At least 55 records · Page 3

Modeling Water Uptake and Pt Utilization in High Surface Area Carbon

Local transport losses limit high-current density performance of fuel-cells, especially at low Pt-loadings. Optimizing catalyst-layer structure and material properties to mitigate these losses is critical for wide-scale fuel-cell commercialization. Carbon supports form the primary porous structure of catalyst layers in which Pt particles are deposited and ionomer films are distributed. Unlike non-porous carbon supports, high surface area carbon support is unique in its relative humidity dependent Pt utilization and performance due to presence of Pt particles in the micropores interior of carbon particles. We model water uptake and Pt utilization in catalyst layers with high-surface-area carbon support. Interactions between functional groups on the carbon pore walls and water play a vital role in controlling water uptake from water vapor by catalyst layers. Ionomer is shown to influence proton access in micropores, even though it may not deposit into the micropores.

08 HYDROGEN↗

Coordinatively unsaturated Al3+ centers as binding sites for active catalyst phases on γ-Al2O3

A combination of ultrahigh resolution spectroscopy and microscopy techniques (ultrahigh magnetic field solid state magic angle spinning nuclear magnetic resonance (MAS-NMR) and high-resolution scanning transmission electron microscopy (HR-STEM)) coupled with first principles DFT calculations reveal the nature of anchoring sites of a catalytically active phase onto the surface of γ-Al2O3. The results obtained unambiguously prove that coordinatively unsaturated penta-coordinate Al3+ (Al3+penta) centers present on the (100) facets of the γ-Al2O3 surface are the sites where the anchoring of Pt occurs. At low loadings, the active catalytic phase is atomically dispersed on the support surface (Pt/ Al3+penta=1), while two dimensional Pt rafts form at higher coverages.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling Low-Platinum-Loading Effects in Fuel-Cell Catalyst Layers

The cathode catalyst layer within a proton-exchange-membrane fuel cell is the most complex and critical, yet least understood, layer within the cell. The exact method and equations for modeling this layer are still being revised and will be discussed in this paper, including a 0.8 reaction order, existence of Pt oxides, possible non-isopotential agglomerates, and the impact of a film resistance towards oxygen transport. While the former assumptions are relatively straightforward to understand and implement, the latter film resistance is shown to be critically important in explaining increased mass-transport limitations with low Pt-loading catalyst layers. Model results demonstrate agreement with experimental data that the increased oxygen flux and/or diffusion pathway through the film can substantially decrease performance. Also, some scale-up concepts from the agglomerate scale to the more macroscopic porous-electrode scale are discussed and the resulting optimization scenarios investigated.

30 DIRECT ENERGY CONVERSION↗

Investigation of Membrane Chemical Degradation as a Function of Catalyst Platinum Loading

Membrane chemical degradation is one of many factors that can impact fuel cell durability. Additionally, the fuel cell’s lifetime heavily depends on the membrane and its ability to maintain chemical and mechanical integrity. Previous studies indicate that chemical degradation is due to the formation of hydroxyl radicals that attack the polymer structure resulting in membrane thinning, pinhole formation, and the release of fluoride and sulfate ions. Membrane durability was investigated using ultra-low Pt electrode loadings (≤ 0.1 mg Pt cm -2 ). Accelerated stress testing (US-DOE protocols) demonstrated that the degradation rate was found to increase with higher Pt loadings. This is most likely due to more heterogeneous sites for radical formation due to hydrogen crossover to the cathode. We also explored membrane degradation rates while varying catalyst layer thickness, ionomer to carbon ratio, and types of carbon support. All of the aforementioned variables impact the membrane degradation rates.

25 ENERGY STORAGE↗

Atomically dispersed single iron sites for promoting Pt and Pt 3 Co fuel cell catalysts: performance and durability improvements

Significantly reducing platinum group metal (PGM) loading while improving catalytic performance and durability is critical to accelerating proton-exchange membrane fuel cells (PEMFCs) for transportation. In this study, we report an effective strategy to boost PGM catalysts through integrating PGM-free atomically-dispersed single metal active sites in the carbon support toward the cathode oxygen reduction reaction (ORR). We achieved uniform and fine Pt nanoparticle (NP) (~2 nm) dispersion on an already highly ORR-active FeN 4 site-rich carbon (FeN 4 –C). Furthermore, we developed an effective approach to preparing a well-dispersed and highly ordered L1 2 Pt 3 Co intermetallic nanoparticle catalyst on the FeN 4 –C support. DFT calculations predicted a synergistic interaction between Pt clusters and surrounding FeN 4 sites through weakening O 2 adsorption by 0.15 eV on Pt sites and reducing activation energy to break O–O bonds, thereby enhancing the intrinsic activity of Pt. Experimentally, we verified the synergistic effect between Pt or Pt 3 Co NPs and FeN 4 sites, leading to significantly enhanced ORR activity and stability. Especially in a membrane electrode assembly (MEA) with a low cathode Pt loading (0.1 mg Pt cm –2 ), the Pt/FeN 4 –C catalyst achieved a mass activity of 0.451 A mg Pt –1 and retained 80% of the initial values after 30 000 voltage cycles (0.60 to 0.95 V), exceeding DOE 2020 targets. Furthermore, the Pt 3 Co/FeN 4 catalyst achieved significantly enhanced performance and durability concerning initial mass activity (0.72 A mg Pt –1 ), power density (824 mW cm –2 at 0.67 V), and stability (23 mV loss at 1.0 A cm –2 ). The approach to exploring the synergy between PGM and PGM-free Fe–N–C catalysts provides a new direction to design advanced catalysts for hydrogen fuel cells and various electrocatalysis processes.

25 ENERGY STORAGE↗

Anion exchange membrane fuel cells: Current status and remaining challenges

The anion exchange membrane fuel cell (AEMFC) is an attractive alternative to acidic proton exchange membrane fuel cells, which to date have required platinum-based catalysts, as well as acid-tolerant stack hardware. The AEMFC could use non-platinum-group metal catalysts and less expensive metal hardware thanks to the high pH of the electrolyte. Over the last decade, substantial progress has been made in improving the performance and durability of the AEMFC through the development of new materials and the optimization of system design and operation conditions. Here in this perspective article, we describe the current status of AEMFCs as having reached beginning of life performance very close to that of PEMFCs when using ultra-low loadings of Pt, while advancing towards operation on non-platinum-group metal catalysts alone. In the latter sections, we identify the remaining technical challenges, which require further research and development, focusing on the materials and operational factors that critically impact AEMFC performance and/or durability. Finally, these perspectives may provide useful insights for the development of next-generation of AEMFCs.

30 DIRECT ENERGY CONVERSION↗

Striving toward noble-metal-free photocatalytic water splitting: The hydrogenated-graphene-TiO 2 prototype

Graphane, graphone and hydrogenated graphene (HG) have been extensively studied in recent years due to their interesting properties and potential use in commercial and industrial applications. The present study reports investigation of hydrogenated graphene/TiO 2-x (HGT) nanocomposites as photocatalysts for H 2 and O 2 production from water without the assistance of a noble metal co-catalyst. By combination of several techniques, the morphologies, bulk/atomic structure and electronic properties of all the powders were exhaustively interrogated. Hydrogenation treatment efficiently reduces TiO 2 nanoparticles, while the graphene oxide sheets undergo the topotactic transformation from a graphene-like structure to a mixture of graphitic and turbostratic carbon (amorphous/disordered) upon altering the calcination atmosphere from a mildly reducing to a H 2 -abundant environment. Remarkably, the hydrogenated graphene-TiO 2-x composite that results upon H 2 -rich reduction exhibits the highest photocatalytic H 2 evolution performance equivalent to low loading of Pt (~0.12 wt%), whereas the addition of HG suppresses the O 2 production. As a result, we propose that such an enhancement can be attributed to a combination of factors including the introduction of oxygen vacancies and Ti 3+ states, retarding the recombination of charge carriers and thus, facilitating the charge transfer from TiO 2 -x to the carbonaceous sheet.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Stabilizing atomic Pt with trapped interstitial F in alloyed PtCo nanosheets for high-performance zinc-air batteries

Recently, considerable attention has been paid to the stabilization of atomic platinum (Pt) catalysts on desirable supports in order to reduce Pt consumption, improve the catalyst stability, and thereafter enhance the catalyst performance in renewable energy devices such as fuel cells and zinc-air batteries (ZABs). Herein, we rationally designed a novel strategy to stabilize atomic Pt catalysts in alloyed platinum cobalt (PtCo) nanosheets with trapped interstitial fluorine (SA-PtCoF) for ZABs. The trapped interstitial F atoms in the PtCoF matrix induce lattice distortion resulting in weakening of the Pt–Co bond, which is the driving force to form atomic Pt. As a result, the onset potentials of SA-PtCoF are 0.95 V and 1.50 V for the oxygen reduction and evolution reactions (ORR and OER), respectively, superior to commercial Pt/C@RuO 2 . When used in ZABs, the designed SA-PtCoF can afford a peak power density of 125 mW cm -2 with a specific capacity of 808 mA h g Zn -1 and excellent cyclability over 240 h, surpassing the state-of-the-art catalysts.

25 ENERGY STORAGE↗

Experimental results with fuel cell start-up and shut-down. Impact of type of carbon for cathode catalyst support

Separate testing protocols for fuel cell startups and shutdowns were developed to distinguish between their effects on reverse currents and CO 2 evolution. The internal currents and the local potentials were measured with different membrane-electrode assemblies (MEAs): we examined the influence of the type of carbon for cathode catalyst support as well as the mitigating effect of low anode Pt loading. In conclusion, significant differences were observed and the experiments also confirmed previous results that the evolved CO 2 accounts for less than 25% of the total exchanged charge.

30 DIRECT ENERGY CONVERSION↗

Contaminant Cation Effect on Oxygen Transport through the Ionomers of Polymer Electrolyte Membrane Fuel Cells

We characterized the effects of cobalt (Co 2+ ) and other cation contaminants on the oxygen (O 2 ) transport properties of the PFSA ionomer used in polymer electrolyte membrane fuel cells (PEMFCs) and gained insight into the mechanisms by which contaminant cations inhibit O 2 transport. Such cations can be released by alloy catalysts and environmental conditions and pose a significant challenge to maintaining high current density performance with low platinum (Pt) loadings. We used a test cell capable of isolating the ionomer from the membrane electrode assembly (MEA), allowing for O 2 transport resistance (R O2 ) measurements using a limiting current technique. We contaminated ionomer membranes with Li + , Na + , Ni 2+ , Co 2+ , and Ce 3+ and found a general increase in R O2 for increased contamination levels and decreased water activity. In addition, our Co 2+ results indicated distinct concentration-dependent regimes. The other cation-form ionomers allowed us to separate the impacts of ion pair strength, multivalency, and reduced water uptake. We believe that these factors cause a more compressed hydrophilic domain and tortuous O 2 diffusion path, and a commensurate increase in R O2 . Lastly, we studied the impact of Co 2+ on an operating PEMFC and found an increase in R O2 consistent with the results of our isolated membrane tests.

25 ENERGY STORAGE↗

Mass-transport properties of electrosprayed Pt/C catalyst layers for polymer-electrolyte fuel cells

Mass-transport properties of electrosprayed catalyst-layers based on Pt/C and ionomer (Nafion) are investigated with hydrogen limiting-current technique, water-vapor-uptake, scanning transmission microscopy (STEM), single-cell testing, and impedance spectroscopy. The hydrogen limiting-current technique provides the transport resistance of the layers ( R CL m t ), which demonstrates to be lower in electrosprayed layers compared with conventional layers, especially at very low platinum loadings (0.025 mg Pt ·cm -2 ) and low cell temperature, denoting superior mass-transport properties. Images of the distribution of Pt, F, and C elements reveal the ionomer preferentially interacting with the Pt nanoparticles. Water-vapor-uptake experiments show larger vapor absorption for electrosprayed than conventional catalyst layers. Such large water-vapor uptake capability is combined with superhydrophobicity, ie. very low interaction with water in liquid phase (wettability). Both apparently contradictory properties result from a particular configuration of the amphiphilic ionomer in the electrosprayed layers, and provide ideal conditions for high mass transport and ionic conductivity in a catalyst layer. Electrosprayed layers as cathode catalyst layers reflect peak response at a loading of 0.17 mg Pt ·cm -2 (18 μm layer thickness when using Pt/C 20 wt% catalyst) where they provide minimal mass-transport and polarization resistances.

08 HYDROGEN↗

Activity and selectivity control by niobium for the preferential oxidation of co on pt supported catalysts

The promotional effect of Nb on Pt supported on alumina or on niobia, was studied for the preferential oxidation of CO (PROX) in hydrogen. The results show a unique effect of Nb as a promoter to Pt. At low Nb loadings on Pt/alumina, the CO oxidation activity and selectivity are significantly increased. The CO selectivity is 100% at conversions up to about 60%. For Pt supported on Nb{sub 2}O{sub 5}, however, the CO oxidation activity is strongly suppressed with low CO conversion but high H{sub 2} oxidation activity. Pt on niobia, therefore, is poorly selective for the PROX reaction, but is an active hydrogen oxidation catalyst, resistant to CO poisoning. For Pt supported on highly loaded Nb-alumina or Nb{sub 2}O{sub 5}, XPS indicate an increase in the Pt and Nb oxidation states. These surface changes also correlate with changes in the DRIFTS spectra suggesting that CO is more weakly adsorbed on Pt/Nb{sub 2}O{sub 5} compared to Pt/Al{sub 2}O{sub 3}, or Pt/Nb-Al{sub 2}O{sub 3}.

08 HYDROGEN↗

Investigating the Catalytic Requirements of Perovskite Fuel Electrodes Using Ultra-Low Metal Loadings

Solid Oxide Fuel Cells (SOFC) with La 0.3 Sr 0.7 TiO 3 (LST)–yttria-stabilized ZrO 2 (YSZ) anodes were prepared by impregnation of LST into porous YSZ scaffolds and then modified by Atomic Layer Deposition (ALD) of Ni, Pt, Pd, Fe, Co. and CeO 2 . Weight loadings as low as 0.01% of Pt, Ni, and Pd were sufficient to decrease anode impedances by orders of magnitude for operation in humidified H 2 at 973 K. The effects of CeO 2 , Co, and Fe were less but still significant. Sintering at higher temperatures was important. Furthermore, possible ways of stabilizing the metal particles and implications for developing ceramic anodes are discussed.

25 ENERGY STORAGE↗

Underlying Substrate Effect on Electrochemical Activity for Hydrogen Evolution Reaction with Low‐Platinum‐Loaded Catalysts

Platinum is known as the best catalyst for the hydrogen evolution reaction (HER) but the scarcity and high cost of Pt limit its widespread applicability. Herein, the role of the underlying substrate on the HER activity of dispersed Pt atoms is uncovered. A direct current magnetron sputtering technique is utilized to deposit transition metal (TM) thin films of W, Ti, and Ta as underlying substrates for extremely low loading of Pt (<1.5 at%). The electrocatalytic performance of as‐synthesized samples for the HER is examined in both alkali and acidic media. The results show that despite the low loading of Pt, the Pt/TM catalysts produce hydrogen at a rate comparable to that of pristine bulk Pt. Pt/TM catalysts also display good stability with less than 5% decay in performance after 10 h of continuous HER operation. Based on the computational study, the excellent performance is attributed to the modified electronic properties of the Pt atoms, offering ideal binding energy for HER due to interaction with the underlying substrates. This work provides a robust and industry‐friendly route toward designing efficient catalytic systems for important electrochemical reactions such as HER and others.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultralow platinum loading for redox-flow battery by electrospinning the electrocatalyst and the ionomer in core-shell fibers

Hydrogen Bromine Redox Flow Batteries (HBRFB) are promising candidates for large scale energy storage, having an excellent balance of system, inexpensive and abundant electrolytes, high power density and near zero kinetic limitations. However, they suffer from corrosion of the hydrogen electrode due to bromine species crossover, which requires a high loading of precious group metal (PGM) electrocatalyst. Herein, a standard catalyst has been used in an electrospun (ES) fiber mat electrode, allowing for a significant (six-fold) reduction in platinum loading from 0.3 mg Pt /cm 2 down to 0.05 mg Pt /cm 2 . At this very low loading, the electrospun electrode attained an impressive specific power of 11.5W/mg Pt , and exhibited excellent durability, with constant power output for 140 charge/discharge cycles. Further, the excellent performance of the electrospun hydrogen electrode is attribute to its unique core-shell nanofiber structure, which improves the stability of the catalyst by preventing bromide species from reaching the catalyst surface.

25 ENERGY STORAGE↗

Performance and cost of automotive fuel cell systems with ultra-low platinum loadings.

An automotive polymer-electrolyte fuel cell (PEFC) system with ultra-low platinum loading (0.15 mg-Pt cm{sup -2}) has been analyzed to determine the relationship between its design-point efficiency and the system efficiency at part loads, efficiency over drive cycles, stack and system costs, and heat rejection. The membrane electrode assemblies in the reference PEFC stack use nanostructured, thin-film ternary catalysts supported on organic whiskers and a modified perfluorosulfonic acid membrane. The analyses show that the stack Pt content can be reduced by 50% and the projected high-volume manufacturing cost by >45% for the stack and by 25% for the system, if the design-point system efficiency is lowered from 50% to 40%. The resulting penalties in performance are a <1% reduction in the system peak efficiency; a 2-4% decrease in the system efficiency on the urban, highway, and LA92 drive cycles; and a 6.3% decrease in the fuel economy of the modeled hybrid fuel-cell vehicle on the combined cycle used by EPA for emission and fuel economy certification. The stack heat load, however, increases by 50% at full power (80 kW{sub e}) but by only 23% at the continuous power (61.5 kW{sub e}) needed to propel the vehicle on a 6.5% grade at 55 mph. The reduced platinum and system cost advantages of further lowering the design-point efficiency from 40% to 35% are marginal. The analyses indicate that thermal management in the lower efficiency systems is very challenging and that the radiator becomes bulky if the stack temperature cannot be allowed to increase to 90-95 C under driving conditions where heat rejection is difficult.

30 DIRECT ENERGY CONVERSION↗

NO{sub 2} gas sensing of flame-made Pt-loaded WO{sub 3} thick films

Unloaded WO{sub 3} and 0.25–1.0 wt% Pt-loaded WO{sub 3} nanoparticles for NO{sub 2} gas detection were synthesized by flame spray pyrolysis (FSP) and characterized via X-ray diffraction (XRD), scanning electron microscopy (SEM) and high resolution transmission electron microscopy (HRTEM). The BET surface area (SSA{sub BET}) of the nanoparticles was measured by nitrogen adsorption. The NO{sub 2} sensing properties of the sensors based on unloaded and Pt-loaded WO{sub 3} nanoparticles were investigated. The results showed that the gas sensing properties of the Pt-loaded WO{sub 3} sensors were excellent to those of the unloaded one. Especially, 0.25 wt% Pt-loaded WO{sub 3} sensor showed highest response to NO{sub 2} than the others at low operating temperature of 150 °C. - Graphical abstract: The response of 0.25 wt% Pt-loaded WO3 sensor was 637 towards NO{sub 2} concentration of 10 ppm at 150 °C. - Highlights: • Unloaded and Pt-loaded WO{sub 3} nanoparticles for NO{sub 2} gas detection were synthesized by flame spray pyrolysis (FSP). • Gas sensing properties of the Pt-loaded WO{sub 3} sensors were excellent to those of the unloaded one. • 0.25 wt% Pt-loaded WO{sub 3} sensor showed highest response to NO{sub 2} at low operating temperature of 150 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗