Search NASA⌕ Search

SEARCH · Search NASA

Results for “polymer stability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Study of thermal stability and degradation of fire resistant candidate polymers for aircraft interiors

The thermochemistry of bismaleimide resins and phenolphthalein polycarbonate was studied. Both materials are fire-resistant polymers and may be suitable for aircraft interiors. The chemical composition of the polymers has been determined by nuclear magnetic resonance and infrared spectroscopy and by elemental analysis. Thermal properties of these polymers have been characterized by thermogravimetric analyses. Qualitative evaluation of the volatile products formed in pyrolysis under oxidative and non-oxidative conditions has been made using infrared spectrometry. The residues after pyrolysis were analyzed by elemental analysis. The thermal stability of composite panel and thermoplastic materials for aircraft interiors was studied by thermogravimetric analyses.

Hsu, M. T. S.↗

High temperature polymers - A review of novel thermally stable hexafluoroisopropylidene-containing polymers

The synthesis and properties to date of several novel HFIP-containing polymers and copolymers are presented. Thermal analyses of polyether ketones (PEK), aromatic polyesters, and polymers from a novel 18F-diacid were performed on a thermal analyzer. All three polymer types exhibited enhanced solubility, thermal stability, and low dielectric constants that are predicted for polymers containing the HFIP moiety. The moderate thermal stability observed in the polymers derived from the 18F-diacid is attributed to the oxidatively weak methylene linkage between the HFIP groups and the phenyl rings. PEKs and polyarylates show potential as high emissivity coatings under conditions where atomic oxygen is present.

Kane, K. M.↗

A study of the UV and VUV degradation of FEP

UV and VUV degradation of fluorinated ethylene propylene (FEP) copolymer was studied using electron spin resonance (ESR) spectroscopy, x-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM). The ESR study revealed the formation of a terminal polymer radical. The stability of this radical was investigated under different environments. An XPS study of FEP film exposed to VUV and atomic oxygen showed that oxidation takes place on the polymer surface. The study revealed also that the percentage of CF2 in the polymer surface decreased with exposure time and the percentage of CF, CF3, and carbon attached to oxygen increased. SEM micrographs of FEP film exposed to VUV and atomic oxygen identified a rough surface with undulations similar to sand dunes.

George, Graeme A.↗

New RTM/RI Resins for the HSCT

In the first portion of this work, 1,2,3,3,4,4-hexafluoro-1,2-bis[4-(dimethylhydroxysilyl)phenoxy]cyclobutane and 1,2,3,3,4,4-hexafluoro-1,2-bis[3-(dimethylhydroxysilyl)phenoxy]cyclobutane were prepared and homopolymerized to afford polymers with excellent thermal stability and Tgs of 27 C and -12 C, respectively. Despite the moderately high wt% of fluorin in the polymer structure (23.8%), these polymers had poor fuel resistance. In fact, swelling measurements indicate that these polymers had apparent solubility parameters of about 18.2 J (exp 1/2) m (exp -3/2) (toluene). Copolymerization of the disilanol monomers with fluorosilicone monomers afforded copolymers containing 20-30 wt% of the perfluorocyclobutane-containing structure displayed adequate fuel resistance, enhanced thermal stability, and a Tg low enough to meet the requirements of a High Speed Civil Transport (HSCT) fuel tank sealant. In the second part of this work, trifluorovinylether-terminated oligomers were prepared and polymerized via cyclodimerization. Initially, an alpha, omega-silanol-terminated fluorosilicone was endcapped with trifluorovinylether end groups via a two-step synthetic sequence. The oligomer was thermally cyclodimerized to a polymer that displayed thermal stability similar to that of a fluorosilicone homopolymer. Second, 1,3-bis[4-trifluorovinyl(oxy)phenyl]-1,3-(3,3,3-trifluoropropyl)dimethyldisiloxane and 1,3-bis{3-trifluorovinyl(oxy)phenyl]-1,3-(3,3,3-trifluoropropyl)dimethyldisiloxane were prepared and cyclodimerized to afford polymers that contained pendant trifluoropropyl groups. The pendant trifluoropropyl groups did enhance solvent resistance in aliphatic hydrocarbon solvents, however, no improvement was observed in aromatic hydrocarbon solvents. These polymers also displayed excellent thermal stability. In the last part of this work, a series of monomers was prepared by the DCC-promoted esterification of 4-[trifluorovinyl(oxy)benzoic acid with alpha, omega-functionalized hydrogenated and partially fluorinated alcohols. The monomers were cyclodimerized to the corresponding polymers. The polymers that did not contain beta hydrogens displayed significantly higher thermal stability than the fully hydrogenated polymers. A commercially-available alpha,omega-hydroxy-terminated perfluoropolyether was then functionalized with 4-[trifluorovinyl(oxy)benzoylchloride. An attempt was made to polymerize the resulting oligomer via the cyclodimerization of the terminal trifluorovinylether moieties. Although the viscosity of the oligomer increased significantly during polymerization, Gel Permeation Chromatography (GPC) analysis revealed that the Tetrahydrofuran (THF) soluble portion of the polymer did not have high molecular weight.

Harris, Frank W.↗

Thermally stable macromolecules.

Man-made polymers are compared with certain naturally occurring polymers which have long been used at elevated temperatures. The pyrolysis of model compounds is discussed together with aspects of thermogravimetric analysis, torsional braid analysis, and questions of chemical and radiation stability. Some structure-property relationships are examined, giving attention to asbestos, mica, graphite, and diamond. Questions of bond strengths are investigated along with the stability of ladder polymers and some fundamental concepts in the synthesis of aromatic and heteroaromatic polymers. The substances considered include aromatic single-strand polymers, heteroaromatic polymers, polymers obtained by addition polymerizations, and nonhydrogen-containing polymers. Future trends are also explored.

Pezdirtz, G. F.↗

Conformal Membrane Reflectors for Deployable Optics

This presentation reports the Phase I results on NASA's Gossamer Spacecraft Exploratory Research and Technology Program. Cornerstone Research Group, Inc., the University of Rochester, and International Photonics Consultants collaborated to investigate the feasibility of free-standing, liquid-crystal-polymer (LCP) reflectors for integration into space-based optical systems. The goal of the program was to achieve large-diameter, broadband. reflective membranes that are resistant to the effects of space, specifically cryogenic environments and gamma-ray irradiation. Additionally, we assessed the applicability of utilizing the technology as tight sails, since, by their very nature, these films offer high-reflectivity at specified wavelengths. Previous research programs have demonstrated all-polymer, narrow-band Specular reflectors and diffuse membrane reflectors. The feasibility of fabricating an all-polymer broadband specular reflector and a narrow-band specular membrane reflector was assessed in the Phase I Gossamer program. In addition, preliminary gamma irradiation studies were conducted to determine the stability of the polymer reflectors to radiation. Materials and process technology were developed to fabricate coupon-scale reflectors of both broad- and narrow-band specular reflectors in Phase 1. This presentation will report the results of these studies, including, the performance of a narrow-band specular membrane. Gamma irradiation exposures indicate limited impact on the optical performance although additional exposure studies are warranted. Plans to scale up the membrane fabrication process will be presented.

Hood, Patrick J.↗

A ceramic matrix composite based on polymerization and pyrolysis of ethynylated aromatics

A number of ethynylated aromatic monomers recently have been synthesized which thermally homopolymerize and copolymerize to produce rigid, highly cross-linked polymers with high thermal stability (Tg of about 450 C). On pyrolysis, these polymers lose few volatiles (more than 85 percent char yield) to yield carbon bodies of relatively low porosity. These properties render the ethynylated aromatics of significant interest as matrices for high temperature composites. Incorporation of a SiC particle filler in the matrix improves the rheology of the system and minimizes shrinkage during pyrolysis. Several unidirectional composites have been fabricated combining a graphite or boria-alumina-silica continuous reinforcement with an ethynylated aromatic polymer matrix and SiC filler. Thermogravimetric analysis of composite pyrolysis behavior was used to determine reaction kinetics and to establish a composite fabrication cycle. Composites retained 95 percent of their green weight on pyrolysis. Microstructure of the green and pyrolyzed composites is characterized for materials pyrolyzed at 600 C in vacuum and argon as well as for laminates heated at 1200 C in argon following pyrolysis.

Hurwitz, F. I.↗

Dispersions of Carbon nanotubes in Polymer Matrices

Dispersions of carbon nanotubes exhibiting long term stability are based on a polymer matrix having moieties therein which are capable of a donor-acceptor complexation with carbon nanotubes. The carbon nanotubes are introduced into the polymer matrix and separated therein by standard means. Nanocomposites produced from these dispersions are useful in the fabrication of structures, e.g., lightweight aerospace structures.

Wise, Kristopher Eric↗

Open cell fire-resistant foam

Candidate polyphosphazene polymers were investigated to develop a fire-resistant, thermally stable and flexible open cell foam. The copolymers were prepared in several mole ratios of the substituent side chains and a (nominal) 40:60 derivative was selected for formulation studies. Synthesis of the polymers involved solution by polymerization of hexachlorophosphazene to soluble high molecular weight poly(dichlorophosphazene), followed by derivatization of the resultant polymer in a normal fashion to give polymers in high yield and high molecular weight. Small amounts of a cure site were incorporated into the polymer for vulcanization purposes. The poly(aryloxyphosphazenes) exhibited good thermal stability and the first polymer mentioned above exhibited the best thermal behavior of all the candidate polymers studied.

Thompson, J. E.↗

Liquid crystalline polymers

The remarkable mechanical properties and thermal stability of fibers fabricated from liquid crystalline polymers (LCPs) have led to the use of these materials in structural applications where weight savings are critical. Advances in processing of LCPs could permit the incorporation of these polymers into other than uniaxial designs and extend their utility into new areas such as nonlinear optical devices. However, the unique feature of LCPs (intrinsic orientation order) is itself problematic, and current understanding of processing with control of orientation falls short of allowing manipulation of macroscopic orientation (except for the case of uniaxial fibers). The current and desirable characteristics of LCPs are reviewed and specific problems are identified along with issues that must be addressed so that advances in the use of these unique polymers can be expedited.

Source record↗

Fire and heat resistant laminating resins based on maleimido and citraconimido substituted 1-(diorgano oxyphosphonyl) methyl -2,4- and -2,6- diaminobenzenes

A class of fire and heat resistant bisimide resins prepared by thermal polymerization of maleimido or citraconimido substituted 1-((dialkoxyphosphonyl) methyl)-2-4 and -2,6-diaminobenzenes are described. The polymer precursors are prepared by reacting 1-((diorganooxyphosphonyl) methyl)-2-4 and -2,6-diaminobenzenes with maleic anhydride or citraconic anhydride in a mole ratio 1:2. Chain extension of the monomers is achieved by reacting the mono-N-maleimido derivatives of 1-((diorganooxyphosphonyl) methyl)-2,4 and -2,6-diaminobenzenes with aryl tetracarboxylic dianhydrides, such as benzophenone tetracarbocylic dianhydride, or aryl diisocyanates, such as methylenebis (4-phenylisocyanate), in a mole ratio 2:1. The polymerization of the monomers is studied by differential scanning calorimetry (DSC) and the thermal stability of the polymers is ascertained by thermogravimetric analysis (TGA).

Mikroyannidis, John A.↗

Fire and heat resistant laminating resin based on maleimido and citraconimido substituted 1-(diorganooxyphosphonyl-methyl)-2,4- and -2,6-diaminobenzenes

The subject invention pertains to a novel class of fire-and heat-resistant bisimide resins prepared by thermal polymerization of maleimido or citraconimido substituded 1-(dialkoxyphosphonyl)-methyl-2-4 and -2,6-diaminobenzenes. Typical polymer presursors have the chemical structure wherein R is alkyl, substituted alkyl or aryl, and R sup 1 is hydrogen or lower alkyl. The polymer precursors are prepared by reacting 1-(diorganooxyphosphonyl)methyl-2-4 and -2,6-diaminobenzenes with maleic anhydride or citraconic anhydride in a mole ratio 1:2. Chains extension of the monomers is achieved by reacting the mono-N-maleimido derivatives of 1-(diorganooxyphosphonyl)methyl-2,4 and -2,6-diaminobenzenes with aryl tetracarboxylic dianhydrides, such as benzophenone tetracarboxylic diandydride, or aryl diisocyanates, such as methylenebis (4-phenylisocyanate), in a mole ratio 2:1. The polymerization of the monomers is studied by differential scanning calorimetry (DSC) and the thermal stability of the polymers is ascertained by thermogravimetric analysis (TGA).

James M Beggs↗

Fire and heat resistant laminating resins based on malemeido and citraconimido substituted 1 -2,4- and -2,6- diaminobenzenes

A novel class of fire and heat resistant bisimide resins prepared by thermal polymerization of maleimido or citraconimido substituted 1-(dialkox phosphonyl) methyl-2-4 and -2,6-diamino benzenes was presented. The polymer precursors are prepared by reacting 1-(diorgano oxyphosphonyl) methyl-2-4- and -2,6-diamino benzenes with maliec anhydride or citraconic anhydride in a mole ratio 1:2. Chain extension of the monomers is achieved by reacting the mono-N-maleimido derivaties of 1 (diorgano oxyphosphonyl) methyl -2,4- and -2,6-diamino benzenes with aryl tetracarboxylic dianhydrides, such as benzophenone tetracarboxylic dianhydride, or aryl diisocyanates, such as methylene bis(4-phenyl isocyanate), in a mole ratio 2:1. The polymerization of the monomers is studied by diferential scanning calorimetry and the thermal stability of the polymers is ascertained by thermogravimetric analysis.

Mikroyannidis, John A.↗

Polymer-Induced Depletion Interaction and Its Effect on Colloidal Sedimentation in Colloid-Polymer Mixtures

In this paper we focus on the polymer-induced depletion attraction and its effect on colloidal sedimentation in colloid-polymer mixtures. We first report a small angle neutron scattering (SANS) study of the depletion effect in a mixture of hard-sphere-like colloid and non-adsorbing polymer. Then we present results of our recent sedimentation measurements in the same colloid-polymer mixture. A key parameter in controlling the sedimentation of heavy colloidal particles is the interparticle potential U(tau), which is the work required to bring two colloidal particles from infinity to a distance tau under a give solvent condition. This potential is known to affect the average settling velocity of the particles and experimentally one needs to have a way to continuously vary U(tau) in order to test the theory. The interaction potential U(tau) can be altered by adding polymer molecules into the colloidal suspension. In a mixture of colloid and non-adsorbing polymer, the potential U(tau) can develop an attractive well because of the depletion effect, in that the polymer chains are expelled from the region between two colloidal particles when their surface separation becomes smaller than the size of the polymer chains. The exclusion of polymer molecules from the space between the colloidal particles leads to an unbalanced osmotic pressure difference pushing the colloidal particles together, which results in an effective attraction between the two colloidal particles. The polymer-induced depletion attraction controls the phase stability of many colloid-polymer mixtures, which are directly of interest to industry.

Tong, Penger↗

Numerical simulation of non-Newtonian free shear flows

Free shear flows, like those of mixing layers, are encountered in aerodynamics, in the atmosphere, and in the ocean as well as in many industrial applications such as flow reactors or combustion chambers. It is, therefore, crucial to understand the mechanisms governing the process of transition to turbulence in order to predict and control the evolution of the flow. Delaying transition to turbulence as far downstream as possible allows a gain in energy expenditure while accelerating the transition can be of interest in processes where high mixing is desired. Various methods, including the use of polymer additives, can be effective in controlling fluid flows. The drag reduction obtained by the addition of small amounts of high polymers has been an active area of research for the last three decades. It is now widely believed that polymer additives can affect the stability of a large variety of flows and that dilute solutions of these polymers have been shown to produce drag reductions of over 80 percent in internal flows and over 60 percent in external flows under a wide range of conditions. The major thrust of this work is to study the effects of polymer additives on the stability of the incompressible mixing layer through large scale numerical simulations. In particular, we focus on the two dimensional flow and examine how the presence of viscoelasticity may affect the typical structures of the flow, namely roll-up and pairing of vortices.

Homsy, G. M.↗

Polymer/Silicate Nanocomposites Developed for Improved Strength and Thermal Stability

Over the past decade, polymer-silicate nanocomposites have been attracting considerable attention as a method of enhancing polymer properties. The nanometer dimensions of the dispersed silicate reinforcement can greatly improve the mechanical, thermal, and gas barrier properties of a polymer matrix. In a study at the NASA Glenn Research Center, the dispersion of small amounts (less than 5 wt%) of an organically modified layered silicate (OLS) into the polymer matrix of a carbon-fiber-reinforced composite has improved the thermal stability of the composite. The enhanced barrier properties of the polymer-clay hybrid are believed to slow the diffusion of oxygen into the bulk polymer, thereby slowing oxidative degradation of the polymer. Electron-backscattering images show cracking of a nanocomposite matrix composite in comparison to a neat resin matrix composite. The images show that dispersion of an OLS into the matrix resin reduces polymer oxidation during aging and reduces the amount of cracking in the matrix significantly. Improvements in composite flexural strength, flexural modulus, and interlaminar shear strength were also obtained with the addition of OLS. An increase of up to 15 percent in these mechanical properties was observed in composites tested at room temperature and 288 C. The best properties were seen with low silicate levels, 1 to 3 wt%, because of the better dispersion of the silicate in the polymer matrix.

Campbell, Sandi G.↗

Microstructural, Strength, and Creep Characterization of Sylramic™, Sylramic™-iBN and Super Sylramic™-iBN SiC Fibers

The chemical composition, microstructure, strength, and thermal stability of polymer-derived Sylramic™ SiC fibers fabricated by Dow Corning and COI Ceramics, Inc., and nitrogen-treated Sylramic™ SiC fibers, referred to as Sylramic™-iBN and Super Sylramic™-iBN SiC fibers, were investigated and compared. The baseline Sylramic™ SiC fibers fabricated by both vendors as well as the nitrogen-treated Sylramic™ SiC fibers are composed mostly of β-SiC (~97 wt%) with small amounts of TiB2 (~2 wt%), amorphous carbon (~1 wt%) and trace amounts of B4C. Most of the amorphous carbon is segregated at the core/interior of the fibers. Both baseline and nitrogen-treated Sylramic™ SiC fibers have similar grain size and pore size distribution, except for a thin layer of in-situ grown crystalline BN (30 to 70 nm) on the surface of Sylramic™-iBN and Super Sylramic™-iBN fibers. Wide variation in strength within a batch as well as between batches is observed in both baseline and nitrogen-treated Sylramic™ SiC fibers but both types of fibers are microstructurally stable at temperatures to 1800°C in argon and nitrogen environments compared to Nicalon™-S and Tyranno®-SA SiC fibers. Under the same creep condition, Super Sylramic™-iBN fibers show better creep resistance compared to Sylramic™, Sylramic™-iBN, Hi-Nicalon™-S, and Tyranno®-SA fibers. Possible reasons for strength variability and the mechanism of in-situ BN formation on Sylramic™ SiC fibers are discussed.

SiC fibers↗

Development of a special purpose spacecraft interior coating, phase 1

Coating formulations were developed consisting of latex blends of fluorocarbon polymers, acrylic resins, stabilizers, modifiers, other additives, and a variety of inorganic pigments. Suitable latex primers were also developed from an acrylic latex base. The formulations dried to touch in about one hour and were fully dry in about twenty-four hours under normal room temperature and humidity conditions. The resulting coatings displayed good optical and mechanical properties, including excellent bonding to (pre-treated) substrates. In addition, the preferred compositions were found to be self-extinguishing when applied to nonflammable substrates and could meet the offgassing requirements specified by NASA for the intended application. Improvements are needed in abrasion resistance and hardness.

Bartoszek, E. J.↗