Distinct Melt Infusion Architectures of Antiperovskite Solid Electrolytes

Antiperovskite solid electrolytes are an emerging class of lithium‐ion conductors distinguished by their unusually low melting points, enabling scalable, low‐temperature processing routes not accessible to most solid electrolytes. In this work, we synthesize phase‐pure chloride (Cl), bromide (Br), and mixed halide (ClBr) variants of antiperovskites and investigate their ionic conductivities in both powder and hot‐pressed forms. Hot pressing significantly enhances conductivity across all compositions, while energy‐dispersive X‐ray spectroscopy (EDS) of the mixed halide system reveals halide surface migration during densification. We further investigate the melt‐infiltration behavior of these electrolytes into substrates relevant to solid‐state battery architectures, including Al and Cu current collectors, conventional NMC and LFP cathodes, and a foamed NMC cathode with a highly porous architecture. The foamed cathode enables deep and uniform electrolyte penetration, highlighting the role of electrode architecture in facilitating melt infiltration. Across all substrates, electrolyte halide chemistry strongly influences wetting behavior, penetration depth, and resulting microstructural morphology. Together, these results establish clear processing–structure relationships for melt‐infiltrated antiperovskite solid electrolytes and demonstrate how electrolyte chemistry and electrode architecture govern interfacial morphology during integration, providing practical guidelines for processing and structural design in solid‐state battery systems.

antiperovskite↗

Nanoscale interfacial melting enables bonding during high velocity microparticle impacts

Melting during high-velocity particle impact has been understood to be typically detrimental to bonding by lowering the strength at the interface and promoting rebound before solidification can occur. Here we establish a possible remedy to this challenge: by dramatically restricting the volume of molten material, its resolidification is accelerated, effectively forming a nanoscale, braze-type joint during impact. In-situ single particle impact imaging is combined with post-mortem structural and chemical analyses to reveal a regime where adhesion is governed not by extensive plastic deformation, but by the kinetics of melt layer resolidification. Furthermore, these findings redefine the role of melting in impact-based processes, establishing transient melting and rapid solidification as a viable strategy for engineering successful adhesion events.

Additive manufacturing↗

Multistage nucleation pathway in LiF molten salt mirrors the crystal–melt interface structure

Despite over a century of studies, fundamental questions remain about the processes governing crystal nucleation from melts or solutions. Research over the past three decades has presented mounting evidence for kinetic pathways of crystal nucleation that are more complex than envisioned by the simplest forms of classical theory. Such observations have been presented for colloidal and elemental systems with covalent and metallic bonding. Despite the technological and geochemical importance of molten salts, similar studies for these ionically bonded systems are currently lacking. Here we develop a machine learning interatomic potential for a model ionic system: LiF. The potential features quantum-level accuracy for both liquid and multiple solid polymorphs over wide temperature and pressure ranges and accurately reproduces experimentally measured properties. Thanks to the efficiency of the potential, which enables microsecond-scale molecular dynamics simulations, induction times for nucleation of LiF solids from their melts are computed over a range of undercoolings. With the aid of a set of robust local order parameters established here, the simulations reveal that homogeneous crystal nucleation in undercooled melts preferentially initiates from liquid regions showing slow dynamics and high bond orientational order simultaneously, and the second-shell order of both precritical nuclei and the surface of postcritical nuclei is dominated by hexagonal close packing and body-centered cubic local structure, even though the nucleus core is dominated by face-centered cubic structure corresponding to the stable rocksalt crystal structure. Finally, we establish a connection between the crystallization pathway and the equilibrium crystal-melt interface structure.

Applied Physical Sciences↗

The effect of blue and infrared laser melting frequency on oxide morphology in 304L

Continuous Wave Laser Beam (LB) melting offers control over the localised heating and cooling of melt pools for welding, brazing, additive manufacturing and solidification. Research into laserliquid metal interactions has primarily focused on the heat and mass transport under large thermal gradients imposed by the localised melting conditions. Recent commercial availability of blue (450 nm) wavelength lasers has enabled the printing of material with poor IR (1064) nm attenuation like Cu. However, little research has been conducted into varying input laser frequency and scan rate at fixed absorption to understand the effects of laser light on surface oxide formation and the underlying liquid metal thermodynamic response. Here, this article conducts laser melting of 304L under Blue (450 nm) and Infrared (IR, 1064 nm) laser frequencies and examines their impact on laser oxide thickness, chemistry and coloration. We find that laser frequencies induce changes in the oxide layer thickness and chemistry that cannot be explained using conventional thermal absorption shifts and fluid dynamics. We suggest that light coupling may have thermodynamic implications for the chemical potential of the liquid metal, which may drive the observed phase behaviour. Identifying mechanisms for the tuning of the chemical potential via laser frequency control could enable the ability to control solidification microstructure and atomic ordering in laser welding and additive manufacturing processes.

304L↗

Preliminary hyperspectral neutron radiography of binder jet 3D printed and melt infiltrated Si–SiC

The preliminary results of hyperspectral neutron radiography of Si–SiC made with binder jet additive manufacturing, subsequent carbon addition, and silicon melt infiltration are presented. The samples were measured in the processing states before and after the melt infiltration to determine if neutrons would help characterize the microstructure to better understand the melt infiltration process. Theoretical Bragg edges were calculated for comparison with the radiographic results. The changes in the Bragg edges from pre- to post-infiltrated reaction-bonded SiC were evident, that could be used to address the differences in microstructures. In conclusion, the preliminary results presented in this study demonstrated that neutron Bragg-edge imaging is possible with Si–SiC reaction-bonded ceramics and can help determine the microstructure of melt infiltrated samples.

SiC↗

Fragile-to-strong transition in liquid As 2 S 3 under pressure: The effect of melt metallization

The well-known classification of glass-forming melts into fragile and strong liquids has several notable exceptions, including water, silica, and certain phase-change materials (PCMs). These exceptional fluid systems exhibit a fragile-to-strong transition (FST) upon cooling: a transformation from a high-temperature liquid with fast atomic dynamics, low viscosity, and low flow activation energy, to a viscous supercooled melt with high energy barriers near the glass transition temperature T g . This behavior is critically important for non-volatile memories, photonic tensor cores, reconfigurable metamaterials, and other devices, that use PCMs, enabling nanosecond-scale crystallization in the fragile regime and long data retention in the strong regime near or below T g . A significant structural transformation is expected between these two viscosity regimes, along with a semiconductor-metal (SC-M) transition upon heating, driven by high internal pressure and associated density increase. By applying high external pressure to the canonical low-conducting chalcogenide melt As 2 S 3 , we observed both the FST and the SC-M transition, occurring simultaneously within the same domain of the P, T−phase space. These findings suggest that the FST is not limited to a few exceptional liquids but is a common phenomenon, at least in systems that exhibit melt metallization within specific regions of their P, T−phase diagrams.

first-principles molecular dynamics↗

Phase change material-to-refrigerant heat exchangers: Experimental validation and uneven melting analysis

Thermal energy storage (TES) using phase change materials (PCMs) enables load shifting and reduces mismatches between the building's thermal demand and the heat pump (HP) system's thermal capacity. While most TES studies have focused on single-phase heat transfer fluids, PCM-to-refrigerant heat exchangers (PRHX), in which the refrigerant undergoes liquid-vapor phase change, remain largely underexplored. Here, to address this gap, this study systematically investigates a shell-and-tube PRHX operating as the condenser in an HP through experiments and simulations. A two-dimensional enthalpy-based finite-volume PRHX model was developed and validated against experimental data, including refrigerant and PCM temperature profiles, PRHX capacity, and system-level performance. Results show three characteristic stages: Stage I, the condenser temperature rapidly increases with PCM in the solid state absorbing sensible heat; Stage II, stable operation during PCM phase change; and Stage III, performance decline once part of the PCM becomes fully melted. Heat transfer analysis revealed that uneven PCM melting along the condenser length was driven primarily by variations in the refrigerant-side heat transfer coefficient, rather than local approach temperature differences. Further study demonstrated that minimizing refrigerant outlet subcooling led to more uniform PCM melting and extended Stages I and II by up to 89%. This paper provides a validated PRHX model, clarifies the mechanisms of uneven PCM melting, and highlights subcooling control as an effective strategy to improve TES performance in HP systems without requiring secondary loops.

Graphite matrix↗

High-pressure high-temperature melting and recrystallization of nanolamellar high-entropy alloys

Additively manufactured (AM) High Entropy Alloys (HEAs) are notable for their exceptional high-yield strength and large tensile ductility. The nanolamellar Eutectic HEA (EHEA) AlCoCrFeNi 2.1 was fabricated by laser powder bed fusion (L-PBF) in the as-printed form (EHEA1) and subsequently annealed at 1000oC (EHEA2) and 600oC (EHEA3) to achieve a broad range of mechanical properties. EHEA2 and EHEA3 samples were studied using Scanning transmission electron microscopy (STEM), energy dispersive X-ray diffraction (EDXRD) at high-pressures and high temperatures, nanoindentation hardness and modulus measurements. According to EDXRD EHEA2 and EHEA3 are composed of B2 and L1 2 phases. High-pressure high-temperature EDXRD studies show melting for EHEA2 at 1698 ± 25 K at a pressure of 6.5 GPa and melting for EHEA3 at 1598 ± 25 K at a pressure of 5.8 GPa. Post-melt and recrystallized samples were recovered at ambient conditions, and XRD analysis showed retention of B2 and L1 2 phases, although a new σ phase appeared for both EHEA2 and EHEA3 samples due to high-pressure and high-temperature melting and recrystallization experiment. SEM analysis also demonstrated the preservation of the nanolamellar morphology. Nanoindentation studies revealed that recrystallized EHEAs retain their original mechanical property hierarchy, with EHEA3 being 47% harder than EHEA2, largely related to higher content of B2-phase and retention of nanolamellar morphology. We also present Pressure-Volume-Temperature (P-V-T) data for 3-D printed and annealed eutectic high entropy alloys and extract mechanical and thermal properties data.

36 MATERIALS SCIENCE↗

Melting of charge density waves in low dimensions

Charge density waves (CDWs) are collective electronic states that can reshape and melt, even while confined within a rigid atomic crystal. In two dimensions, melting is predicted to be distinct, proceeding through partially ordered nematic and hexatic states that are neither liquid nor crystal. Here, we measure and explain how continuous, hexatic melting of incommensurate CDWs occurs in low-dimensional materials. As a CDW is thermally excited, disorder emerges progressively—initially through smooth elastic deformations that modulate the local wavelength and subsequently via the nucleation of topological defects. Experimentally, we track three hallmark signatures of CDW melting—azimuthal superlattice peak broadening, wavevector contraction, and integrated intensity decay.

42 ENGINEERING↗

Solidification cracking of laser melted commercial-purity tungsten

The high melting temperature of tungsten (W) makes it an attractive candidate for energy generation applications; however, its use is limited by its poor ductility at low temperatures. This limitation affects even melt-based additive manufacturing (AM) processes such as laser powder bed fusion (PBF-LB), with as-fabricated pure W exhibiting both longitudinal and transverse cracks. Metallurgical and processing factors that affect these cracks are still being explored. This work utilizes powderless single-tracks on pure W plates made over a range of power and velocity combinations in three unique PBF-LB setups: one with flowing argon, one with continuous vacuum, and an in situ high-speed synchrotron X-ray radiography setup. Each had different oxygen activities in their build environments. Longitudinal cracks with oxides appearing to exude from the crack were found for tracks deposited in a build environment with argon shield gas, while no such cracks were observed for builds conducted in vacuum. A calculation showed that direct oxygen ingress into the melt pool from the build environment is negligible when argon shield gas is present. Thus, incorporation of spatter is a likely mechanism for oxygen ingress into the melt pool. Radiography showed extensive keyholing, spatter generation, and crack formation at keyhole porosity. A heat transfer calculation showed the crack formation time was consistent with cooling below its ductile-to-brittle transition (DBT) temperature. This work identifies solidification cracking as a feasible mechanism in pure W beyond the well-known DBT related cracking.

Materials science↗

High temperature melting of dense molecular hydrogen from machine-learning interatomic potentials trained on quantum Monte Carlo

We present results and discuss methods for computing the melting temperature of dense molecular hydrogen using a machine learned model trained on quantum Monte Carlo data. In this newly trained model, we emphasize the importance of accurate total energies in the training. We integrate a two phase method for estimating the melting temperature with estimates from the Clausius–Clapeyron relation to provide a more accurate melting curve from the model. We make detailed predictions of the melting temperature, solid and liquid volumes, latent heat, and internal energy from 50 to 180 GPa for both classical hydrogen and quantum hydrogen. At pressures of roughly 173 GPa and 1635 K, we observe molecular dissociation in the liquid phase. Here, we compare with previous simulations and experimental measurements.

08 HYDROGEN↗

Analytical model for balling defects in laser melting using rivulet theory and solidification

In laser welding and additive manufacturing communities, the balling (humping) defect is primarily attributed to the Plateau–Rayleigh fluid instability (PRI) with a few authors suggesting fluid jetting and volume conservation as alternative mechanisms. As analytical descriptions of these mechanisms are unavailable, combining them into a single formalism is unfeasible. We present a new model of PRI with higher accuracy, accounting for competition with solidification, to compare the expected behavior with known experimental trends when fluid jetting is neglected. We adapt a rivulet instability model from fluid physics to account for the stabilizing effects of the substrate, which the traditional cylindrical-jet geometry does not account for and estimate the instability growth rate. Our model yields a continuous transition from non-balling to balling hitherto lacking in current literature and predicts instability growth at higher wavelengths with strong sensitivity to the solidification front curvature. While the fluid surface is most unstable for shallow melt pools, the absolute magnitude of balling relevant to printing defects scales with melt pool depth and has a maximum for a given melt pool geometry. Synchrotron-based x-ray radiography of thin samples indicates that PRI growth rates and solidification can be comparable in magnitude and thus compete, as we find in this work. We predict that deviations between model predictions and our experimental results demonstrate the importance of fluid flows and heat transport in the balling process. Our experiments further demonstrate at least one mechanism by which the melt pool length and the balling wavelength are not equivalent, as commonly claimed.

Taylor, Z. [Stanford Univ., CA (United States); SL↗

Melting temperature of bismuth to 55 GPa using synchrotron X-ray phase contrast imaging

The melting temperature of elemental bismuth under high pressure has been measured to 55 GPa using synchrotron X-ray phase-contrast imaging in the laser-heated diamond anvil cell. Imaging of solid-liquid interface formation, combined with radiometric temperature and X-ray diffraction measurements, reveals a pronounced reduction in melting boundary slope in Bi-V with pressure. The unusually steep initial slope is attributed to low configurational entropy of melting, arising from structural ordering and coordination matching in the cool liquid, while slope reduction is driven by entropy increase correlated with significant liquid structure changes with rising pressure and temperature. Finally, the data rule out kinetic effects on melting in shock compression experiments and demonstrate the need for improved theoretical phase diagrams.

Materials science↗

Melting curves of atomic hydrogen and deuterium calculated using path-integral Monte Carlo

We calculate the melting line of atomic hydrogen and deuterium up to 900 GPa with path-integral Monte Carlo using a machine-learned interatomic potential. We improve upon previous simulations of melting by treating the electrons with reptation quantum Monte Carlo, and by performing solid and liquid simulations using isothermal-isobaric path-integral Monte Carlo. Here, the resulting melting line for atomic hydrogen is higher than previous estimates. There is a small but resolvable decrease in the melting temperature as pressure is increased, which can be attributed to quantum effects.

08 HYDROGEN↗

New Constraints on the Melting Temperature and Phase Stability of Shocked Iron up to 270 GPa Probed by Ultrafast X-Ray Absorption Spectroscopy

Studying the properties and phase diagram of iron at high-pressure and high-temperature conditions has relevant implications for Earth’s inner structure and dynamics and the temperature of the inner core boundary (ICB) at 330 GPa. Also, a hexagonal-closed packed to body-centered cubic (bcc) phase transition has been predicted by many theoretical works but observed only in a few experiments. The recent coupling of high-power laser with advanced x-ray sources from synchrotrons allows for novel approaches to address these issues. Here, we present a study on shock compressed iron up to 270 GPa and 5800 K probed by single-pulse (100 ps FWHM) x-ray absorption spectroscopy (XAS). Based on the analysis of the XAS spectra, we provide structural identification and bulk temperature measurements along the Hugoniot up to the melting. These results rule out the predicted transition to a high-temperature bcc phase and allow one to discriminate among existing equations of state models and melting curves. In particular, we report the first bulk temperature measurement in shock compressed iron on the melting plateau at 240(20) GPa and 5345(600) K. The melting curve resulting from our work extrapolates to a temperature of 6202(514) K at 330 GPa and represents a refined upper bound for the ICB temperature. Published by the American Physical Society 2024

Balugani, S.↗

Melt Pool characteristics on surface roughness and printability of 316L stainless steel in laser powder bed fusion

Purpose Surface quality and porosity significantly influence the structural and functional properties of the final product. This study aims to establish and explain the underlying relationships among processing parameters, top surface roughness and porosity level in additively manufactured 316L stainless steel. Design/methodology/approach A systematic variation of printing process parameters was conducted to print cubic samples based on laser power, speed and their combinations of energy density. Melt pool morphologies and dimensions, surface roughness quantified by arithmetic mean height (Sa) and porosity levels were characterized via optical confocal microscopy. Findings The study reveals that the laser power required to achieve optimal top surface quality increases with the volumetric energy density (VED) levels. A smooth top surface (Sa < 15 µm) or a rough surface with humps at high VEDs (VED > 133.3 J/mm 3 ) can serve as indicators for fully dense bulk samples, while rough top surfaces resulting from melt pool discontinuity correlate with high porosity levels. Under insufficient VED, melt pool discontinuity dominates the top surface. At high VEDs, surface quality improves with increased power as mitigation of melt pool discontinuity, followed by the deterioration with hump formation. Originality/value This study reveals and summarizes the formation mechanism of dominant features on top surface features and offers a potential method to predict the porosity by observing the top surface features with consideration of processing conditions.

Engineering↗

Sulfur speciation in dacitic melts using X-ray absorption near-edge structure spectroscopy of the S K -edge (S-XANES): Consideration of radiation-induced changes and the implications for sulfur in natural arc systems

Abstract The synchrotron technique of micro X-ray absorption near-edge structure spectroscopy at the sulfur K-edge (S-XANES) provides a unique opportunity to measure the proportion of different oxidation states of sulfur (S) in silicate glasses. Although applied extensively in the analysis of basaltic silicate glasses, few S-XANES studies have investigated variations in S oxidation states with fO2 in felsic silicate glasses. In addition, no study has systematically compared the S-XANES results obtained from the same samples at different photon flux densities to quantify the relationship between exposure time and changes in S speciation in silicate glass, as has been done for Fe and V. This study evaluates observed differences in S speciation measured in experimentally produced H2O-saturated dacitic glasses over a range of reducing to oxidizing conditions (from log fO2 = ΔFMQ-0.7 to ΔFMQ+3.3; FMQ is the fayalite-magnetite-quartz mineral redox buffer) and equilibrated at 1000 °C and 300 MPa. S-XANES spectra were collected at three different photon flux densities using three microspectroscopy beamlines. As is observed in S-XANES analyses of basaltic silicate glasses, beam-induced changes to the S6+/ΣS are observed as a function of photon flux density and beam exposure time. Our results demonstrate that silicate glasses of dacitic composition undergo beam-induced photo-reduction in samples equilibrated at ΔFMQ > +1.75 and photo-oxidation if equilibrated at ΔFMQ < +1. The time required to observe beam-induced changes in the spectra varies as a function of flux density, and our study establishes an upper photon density limit at ~1.0 × 1012 photons/µm2. The S6+/ΣS calculated from spectra collected below this absorbed photon limit at intermediate flux densities (~1–4 × 109 photons/s per µm2) are affected by beam damage, as no conditions were found to be completely free of beam-induced changes. However, the S6+/ΣS ratios calculated below the limit at intermediate flux densities are consistent with thermodynamic constraints, demonstrating that S6+/ΣS ratios calculated from S-XANES spectra can be considered reliable for estimating the oxygen fugacity. Our results carry important implications for the S budget of felsic magmas and dissolution mechanisms in evolved melts. While our results from all three flux densities show the presence of S4+ dissolved in relatively oxidized (ΔFMQ > +1.75) dacitic glass, even in the spectra exposed to the lowest photon densities, we are unable to rule out the possibility that the S4+ signal is the result of instantaneous X-ray irradiation induced beam damage using S-XANES alone. When our spectra are compared to S-XANES spectra from basaltic silicate glasses, important differences exist in the solubility of S2– and S6+ between dacitic silicate melts, pointing to differences in solubility mechanisms as melt composition changes. This study highlights the need for further investigation into beam damage systematics, presence of S4+, and the solubility mechanisms of different oxidation states of S as silicate melt composition changes.

Geochemistry & Geophysics↗

Optimization of Scrap Melting Using an Electric Arc in Steel Manufacturing

Steel industry is crucial to the national economy and security. Around 67% of crude steel in the U.S is produced in electric arc furnaces (EAF), which is energy intensive. Around 140 EAFs operate in the U.S., consuming about 8.6x10 7 MMBtu/year of electricity. One of major challenges for EAFs includes maximizing the efficiency of the electrical energy provided in the form of electric arcs to melt various scrap mixes. To address this issue, a computational fluid dynamics (CFD) methodology is chosen to analyze scrap melting using the electric arc. Due to complex furnace phenomena and the wide variety of potential scenarios, high performance computing (HPC) is essential to yield comprehensive and detailed CFD analyses and systematic parametric studies for optimized EAF operation. The objectives are to 1) simulate scrap melting using electric arc, 2) evaluate electrode/arc position for optimum scrap melting and 3) establish reduced order model for CFD data-base for fast model calculation.