Search NASA⌕ Search

SEARCH · Search NASA

Results for “module degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Comparative Analysis of Hotspot Stress Endurance in Pristine and Thermal Cycled Prestressed Glass–Glass Photovoltaic Modules

Hotspots pose a significant long-term reliability challenge in photovoltaic (PV) modules that can have a detrimental impact on the efficiency, safety, and financial viability of a PV system. This paper aims to evaluate the endurance of hotspot stress in pristine and prestressed glass–glass (GG) modules. The accelerated prestressing was conducted for 600 thermal cycles (TC600) to represent decades of field exposure. GG modules are quickly becoming an alternative to the traditional glass–backsheet (GB) modules that have been the industry standard. Unlike other conventional studies that subject only pristine modules to hotspot stress, this paper evaluates the performance of an accelerated/simulated field-aged GG module (using TC600) and a pristine GG module. Pre- and post-characterizations were performed before and after each test to determine changes in electrical performance and observe any defects in GG modules. During the hotspot test, an approximately 200 °C maximum cell temperature was observed with a cell shading of 25% (the worst-case shading ratio). After the hotspot test, electroluminescence imaging indicated that most cells in the prestressed GG module exhibited severe damage whereas no significant defects were evident in the pristine GG module where the prestressed GG module degraded 8.2% and the pristine GG module degraded 1.5% in maximum power. These findings are critical for the industry, considering that GG bifacial modules will dominate the market.

14 SOLAR ENERGY↗

On the Path to SunShot - The Role of Advancements in Solar Photovoltaic Efficiency, Reliability, and Costs

Although tremendous progress has been made in reducing the cost of PV systems, additional LCOE reductions of 40%–50% between 2015 and 2020 will be required to reach the SunShot Initiative’s targets (see Woodhouse et al. 2016). Understanding the tradeoffs between installed prices and other PV system characteristics—such as module efficiency, module degradation rate, and system lifetime—are vital. For example, with 29%-efficient modules and high reliability (a 50-year lifetime and a 0.2%/year module degradation rate), a residential PV system could achieve the SunShot LCOE goal with modules priced at almost $1.20/W. But change the lifetime to 10 years and the degradation rate to 2%/year, and the system would need those very high-efficiency modules at zero cost to achieve the same LCOE. Although these examples are extreme, they serve to illustrate the wide range of technological combinations that could help drive PV toward the LCOE goals. SunShot’s PV roadmaps illustrate specific potential pathways to the target cost reductions.

14 SOLAR ENERGY↗

Accelerated Stress Testing of Perovskite Photovoltaic Modules: Differentiating Degradation Modes with Electroluminescence Imaging

Herein, electroluminescence (EL) and thermal imaging are used to examine p–i–n metal halide perovskite (MHP) photovoltaic (PV) mini-modules (MA0.6FA0.4PbI3, 20 cells, 78 cm2) before and after indoor-accelerated stress testing or outdoor deployment. Distinct spatial patterns in the EL images emerge, which depend on the external stress conditions experienced by the mini-module. Imaging results highlight a distribution of dark speckle features that dominate after UV stress, attributed to widespread interfacial contact degradation. Lateral intensity gradients across cells dominate after thermal cycling (TC) stress, attributed to current crowding near scribe defects. While current–voltage analysis alone does not give full insight on the degradation process, this study shows that distinct degradation modes can be further defined by multimodal electro-optical imaging (i.e., EL combined with photoluminescence and dark lock-in thermography). Neither UV exposure nor TC-accelerated stress testing alone replicates the same degradation signatures observed after outdoor deployment, suggesting that multiple degradation modes occur under concurrent stressors outdoors. Finally, spatial characterization of degradation modes in MHP PV mini-modules before and after accelerated stress testing lays the groundwork for developing targeted accelerated stress testing procedures through comparison with outdoor aging.

14 SOLAR ENERGY↗

Evaluating and predicting molecular mechanisms of adhesive degradation during field and accelerated aging of photovoltaic modules

Extending photovoltaic (PV) module lifetimes beyond 30 years is a goal of significant priority. A challenge that must first be addressed, however, is the development of a predictive reliability model that captures the synergy of terrestrial stressors on module degradation, particularly at encapsulant interfaces. Using a metrology designed specifically for PV modules, a comprehensive study of the widely used ethylene vinyl acetate encapsulant was performed in which encapsulant adhesion was evaluated as a function of environmental stressors (UV exposure, temperature, and humidity) for modules aged both under accelerated lab and internationally located field conditions for months to nearly 3 decades. Mechanical and chemical characterization methods are combined with fundamental polymer reaction engineering to unravel the degradation processes active at the molecular scale that lead to encapsulant delamination. An analytical and modular model framework is put forward enabling the prediction of long-term PV module durability, starting from fundamental principles at the molecular level and explicitly accounting for bond rupture events in the bulk encapsulant and at the encapsulant interfaces. Successful parameter tuning to adhesion data indicates a dominant occurrence of deacetylation, β-scission, and hydrolytic depolymerization, respectively. The model contributes to the longstanding challenge of predicting module lifetimes in any geographic location while minimizing time-consuming and costly aging studies.

14 SOLAR ENERGY↗

Use of non-contact voltmeter to quantify potential induced degradation in CdTe modules

Potential induced degradation (PID) is a significant reliability issue for photovoltaic modules in the field. Conventionally, to detect the PID-affected modules, all the modules in a string are individually disconnected and measured using I-V (current–voltage) tracers. It is extremely time-consuming, expensive and unsafe (if the module connectors are field aged) approach. In our approach, we aim detecting the PID-affected modules quickly, inexpensively and safely without disconnecting individual modules in the string. In this study, contactless electrostatic voltmeter’s (ESV) strength was explored to detect the PID-affected cadmium telluride (CdTe) modules in a string. These contactless measurements on high-voltage PV strings could make this technique unique and preferable to detect PID-affected modules in a string compared to the I-V curve method. In this work, a CdTe module was stressed for PID using the Aluminum (Al) foil method in a walk-in environmental chamber, which resulted in a reduction of module's peak current (I max ), peak voltage (Vmax), and fill factor (FF), and hence power (Pmax). Outdoor light I-V, EL, and ESV measurements were performed pre- and post-PID to determine the effectiveness of the non-contact ESV technique. Further, the ESV technique successfully detected the change in V max , and hence Pmax, compared to the pre-and post-PID conditions. A difference of less than 2% was observed in the results of the non-contact and non-interruptive method compared to the conventionally used interruptive voltmeter or I-V tracer method. This technique and the test results demonstrate a significant promise to identify poor-performing modules in PV string without disconnection of individual modules in the string.

14 SOLAR ENERGY↗

Review of Potential–Induced Degradation in Bifacial Photovoltaic Modules

Bifacial modules are increasingly deployed in the field and are expected to represent half of the market share within 10 years. Their rear structure differs from monofacial modules to allow additional light absorption. However, it brings new reliability challenges to address. In particular, the risk of potential-induced degradation (PID) is increased as both module sides are impacted. Different PID processes have been identified in the literature: shunting type (PID-s), polarization type (PID-p), Na penetration type, and corrosion type (PID-c). Their occurrence depends on the photovoltaic system configuration as well as the module's materials. Apart from PID-s, PID processes are not well understood and extensive research is needed to elucidate the PID scenario and underlying mechanisms. Herein, current knowledge about PID processes and their impact on the main bifacial modules in the market are gathered with the aim to guide future research. Bifacial module technologies and leakage current paths leading to PID are described. Indoor and outdoor PID testing methods are detailed. For each bifacial module technology, the PID processes are investigated with their indicators, mechanism and recovery process. Furthermore, PID-impacting factors and limitation solutions are finally reported and a state of the art on PID modeling is presented.

14 SOLAR ENERGY↗

Towards Commercialization of Low-Cost, Crack-Tolerant, Screen-Printable Metallization by Full-Size Module Testing and Field Characterization

This project is motivated by the need to develop a materials engineering solution to reduce solar module degradation caused by cell cracks. The cell-crack-induced power loss is a long-term degradation mechanism and one of the main causes of solar panel field failures. Cell cracks can occur during module fabrication, transportation, installation, and long-term operation due to thermomechanical stressors. Our team’s internal estimation – based on the national weather pattern, frequency of severe weather, and 39- GW asset survey by Heliolytics – reveals that the cell-crack-induced module degradation translates to lost revenues >$17B over an average 5-year period for solar farm owners and to reduced reliability (<25 years panel lifetime) for solar energy consumers. In response to this challenge, the prime recipient offers a metal matrix composite (MMC) silver paste that is tailor-engineered for screen-printing gridlines and busbars, which serve as the electrical contacts on solar cells. We formulate our MMC paste by adding low-cost (∼0.02¢/WDC for research grade), surface-engineered carbon nanotubes to commercially available silver paste. The MMC paste offers a drop-in, cost-effective solution to cell cracks for solar cell and module manufacturers. The main goal of this project was to conduct field-relevant, module-level analysis and qualification of MMC metallization.

14 SOLAR ENERGY↗

Near-Busbar Degradation of Screen-Printed Metallization in Silicon Photovoltaic Modules

We study photovoltaic (PV) module degradation after extended accelerated stress testing including 2000 hours of damp heat followed by a current-injection procedure meant to stabilize defects linked to light-induced degradation. In addition to de-stabilization/recovery of light-induced defects, we observe severe series resistance due to loss of contact between the Si cell and near-busbar screen-printed metallization (i.e. grid finger delamination). Using scanning electron microscopy and energy dispersive x-ray spectroscopy on cell fragments cored from the module, we show poor contact is caused by a gap between the screen-printed Ag metallization and Si due to missing glass frit.

degradation↗

Development of Low-Cost, Crack-Tolerant Metallization Using Screen Printing

One of the ways to reduce the cost of solar electricity to 3/kWh, thus reaching parity with fossil-fuel-based generation, is to reduce the degradation rate of solar modules and extend their lifetime well beyond 30 years. The extended module lifetime in turn can positively influence the financial model and the bankability of utility-scale PV projects. Today, the highest-riskpriority solar module degradation mechanism is what is known as hot spots, often induced by cell cracks. In order to address this degradation mechanism, we make use of low-cost, multi-walled carbon nanotubes embedded in commercial screen-printable silver pastes. When the carbon nanotubes are properly functionalized and appropriately incorporated into commercial silver pastes, the resulting metal contacts on solar cells, after screen-printing and firing, show exceptional fracture toughness. These composite metal contacts possess increased ductility, electrical gap-bridging capability up to 50 um, and 'self-healing' to regain electrical continuity even after cycles of complete electrical failure under extreme strain.

14 SOLAR ENERGY↗