Search NASA⌕ Search

SEARCH · Search NASA

Results for “lapping”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Global-Local Finite Element Analysis of Bonded Single-Lap Joints

Adhesively bonded lap joints involve dissimilar material junctions and sharp changes in geometry, possibly leading to premature failure. Although the finite element method is well suited to model the bonded lap joints, traditional finite elements are incapable of correctly resolving the stress state at junctions of dissimilar materials because of the unbounded nature of the stresses. In order to facilitate the use of bonded lap joints in future structures, this study presents a finite element technique utilizing a global (special) element coupled with traditional elements. The global element includes the singular behavior at the junction of dissimilar materials with or without traction-free surfaces.

Kilic, Bahattin↗

Nonlinear Analysis of Bonded Composite Tubular Lap Joints

The present study describes a semi-analytical solution method for predicting the geometrically nonlinear response of a bonded composite tubular single-lap joint subjected to general loading conditions. The transverse shear and normal stresses in the adhesive as well as membrane stress resultants and bending moments in the adherends are determined using this method. The method utilizes the principle of virtual work in conjunction with nonlinear thin-shell theory to model the adherends and a cylindrical shear lag model to represent the kinematics of the thin adhesive layer between the adherends. The kinematic boundary conditions are imposed by employing the Lagrange multiplier method. In the solution procedure, the displacement components for the tubular joint are approximated in terms of non-periodic and periodic B-Spline functions in the longitudinal and circumferential directions, respectively. The approach presented herein represents a rapid-solution alternative to the finite element method. The solution method was validated by comparison against a previously considered tubular single-lap joint. The steep variation of both peeling and shearing stresses near the adhesive edges was successfully captured. The applicability of the present method was also demonstrated by considering tubular bonded lap-joints subjected to pure bending and torsion.

E. Oterkus↗

Microstructure and texture evolution of friction stir lap welded dissimilar multi-aluminum stack

Here this work investigates the microstructural evolution of a dissimilar multiple-aluminum alloy stack (AA7055, AA7055, AA6022) produced by friction stir lap welding (FSLW). A through-thickness analyses of grain orientation map, grain size and distribution, strain distribution, and texture evolution by electron backscattered diffraction-based characterization technique were performed. Two different welding parameters (combination of tool rotation and traverse speed) were used to study the effects of the welding parameters on these microstructural characteristics. The study shows that higher welding speed and higher rotation speed of the FSLW tool yield finer grains. FSLW resulted in shear texture formation in the weld regions due to high welding speeds. This texture development in the nugget zone is consistent with shear deformation, and (111) pole figures show ideal shear texture components. The Stir Zone (SZ) exhibits shear texture (A/A ̅ and B/B ̅ components), consistent with other shear-assisted processes. Recrystallization mechanisms observed are CDRX in SZ and DDRX in TMAZ (Thermo-Mechanically Affected Zone). Interface analysis reveals the presence of oxide layers between different aluminum sheets, affecting joint mechanical performance. The mechanical property of the lap welded joints was presented in terms of microhardness distribution across the weld cross section. Slightly higher hardness in higher speed welding setup was observed throughout the SZ and AA6022 layer, indicating greater grain refinement and uniform grain structure distribution.

36 MATERIALS SCIENCE↗

Summative Mass Analysis of Algal Biomass - Integration of Analytical Procedures: Laboratory Analytical Procedure (LAP)

This document guides the integration of laboratory analytical procedures (LAPs) to measure algal biomass constituents in an unambiguous manner and ultimately achieve mass balance closure for algal biomass samples. Many of these methods build on years of research in the algal biomass analytical field i. By combining the appropriate LAPs, the goal is to break the biomass sample down into constituents that sum as close to 100% by weight as possible. Some of these constituents are individual components, such as individual carbohydrates and lipids as total fatty acids, and some can be groups of compounds, such as extractable lipids. The goal of these analyses is to characterize the major biochemical constituents in algae, but we recognize that with the current state-of-the- art methods the summative mass accounting does not always achieve 100%, and the degree to which biomass can be described is highly dependent on the origin, strain, and cultivation conditions of the algae. This document covers the summative mass balance measurements for algal biomass only.

09 BIOMASS FUELS↗

THE ROLE OF FRACTURE PROPERTIES ON LAP JOINT STRENGTH OF FRICTION STIR WELDED AA7055-T6 SHEETS

Friction stir lap welded (FSLW) joints have weight-saving potential in aluminum-intensive automotive assembly. However, FSLW also modifies the material microstructure close to the joint. Optimizing the FSLW process requires understanding the relationship between the strength and the joint's microstructure. In previous studies, efforts have been dedicated to determining the effects of local softening, the shape of the oxide line, and porosity. However, the impact of changes to the fracture properties on the joint's strength has not been studied. In this work, strength testing, and simulations, aided by material characterization, were used to determine the role of fracture properties on the shear strength of a 3-sheet (aluminum alloys 7055-7055-6022) lap joint. Characterization involved testing for fracture properties in the weld region. This data was then implemented into finite element simulations. As a result, the joint strength was predicted with a deviation of less than 6% from the experimental value. Comparison with strength prediction using only the base metal properties indicates that fracture property in the nugget region determines the strength of AA7055 FSLW.

Finite element analysis, Friction stir welding, ma↗

Friction Stir Lap Welding of Magnesium Alloy to Steel: A Preliminary Investigation

An initial study was made to evaluate the feasibility of joining Magnesium alloy AZ31 sheet to galvanized steel sheet in lap configuration using friction stir welding (FSW). Two different automotive sheet steels were used for comparative evaluation of the dissimilar joining potential; a 0.8mm thick, electro galvanized (EG) mild steel, and a 1.5mm thick hot dipped galvanized (HDG) high-strength, low-alloy steel (HSLA). These steels were joined to 2.33mm thick AZ31B magnesium sheet. A single FSW tool design was used for both dissimilar welds, and process parameters were kept the same. Average peak load for the AZ31-1.5 mm steel weld joint in lap shear mode was found to be 6.3 ± 1.0 kN. For the AZ31-0.8 mm steel weld, joint strength was 5.1 ± 1.5 kN. Microstructural investigation indicates melting of the Zn coating at the interface and subsequent alloying with the Mg sheet resulting in formation of solidified Zn-Mg alloy layer at AZ31/steel interface.

36 MATERIALS SCIENCE↗

Friction Stir Lap Welding 0.8-mm-Thick 2024 Aluminum Alloy with the Assistance of Stationary Shoulder

In this work, 0.8-mm-thick 2024 aluminum alloy was friction stir lap welded with the assistance of a stationary shoulder system. The joint surface formation, microstructure and mechanical properties of the welded joints were studied. The results showed that sound joints without defect could be obtained at a wide parameter range because stationary shoulder increased the material flow during welding. The stationary shoulder decreased the joint roughness from 125.5 to 58.9 µm. A thickness reduction of 4% was achieved at a welding speed of 200 mm/min. The joint fabricated by the stationary shoulder system had superior lap shear properties compared to the joint fabricated using the conventional tool. A high failure load of 7440 N was achieved at welding speed of 200 mm/min. The joint presented tensile fracture mode and the fracture morphology showed typical ductile fracture.

36 MATERIALS SCIENCE↗

Joining aluminum to titanium alloy by friction stir lap welding with cutting pin

Aluminum 1060 and titanium alloy Ti-6Al-4V plates were lap joined by friction stir welding. A cutting pin of rotary burr made of tungsten carbide was employed. The microstructures of the joining interface were observed by scanning electron microscopy. Joint strength was evaluated by a tensile shear test. During the welding process, the surface layer of the titanium plate was cut off by the pin, and intensively mixed with aluminum situated on the titanium plate. The microstructures analysis showed that a visible swirl-like mixed region existed at the interface. In this region, the Al metal, Ti metal and the mixed layer of them were all presented. The ultimate tensile shear strength of joint reached 100% of 1060Al that underwent thermal cycle provided by the shoulder. - Highlights: Black-Right-Pointing-Pointer FSW with cutting pin was successfully employed to form Al/Ti lap joint. Black-Right-Pointing-Pointer Swirl-like structures formed due to mechanical mixing were found at the interface. Black-Right-Pointing-Pointer High-strength joints fractured at Al suffered thermal cycle were produced.

36 MATERIALS SCIENCE↗

Liquid metal embrittlement in laser lap joining of TWIP and medium-manganese TRIP steel: The role of stress and grain boundaries

Highlights: • This work shows liquid metal embrittlement in externally loaded laser lap welding. • Results confirmed a direct relation between external load and LME susceptibility. • TWIP steel showed a higher LME susceptibility compared to medium-Mn TRIP steel. • Results indicated stress-assisted diffusion of Zn into austenite grain boundaries. • High angle grain and Σ3 twinning boundaries play major role in Zn penetration. - Abstract: High-Manganese austenite-containing steels with superior combination of strength and ductility have shown potential for enhancement of passenger safety and body-in-white (BIW) weight reduction. Even though Zn-coated austenitic steels have improved corrosion resistance, they are highly susceptible to liquid metal embrittlement (LME) during welding. The present work is aimed to address LME susceptibility during restrained laser lap joining of high-Mn twinning induced plasticity (TWIP) and medium-Mn transformation induced plasticity (MMn-TRIP) steels. Electron probe micro-analysis (EPMA) results showed that stress-assisted diffusion of Zn into the austenite grain boundaries and further liquid Zn formation by a peritectic reaction lead to grain boundary decohesion. Electron backscatter diffraction (EBSD) results demonstrated that high angle and special grain boundaries are prone to Zn-penetration within the heat-affected-zone (HAZ). Additionally, LME sensitivity was observed to be highly dependent on the magnitude of applied stress.

36 MATERIALS SCIENCE↗

Lap shear strength and healing capability of self-healing adhesive containing epoxy/mercaptan microcapsules

The aim of this work is to develop a self-healing polymeric adhesive formulation with epoxy/mercaptan microcapsules. Epoxy/mercaptan microcapsules were dispersed into a commercialize two-part epoxy adhesive for developing self-healing epoxy adhesive. The influence of different content of microcapsules on the shear strength and healing capability of epoxy adhesive were investigated using single-lap-joints with average thickness of adhesive layer of about 180 µm. This self-healing adhesive was used in bonding of 5000 series aluminum alloys adherents after mechanical and alkaline cleaning surface treatment. The adhesion strength was measured and presented as function of microcapsules loading. The results indicated that the virgin lap shear strength was increased by about 26% with addition of 3 wt% of self-healing microcapsules. 12% to 28% recovery of the shear strength is achieved after self-healing depending on the microcapsules content. Scanning electron microscopy was used to study fracture surface of the joints. The self-healing adhesives exhibit recovery of both cohesion and adhesion properties with room temperature healing.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Demonstration of a new unstructured mesh IMC x-ray transport capability in LAP codes

The Advanced Simulation and Computing (ASC) Transport project’s Jayenne Implicit Monte Carlo (IMC) transport library now includes an unstructured mesh capability and is available in a Lagrangian Applications Project (LAP) code. In this presentation, we discuss recent work by the LAP and Transport projects that provides an IMC transport capability for radiation hydrodynamics in the Lagrangian frame. Verification problems testing the new capabilities have been simulated and analyzed, i.e. Marshak wave, Mach 45, Su-Olsen, picket fence, and crooked pipe, both in one and two dimensions. We also present results on two stretch goal problems: a simplified COAX high energy density physics experiment and a supernova shock simulation. Finally, we identify current limitations and future work needed to bring a full capability to the user community.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Demonstration of a new unstructured mesh IMC x-ray transport capability in LAP codes

In this document, the Advanced Simulation and Computing (ASC) Transport Project’s Jayenne team presents evidence that the Los Alamos National Laboratory (LANL) Level 2 milestone statement, Demonstrate a new unstructured mesh IMC x-ray transport capability in LAP codes, due Q4 FY20, has been satisfied with the release and integration of the Jayenne team’s Implicit Monte Carlo (IMC) solver libraries into the lumos multiphysics solver. The Jayenne project’s software includes the algorithms and features prescribed by the milestone description. The lumos software is maintained by the Lagrangian Applications Project (LAP) along with the hydrodynamics code flag and operates under the same ASC program as Jayenne. A set of demonstration problems has been specified, executed, and analyzed.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Corrosivity Screening of Pyrolysis Bio-Oils by Short-Term Alloy Exposures. Laboratory Analytical Procedure (LAP), Issue Date: May 12, 2022

Bio-oils contain organic acids and oxygenated compounds that can lead to corrosion issues during bio-oil processing and storage. This Laboratory Analytical Procedure (LAP) allows for rapid screening of a bio-oil's corrosivity without the need for complex equipment and long-term exposures. A robust and repeatable method for assessing the corrosivity of bio-oils is necessary in order to remove materials degradation as an obstacle to research, upgrading, use and storage of bio-oils. This LAP involves the incubation of a representative alloy, 410 stainless steel (410 SS), specimen in bio-oil over a period of 48 hours at 50 degrees C in a sealed container. The corrosive species in the bio-oil react with and deplete alloy elements such as iron (Fe) and/or chromium (Cr) from the specimen into the bio-oil solution. The depletion of Fe and Cr from the specimen results in a significant mass loss that can be recorded. The mass loss is directly correlated to the corrosivity of a bio-oil. Examples of bio-oils in scope include the ones produced by fast pyrolysis and catalytic fast pyrolysis, as well as liquids produced from hydrothermal liquefaction.

09 BIOMASS FUELS↗

A fracture mechanics analysis of adhesive failure in a single lap shear joint.

Discussion of adhesive fracture of single lap shear joints in terms of a maximum stress criterion and an energy balance. The Goland and Reissner (1944) analysis is used to determine the stress distribution in the adhesive assembly, and the results obtained are introduced into an energy balance to determine the initiation of adhesive fracture. In the stress analysis the loads at the edges of the joint are first determined. This is a problem in which the deformation of the joint sheets must be taken into account and is solved by using the finite-deflection theory of cylindrically bent plates. Then the stress in the joint due to applied loads is determined. This problem is formulated as one in plane strain consisting of two rectangular sheets of equal thickness and unit width. With the aid of this stress analysis and the stresses obtained from the conditions of equilibrium the contributions to the energy change with crack length are calculated. The analysis performed is then compared with a maximum stress criterion for a lap joint.

Devries, K. L.↗

Determination of bulk diffusion lengths for angle-lapped semiconductor material via the scanning electron microscope: A theoretical analysis

A standard procedure for the determination of the minority carrier diffusion length by means of a scanning electron microscope (SEM) consists in scanning across an angle-lapped surface of a P-N junction and measuring the resultant short circuit current I sub sc as a function of beam position. A detailed analysis of the I sub sc originating from this configuration is presented. It is found that, for a point source excitation, the I sub sc depends very simply on x, the variable distance between the surface and the junction edge. The expression for the I sub sc of a planar junction device is well known. If d, the constant distance between the plane of the surface of the semiconductor and the junction edge in the expression for the I of a planar junction is merely replaced by x, the variable distance of the corresponding angle-lapped junction, an expression results which is correct to within a small fraction of a percent as long as the angle between the surfaces, 2 theta sub 1, is smaller than 10 deg.

Vonroos, O.↗

A critical examination of stresses in an elastic single lap joint

The results of an approximate nonlinear finite-element analysis of a single lap joint are presented and compared with the results of a linear finite-element analysis, and the geometric nonlinear effects caused by the load-path eccentricity on the adhesive stress distributions are determined. The results from finite-element, Goland-Reissner, and photoelastic analyses show that for a single lap joint the effect of the geometric nonlinear behavior of the joint has a sizable effect on the stresses in the adhesive. The Goland-Reissner analysis is sufficiently accurate in the prediction of stresses along the midsurface of the adhesive bond to be used for qualitative evaluation of the influence of geometric or material parametric variations. Detailed stress distributions in both the adherend and adhesive obtained from the finite-element analysis are presented to provide a basis for comparison with other solution techniques.

Cooper, P. A.↗

An analysis of interface crack in adhesively bonded lap shear joints

This paper presents an analytical study of interface crack problems in adhesively bonded lap shear joints. A convenient and accurate method of analysis is developed on the basis of conservation laws in elasticity and of the fundamental relationships in fracture mechanics of interface crack problems. The problem is eventually reduced to a system of linear algebraic equations of mixed-mode stress intensity factor solutions. One of the salient features of the present approach is that the interface crack-tip stress intensity solutions can be determined accurately and directly by the information extracted from the far field. Solutions of the interface crack problems in lap shear joints have been obtained for the cases of various adhesive/adherend material systems and geometric configurations of the crack and the joint. Of particular interest is the evaluation of the mixed-mode stress intensity factors and the associated energy release rates. They are determined explicitly to illustrate the fundamental nature of the joint fracture problem.

Wang, S. S.↗

Analysis and test of bonded single lap joints with preformed adherends

A theoretical and experimental study has been conducted to investigate the load transfer of a single lap joint where the adherends have been preformed so that the angle between the line of action of the applied in-plane force and the bond line is reduced. The preforming of the adherend reduces the moment resultant in the adherend at the edge of the overlap region which reduces both the maximum peel and shear stresses in the adhesive, and gives a more uniform shear distribution in the adhesive. An increase in static load transfer of up to 120 percent has been shown, and several orders of magnitude increase in fatigue life have been achieved with modest preform angles. Thus, sizeable benefits can be obtained in the fatigue life or additional load capacity of bonded single lap joints by preforming the adherends.

Sawyer, J. W.↗