Interlaminar Fracture Toughness Testing of Nb3Sn Insulation Systems

Epoxy cracking has been the main suspected contributor to training in Nb3Sn magnets for some time, as it leads to energy release and magnet quenching. Cracking in a superconducting composite can occur from several modes, and the likelihood of these modes is not well understood. Failure has been observed between insulation systems and the superconducting cable itself rather than within the cable or insulation. To target the behavior at the interface, samples have been fabricated and tested for mode I fracture toughness in an adapted version of ASTM D5528. This work seeks to better characterize the fracture toughness of this interface to better understand how to model and design insulation systems.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

SA508 low alloy steel to 316L stainless steel dissimilar metal joint made by powder metallurgy hot isostatic pressing

Joining ferritic SA508 low alloy steel (LAS) and austenitic 316 L stainless steel (SS) via powder metallurgy hot isostatic pressing (PM-HIP) was evaluated as an alternative method to welding. This study investigated the mechanical and microstructural evolutions of the bimetallic interface under different joint designs and heat treatments. Here, the direct joining of dissimilar metal alloys by PM-HIP method resulted in two designs: 1) powder SA508 to solid bar 316 L (P508–B316L) and 2) powder 316 L solid bar SA508 (P316L-B508). In both cases, P508–B316L and P316L-demonstrated satisfactory tensile strength, however, high hardness and severe depreciation in toughness were located on the bimetallic interface. The mechanisms responsible for the detrimental mechanical properties were verified. Large oxides were observed in P508–B316L due to the prior powder boundary (PPB) oxides present in SA508 powder. The intense sensitization occurred from the formation of M 23 C 6 carbides, consequently from the slow cooling after PM-HIP in P316L-B508. Post-HIP heat treatments were explored to reduce the distance of carbide formation; however, the heat treatment could not eliminate the carbides. The experimental results were compared to the diffusion couple simulation as a function of carbide formation with distance. The analysis also showed the high hardness at the bimetallic interface was primarily contributed by solid solution strengthening. In conclusion, the direct joining of P316L-B508 and P508–B316L via PM-HIP was deemed to be unfeasible, and a transitional material is necessary to impede the diffusion of carbon.

316L stainless Steel↗

The potential for ductility enhancement from surface and interface dislocation sources in NiAl

Limited ductility and toughness of NiAl and related aluminides near room temperature pose major problems in their potential application as structural materials. An analysis of these problems is presented as part of a review of the flow and fracture behavior of binary NiAl. Following this discussion is a demonstration that conditions of elastic and plastic constraint associated with phase boundaries afforded by surface films, internal lamellae, or precipitates may introduce sufficient densities of mobile dislocations to enhance the ductility of NiAl-based materials by significant amounts. Examples of this behavior are presented for several model materials, including 001- and 123-oriented single crystals of oxide-coated NiAl, directionally solidified beta-gamma-prime (Ni70Al30) and beta-gamma (Ni50Fe30Al20) in situ composites, and several NiAl/precipitate systems. The nature of the resulting dislocation substructures and the effects of several materials variables are described.

Noebe, R. D.↗

Constitutive Modeling of the Facesheet to Core Interface in Honeycomb Sandwich Panels Subject to Mode I Delamination

A new cohesive zone traction-separation law, which includes the effects of fiber bridging, has been developed, implemented with a finite element (FE) model, and applied to simulate the delamination between the facesheet and core of a composite honeycomb sandwich panel. The proposed traction-separation law includes a standard initial cohesive component, which accounts for the initial interfacial stiffness and energy release rate, along with a new component to account for the fiber bridging contribution to the delamination process. Single cantilever beam tests on aluminum honeycomb sandwich panels with carbon fiber reinforced polymer facesheets were used to characterize and evaluate the new formulation and its finite element implementation. These tests, designed to evaluate the mode I toughness of the facesheet to core interface, exhibited significant fiber bridging and large crack process zones, giving rise to a concave downward concave upward pre-peak shape in the load-displacement curve. Unlike standard cohesive formulations, the proposed formulation captures this observed shape, and its results have been shown to be in excellent quantitative agreement with experimental load-displacement and apparent critical energy release rate results, representative of a payload fairing structure, as well as local strain fields measured with digital image correlation.

composites↗

Ab Initio Study of Energetics, Charge Transfer, and Atomic Structures of FCC Fe/NbC Interfaces with and Without N Doping: From Coherent to Semi-coherent Interfaces

Nitrogen is added to stainless steels to improve their toughness and corrosion resistance. However, it is not well understood how nitrogen may impact the precipitate/matrix interfacial properties. In this work, we consider the (FCC) Fe (001)/NbC (001) interface as a model system to study how interfacial structure, energy, and electron charge are affected by nitrogen using DFT calculations. We compare the structures and energetics of coherent and semi-coherent interfaces by including the elastic contribution component. It is found that nitrogen does not have a significant effect on either the interfacial energy or the atomic arrangement near the interface region. A highly intricate bonding feature is revealed near heterophase interfaces between alloy elements, in which metallic and covalent features are present together with charge transfer. Additionally, the work on determining accurate interfacial energies is at the core of all quantitative precipitation modeling efforts (in particular, in the XMAT Program). In turn, nucleation, growth/dissolution, and coarsening of precipitates contribute critically to the material’s ability to withstand creep, creep fatigue, and other detrimental processes reducing its service life. It is for this reason that developing quantitative understanding of interfaces and their energetics in materials is so important for their development and further improvement.

36 MATERIALS SCIENCE↗

Role of water in fracture of modified silicate glasses

Decarbonizing the glass industry requires alternative melting technology, as current industrial melting practices rely heavily on fossil fuels. Hydrogen has been proposed as an alternative to carbon-based fuels, but the ensuing consequences on the mechanical behavior of the glass remain to be clarified. A critical distinction between hydrogen and carbon-based fuels is the increased generation of water during combustion, which raises the equilibrium solubility of water in the melt and alters the behavior of the resulting glass. A series of five silicate glasses with 80% silica and variable [Na 2 O]/([H 2 O] + [Na 2 O]) ratios were simulated using molecular dynamics to elucidate the effects of water on fracture. Several fracture toughness calculation methods were used in combination with atomistic fracture simulations to examine the effects of hydroxyl content on fracture behavior. Here, this study reveals that the crack propagation pathway is a key metric to understanding fracture toughness. Notably, the fracture propagation path favors hydrogen sites over sodium sites, offering a possible explanation of the experimentally observed effects of water on fracture properties.

36 MATERIALS SCIENCE↗

FaceSheet Push-off Tests to Determine Composite Sandwich Toughness at Cryogenic Temperatures

A new novel test method, associated analysis, and experimental procedures are developed to investigate the toughness of the facesheet-to-core interface of a sandwich material at cryogenic temperatures. The test method is designed to simulate the failure mode associated with facesheet debonding from high levels of gas pressure in the sandwich core. The effects of specimen orientation are considered, and the results of toughness measurements are presented. Comparisons are made between room and liquid nitrogen (-196 C) test temperatures. It was determined that the test method is insensitive to specimen facesheet orientation and strain energy release rate increases with a decrease in the test temperature.

Gates, Thomas S.↗

An isotropic zero thermal expansion alloy with super-high toughness

Zero thermal expansion (ZTE) alloys with high mechanical response are crucial for their practical usage. Yet, unifying the ZTE behavior and mechanical response in one material is a grand obstacle, especially in multicomponent ZTE alloys. Herein, we report a near isotropic zero thermal expansion (α l = 1.10 × 10 -6 K -1 , 260–310 K) in the natural heterogeneous LaFe 54 Co 3.5 Si 3.35 alloy, which exhibits a super-high toughness of 277.8 ± 14.7 J cm -3 . Chemical partition, in the dual-phase structure, assumes the role of not only modulating thermal expansion through magnetic interaction but also enhancing mechanical properties via interface bonding. The comprehensive analysis reveals that the hierarchically synergistic enhancement among lattice, phase interface, and heterogeneous structure is significant for strong toughness. Our findings pave the way to tailor thermal expansion and obtain prominent mechanical properties in multicomponent alloys, which is essential to ultra-stable functional materials.

36 MATERIALS SCIENCE↗

Factors influencing the Mode I interlaminar fracture toughness of a rubber toughened thermoplastic matrix composite

The use of a rubber modified thermoplastic resin has been investigated as a method to improve the Mode I interlaminar fracture toughness of a unidirectional continuous carbon fiber composite. Test results show that the improvement in the fracture toughness is less than expected due to rubber particle agglomeration, solvent and molding induced crystallization of the matrix and poor fiber/matrix adhesion. The plastic zone in composites utilizing tough matrices can extend well beyond a single interfibrillar spacing. However, the development of the plastic zone is limited due to the failure of the fiber/matrix interface. In order to fully evaluate the potential of tough composites using toughened matrices, any improvement made in the matrix toughness must be coupled with improvements in the fiber/matrix adhesion.

Parker, D. S.↗

Imparting strength and toughness to brittle composites

Appropriate intermittent coatings of fibers can produce areas of low and high toughness in brittle composites. Experiments using silicon vacuum grease (SVG) and polyurethane varnish (PUV) coatings that achieve weakly and strongly bonded interfaces are described. Tensile strength and edge-crack fracture toughness for both SVG and PUV coatings were plotted against the percentage coating (C). Both coating materials maintain tensile strengths in the order of the rule of mixture strength values up to a large C. It is suggested that both materials produce similar coated interfacial shear strengths while producing different effects on toughness.

Atkins, A. G.↗

New Testing Tool For Composite Interfaces

Mechanical strength of fiber/matrix interface key factor in overall strength and toughness of composite material. Desktop fiber pushout apparatus generates load and acoustic-emission (soundwave) data as function of translation-table displacement. Video camera gives view of specimen. Compact, easy to operate, and inexpensive. Appropriate for wide range of composites, including metal, intermetallic, and ceramic matrix composites. Not restricted to aerospace/aeronautics applications.

Eldridge, Jeffrey I.↗

Characterization of Hybrid CNT Polymer Matrix Composites

Carbon nanotubes (CNTs) have been studied extensively since their discovery and demonstrated at the nanoscale superior mechanical, electrical and thermal properties in comparison to micro and macro scale properties of conventional engineering materials. This combination of properties suggests their potential to enhance multi-functionality of composites in regions of primary structures on aerospace vehicles where lightweight materials with improved thermal and electrical conductivity are desirable. In this study, hybrid multifunctional polymer matrix composites were fabricated by interleaving layers of CNT sheets into Hexcel® IM7/8552 prepreg, a well-characterized toughened epoxy carbon fiber reinforced polymer (CFRP) composite. The resin content of these interleaved CNT sheets, as well as ply stacking location were varied to determine the effects on the electrical, thermal, and mechanical performance of the composites. The direct-current electrical conductivity of the hybrid CNT composites was characterized by in-line and Montgomery four-probe methods. For [0](sub 20) laminates containing a single layer of CNT sheet between each ply of IM7/8552, in-plane electrical conductivity of the hybrid laminate increased significantly, while in-plane thermal conductivity increased only slightly in comparison to the control IM7/8552 laminates. Photo-microscopy and short beam shear (SBS) strength tests were used to characterize the consolidation quality of the fabricated laminates. Hybrid panels fabricated without any pretreatment of the CNT sheets resulted in a SBS strength reduction of 70 percent. Aligning the tubes and pre-infusing the CNT sheets with resin significantly improved the SBS strength of the hybrid composite To determine the cause of this performance reduction, Mode I and Mode II fracture toughness of the CNT sheet to CFRP interface was characterized by double cantilever beam (DCB) and end notch flexure (ENF) testing, respectively. Results are compared to the control IM7/8552 laminate.

Grimsley, Brian W.↗

The Chemical Nature of the Fiber/resin Interface in Composite Materials

Carbon fiber/epoxy resin composites are considered. The nature of the fiber structure and the interaction that occurs at the interface between fiber and matrix are emphasized. Composite toughness can be improved by increased axial tensile and compressive strengths in the fibers. The structure of carbon fibers indicates that the fiber itself can fail transversely, and different transverse microstructures could provide better transverse strengths. The higher surface roughness of lower modulus and surface-treated carbon fibers provides better mechanical interlocking between the fiber and matrix. The chemical nature of the fiber surface was determined, and adsorption of species on this surface can be used to promote wetting and adhesion. Finally, the magnitude of the interfacial bond strength should be controlled such that a range of composites can be made with properties varying from relatively brittle and high interlaminar shear strength to tougher but lower interlaminar shear strength.

Diefendorf, R. J.↗

Interface effects in interlaminar fracture of thermoplastic composites

Mode I interlaminar fracture toughness was determined on a series of unidirectional poly(phenylene oxide)/carbon fiber composites using the double cantilever beam test. Initial toughness for growth of a delamination from an insert depends on fiber type, and ranges from 190 to 440 J/sq m, with intermediate modulus fibers tending to give lower values than high-strain fibers. Low toughness values are attributed to poor fiber-matrix adhesion. As a delamination progress down the beam, fiber bridging increases the apparent toughness by up to a factor of 7, depending on the fiber.

Hinkley, J. A.↗

Deformation and fracture of a directionally solidified NiAl-28Cr-6Mo eutectic alloy

A directionally solidified alloy based on the NiAl-(Cr, Mo) eutectic was examined by transmission and scanning electron microscopy to characterize the microstructure and room temperature deformation and fracture behavior. The microstructure consisted of a lamellar morphology with a group of zone axes (111) growth direction for both the NiAl and (Cr, Mo) phases. The interphase boundary between the eutectic phases was semicoherent and composed of a well-defined dislocation network. In addition, a fine array of coherent NiAl precipitates was dispersed throughout the (Cr, Mo) phase. The eutectic morphology was stable at 1300 K with only coarsening of the NiAl precipitates occurring after heat treatment for 1.8 ks (500 h). Fracture of the aligned eutectic is characterized primarily by a crack bridging/renucleation mechanism and is controlled by the strength of the semicoherent interface between the two phases. However, contributions to the toughness of the eutectic may arise from plastic deformation of the NiAl phase and the geometry associated with the fracture surface.

Chen, X. F.↗

Offset-Stoichiometric Reflowable Composite Bonding Method with Adhesive for Mitigating Strict Faying Surface Tolerances

Inherent susceptibility of adhesive bonds to miniscule quantities of contamination can cause undetectable weakened bonds. For this reason, the Federal Aviation Administration (FAA) places strict regulations on adhesively bonded joints in primary aircraft structures. To meet certification requirements aircraft manufactures resort to redundant load paths in the form of fasteners which inherently add weight to the structure and increase manufacturing time. In prior work, a secondary bonding technique called AERoBOND was developed, which utilized off-stoichiometric epoxymatrix resins to facilitate reflow and diffusion of the resin within the joint interface during a secondary bonding/cure process, thus achieving a bond similar to a co-cured joint. However, the AERoBOND process required tight spatial tolerances between the two parts being joined. This study examined the utilization of conventional adhesive with the AERoBOND method to act as a filler in the joint line, effectively reducing the need for tight tolerances on the joining parts and serving as a flexible alternative for existing manufacturing processes. Ultrasonic inspection, optical microscopy, and ASTM International standard tests were performed to analyze the joints for defects and to quantify the mode-I and mode-II interlaminar fracture toughness and short beam strength of the proposed methodology with varying manufacturing parameters. The comprehensive results indicate that the AERoBOND+ method with and without surface preparation performs comparably to co-cured and conventional, adhesively bonded joints when secondary cured in an autoclave with 791 kPa of pressure. As an example, the AERoBOND+ panel without surface preparation bonded with 791 kPa of pressure (referred to as AB+3 throughout paper) had a mode-I fracture toughness (G Ic ) of 0.643 kJ/m 2 and a mode-II fracture toughness (G IIc ) of 4.000 kJ/m 2 in the non-precracked condition and 4.218 kJ/m 2 in the precracked condition at the adhesive-to-prepreg interface. These results were 96%, 142%, and 217%, respectively, of a co-cured baseline panel (referred to as C1 throughout paper).

Composites↗