigger particles, smaller particles have lower surface intercalation at any given cell SOC, which may significantly reduce the overpotential in the graphite electrodes and mitigate the onset of Li plating. This agrees well with experimental observations.
This project accomplished the goal of developing SPM imaging and analysis of local composition of the SEI layer on graphite electrodes in model and composite Li-ion electrodes during charge/discharge process. A scanning probe microscope was used to detect and image chemical composition and structure changes in the SEI layer on graphite electrode at different state of charge.
A barrier to the widespread adoption of electric vehicles is enabling fast charging lithium-ion batteries. At normal charging rates, lithium ions intercalate into the graphite electrode. At high charging rates, lithiation is inhomogeneous, and metallic lithium can plate on the graphite particles, reducing capacity and causing safety concerns. We have built a cell for conducting high-resolution in situ X-ray microtomography experiments to quantify three-dimensional lithiation inhomogeneity and lithium plating. Our studies reveal an unexpected correlation between these two phenomena. During fast charging, a layer of mossy lithium metal plates at the graphite electrode–separator interface. The transport bottlenecks resulting from this layer lead to underlithiated graphite particles well-removed from the separator, near the current collector. These underlithiated particles lie directly underneath the mossy lithium, suggesting that lithium plating inhibits further lithiation of the underlying electrode.
Graphical abstract: The fitting results of R{sub sei} and R{sub ct} of three graphite/Li cells. Besides three graphite/Li cells show the similar R{sub sei}, the NG198/Li cell demonstrates a higher R{sub ct} value in all test temperatures. Especially, the R{sub ct} at 333 K is even up to 355.8 Ω cm{sup 2}. Obviously, the narrow distribution of edge plane for NG198 caused this result, and then greatly restricts its cell capacity. By contrast, CMB with bigger specific surface area and more Li{sup +} insertion points shows lower resistance at room temperature, which should help to improve its capacity. - Highlights: • SEI film is closely related to graphite structures and formation temperature. • The graphite with bigger surface area and more Li{sup +} insertion points behaves better. • The graphite with narrow edge plane is uncompetitive for ionic liquid electrolyte. - Abstract: The electrochemical behaviors of natural graphite (NG198), artificial graphite (AG360) and carbon microbeads (CMB) in an ionic liquid based electrolyte are investigated by cyclic voltammetry (CV). The surface and structure of three graphite materials are characterized by scanning electron microscope (SEM) and X-ray diffraction (XRD) before and after cycling. It is found that solid electrolyte interface (SEI) is closely related to graphite structure. Benefiting from larger specific surface area and more dispersed Li{sup +} insertion points, CMB shows a better Li{sup +} insertion/de-insertion behavior than NG198 and AG360. Furthermore, electrochemical impedance spectra (EIS) prove that the SEI of different graphite electrodes has different intrinsic resistance and Li{sup +} penetrability. By comparison, CMB behaves better cell performances than AG360, while the narrow edge plane makes NG198 uncompetitive as a potential anode for the ionic liquids (ILs)-type Li-ion battery.
The morphology of electrode materials plays a crucial role in determining the performance of lithium-ion batteries. Traditional computational models often simplify graphite flakes as uniformly sized spheres, which limits their predictive accuracy. In this study, we present a computational workflow that overcomes these limitations by incorporating a more realistic representation of graphite morphologies. This workflow is designed to be flexible and reproducible, enabling efficient evaluation of electrochemical performance across diverse material structures. By exploring different graphite morphologies, our approach accelerates the optimization of material preparation techniques and processing conditions. Our findings reveal that incorporating greater morphological complexity leads to significant deviations from classical model predictions. Instead, our refined model offers a more accurate representation of battery discharge behavior, closely aligning with experimental data. This improvement underscores the importance of detailed morphological descriptions in advancing battery design and performance assessments. To promote accessibility and reproducibility, we provide the developed code for seamless integration with the COMSOL API, allowing researchers to implement and adapt it easily. This computational framework serves as a valuable tool for investigating the impact of graphite morphology on battery performance, bridging the gap between theoretical modeling and experimental validation to enhance lithium-ion battery technology.
We report nanosecond pulsed laser annealing significantly improves cyclability and current carrying capacity of lithium-ion batteries (LIBs). This improvement is achieved by engineering of microstructure and defect contents present in graphite in a controlled way by using pulsed laser annealing (PLA) to increase the number density of Li + ion trapping sites. The PLA treatment causes the following changes: (1) creates surface steps and grooves between the grains to improve Li + ion charging and intercalation rates; (2) removes inactive polyvinylidene difluoride (PVDF) binder from the top of graphite grains and between the grains which otherwise tends to block the Li + migration; and (3) produces carbon vacancies in (0001) planes which can provide Li + charging sites. From X-ray diffraction data, we find upshift in diffraction peak or reduction in planar spacing, from which vacancy concentration was estimated to be about 1.0%, which is higher than the thermodynamic equilibrium concentration of vacancies. The laser treatment creates single and multiple C vacancies which provide sites for Li + ions, and it also produces steps and grooves for Li + ions to enter the intercalating sites. It is envisaged that the formation of these sites enhances Li+ ion absorption during charge and discharge cycles. The current capacity increases from an average 360 mAh/g to 430 mAh/g, and C–V shows significant reduction in SEI layer formation after the laser treatment. If the vacancy concentration is too high and charge-discharge cycles are long, then trapping of electrons by Li + may occur, which can lead to Li 0 formation and Li plating causing reduction in current capacity.
Extreme fast charging (≤ 15 min) of lithium-ion batteries is highly desirable to accelerate mass-market adoption of electric vehicles. However, significant capacity fading, as well as safety issues due to the lithium plating caused by the fast charging rate, limit its implementation. In this study, we investigated the fast-charging capability of graphite materials with various particle sizes. To eliminate the Li + ion concentration gradient effect across the thickness of the electrode, ultra-thin-layer graphite electrodes were developed to investigate the "real" fast-charging capability of graphite at the particle level. Electrochemical assessments as well as microscopic characterizations revealed that smaller particles exhibited superior fast-charging performance, featuring enhanced capacity reversibility, faster charging rate, and less lithium plating under the same fast-charging conditions. It is shown that small-particle graphite (mean radius of 3.3 μm) could withstand a 4C charge (to 80 % state-of-charge) without plating, with minimal plating occurring at 6C. Thicker particles exhibited plating at lower C-rates. Since the experimental data could not directly explain whether intra-particle diffusion limitations or interfacial reaction limitations dominated the plating mechanism, the pseudo-2-dimensional model was used to evaluate the most likely plating mechanism. The model suggested that particle-level diffusion is the dominant mechanism contributing to plating at high rates. Finally, this work provides comprehensive insights into the particle size effects on fast-charging capability, offering a better understanding of fast-charging behavior and valuable guidance for designing optimal electrode architecture for high-rate lithium-ion batteries.
Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.
Fast charging of high-capacity anodes is challenging due to lithium plating reactions, which lead to poor cycling performance and safety concerns. Thus, accurate predictions of plating onset and an understanding of this electrochemical process are crucial for robust battery design. However, the most commonly used models, based on porous electrode theory (e.g., the pseudo-2D model), are notoriously difficult to calibrate due to their complexity, limiting their predictive power. This work studies the process of lithium plating during fast charging of (small-particle) graphite half-cells by measuring local reaction progression and plating behavior using optical operando techniques. These experiments employ a realistic 1D graphite electrode geometry with commercially-relevant mass loading charged at fast charge rates. It is demonstrated that the local reaction progression and plating onset can not only be predicted accurately with a p2D numerical model, but that these processes follow a simple scaling law. Remarkably, the entire reaction histories of different electrodes charged at different rates (e.g., 160 μm thickness at 0.5C, 111 μm at 1C or 66 μm at 4C) were observed to have self-similar intercalation profiles. It is demonstrated that plating onset is in turn governed by the reaction profile which explains why both processes exhibit the same scaling behavior. Finally, operando measurements of local reaction dynamics are conducted for the first time in electrodes with channeled architectures, quantitatively determining how channels affect reaction uniformity and plating onset. Together, these results reveal underlying simplicity in the complex electrochemical environment of fast charging and lithium plating, improving understanding of this process. These fundamental insights are broadly applicable for design processes, modeling and experimental evaluation of lithium ion batteries.