Structure and corrosion behavior of platinum/ruthenium/nitrogen doped diamondlike carbon thin films

Platinum/ruthenium/nitrogen doped diamondlike carbon (PtRuN-DLC) thin films were deposited on p-Si (100) substrates with dc magnetron cosputtering by varying the dc power applied to a Pt{sub 50}Ru{sub 50} target to investigate the effect of Pt and Ru incorporation in the films on the bonding structure, adhesion strength, surface morphology, and corrosion behavior of the films by means of X-ray photoelectron spectroscopy, micro-Raman spectroscopy, microscratch test, atomic force microscopy, scanning electron microscopy, and potentiodynamic polarization test. It was found that the incorporation of Pt and Ru in the N-DLC films improved the corrosion resistance of the films in a 0.1M NaCl solution at lower polarization potentials though more sp{sup 2} bonds were formed in the films. However, the films with higher Pt and Ru contents degraded earlier than the ones with lower Pt and Ru contents at higher polarization potentials.

36 MATERIALS SCIENCE↗

Eu oxidation state in fluorozirconate-based glass ceramics

The influence of InF{sub 3} doping and remelting on Eu-doped fluorozirconate-based glass ceramics was investigated using near-edge x-ray absorption and optical spectroscopy. It was found that the addition of InF{sub 3} to the melt decreases the Eu{sup 2+}/Eu{sup 3+} mole ratio, while remelting leads to a significant change in the Eu{sup 2+}/Eu{sup 3+} ratio in favor of Eu{sup 2+}. Photoluminescence spectroscopy shows that additional annealing steps lead to the formation of BaCl{sub 2} nanoparticles in the glass. In as-made glass ceramics containing InF{sub 3}, a phase transition of the nanoparticles from hexagonal to orthorhombic structure is observed. This phase transition is not observed in the remelted glasses studied here.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Enhanced visible-light absorption and dopant distribution of iodine-TiO{sub 2} nanoparticles synthesized by a new facile two-step hydrothermal method

In order to prepare visible-light responsive iodine-doped TiO{sub 2}, a new facile synthetic approach was proposed, which started with the cost-efficient and environmentally friendly precursor of undoped anatase TiO{sub 2} to form nanotube structures as templates that collapsed and recrystallized into I-TiO{sub 2} nanopowders in HIO{sub 3} solution, followed by annealing at different temperatures. The modification of TiO{sub 2} to incorporate iodine and form titanium dioxide with significantly enhanced absorption in the visible range of the spectrum was investigated. The extent of iodine dopant incorporation was determined by X-ray photoelectron spectroscopy (XPS) and energy dispersive X-ray analysis (EDX) and was found to be homogenously distributed on each nanostructure as determined by electron energy-loss spectroscopy (EELS) elemental mapping and EDX spectroscopy. The modified TiO{sub 2} exhibits a dramatically extended absorption edge beyond 800 nm as compared to the original and unmodified TiO{sub 2}. - Graphical abstract: As-synthesized I-TiO{sub 2} nanoparticles show significantly enhanced visible-light absorption, with the dopant iodine homogenously dispersed on each I-TiO{sub 2} nanostructure based on EELS elemental mapping. Highlights: > Iodine-TiO{sub 2} nanoparticles by a new facile two-step hydrothermal method. > Significantly enhanced light absorption in the visible range of the spectrum. > Homogenous dopant distribution within each nanostructure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rare-Earths Centers (Sm{sup 3+}, Eu{sup 3+}, Yb{sup 3+}) in MeF{sub 2}(Me = Ca, Sr, Ba, Cd) Crystals

Rare-earth elements RE{sup 3+}(RE = Sm, Eu, Yb) form impurity centers in fluorite-like crystals MeF{sub 2}(Me = Ca, Sr, Ba, Cd). The crystal structure of cubic, trigonal and tetragonal centers in MeF{sub 2} has been investigated in the framework of shell model and pair potential approximation. The crystal field parameters were calculated with the exchange charges model, using the optimized geometry of the doped host matrix. With these parameters we have been calculated the optical spectra and spin-Hamiltonian (g-factors) of RE{sup 3+} in MeF{sub 2}, for some combination of R{sup 3+} and MeF{sup 2}. The obtained results were discussed and comparison with experimental data was made. A good agreement confirms the method and model of calculations.

36 MATERIALS SCIENCE↗

Simultaneous pore enlargement and introduction of highly dispersed Fe active sites in MSNs for enhanced catalytic activity

An effective post-hydrothermal treatment strategy has been developed to dope highly dispersed iron catalytical centers into the framework of mesoporous silica, to keep the particle size in nanometric scale, and in the meanwhile, to expand the pore size of the synthesized mesoporous silica nanoparticles (MSNs). Characterization techniques such as XRD, BET, SEM and TEM support that the synthesized samples are long period ordered with particles size about 100 nm and a relatively large pore size of ca. 3.5 nm. UV-vis, XPS and EPR measurements demonstrate that the introduced iron active centers are highly dispersed in a coordinatively unsaturated status. NH{sub 3}-TPD verifies that the acid amount of iron-doped MSNs is quite high. The synthesized nanocatalysts show an excellent catalytic performance for benzylation of benzene by benzyl chloride, and they present relatively higher yield and selectivity to diphenylmethane with a lower iron content and much shorter reaction time. - Graphical abstract: Uniform MSNs with iron active centers and large pore size have been prepared by a newly developed strategy, which demonstrates enhanced catalytic performance for benzylation of benzene by benzyl chloride. Highlights: Black-Right-Pointing-Pointer Iron species were introduced into the framework of mesoporous silica nanoparticles with uniform dispersion. Black-Right-Pointing-Pointer The pore sizes of the synthesized nanocatalysts were expanded. Black-Right-Pointing-Pointer The acidic site quantities were quite high and the acidic centers were accessible. Black-Right-Pointing-Pointer The nanocatalysts presented higher yield and selectivity to diphenylmethane with significantly lower Fe content.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

First-principles electronic structure and formation energies of group V and VII impurities in the α-Fe{sub 2}O{sub 3} alloys

Based on density functional theory, the electronic structures, formation energy, and transition level of the selected group V and VII impurities in α-Fe{sub 2}O{sub 3} are investigated by means of first-principles methods. Numerical results show that the group V and VII atoms-doped α-Fe{sub 2}O{sub 3} can be energetically favorable under the Fe-rich condition. Group V atom substituting O atom can induce the acceptor impurity level, while the deep donor impurity states are formed inside the band gap when group VII atom substitute O atom in the α-Fe{sub 2}O{sub 3}. Moreover, our results show that halogen atom F substituting O atom should be very easy in the α-Fe{sub 2}O{sub 3}. In addition, our results also show that for both group V and VII atom-doped α-Fe{sub 2}O{sub 3}, the upper sides of valence band are modified obviously, while the conduction band edge does not change.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Spectrally dependent photovoltages in Schottky photodiode based on (100) B-doped diamond

Spectrally and spatially resolved photovoltages were measured by Kelvin probe force microscopy (KPFM) on a Schottky photo-diode made of a 4 nm thin tungsten-carbide (WC) layer on a 500 nm oxygen-terminated boron-doped diamond epitaxial layer (O-BDD) that was grown on a Ib (100) diamond substrate. The diode was grounded by the sideways ohmic contact (Ti/WC), and the semitransparent Schottky contact was let unconnected. The electrical potentials across the device were measured in dark (only 650 nm LED of KPFM being on), under broad-band white light (halogen lamp), UV (365 nm diode), and deep ultraviolet (deuterium lamp) illumination. Illumination induced shift of the electrical potential remains within 210 mV. We propose that the photovoltage actually corresponds to a shift of Fermi level inside the BDD channel and thereby explains orders of magnitude changes in photocurrent.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structure-composition-luminescence correlations in Sr{sub 2.5-3x/2}Ba{sub 0.5}Sm{sub x}Al{sub 1-y}In{sub y}O{sub 4}F (0.001{<=}x, y{<=}0.1) oxyfluorides

Luminescent materials composed of Sr{sub 2.5-3x/2}Ba{sub 0.5}Sm{sub x}Al{sub 1-y}In{sub y}O{sub 4}F (0.001{<=}x, y{<=}0.1) were prepared by the solid-state reaction method. After the replacement of Sr{sup 2+} and Al{sup 3+} ions by Sm{sup 3+} and In{sup 3+} ions in Sr{sub 2.5}Ba{sub 0.5}AlO{sub 4}F host structure, a novel charge-transfer band centered around 304 nm shifted from 240 nm is monitored; moreover, sharp and well-resolved emission peaks in the {sup 4}G{sub 5/2}{yields}{sup 6}H{sub J} transitions of the Sm{sup 3+} activator are observed. The diverse excitation and emission photoluminescence spectra of Sr{sub 2.5-3x/2}Ba{sub 0.5}Sm{sub x}Al{sub 1-y}In{sub y}O{sub 4}-{alpha}F1-{delta} (0.001{<=}x, y{<=}0.1) phosphors originated by the charge-transfer of the host to the Sm{sup 3+} activator, the f-f transitions in the Sm{sup 3+} ions, and the defect-induced self-activation are also introduced. - Graphical abstract: After the replacement of Sr{sup 2+} and Al{sup 3+} ions by Sm{sup 3+} and In{sup 3+} ions in Sr{sub 2.5}Ba{sub 0.5}AlO{sub 4}F host structure, a novel charge-transfer band centered around 304 nm shifted from 240 nm is monitored; moreover, sharp and well-resolved emission peaks in the {sup 4}G{sub 5/2}{yields}{sup 6}H{sub J} transitions of the Sm{sup 3+} activator are observed (Figure, Left). The diverse excitation and emission photoluminescence spectra of Sr{sub 2.5-3x/2}Ba{sub 0.5}Sm{sub x}Al{sub 1-y}In{sub y}O{sub 4}-{alpha}F1-{delta} (0.001{<=}x, y{<=}0.1) phosphors originated by the charge-transfer of the host to the Sm{sup 3+} activator, the f-f transitions in the Sm{sup 3+} ions, and the defect-induced self-activation are also introduced. Highlights: Black-Right-Pointing-Pointer Strong and well-resolved emitting peaks are monitored in Sm{sup 3+}-doped oxyfluoride phosphors. Black-Right-Pointing-Pointer Diverse excitation and emission spectra of the oxyfluoride phosphors originated from Sm{sup 3+} activator and the defect-induced self-activation were clearly monitored. Black-Right-Pointing-Pointer Oxyfluoride phosphors could be quite effective to prepare white-emitting light for (near)-UV LED applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improved photoelectrochemical responses of Si and Ti codoped alpha-Fe{sub 2}O{sub 3} photoanode films

We studied photoelectrochemical performance of the undoped, Si-doped, Ti-doped, and codoped alpha-Fe{sub 2}O{sub 3} film prepared by ultrasonic spray pyrolysis. Since the ions radius of Si{sup 4+}<Fe{sup 3+}<Ti{sup 4+}, Si and Ti codoping can balance the ion radius difference between Fe{sup 3+} and Si{sup 4+} (or Ti{sup 4+}) and increase the donor concentration. Their donor concentrations, calculated from slopes of the Mott-Schottky plots, are 9.10x10{sup 18} cm{sup -3}, 1.89x10{sup 20} cm{sup -3}, 2.04x10{sup 20} cm{sup -3}, and 7.06x10{sup 20} cm{sup -3}, respectively. Incident photon to current efficiency of the codoped film is 34% at 365 nm and 0.6 V versus Ag/AgCl, much higher than 10%, 20%, and 22% for the undoped, Si-doped, and Ti-doped film, respectively.

36 MATERIALS SCIENCE↗

Dielectric and conductivity relaxation in AgI doped silver selenite superionic glasses

Non-Debye relaxation in superionic AgI-Ag{sub 2}O-SeO{sub 2} glasses has been investigated as a function of frequency and temperature. The experimental data have been analyzed in the framework of complex dielectric permittivity and complex electric modulus formalisms. The dielectric permittivity data have been well interpreted using the Havriliak-Negami function. The electric modulus data have been analyzed by invoking Kohlrausch-Williams-Watts function and various parameters describing the relaxation mechanism have been obtained. The temperature and compositional variation in relaxation times and the activation energy, obtained from dielectric permittivity as well as from electric modulus data, have been compared. The low value of stretched exponential parameter implies a highly nonexponential nature of relaxation and is attributed to the correlated ionic motion. The values of the stretched exponential parameter are observed to be independent of temperature as well as composition. Different scaling formalisms have been applied to understand the temperature and compositional dependence of the relaxation mechanism. The scaling of dielectric loss spectra and electric modulus spectra results in master curves, which signifies that the relaxation mechanism is independent of temperature as well as composition.

36 MATERIALS SCIENCE↗

Improving Er{sup 3+} 1.53 {mu}m luminescence by CeF{sub 3} nanocrystallization in aluminosilicate glass

In order to develop promising materials for the Er{sup 3+}-doped fiber amplifier, transparent glass ceramics containing hexagonal CeF{sub 3} nanocrystals were prepared by melt-quenching and subsequent heating. The obvious Stark splitting in the absorption and emission spectra, the intensification of the 1.53 {mu}m emission, and the prolongation of the Er{sup 3+}:{sup 4}I{sub 13/2} decay lifetime demonstrated the partition of Er{sup 3+} ions into the CeF{sub 3} nanocrystals. Evidently, the efficient cross-relaxation between Ce{sup 3+} and Er{sup 3+}, i.e., Er{sup 3+}:{sup 4}I{sub 11/2}+Ce{sup 3+}:{sup 2}F{sub 5/2}{yields}Er{sup 3+}:{sup 4}I{sub 13/2}Ce{sup 3+}:{sup 2}F{sub 7/2} led to the quenching of the upconversion and the enhancing of the desired Er{sup 3+} 1.53 {mu}m emission. Based on the emission and absorption spectra, it was further calculated that the glass ceramic possesses broad bandwidth as that of the ZBLAN glass, and large emission cross-section close to the silicate glass, for the 1.53 {mu}m emission.

36 MATERIALS SCIENCE↗

Stimulated emission in the red, green, and blue in a nanostructured glass ceramics

Red, green, and blue stimulated emissions have been achieved in Ho{sup 3+} doped oxyfluoride glass ceramic at room temperature. The material shows three emission bands at the red (650 nm), green (545 nm), and blue (488 nm) regions under infrared excitation at 750 nm. These emission bands are caused by a photon avalanche upconversion process previously reported. A pump and probe experimental setup has been designed to show stimulated emissions at the three bands. The pump power threshold for positive gain in the 490 nm band has been estimated around 2.7 kW/cm{sup 2}. Higher thresholds are expected for the other bands.

74 ATOMIC AND MOLECULAR PHYSICS↗

A Model for Atomic Precision p-Type Doping with Diborane on Si(100)-2×1

Diborane (B 2 H 6 ) is a promising molecular precursor for atomic precision p-type doping of silicon that has recently been experimentally demonstrated. In this study, we use density functional theory (DFT) calculations to determine the reaction pathway for diborane dissociating into a species that will incorporate as electrically active substitutional boron after adsorbing onto the Si(100)-2×1 surface. Our calculations indicate that diborane must overcome an energy barrier to adsorb, explaining the experimentally observed low sticking coefficient (<1 × 10 –4 at room temperature) and suggesting that heating can be used to increase the adsorption rate. Upon sticking, diborane has an ≈50% chance of splitting into two BH 3 fragments versus merely losing hydrogen to form a dimer such as B 2 H 4 . As boron dimers are likely electrically inactive, whether this latter reaction occurs is shown to be predictive of the incorporation rate. The dissociation process proceeds with significant energy barriers, necessitating the use of high temperatures for incorporation. Using the barriers calculated from DFT, we parameterize a Kinetic Monte Carlo model that predicts the incorporation statistics of boron as a function of the initial depassivation geometry, dose, and anneal temperature. Our results suggest that the dimer nature of diborane inherently limits its doping density as an acceptor precursor and furthermore that heating the boron dimers to split before exposure to silicon can lead to poor selectivity on hydrogen and halogen resists. This suggests that, while diborane works as an atomic precision acceptor precursor, other non-dimerized acceptor precursors may lead to higher incorporation rates at lower temperatures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Determining the structure of tetragonal Y{sub 2}WO{sub 6} and the site occupation of Eu{sup 3+} dopant

The compound Y{sub 2}WO{sub 6} is prepared by solid state reaction at 750 {sup o}C using sodium chloride as mineralizer. Its structure is solved by ab-initio methods from X-ray powder diffraction data. This low temperature phase of yttrium tungstate crystallizes in tetragonal space group P4/nmm (No. 129), Z=2, a=5.2596(2) A, c=8.4158(4) A. The tungsten atoms in the structure adopt an unusual [WO{sub 6}] distorted cubes coordination, connecting [YO{sub 6}] distorted cubes with oxygen vacancies at the O{sub 2} layers while other yttrium ions Y{sub 2} form [YO{sub 8}] cube coordination. Y{sup 3+} ions occupy two crystallographic sites of 2c (C{sub 4v} symmetry) and 2a (D{sub 2d} symmetry) in the Y{sub 2}WO{sub 6} host lattice. With Eu{sup 3+} ions doped, the high resolution emission spectrum of Y{sub 2}WO{sub 6}:Eu{sup 3+} suggests that Eu{sup 3+} partly substituted for Y{sup 3+} in these two sites. The result of the Rietveld structure refinement shows that the Eu{sup 3+} dopants preferentially enter the 2a site. The uniform cube coordination environment of Eu{sup 3+} ions with the identical eight Eu-O bond lengths is proposed to be responsible for the intense excitation of long wavelength ultraviolet at 466-535 nm. -- Graphical abstract: The excitation and emission spectra of Y{sub 2}WO{sub 6}:Eu{sup 3+} indicates the effect of long wavelength-excited property, which is ascribed to the cube coordination environment of Eu{sup 3+} ions with the uniform Eu-O bond length. Display Omitted Research highlights: Y{sub 2}WO{sub 6} is prepared using sodium chloride as mineralizer. The structure of the compound Y{sub 2}WO{sub 6} is solved by ab-initio methods. The site occupation of Eu{sup 3+} is determined. The cube coordination of Eu{sup 3+} ions is responsible for the long wavelength excitation.

36 MATERIALS SCIENCE↗

Judd-Ofelt analysis, frequency upconversion, and infrared photoluminescence of Ho{sup 3+}-doped and Ho{sup 3+}/Yb{sup 3+}-codoped lead bismuth gallate oxide glasses

Ho{sup 3+}-doped and Ho{sup 3+}/Yb{sup 3+}-codoped lead bismuth gallate (PBG) oxide glasses were prepared and their spectroscopic properties were investigated. The derived Judd-Ofelt intensity parameters (OMEGA{sub 2}=6.81x10{sup -20} cm{sup 2}, OMEGA{sub 4}=2.31x10{sup -20} cm{sup 2}, and OMEGA{sub 6}=0.67x10{sup -20} cm{sup 2}) indicate a higher asymmetry and stronger covalent environment for Ho{sup 3+} sites in PBG glass compared with those in tellurite, fluoride (ZBLAN), and some other lead-contained glasses. Intense frequency upconversion emissions peaking at 547, 662, and 756 nm as well as infrared emissions at 1.20 and 2.05 mum in Ho{sup 3+}/Yb{sup 3+}-codoped PBG glass were observed, confirming that energy transfer between Yb{sup 3+} and Ho{sup 3+} takes place, and a two-phonon-assisted energy transfer from Yb{sup 3+} to Ho{sup 3+} ions was determined by the calculation using phonon sideband theory. The 1.20 mum emission observed was primarily due to the weak multiphonon deexcitation originated from the small phonon energy of PBG glass (approx535 cm{sup -1}). A large product of emission cross-section and measured lifetime (9.93x10{sup -25} cm{sup 2} s) was obtained for the 1.20 mum emission and the gain coefficient dependence on wavelength with population inversion rate (P) was performed. The peak emission cross-section for 2.05 mum emission was calculated to be 4.75x10{sup -21} cm{sup 2}. The relative mechanism of Ho{sup 3+}-doped and Ho{sup 3+}/Yb{sup 3+}-codoped PBG glasses on their spectroscopic properties was also discussed. Our results suggest that Ho{sup 3+}/Yb{sup 3+}-doped PBG glasses are a good potential candidate for the frequency upconversion devices and infrared amplifiers/lasers.

36 MATERIALS SCIENCE↗

Electron nuclear double resonance study of photostimulated luminescence active centers in CsBr:Eu{sup 2+} medical imaging plates

CsBr:Eu{sup 2+} needle image plates exhibit an electron-paramagnetic-resonance (EPR) spectrum at room temperature (RT), whose intensity is correlated with the photostimulated luminescence sensitivity of the plate. This EPR spectrum shows a strong temperature dependence: At RT it is owing to a single Eu{sup 2+} (S =7/2) center with axial symmetry, whereas at T<35 K the spectra can only be explained when two distinct centers are assumed to be present, a minority axial center and a majority center with nearly extremely rhombic symmetry. In this paper these low-temperature centers are studied with electron nuclear double resonance (ENDOR) spectroscopy, which reveals the presence of {sup 1}H nuclei close to the central Eu{sup 2+} ions in the centers. Analysis of the angular dependence of the ENDOR spectra allows to propose models for these centers, providing an explanation for the observed difference in intensity between the spectral components and for their temperature dependence.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis And Luminescence Studies Of Mn doped CaF{sub 2}

Nano particles of CaF{sub 2}:Mn were synthesized by a co-precipitation method. The maximum Mn concentration which could be doped into the CaF{sub 2} lattice was {approx}3%. The photoluminescence and thermally stimulated luminescence (TSL) were studied for different Mn doping. High dopant concentration leads to the appearance of yellow orange luminescence (580 nm) band due to the introduction of excitation levels in the deep UV region. A slight decrease in TSL peak temperature was observed at higher Mn concentrations after attaining a maximum at 1.3% Mn. Based on TSL data optimum doping concentration was found to be 2.5%. These nanoparticles were further hot pressed in vacuum to produce optically transparent ceramic.

36 MATERIALS SCIENCE↗

Transparent oxyfluoride glass ceramics co-doped with Er{sup 3+} and Yb{sup 3+} - Crystallization and upconversion spectroscopy

Transparent glass ceramics in the system SiO{sub 2}-B{sub 2}O{sub 3}-PbO-CdO-PbF{sub 2}-CdF{sub 2}-YbF{sub 3}-ErF{sub 3} showing infrared to visible anti-Stokes (upconversion) luminescence are studied in the present work. The glass compositions have been optimized in order to reduce the melting temperature and, hence, to obtain laboratory scale samples with good optical quality. Erbium-doped nanoscale Pb{sub 4}Yb{sub 3}F{sub 17} crystals are precipitated in the precursor glasses during annealing at temperatures 30-40 K above T{sub g}. A kinetically self-constrained growth explains the nano sizes of the crystals. Both the Stokes and anti-Stokes luminescence spectra of glasses could be explained with clustering of the Yb{sup 3+} and Er{sup 3+} ions in fluorine-rich regions. At the annealing temperature these regions act as nucleation precursors. The crystal growth further enhances the local concentration of these ions. Consequently, a series of energy transfer and energy cross relaxation processes occurs between adjacent rare earth ions leading to the observed luminescence spectra of the glass ceramics studied. -- Graphical abstract: A highly viscous shell (shown in the picture in dark blue) is build around the growing crystal (white circles). When the shell's T{sub g} approaches the annealing temperature, the crystal growth is fully suppressed for kinetic reasons. The upconversion luminescence, resulting from the simultaneous absorption of two and even three infrared photons, is depicted schematically in the right part of the figure. Display Omitted Highlights: {yields} New oxyfluoride glass compositions with reduced melting temperature are formulated. {yields} The phase Pb{sub 4}Yb{sub 3}F{sub 17} doped with Er{sup 3+} ions crystallizes in these glasses. {yields} A kinetically self-constrained growth explains the nano sizes of the crystals. {yields} Clustering of Yb{sup 3+}, Er{sup 3+} and Pb{sup 2+} ions into fluorine-rich glass regions is observed. {yields} The luminescence of glass-ceramics is consistent with its structure.

36 MATERIALS SCIENCE↗