Search NASA⌕ Search

SEARCH · Search NASA

Results for “interface reinforcement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Solid Oxide Fuel Cell Seal Glass - BN Nanotubes Composites

Solid oxide fuel cell seal glass G18 composites reinforced with approx.4 weight percent of BN nanotubes were fabricated via hot pressing. Room temperature strength and fracture toughness of the composite were determined by four-point flexure and single edge V-notch beam methods, respectively. The strength and fracture toughness of the composite were higher by as much as 90% and 35%, respectively, than those of the glass G18. Microscopic examination of the composite fracture surfaces using SEM and TEM showed pullout of the BN nanotubes, similar in feature to fiber-reinforced ceramic matrix composites with weak interfaces. Other mechanical and physical properties of the composite will also be presented.

Bansal, Narottam P.↗

Economical Fabrication of Thick-Section Ceramic Matrix Composites

A method was developed for producing thick-section [>2 in. (approx.5 cm)], continuous fiber-reinforced ceramic matrix composites (CMCs). Ultramet-modified fiber interface coating and melt infiltration processing, developed previously for thin-section components, were used for the fabrication of CMCs that were an order of magnitude greater in thickness [up to 2.5 in. (approx.6.4 cm)]. Melt processing first involves infiltration of a fiber preform with the desired interface coating, and then with carbon to partially densify the preform. A molten refractory metal is then infiltrated and reacts with the excess carbon to form the carbide matrix without damaging the fiber reinforcement. Infiltration occurs from the inside out as the molten metal fills virtually all the available void space. Densification to <5 vol% porosity is a one-step process requiring no intermediate machining steps. The melt infiltration method requires no external pressure. This prevents over-infiltration of the outer surface plies, which can lead to excessive residual porosity in the center of the part. However, processing of thick-section components required modification of the conventional process conditions, and the means by which the large amount of molten metal is introduced into the fiber preform. Modification of the low-temperature, ultraviolet-enhanced chemical vapor deposition process used to apply interface coatings to the fiber preform was also required to accommodate the high preform thickness. The thick-section CMC processing developed in this work proved to be invaluable for component development, fabrication, and testing in two complementary efforts. In a project for the Army, involving SiC/SiC blisk development, nominally 0.8 in. thick x 8 in. diameter (approx. 2 cm thick x 20 cm diameter) components were successfully infiltrated. Blisk hubs were machined using diamond-embedded cutting tools and successfully spin-tested. Good ply uniformity and extremely low residual porosity (<2 percent) were achieved, the latter being far lower than that achieved with SiC matrix composites fabricated via CVI or PIP. The pyrolytic carbon/zirconium nitride interface coating optimized in this work for use on carbon fibers was incorporated in the SiC/SiC composites and yielded a >41 ksi (approx. 283 MPa) flexural strength.

Babcock, Jason↗

An Investigation on the Use of a Laser Ablation Treatment on Metallic Surfaces and the Influence of Temperature on Fracture Toughness of Hybrid Co-Cured Metal-PMC Interfaces

Hybrid composite laminates that contain alternating layers of titanium alloys and carbon fabric reinforced polyimide matrix composites (PMC) are excellent candidates for light-weight, high-temperature structural materials for high-speed aerospace vehicles. The delamination resistance of the hybrid titanium-PMC interface is of crucial consideration for structural integrity during service. Here, we report the first investigations on the use of laser ablation in combination with sol-gel treatment technique on Ti/NiTi foil surfaces in co-cured hybrid polyimide matrix composite laminates. Mode-I and mode-II fracture toughness of the hybrid Ti/NiTi-PMC interface as a function of temperature were determined via experimental testing and finite element analysis.

Connell, John↗

Investigation of interfacial shear strength in a SiC fibre/Ti-24Al-11Nb composite by a fibre push-out technique

A fiber push-out technique applied at several sample thicknesses was used to determine both the debond shear stress and the frictional shear stress at the fiber-matrix interface at room temperautre for a unidirectional SiC fiber-reinforced T-24Al-11Nb (in at. pct) composite prepared by a powder cloth technique. The push-out technique measures the separate contributions of bond strength and friction to the mechanical shear strength at the fiber-matrix interface. It was found that the fiber-matrix bond shear strength of this material is significantly higher than the fiber-matrix frictional shear stress (119.2 and 47.8 MPa, respectively).

Eldridge, J. I.↗

Chemical interactions in the aluminum-carbon and aluminum-silicon carbide systems

XPS was used to investigate the influence of O2 and H2O on the formation of aluminum carbide at Al-C and Al-SiC interfaces. It was determined that dosing the interfaces with H2O catalyzed the formation of aluminum carbide in both systems. This result is consistent with the oxidation model of carbide formation (developed to understand the kinetics of aluminum carbide formation at graphite-aluminum interfaces). These results imply that the formation of aluminum carbide in graphite- and SiC-reinforced metal-matrix composites, which severely degrades the composite mechanical properties by degrading the fiber and interface strength is catalyzed.

Maruyama, Benji↗

X-ray photoelectron spectroscopy study of catalyzed aluminum carbide formation at aluminum-carbon interfaces

Aluminum carbide may form at aluminum-graphite interfaces during the high-temperature processing of graphite fiber-reinforced aluminum metal matrix composites. The chemical interactions leading to the formation of the aluminum carbide in the solid state involve the breaking of the carbon-carbon bonds within the graphite, the transport of the carbon atoms across the interface, and the reaction with the aluminum to form Al4C3. The aluminum carbide formation process has been followed using X-ray photoelectron spectroscopy of model, thin-film, reaction couples. The overall reaction is shown to be catalyzed by the presence of water vapor. Water at the interface increases reaction kinetics by apparently weakening the bonds between the surface carbon atoms and their substrate. This result is in general agreement with what is known to occur during the oxidation of graphite in air.

Rabenberg, L.↗

Interface control and mechanical property improvements in silicon carbide/titanium composites

Several composite systems made of titanium matrix reinforced with silicon carbide fiber were investigated to obtain a better understanding of composite-degradation mechanisms and to develop techniques to minimize loss of mechanical properties during fabrication and in service. Emphasis was on interface control by fiber or matrix coatings. X-ray diffraction studies on planar samples showed that the formation of titanium silicides was greatly inhibited by the presence of aluminum or Ti3A1 layers at the fiber-matrix interface, with the Ti3A1 being more effective in reducing the reactions. Fiber studies showed that coating the fiber with a 1-micron-thick layer of aluminum improved the as-fabricated strength of a stoichiometric SiC fiber and reduced the fiber degradation during exposure to composite-fabrication conditions. Applying an interfacial barrier by coating the matrix foils instead of the fibers was found to be an effective method for improving composite strength. Reducing the fabrication temperature also resulted in significant improvements in composite strengths. Good-quality, well-consolidated composites were fabricated at temperatures well below those currently used for SiC-Ti composite fabrication.

Brewer, W. D.↗

Influence of interfacial shear strength on the mechanical properties of SiC fiber reinforced reaction-bonded silicon nitride matrix composites

An evaluation is made of the influence of interfacial microstructure and shear strength on the mechanical properties of a 30 vol pct uniaxially-aligned SiC fiber-reinforced reaction-bonded Si3N4-matrix composite whose interface microstructure was varied through control of fabrication conditions and by heat-treatment in an oxidizing environment. The carbon-rich coating of the as-produced SiC fibers was stable in composites fabricated at 1200 C in an N or N + 4-percent H mixture for 40 hrs. This coating was degraded in composites fabricated at 1350 C in N + 4 percent H for 40 and 72 hrs, as well as after heat-treatment in an oxidizing environment at 600 C for 100 hrs even after fabrication at 1200 C in N. This degradation occurred via carbon removal.

Bhatt, Ramakrishna T.↗

The Effect of Microstructure on Mechanical Properties of Directionally Solidified Al2O3/ZrO2(Y2O3) Eutectic

The eutectic architecture of a continuous reinforcing phase within a higher volume fraction phase or matrix can be described as a naturally occurring in-situ composite. Here we report the results of experiments aimed at identifying the sources of high temperature creep resistance and high levels of strength in a two phase Al2O3/ZrO2(Y2O3) system. The mechanical properties of two phase Al2O3/ZrO2(Y2O3) eutectic are superior to those of either constituent alone due to strong constraining effects provided by the coherent interfaces and microstructure. The AlO3/ZrO2(Y2O3) eutectic maintains a low energy interface resulting from directional solidification and can produce strong and stable reinforcing phase/matrix bonding. The phases comprising a eutectic are thermodynamically compatible at higher homologous temperatures than man-made composites and as such offer the potential for superior high temperature properties.

Sayir, Ali↗

Fiber-Reinforced Reactive Nano-Epoxy Composites

An ultra-high-molecular-weight polyethylene/ matrix interface based on the fabrication of a reactive nano-epoxy matrix with lower surface energy has been improved. Enhanced mechanical properties versus pure epoxy on a three-point bend test include: strength (25 percent), modulus (20 percent), and toughness (30 percent). Increased thermal properties include higher Tg (glass transition temperature) and stable CTE (coefficient of thermal expansion). Improved processability for manufacturing composites includes faster wetting rates on macro-fiber surfaces, lower viscosity, better resin infusion rates, and improved rheological properties. Improved interfacial adhesion properties with Spectra fibers by pullout tests include initial debonding force of 35 percent, a maximum pullout force of 25 percent, and energy to debond at 65 percent. Improved mechanical properties of Spectra fiber composites (tensile) aging resistance properties include hygrothermal effects. With this innovation, high-performance composites have been created, including carbon fibers/nano-epoxy, glass fibers/nano-epoxy, aramid fibers/ nano-epoxy, and ultra-high-molecularweight polyethylene fiber (UHMWPE).

Zhong, Wei-Hong↗

Wave propagation in composite media and material characterization

Characteristics of wave propagation in an undamaged composite medium are influenced by many factors, the most important of which are: microstructure, constituent properties, interfaces, residual stress fields, and ply lay-ups. Measurements of wave velocities, attenuation, and dispersion provide a powerful tool for nondestructive evaluation of these properties. Recent developments are reviewed for modeling ultrasonic wave propagation in fiber and particle-reinforced composite media. Additionally, some modeling studies are reviewed for the effects of interfaces and layering on attenuation and dispersion. These studies indicate possible ways of characterizing material properties by ultrasonic means.

Datta, Subhendu K.↗

Fracture problems in composite materials

A series of fracture problems in composite materials are identified, their methods of solution are briefly discussed, and some sample results are presented. The main problem of interest is the determination of the stress state in the neighborhood of localized imperfections such as cracks and inclusions which may exist in the composite. Particular emphasis is placed on the evaluation of quantities such as the stress intensity factors, the power of the stress singularity, and the strain energy release rate, which may be used directly or indirectly in connection with an appropriate fracture criterion for the prediction of fracture initiation and propagation load levels. The topics discussed include a crack in layered composites, a crack terminating at and going through a bi-material interface, a penny-shaped crack in a filament-reinforced elastic matrix, and inclusion problems in bonded materials.

Erdogan, F.↗

The Role of the Interface in Refractory Metal Alloy Composites

Creep-rupture and tensile tests have been used to evaluate thoriated W-wire reinforced Nb-1 percent Zr alloy matrix composites fabricated via arc-spray monotape technique. A significant creep strength enhancement was observed over the unreinforced matrix alloy while matrix integrity was maintained; the fiber/matrix interface phase is noted to be a strong and ductile W/Nb alloy, which is formed due to the mutual solubility of the constituent metals. High strength, toughness, and thermal stability are demonstrated by this material system, which is also resistant to liquid alkali metal corrosion.

Grobstein, Toni↗

Effects of Fiber/Matrix Interface and its Composition on Mechanical Properties of Hi-Nicalon/Celsian Composites

To evaluate the effects of fiber coatings on composite mechanical properties. unidirectional celsian matrix composites reinforced with uncoated Hi-Nicalon fibers and those precoated with a dual BN/SiC layer in two separate batches (batch 1 and batch 2) were tested in three-point flexure. The uncoated-fiber reinforced composites showed catastrophic failure with strength of 210+/-35 MPa and a flat fracture surface. In contrast, composites reinforced with coated fibers exhibited graceful failure with extensive fiber pullout and showed significantly higher ultimate strengths, 904 and 759 MPa for the batch 1 and 2 coatings. respectively. Fiber push-in tests and microscopic examination indicated no chemical reaction at the uncoated or coated fiber-matrix interfaces that might be responsible for fiber strength degradation. Instead, the low strength of composite with uncoated fibers was due to degradation of the fiber strength from mechanical damage during composite processing. Despite identical processing, the first matrix cracking stresses (Sigma(sub mc)) of the composites reinforced with fibers coated in batch 1 and batch 2 were quite different, 436 and 122 MPa, respectively. The large difference in Sigma(sub mc) of the coated-fiber composites was attributed to differences in fiber sliding stresses (Tau(sub friction)), 121.2+/-48.7 and 10.4+/-3.1 MPa, respectively. for the two composites as determined by the fiber push-in method. Such a large difference in Tau(sub friction). for the two composites was found to be due to the difference in the compositions of the interface coatings. Scanning Auger microprobe analysis revealed the presence of carbon layers between the fiber and BN. and also between the BN and SiC coatings in the composite showing lower Tau(sub friction). This resulted in lower Sigma(sub mc) in agreement with the ACK theory. The ultimate strengths of the two composites depended mainly on the fiber volume fraction and were not significantly effected by Tau(sub friction) values, as expected. The poor reproducibility of the fiber coating composition between the two batches was judged to be the primary source of the large differences in performance of the two composites.

Bansal, Narottam P.↗

An Investigation of Reliability Models for Ceramic Matrix Composites and their Implementation into Finite Element Codes

The development of modeling approaches for the failure analysis of ceramic-based material systems used in high temperature environments was the primary objective of this research effort. These materials have the potential to support many key engineering technologies related to the design of aeropropulsion systems. Monolithic ceramics exhibit a number of useful properties such as retention of strength at high temperatures, chemical inertness, and low density. However, the use of monolithic ceramics has been limited by their inherent brittleness and a large variation in strength. This behavior has motivated material scientists to reinforce the monolithic material with a ceramic fiber. The addition of a second ceramic phase with an optimized interface increases toughness and marginally increases strength. The primary purpose of the fiber is to arrest crack growth, not to increase strength. The material systems of interest in this research effort were laminated ceramic matrix composites, as well as two- and three- dimensional fabric reinforced ceramic composites. These emerging composite systems can compete with metals in many demanding applications. However, the ongoing metamorphosis of ceramic composite material systems, and the lack of standardized design data has in the past tended to minimize research efforts related to structural analysis. Many structural components fabricated from ceramic matrix composites (CMC) have been designed by "trial and error." The justification for this approach lies in the fact that during the initial developmental phases for a material system fabrication issues are paramount. Emphasis is placed on demonstrating feasibility rather than fully understanding the processes controlling mechanical behavior. This is understandable during periods of rapid improvements in material properties for any composite system. But to avoid the ad hoc approach, the analytical methods developed under this effort can be used to develop rational structural design protocols.

Duffy, Stephen F.↗

Effective thermal conductivity of composites with fibre-matrix debonding

Debonding of the fiber-matrix interface is a major cause for the degradation of the mechanical properties and the loss of thermal conductivity of fiber-reinforced composites. This paper discusses two analytical approaches for modeling the thermal conduction problem of composites. One is based on the concept of modeling the thermal barrier by an equivalent heat transfer coefficient at the fiber-matrix interface, as described by Hasselman and Johnson (1987) and Benveniste and Miloh (1986). The other approach, suggested by Hatta and Taya (1986), is by treating a composite with debonded interface as a coated-fiber composite. The major advantage of the latter aproach is that the thickness of the fiber coating can be realistically modeled depending upon the extent of degradation of the composite with the thermal conductivity of the coating as that of air.

Fadale, T. D.↗

Microcracking mechanisms and interface toughening of semi-IPN polyimide matrix composites

A new research program was initiated as a preliminary phase. The following three objectives are being pursued for the overall program: to elucidate the mechanisms of microcracking for graphite fiber-reinforced semi-IPN polyimide matrix composites under mechanical and thermal cyclic loading; to devise material engineering solutions for possible improvement of fatigue damage resistance (or the increase of fatigue endurance strength) of semi-IPN matrix composites by tailoring of modulus and toughness of fiber-resin interface region; and to assess processing characteristics of the composites and their roles in controlling the resistance of composites to microcracking and the effectiveness of interface toughening. The main emphasis was placed upon the initial screening of material systems and optimization of processing conditions for semi-IPN matrix composites with tailored interface. As a first set of control material systems to study, the composites were prepared with unsized Celion 6000 graphite fiber reinforcement and the following resin matrices of varied fracture toughness: PMR-15 thermoset polyimide, semi-IPN of PNR-15 thermoset polyimide and NR150B2 thermoplastic polyimide in 75/25 ratio, and semi-IPN of PMR-15 and NR150B2 in 50/50 ratio. For the composites with the resin matrix of semi-IPN in 75/25 ratio, interface tailoring was attempted by using graphite fibers coated with the resins of systematically varied fracture toughness. In the continuing work, a broad range of interlayer toughness will be achieved by coating the fibers with reactants of semi-IPN having lower or higher content of thermoplastic constituent in comparison with the composition of surrounding resin matrix. In pursuing the objectives of the overall research program, the respective roles and interaction of critical parameters were defined.

Lee, Byung L.↗

Scaling effects of defects in fiber-reinforced composites

Material defects may be introduced willingly or unwillingly during material manufacturing and structural component fabrication stages. Their presence in the material plays a dominant role in determining the material's strength and the associate failure mechanisms. In the sense that the size and the number of defects may increase with the volume of the material, the effect of dimensional scaling may manifest itself in the dependence of material strength on volume. Or, alternatively, there may exist a scaling effect of material defects. In fiber-reinforced composites, manufacturing or fabrication defects may come in several forms: matrix voids, matrix microcracks, fiber misalignment, broken fibers, or interface disbonds, just to mention a few. These are interacting and competing defects in the sense that one type of defect may become dominant under one stress condition and another type of defect may become dominant under a different stress condition. This happens because the fiber reinforcement network, together with the distribution of defects, constitutes the prime microstructure of the composite, and there exist continued interactions between the evolving microstructure and the distribution of defects. In the process, the scaling effects of defects are complicated by this interaction. In this presentation, the scaling effects of defects in fiber-reinforced composites will be briefly discussed with the introduction of the concept of effective defects. It is then shown with the aid of some actual experimental and analysis results that the scaling effects are very much present, but they are regulated by the characteristic dimension of the composite microstructure due to the aforementioned microstructure-defect interaction effect.

Wang, A. S. D.↗