Search NASA⌕ Search

SEARCH · Search NASA

Results for “oxidation kinetics”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

High temperature oxidation of corrosion resistant alloys from machine learning

Parabolic rate constants, k p , were collected from published reports and calculated from corrosion product data (sample mass gain or corrosion product thickness) and tabulated for 75 alloys exposed to temperatures between ~800 and 2000 K (~500–1700 °C; 900–3000°F). Data were collected for environments including lab air, ambient and supercritical carbon dioxide, supercritical water, and steam. Materials studied include low- and high-Cr ferritic and austenitic steels, nickel superalloys, and aluminide materials. A combination of Arrhenius analysis, simple linear regression, supervised and unsupervised machine learning methods were used to investigate the relations between composition and oxidation kinetics. The supervised machine learning techniques produced the lowest mean standard errors. The most significant elements controlling oxidation kinetics were Ni, Cr, Al, and Fe, with Mo and Co composition also found to be significant features. The activation energies produced from the machine learning analysis were in the correct distributions for the diffusion constants for the oxide scales expected to dominate in each class.

Materials Science↗

FWP FEAA149: “Next Generation Environmental Barrier Coatings”

Environmental barrier coatings (EBCs) are required coatings for utilization of SiC/SiC ceramic matrix composite (CMC) components in gas turbines, where the EBC represents the life-limiting factor for such components. EBC/CMC systems have shown success in aero-engine applications with increased turbine inlet temperatures and improved efficiencies, which are achieved through higher temperature stability, lower density, and decreased reliance on cooling air compared to traditional superalloys. While industrial gas turbines (IGTs) do not currently utilize SiC/SiC CMCs, the current shift towards low-carbon or carbon-free fuel sources for power generation could result in a need for EBC/CMC components with higher temperature capabilities. In this work, three tasks were outlined to improve understanding of EBC lifetimes to encourage use in IGTs with carbon-free fuel such as hydrogen: 1. Define the bond coating oxidation kinetics and EBC failure criteria, 2. Measure thermal expansion coefficients of each layered material, and 3. Perform advanced characterization and modeling to assess EBC lifetimes. Cyclic steam oxidation tests were conducted on various EBC/Si/SiC chemistries and EBC/SiC architectures to define substrate oxidation kinetics and EBC failure modes. An open-source code was developed to quantify the undulating thermally grown oxide thickness with thousands of measurements from specimen cross-section images. Bond coating oxidation kinetics were determined and used to develop a kinetic and thermodynamic model for predicting EBC lifetimes. High-temperature Raman spectroscopy was utilized for determining the SiO 2 thermally grown oxide phase transformation as the life-limiting feature for EBCs. Model efforts supported the claim that the SiO 2 phase transformation causes elevated stress during thermal cycling with associated cracking that decreases the adhesion strength of the EBC, eventually resulting in coating spallation. The finite element model subroutine will be made publicly available upon internal review. Further development of an EBC lifetime model for IGTs involves definition of a critical SiO 2 thickness for EBC spallation and must also consider both environmental (gas velocity, pressure, etc.) and specimen (EBC dopants, layer architectures, etc.) effects into predicted bond coating oxidation kinetics for long-lifetime components.

36 MATERIALS SCIENCE↗

Phase-field modeling of alloy oxidation at high temperatures

Oxide growth is a complex process involving transport of reactive species, heterogeneous reactions, and microstructure evolution. Predicting oxidation kinetics and especially the oxide morphological change has been a long-standing challenge. Here we develop a phase-field model for predicting the oxide growth kinetics of a multicomponent alloy during high temperature oxidation, focusing on internal oxidation (non-protective) and its transition to external oxidation (protective). In this work, the predicted kinetics and oxide morphology are analyzed and compared to the classical Wagner’s theory and an existing analytical model by Zhao and Gleeson. Some assumptions used in the analytical models and the limitation are discussed. In addition, it is demonstrated that the morphology and distribution of the initial oxide nuclei play an important role in the later stage oxide connectivity and thus the transition to external oxidation.

36 MATERIALS SCIENCE↗

A kinetic model for simulating non-equilibrium mass transport in oxides applied to hematite growth under irradiation

We propose an approach to simulating the dynamic evolution and transport of charged point defects within and through the oxide scales that form during corrosion. The method follows the cluster dynamics formalism widely adopted for radiation damage in solids, which can apply in both quasi-static and far from equilibrium conditions, such as in radiation environments. By treating each charged defect as a cluster of an atomic defect and associated unit charges, the proposed model flexibly allows charge state transitions and shifts in the Fermi level by absorption and emission of charge carriers from point defects in a reaction network with rates constrained by local equilibrium. Applying this model to hematite predicts changes in self-diffusion and oxidation kinetics in irradiation environments, surprisingly showing reduced oxidation rates in many conditions, despite enhanced self-diffusion. In conclusion, the origin of this effect lies in a change in Fermi level induced by excess vacancies formed under irradiation, which in turn suppresses the transport of cation interstitials which facilitate hematite growth.

36 MATERIALS SCIENCE↗

White-light interferometry for early-stage metal oxide growth characterization

Oxidation of metals can provide a functional oxide film or an oxide layer that can lead to material degradation causing performance limiting concerns. Because of the technological and economic impacts of oxidation, understanding early-stage oxidation growth and its mechanisms is of high importance. Unfortunately, poor empirical data during early-stage oxidation has left our current understanding of oxidation incomplete and woefully inadequate. Measurement techniques previously used for oxidation kinetics characterization include microbalance, x-ray diffraction, Fourier-transform infrared spectroscopy, and spectroscopic ellipsometry. However, these techniques lack the necessary time-resolution or vertical resolution in addition to not providing any spatial data, which is essential to early-stage oxidation studies to understand both oxidation kinetics and mechanisms. Here, a novel rapid and surface-sensitive data collection technique that provides three-dimensional spatial data of a growing oxide layer with sub-nanometer thickness resolution using white-light interferometry has been developed. This technique will be the first technique capable of providing real-time spatial results of early-stage oxidation growth. The effectiveness of this characterization tool is shown by observing the early-stage oxidation kinetics and film cracking of uranium heated to 90 °C under 500 torr of pure O 2 . Initially a parabolic oxidation growth is observed. Once the oxide layer reaches ≈ 30 nm, the epitaxial stresses between the uranium substrate and oxide film layer causes localized cracking in addition to the observed transition of the parabolic growth rate to a linear growth rate. The results of the white-light interferometry are verified by glancing incidence x-ray diffraction.

47 OTHER INSTRUMENTATION↗

Oxidation Lifetime Modeling of 625 and 120 Foils After Long-term Exposure in Flowing Air + 10% ${\hbox {H}_2\hbox {O}}$ at 700 and 800 $^\circ$C

A model describing oxidation kinetics considering simultaneous oxidation and volatilization of external oxide scales was integrated with a CALPHAD-based coupled thermodynamic and kinetic approach to predict the oxidation-induced lifetime of foils of alloys 625 and 120. Long-term exposures in flowing air +10% H 2 O at 700 and 800 °C under two flow velocities were used to validate the modeling results. The time to a critical Cr concentration of 10 wt% at the oxide/alloy interface, t 10 , was shown to correlate with the breakdown of the Cr 2 O 3 scale for the studied experimental conditions. Finally, the modeling approach was extended to consider time-dependent oxidation and volatilization rate constants to develop a more appropriate lifetime criterion for microturbine recuperator foils.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High and Ultra-High Temperature Reaction Kinetics by Single Nanoparticle Mass Spectrometry

Methodology is presented for non-destructive, optically-detected single nanoparticle (NP) mass spectrometry, with the goal of extracting surface reaction kinetics for single NPs at high temperatures. Methods for determining the NP charge, mass, and temperature as a function of time are discussed, and the data are used to extract both the absolute kinetics for mass change, as well as the efficiencies of the surface processes that cause them. Factors that contribute to the uncertainties in absolute and relative mass determination, and in the resulting kinetic parameters, are discussed. The method allows the NP-to-NP variations in initial reactivity to be measured directly, along with the time evolution of reactivity resulting from NP structural/compositional changes that occur under reaction conditions. The strengths and limitations of single nanoparticle mass spectrometry as a high temperature surface kinetics tool are discussed in the context of sublimation and O2 oxidation kinetics experiments for single hafnium (Hf) NPs at temperatures ranging above 2400 K. The Hf oxidation kinetics are compared to analogous oxidation experiments for silicon, graphite, and carbon black NPs. In all four cases, the oxidation chemistry was dominated by processes that result in net mass loss, and the distinct mechanisms responsible are discussed. All four NPs also eventually passivated, i.e., the efficiencies for oxidative etching decreased by at least two orders of magnitude, relative to the initial efficiencies. Furthermore, the passivation mechanisms, which are quite different for carbon, compared to silicon or hafnium, are discussed. Carbon NP passivation is attributed to structural isomerization leading to fully coordinated, fullerene-like NP surfaces, while for silicon and hafnium, passivation results from delayed formation of an oxide layer, triggered by accumulation of oxygen in the NP sub-surface region.

36 MATERIALS SCIENCE↗

The microscopic mechanisms of high temperature oxidation of Haynes 282

Nickel-based superalloy finds widespread applications in aerospace and extreme environments. They are known for their high temperature oxidation resistance under extended periods. However, the oxide formation and evolution which sets the stages for the later parabolic oxidation kinetics is not fully understood. This paper aims to provide new insights into the transient stage oxidation mechanism and kinetics of a typical Ni-based superalloy (Haynes 282). While tracking the chemical and microstructural evolution under micrometer scale at 800°C, we show that the oxide scale and its grain boundary species change significantly during the initial stages of oxidation and can have a profound impact on the oxidation kinetics. Cr 2 O 3 forms initially at the grain boundary along with minor amount of Al 2 O 3 . Then, the grain boundary region is enriched with copious amounts TiO 2 while Cr migrates away from the grain boundary. A noticeable change in the isothermal oxidation kinetics observed likely results from a mechanistic change from uniform surface oxidation to preferential outward diffusion of Ti 4+ ions through the grain boundary. Through first-principles calculations combined with energy dispersive spectroscopy, we confirmed the preferential outward diffusion of Ti 4+ ions as the diffusion barrier is lower for Ti than Cr along the grain boundaries. In conclusion, these findings highlight the critical role of early-stage grain boundary oxidation dynamics in dictating the long-term oxidation resistance of Ni-based superalloys and provide a foundation for future strategies to enhance their performance in extreme environments.

DFT↗

Uranium nitride (UN) pellets with controllable microstructure and phase – fabrication by spark plasma sintering and their thermal-mechanical and oxidation properties

Dense uranium mononitride (UN) pellets with controlled microstructures and tailored grain size from large-grained to a few microns are synthesized by spark plasma sintering (SPS) combined with high energy ball milling. The impacts of the sintering conditions on fuel microstructure, grain size, physical density, and phase behavior are systematically investigated, and the thermal-mechanical properties and oxidation behavior of the SPS densified UN pellets are characterized. Higher sintering temperatures and longer ball milling durations and thus finer starting UN powders promote sintering and densification, and dense UN pellets above 95% theoretical density can be achieved by SPS at 1873 K for 10 min. UN phase purity is maintained in the SPS-densified pellets sintered at a lower temperature and short duration. A phase heterogeneity with secondary UO 2 or uranium sesquinitride (U 2 N 3 ) occurs for the UN pellets sintered at higher temperatures using finer UN powders. The hardness and fracture toughness of the SPS-densified UN pellets increase with smaller grain sizes and higher densities to 7.9 GPa and 3.5 MPa m 1/2 , respectively. Furthermore, both small (1–2 μm) and large grain-sized (30–50 µm) UN pellets exhibit good thermal conductivity. Dynamic oxidation testing by a thermogravimetric analyzer in air shows that the onset temperature for oxidation varies with microstructure and phase heterogeneity of the SPS densified UN pellets. Particularly, the smaller-grained (micron-sized) UN pellets containing uranium oxides and U 2 N 3 display lower weight gain and significantly-reduced oxidation kinetics, and full oxidation completes at a temperature above 1173 K when tested with a ramp rate of 10 K/min.

36 MATERIALS SCIENCE↗

Corrosion of Al 2 O 3 /Cr and Ti 2 O 3 /Cr composites in flowing air and CO 2 at 750°C

Hot-pressed Al 2 O 3 /Cr and Ti 2 O 3 /Cr composites were exposed to synthetic air or CO 2 at 750 °C. The Al 2 O 3 /Cr composites formed external Cr 2 O 3 scales, and exhibited slow parabolic oxidation kinetics, in both gases. The Cr 2 O 3 scales formed in CO 2 possessed finer grains, and thickened at a faster rate, than Cr 2 O 3 scales formed in air. The Ti 2 O 3 /Cr composites formed thick external TiO 2 scales with internal oxidation zones that also contained Cr 2 O 3 scales on subsurface Cr grains. After 20 h at 750 °C, the Ti 2 O 3 /Cr composites exhibited parabolic oxidation kinetics in both gases, although the oxidation rates were significantly higher than for the Al 2 O 3 /Cr composites.

36 MATERIALS SCIENCE↗

Elucidating the Role of Electric Fields in Fe Oxidation via an Environmental Atom Probe

Abstract We quantify the effects of intensely applied electric fields on the Fe oxidation mechanism. The specimen are pristine Fe single crystals exposing a variety of surface structures identified by field ion microscopy. These crystals are simultaneously exposed to low pressures of pure oxygen gas, on the order of 10 −7 mbar, while applying intense electric fields on their surface of several tens of volts per nanometer. The local composition of the different surface structures is probed directly and in real time using an Environmental Atom Probe and successfully compared with first principles‐based models. We found that rough Fe{244} and Fe{112} facets are more reactive toward oxygen than compact Fe{024} and Fe{011} facets. Results demonstrate that the influence of an electric field on the oxidation kinetics depends on the timescales that are involved as the system evolves toward equilibrium. The initial oxidation kinetics show that strong increases in electric fields facilitate the formation of an oxide. However, as one approaches equilibrium, high field values mitigate this formation. Ultimately, this study elucidates how high externally applied electric fields can be used to dynamically exploit reaction dynamics at the nanoscale towards desired products in a catalytic reaction at mild reaction conditions.

Lambeets, Sten V. [Physical and Computational Scie↗

Elucidating the Role of Electric Fields in Fe Oxidation via an Environmental Atom Probe

We quantify the effects of intensely applied electric fields on the Fe oxidation mechanism. The specimen are pristine Fe single crystals exposing a variety of surface structures identified by field ion microscopy. These crystals are simultaneously exposed to low pressures of pure oxygen gas, on the order of 10 −7 mbar, while applying intense electric fields on their surface of several tens of volts per nanometer. The local composition of the different surface structures is probed directly and in real time using an Environmental Atom Probe and successfully compared with first principles-based models. We found that rough Fe{244} and Fe{112} facets are more reactive toward oxygen than compact Fe{024} and Fe{011} facets. Results demonstrate that the influence of an electric field on the oxidation kinetics depends on the timescales that are involved as the system evolves toward equilibrium. The initial oxidation kinetics show that strong increases in electric fields facilitate the formation of an oxide. However, as one approaches equilibrium, high field values mitigate this formation. Ultimately, this study elucidates how high externally applied electric fields can be used to dynamically exploit reaction dynamics at the nanoscale towards desired products in a catalytic reaction at mild reaction conditions.

09 BIOMASS FUELS↗

Methanol Partial Oxidation on Cu(111) and PtCu(111) Single-Atom Alloy Surfaces: Effect of Surface Oxygen Coverage on Selectivity

The selective oxidation of methanol to formaldehyde on Cu surfaces is an important and well-studied reaction. However, a systematic analysis of product selectivity as a function of oxygen coverage on Cu(111) and Cu-based single-atom alloys (SAAs) has not been previously reported. In this work, we present a comprehensive investigation of deuterated methanol (CD 3 OH) partial oxidation on Cu(111) and 1% PtCu(111) SAA surfaces as a function of preadsorbed oxygen coverage. Temperature-programmed desorption (TPD) and X-ray photoelectron spectroscopy (XPS) reveal that isolated Pt atoms inhibit the initial surface oxidation of Cu(111) under low oxygen exposures. Despite this difference in oxidation kinetics, the product selectivity remains largely unaffected: on both Cu(111) and PtCu(111), formaldehyde (CD 2 O) is the predominant partial oxidation product over a broad range of oxygen coverages. The selectivity toward formaldehyde peaks at intermediate oxygen coverages (∼0.3 monolayers, ML), indicating the existence of an optimal oxygen loading for partial oxidation. Notably, the similar product selectivities on Cu(111) and PtCu(111) over a range of surface oxygen coverage indicate that Pt single atoms do not significantly alter the reaction pathway or shift the optimal oxygen coverage for formaldehyde formation. Control experiments confirm that Cu(111) is unreactive toward methanol in the absence of oxygen, while PtCu(111) surfaces produce a small amount of formaldehyde even when oxygen is not preadsorbed, indicating that isolated Pt atoms facilitate O−H activation at below 150 K, leading to H 2 desorption, followed by C−D activation at higher temperatures (∼350 K). Density functional theory (DFT)-based calculations show that Pt atoms increase the O 2 dissociation barrier relative to Cu(111), consistent with the observed inhibition of oxidation at low exposures. Overall, this work provides the first detailed selectivity map for methanol oxidation on oxidized Cu(111) and PtCu(111) SAA surfaces. By linking classical mechanistic insights such as methoxy- and formate-mediated pathways with single-atom alloy catalyst design, this work demonstrates that while Pt substitution modulates the oxidation kinetics and oxygen binding, the overall selectivity toward formaldehyde is governed primarily by oxygen coverage. These findings underscore the potential of isolated dopants to tune surface oxidation behavior without compromising the intrinsic partial oxidation selectivity of copper-based catalysts.

36 MATERIALS SCIENCE↗

Experimental and kinetic modeling study of the low- temperature and high-pressure combustion chemistry of straight chain pentanol isomers: 1-, 2- and 3-Pentanol

Pentanols have received significant attention as a potential alternative fuel or fuel additive owing to their high energy densities and low vapor pressure. The development of robust chemical kinetic models for alternative fuels which can provide accurate and efficient predictions of combustion performance across a wide range of engine relevant conditions is important in developing cleaner, more efficient combustors. Although the high temperature oxidation kinetics of pentanol isomers has been researched considerably, their low temperature combustion chemistry needs further investigation. While previously proposed low temperature mechanisms for 1-pentanol based on analogy and rate rules need further refinement, the low temperature oxidation kinetics of 2-pentanol and 3-pentanol has not been studied previously by any means, experimentally or theoretically. A newly developed kinetic mechanism is presented in this work for the three straight chain pentanol isomers: 1-, 2- and 3-pentanol. Low temperature kinetics is based on a recent study by Lockwood et al., 2022 [20] involving theoretical calculations at the CCSD(T)/cc-pV∞Z level of theory for the oxidation pathways involving alcohol peroxy radicals. Rate of production analyses performed in this study highlight the importance of the newly added pressure-dependent reactions of the α-alcohol peroxy radical forming an RO 2 adduct. While the α-alcohol fuel radical reacts with O 2 to directly decompose via a chemically activated pathway at low pressures, the formation of the RO 2 adduct is favored at high pressures. Furthermore, the detailed model is comprehensively validated against new ignition experiments at low temperature and high pressure, together with the wide range of data available in the literature. Both qualitative and quantitative predictions of the experimental data using the proposed kinetic model are satisfactory for all three pentanol isomers studied here.

1-pentanol↗

Steam oxidation and microstructural evolution of rare earth silicate environmental barrier coatings

A primary failure mode for environmental barrier coatings (EBCs) on SiC ceramic matrix composites (CMCs) is the oxidation of the intermediate Si-bond coating, where the formation of SiO 2 at the bond coating–EBC interface results in debonding and spallation. This work compares the microstructure evolution and steam oxidation kinetics of the Si-bond coating beneath yttrium/ytterbium disilicate ((Y/Yb)DS) and ytterbium disilicate/monosilicate (YbDS/YbMS) EBCs to better understand the impact of EBC composition on oxidation kinetics. After 500 1-h cycles at 1350°C, (Y/Yb)DS displayed a decreasing concentration of the monosilicate minor phase and increasing concentration of porosity as furnace cycling time increased, whereas the YbDS/YbMS EBC displayed negligible microstructural evolution. For both EBC systems, thermally grown oxide growth rates in steam were found to increase by approximately an order magnitude compared to dry air oxidation. The (Y/Yb)DS EBC displayed a reduced steam oxidation rate compared to YbDS/YbMS.

36 MATERIALS SCIENCE↗

Role of surface diffusion in formation of unique reactivity for graphite oxidation: Time-resolved measurements in a pulsed diffusion reactor

Quantification of oxidation kinetics is essential to develop graphitic materials for diverse applications: from refractories found in gas-cooled nuclear reactors to catalysts needed for chemical manufacturing. In this work, using well-defined highly oriented pyrolytic graphite, low-pressure isotopic transient experiments combined with controlled annealing periods, we resolve the role of surface diffusion and quantify oxidation kinetics with nanomole-precision. We observe an unexpected increase in reactivity following annealing which is explained by the role of surface diffusion increasing the probability for trapping mobile oxygen at more reactive edge sites. Here, the locus of adsorption and spillover to the basal plane is distinct from the trapping location creating a more active oxygen species. Isotopic products reflect the population dynamics of oxygen added at the edge and surface diffusion that relocates basal plane oxygen to more reactive edge sites. Since this process proceeds in parallel with direct oxidation reactions, it is not likely to be observed using steady-state or conventional ‘bulk’ characterization techniques. Our unique time-resolved non-equilibrium measurement in a well-defined transport regime, enables observation of three distinct behaviors: short-term deactivation due to the balance of rates in oxygen supply/product formation, reactivity increases due to surface diffusion and longer-term reactivity increase with oxygen accumulation.

36 MATERIALS SCIENCE↗

Platinum–Ruthenium Alloys Are Not Bifunctional CO Electro-Oxidation Catalysts: A Kinetic Analysis

Electro-oxidation of CO is a common kinetic bottleneck in many types of fuel cells and organic electrosynthesis processes. Alloys of Pt and Ru are often used as anode catalysts, with high activity attributed to bifunctionality; this suggests that Ru preferentially activates water to form surface hydroxyl groups that can react with Pt-bound CO. However, rigorous kinetic measurements have not confirmed this assertion under steady-state electro-oxidation conditions. Here, CO electro-oxidation is analyzed using several commercial Pt/C and Pt 100-x Ru x /C nanoparticle catalysts in acidic and alkaline electrolytes. Kinetic observables including apparent transfer coefficients and reaction orders are measured and evaluated using a degree of rate control analysis. The kinetic observables for both Pt and PtRu alloys are most consistent with competitive adsorption and Langmuir–Hinshelwood coupling across a single site-type, rather than two distinct sites. Furthermore, the role of Ru in CO electro-oxidation is assigned to be a purely electronic effect.

Alcohols↗

Heat Integration Optimization and Dynamic Modeling Investigation for Advancing the Coal-Direct Chemical Looping Process

The purpose of the project is to address the optimization and startup operation of a modular coal direct chemical looping (CDCL) combustion system integrated with a steam cycle for power generation to reduce the risks involved in further scale-up of the technology. The modular reactor design of the CDCL process provides flexibility in the fabrication of the reactor and in its operating capacity (i.e. turndown ratio) at the cost of a more complex heat exchange network (HEN) design and integration. To address the technology gaps and advance the efficiency and economic feasibility of the CDCL technology, the project will perform a detailed and comprehensive analysis of the integration of a modular CDCL reactor system and a steam cycle system under both static and transient conditions via HEN process performance simulations and system dynamic modeling, respectively. The scope of work consists of 1) Experimental and computational studies of the CDCL combustor reactor 2) Comprehensive static (i.e. steady-state) system HEN design analysis in CDCL 550 MWe commercial unit for power generation and 3) Dynamic modeling of site specific design of 10MWe CDCL large pilot plant. The project team has successfully developed and validated a kinetic model for the oxidation of oxygen carriers in the combustor using the unreacted shrinking core model (UCSM). The model is capable of capturing the oxidation kinetics of fully or partially reduced oxygen carrier particles. A computational fluid dynamics (CFD) model is developed to simulate the hydrodynamics, heat transfer, and chemical reaction occurring in the CDCL combustor. The model is developed in MFIX and ANSYS Fluent. Key aspects of CDCL combustor operation, including heat transfer, oxygen carrier oxidation, and the transport of oxygen carrier particles, are simulated using this CFD model. The HEN for a commercial scale 550 MWe CDCL power plant is simulated and optimized using ASPEN Plus. Practical design considerations are incorporated based on industrial experiences. The performance and cost for the commercial CDCL plant is updated based on these analyses. A dynamic model for the 10 MWe CDCL pilot plant is developed in ProTRAX simulation software. The model is based on the pilot plant design developed in project DE-FE0027654 “10 MWe CDCL Large Pilot Plang – Pre-FEED Study” and the steam cycle data obtained from Dover Light & Power plant. The transient behaviors during pilot plant load variation are simulated using the dynamic model.

01 COAL, LIGNITE, AND PEAT↗