Search NASA⌕ Search

SEARCH · Search NASA

Results for “porosities”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Porosity evolution during heating of copper made from powder by friction extrusion

Here, friction extrusion was used to compact and extrude solid copper rod from feedstock powders. Following extrusion, considerable porosity was observed throughout the extrudate cross section due to the entrained porosity in the feedstock material and the extrusion process. The thermal stability of the extrudate was investigated via a series of heat treatments. Porosity evolution exhibited three distinct stages—an unchanged plateau (0°C–300°C) followed by an abrupt increase (400°C–500°C) and ultimately a reduction, as the temperature increases (>500°C). The peak porosity measured was ~25%. The underlying driving force for pore evolution is described as the competition between the internal pore pressure, material strength, and sintering kinetics, as a function of temperature. The observed porosity evolution and driving force are not expected to be limited to copper. Thus, this manuscript reveals an important consideration regarding elevated-temperature thermal stability as advanced manufacturing methods involving direct powder extrusion are explored.

36 MATERIALS SCIENCE↗

Pore-Scale Study on the Positive Feedback Between Stress and Porosity Caused by Pressure Solution in Porous Media

Pressure solution is an important process in the evolution of sedimentary rocks, which provide storage space for most of our petroleum resources. It directly influences the generation, migration, and storage of petroleum fluids in subsurface sedimentary rocks. Here, in this paper, we develop a pore-scale, mechanochemical model to demonstrate a possible positive feedback between the local porosity and pore surface stress, in which a higher local porosity causes a higher local pore surface stress, thus enhancing pressure solution and consequently further increasing the local porosity. Pore surface stress represents stress on a solid grain adjacent to a pore. Specifically, the pore-scale, mechanochemical model directly simulates the stress distribution over solid and pore surfaces using a finite element model. The dissolution of solids at the solid-pore interfaces under a far-from-equilibrium condition is simulated using a first-order kinetics model that accounts for the local stress distribution. The updated pore geometry, caused by pore surface dissolution, is then used in the stress simulation in the next numerical iteration. Two types of porous media, the Oriskany sandstone and an artificial porous medium with spherical pores, were tested in the mechanochemical simulation. The positive stress-porosity feedback during pressure solution was observed in both samples. In addition, the model quantitatively illustrated the distribution of local mineral dissolution rates on all pore surfaces, as well as its relation to the effective mineral dissolution rate of the entire sample. Based on the comparison between the two porous media, the local mineral dissolution was regulated by pore space distribution, geometry, and coalescence during pressure solution. This work is the first that uses direct, pore-scale numerical simulation to demonstrate the positive stress-porosity feedback during pressure solution, which has the potential to advance the understanding of the mechanical-chemical (MC) coupling in many geological processes that are relevant to subsurface energy systems, such as the recovery of petroleum hydrocarbons and geothermal energy.

CT scanning↗

Sub‐5 Ångstrom Porosity Tuning in Calixarene‐Derived Porous Liquids via Supramolecular Complexation Construction

Abstract Sub‐Ångstrom‐level porosity engineering, which is appealing in gas separations, has been demonstrated in solid carbon, polymer, and framework materials but rarely achieved in the liquid phase. In this work, a gas molecular sieving effect in the liquid phase at sub‐5 Ångstrom scale is created via sophisticated porosity tuning in calixarene‐derived porous liquids (PLs). Type II PLs are constructed via supramolecular complexation between the sodium salts of calixarene derivatives and crown ether solvents. The chemical structure variation and assembly behavior of the porous host upon PL construction are monitored by spectroscopy‐, X‐ray‐, and neutron‐scattering techniques. The presence of permanent porosity in calixarene‐derived PLs is verified by pressure swing gas uptake, altered CO 2 physisorption behavior, and molecular simulations. Sub‐5 Ångstrom porosity tuning within the PL phase is achieved by introducing bulky substituted groups on the benzene ring of the calixarene host, which then greatly affects the dynamic motion and transport behavior of CO 2 molecules and the Xe uptake performance. The approach being demonstrated in this work represents a promising pathway to tune and leverage the porosity effect for enhanced gas uptake capacity and selectivity in liquid sorbents.

Li, Errui [Department of Chemistry University of T↗

Sub-5 Ångstrom Porosity Tuning in Calixarene-Derived Porous Liquids via Supramolecular Complexation Construction

Sub-Ångstrom-level porosity engineering, which is appealing in gas separations, has been demonstrated in solid carbon, polymer, and framework materials but rarely achieved in the liquid phase. In this work, a gas molecular sieving effect in the liquid phase at sub-5 Ångstrom scale is created via sophisticated porosity tuning in calixarene-derived porous liquids (PLs). Type II PLs are constructed via supramolecular complexation between the sodium salts of calixarene derivatives and crown ether solvents. The chemical structure variation and assembly behavior of the porous host upon PL construction are monitored by spectroscopy-, X-ray-, and neutron-scattering techniques. The presence of permanent porosity in calixarene-derived PLs is verified by pressure swing gas uptake, altered CO 2 physisorption behavior, and molecular simulations. Sub-5 Ångstrom porosity tuning within the PL phase is achieved by introducing bulky substituted groups on the benzene ring of the calixarene host, which then greatly affects the dynamic motion and transport behavior of CO 2 molecules and the Xe uptake performance. Further, the approach being demonstrated in this work represents a promising pathway to tune and leverage the porosity effect for enhanced gas uptake capacity and selectivity in liquid sorbents.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Manufacturing porous U10Zr fuels with controlled porosities by SPS and thermal properties

To accommodate the swelling of metallic fuels induced by the fission gas release during burnup in sodium fast reactor for a sodium-free fuel option, advanced U-10Zr fuels with controlled porosity were designed and demonstrated by spark plasma sintering. U-10Zr fuel pellets with manufactured porosities varying from 35% up to fully dense fuel pellets have been fabricated by controlling ball milling times of the starting uranium powders, sintering temperature, pressure, and duration, and the correlation among the microstructure control – porosity – sintering conditions has been established. To further mimick the pore structure in irradiated fuels, different pore formers (NaCl and NH4HCO3) have been used to control the pore size and distribution. Microstructure characterization indicates a lamellar reaction zone of U and Zr, differing from the arc-melted U-10Zr as a result of rapid consolidation of SPS at lower temperature and short durations. The thermal conductivity of U10Zr with different porosities are also measured. Here this work demonstrates the success in manufacturing new metallic fuel forms with controlled porosities and pore distribution, which can be used as model systems to investigate the thermal transfer behavior of metallic fuels in the reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

An assessment of spall failure modes in laser powder bed fusion fabricated stainless steel 316L with low-volume intentional porosity

Here, this paper reports on spall failure and damage modes in Laser Powder Bed Fusion fabricated Stainless Steel 316L (SS316L) with intentional levels of low-volume (1–5 vol. %) porosity and pore sizes of 200, 350, and 500 μm. The fabricated specimens were subjected to uniaxial-strain plate-impact loading at ~4.5 GPa, to initiate incipient spall failure. Analysis of velocimetry profiles measured using multi-probe photon-Doppler velocimetry coupled with post-mortem analysis of soft-recovered samples reveals local suppression of spall failure (termed as spall-dominated) as a function of porosity, as the failure mechanism transitions from spall-centered tensile stress dominated to a pore-centered microstructure-dominated damage mode involving void/crack nucleation and growth at pre-existing pores. The critical porosity level where the suppression of spall failure is first observed, as well as the spall location, is dependent on both the volume fraction and the size of the initially fabricated pores. In samples of 500 μm pore size, the suppression of spall failure is observed with as little as 1 vol. % porosity, while samples with smaller pores (200 μm) still experience spall-centered tensile stress dominated failure with higher levels (5 vol. %) of porosity. In the case of pore-centered microstructure-dominated failure, spall damage can occur but the spall plane is shifted toward the rear free surface, or more generally in areas further away from the region with pores. Highly heterogeneous deformation twinning, shear banding, grain rotation, and cracking are observed in the vicinity of pre-existing pores and expected spall failure sites.

36 MATERIALS SCIENCE↗

Effects of Microstructural Composition, Porosity, and Microcracks on the Elastic Moduli of Nuclear Graphites

The elastic responses of nuclear graphite not only depend on the graphitic content itself but are largely dictated by the microstructural constitution of the material. The types of raw materials combined with the manufacturing processes used to produce the graphite yield the microstructural content that primarily includes graphite filler, graphitized pitch binder, and voids/defects that typically occupy approximately 20% of the volume. Among these microstructural components, porosity and microcracking (considered to be part of voids/defects) heavily influence the overall properties of the material, including the elastic moduli. It is widely accepted that the primary effect of oxidation is to increase porosity, but the related effect on the moduli cannot be explained satisfactorily by simply noting changes to porosity. Models describing the elastic moduli of porous, polycrystalline graphite materials have been developed to interpret experimental determinations of Young's modulus and shear modulus in oxidized graphites. Beyond porosity, the moduli are heavily influenced by microcracks, and their effects can be assessed using physical property models based on orientation distribution coefficients and microcrack-modified, single-crystal moduli to represent the combined effects of crystallite orientation and microcracking. This work demonstrates how most modulus measurements in nuclear graphites can be understood using relatively simple models that describe the effects of porosity and microcracking. We also present directions to be pursued to account for microstructure-related effects that occur as a result of neutron irradiation.

Spicer, James B.↗

Understanding of Low‐Porosity Sulfur Electrode for High‐Energy Lithium–Sulfur Batteries

Abstract The lithium–sulfur (Li–S) battery is a promising technology for large‐scale energy storage and vehicle electrification due to its high theoretical energy density and low cost. Reducing the sulfur cathode porosity has been identified recently as a viable strategy for improving the cell practical energy density and minimizing pore‐filling electrolytes to extend cell life at lean electrolyte conditions. Direct use of a low‐porosity cathode for Li–S battery results in poor electrode wetting, nonuniform electrode reactions, and thus early cell failure. To understand and mitigate the barriers associated with the use of low‐porosity electrodes, multiscale modeling is performed to predict electrode wetting, electrolyte diffusion, and their impacts on sulfur reactions in Li–S cells by explicitly considering the electrode wettability impacts and electrode morphologies. The study elucidates the critical impact of low tortuosity and large channel pore design for promoting electrode wetting and species diffusion. It is suggested that the secondary particle size should be comparable with the electrode thickness to effectively promote electrolyte wettability and sulfur reactivity. This study provides new insights into the low‐porosity electrode material and designs and is expected to accelerate the development of practical high‐energy Li–S batteries.

25 ENERGY STORAGE↗

Vacuum-assisted extrusion to reduce internal porosity in large-format additive manufacturing

Large-scale 3D printing of polymer composite structures has gained popularity and seen extensive use over the last decade. Much of the research related to improving the mechanical properties of 3D-printed parts has focused on exploring new materials and optimizing print parameters to improve geometric control and minimize voids between printed beads. However, porosity at the microstructural level (within the printed bead) has been much less studied although it is almost universally observed at levels of 4 %-10 % when using fiber reinforced materials. This study introduces a vacuum-assist approach that minimizes internal porosity by removing ambient air from the interstitial space between pellets in the hopper and acts as a negative pressure vent for gases that evolve during the initial stages of single-screw extrusion. Vacuum-assisted extrusion was able to reduce porosity below 2 % across a wide range of processing parameters, moisture content, fiber reinforcements, and printing platforms. Specifically, when printing on a large-format extruder (Strangpresse Model-30), the vacuum-assisted extrusion reduced internal porosity by 35–75 % compared to conventional non-vacuum extrusion, and only pores with length scale > 2 microns are affected. The success of this approach prompted the design of a patent-pending continuous vacuum hopper relevant for large-scale 3D printing on commercial systems.

36 MATERIALS SCIENCE↗

Characterization of Porosity and Pore Accessibility of Vitrinite-Rich Bituminous and Subbituminous Coals by Small-Angle Neutron Scattering, Mercury Intrusion Porosimetry, and Low-Pressure N 2 Adsorption

Three bituminous and one subbituminous vitrinite-rich coals were characterized using small-angle neutron scattering with contrast matching, mercury intrusion porosimetry, and low-pressure N 2 adsorption techniques to quantify their porosity and pore accessibility in an effort to assess their solvent extractabilities, as a first approximation, for manufacturing useful end-products. The techniques revealed consistent results while complimenting one another. The total porosity was found to follow the coal rank with the lowest rank having the highest porosity within the studied coals. The amount of inaccessible pores was found to increase with rank for the bituminous coals studied here. Finally, the increase in the ease of accessibility and total porosity with decreasing rank suggested easier penetration of chemical reagents for solvent extraction, for example.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The evolution of coal porosity during pyrolysis

Gasification of coal, municipal waste, or other organic materials is a potential hydrogen source that entails complex thermal decomposition and transport processes. This study provides a multiscale analysis of these processes for sub-bituminous (Usibelli, Healy, Alaska) and lignite (Center, North Dakota) coals and provides data useful for process design. The chemistry, mineralogy, and pore structures of pyrolyzed coal and their evolution with thermal decomposition are discussed. Samples pyrolyzed at 200–1000 °C were analyzed by small-angle neutron scattering; ultra-small, small-, and wide-angle X-ray scattering; and other complementary techniques. Scanning electron microscopy showed new pores in the high-temperature-pyrolyzed material. Upon heating, the coals became progressively denser, and the concentration of hydrogen decreased. Changes in pore volume fell into three temperature ranges: an initial, low-temperature range that, for the Usibelli coal, involved an increase in overall porosity; a mid-temperature range associated with pore volume loss; and a high-temperature range associated with significant porosity increase and char formation. This transformation was paralleled by changes in fractal dimension and correlation length. The higher the pyrolysis temperature the greater the small-pore-volume fraction and overall surface area became. Pyrolysis increased the lateral size of coal crystallites, decreased the amorphous fraction, and increased the aromatics fraction and overall coal rank. Comparisons of neutron and X-ray scattering data and subsequent water uptake studies showed that pre-dried coals can re-hydrate relatively rapidly upon exposure to air, which can significantly affect the porosity calculated from small-angle-scattering data. Fits to the cumulative porosity curves provide a method for modeling the physical and chemical transformation of hydrogen-containing feedstock during gasification.

Anovitz, Lawrence {Larry} [ORNL] (ORCID:0000000226↗

Effect of threshold parameters on infrared segmentation methods for porosity detection in electron beam powder bed fusion

In-situ process monitoring has seen significant interest in additive manufacturing to address qualification and certification goals. This is especially prevalent in metal powder bed fusion processes such as electron beam powder bed fusion (PBF-EB), with layer-wise infrared imaging being commonly used to detect defects. Here, this work compares two different segmentation methods (static thresholding and statistical thresholding) used for detecting porosity from in-situ infrared imaging data for PBF-EB. Samples were manufactured at a variety of focus offset values to induce porosity. Then, the segmented infrared images were compared to ex-situ X-ray computed tomography scans, which served as a ground-truth reference for objective evaluation. Through this analysis framework, the influential parameters, static threshold and N-value (number of standard deviations above the mean pixel value), respectively, for both image segmentation methods were analyzed and compared for their effects on porosity detection. With optimal parameter settings, the two methods had similar porosity detection performance, but the statistical method performed better under a larger variety of parameter settings.

Infrared imaging↗

Sol-gel derived silicate-phosphate glass SiO 2 –P 2 O 5 –CaO–TiO 2 : The effect of titanium isopropoxide on porosity and thermomechanical stability

Despite of several decades lasting extensive research of bioactive and bioresorbable glasses the systematic parametrization and determination of the key factors affecting porosity and thermomechanical characteristics still remains challenging. Here, we present silica-phosphate glasses, with the composition 70SiO 2 - 20P 2 O 5 - (10-x)CaO-xTiO 2 (mol%; x = 0, 2.5, 5, and 7.5), prepared by sol -gel method and reinforced by titanium dioxide via titanium isopropoxide (TTIP) incorporation which demonstrated tunable variation of porosity from micro-to macro -region and superb mechanical integrity during the calcination process. The presence of 7.5 mol% TiO 2 promotes dimensional stability up to 1000°C as investigated by thermomechanical analysis. The XRD showed the dominant presence of silicon phosphate [Si(P 2 O 7 )], titanium phosphate [Ti(P 2 O 7 )] and calcium phosphates [β-Ca(P 2 O 6 ) and γ- Ca 2 (P 2 O 7 )]. The effect of TiO 2 doping on the multiscale morphology and porosity was investigated by means of SEM, MIP, μCT, N 2 adsorption and USAXS/SAXS. Increasing TiO 2 content leads to the formation of open porosity up to 70vol% and drives the formation of a refined interconnected macroporosity of 2-30 μm. In contrast, mesoporosity with a dominance of 3-6nm pores decreases in all samples with increasing TiO 2 content. USAXS/SAXS revealed an increase in primary particle size with increasing TiO 2 content which is in good agreement with the nitrogen physisorption analysis showing that microporosity decreases with increasing TiO2 content.

36 MATERIALS SCIENCE↗

Evolution of Elastic and Mechanical Properties During Fault Shear: The Roles of Clay Content, Fabric Development, and Porosity

Phyllosilicates weaken faults due to the formation of shear fabrics. Although the impacts of clay abundance and fabric on frictional strength, sliding stability, and porosity of faults are well studied, their influence on elastic properties is less known, though they are key factors for fault stiffness. We document the role that fabric and consolidation play in elastic properties and show that smectite content is the most important factor determining whether fabric or porosity controls the elastic response of faults. We conducted a suite of shear experiments on synthetic smectite-quartz fault gouges (10–100 wt% smectite) and sediment incoming to the Sumatra subduction zone. We monitored Vp, Vs, friction, porosity, shear and bulk moduli. We find that mechanical and elastic properties for gouges with abundant smectite are almost entirely controlled by fabric formation (decreasing mechanical and elastic properties with shear). Though fabrics control the elastic response of smectite-poor gouges over intermediate shear strains, porosity is the primary control throughout the majority of shearing. Elastic properties vary systematically with smectite content: High smectite gouges have values of Vp ~ 1,300–1,800 m/s, Vs ~ 900–1,100 m/s, K ~ 1–4 GPa, and G ~ 1–2 GPa, and low smectite gouges have values of Vp ~ 2,300–2,500 m/s, Vs ~ 1,200–1,300 m/s, K ~ 5–8 GPa, and G ~ 2.5–3 GPa. We find that, even in smectite-poor gouges, shear fabric also affects stiffness and elastic moduli, implying that while smectite abundance plays a clear role in controlling gouge properties, other fine-grained and platy clay minerals may produce similar behavior through their control on the development of fabrics and thin shear surfaces.

58 GEOSCIENCES↗

Correlations between thermal history and keyhole porosity in laser powder bed fusion

Additive manufacturing has the potential to revolutionize the production of metallic components as it yields near net shape parts with complex geometries and minimizes waste. At the present day, additively manufactured components face qualification and certification challenges due to the difficulty in controlling defects. This has driven a significant research effort aimed at better understanding and improving processing controls – yielding a plethora of in-situ measurements aimed at correlating defects with material quality metrics of interest. In this work, we develop machine-learning methods to learn correlations between thermal history and subsurface porosity for a variety of print conditions in laser powder bed fusion. Un-normalized surface temperatures (in the form of black-body radiances) are obtained using high-speed infrared imaging and porosity formation is observed in the sample cross-section through synchrotron x-ray imaging. To demonstrate the predictive power of these features, we present four statistical machine-learning models that correlate temperature histories to subsurface porosity formation in laser fused Ti-6Al4V powder.

36 MATERIALS SCIENCE↗

Dissolution and reprecipitation of amorphous silica in silica Rich shales induces Non-Monotonic evolution of porosity in acidic reactive environments

Advances in sustainable subsurface energy technologies are crucial for meeting our energy and resource needs for a climate-resilient future. Novel strategies to harness subsurface shale reservoirs for recovering valuable metals and for enabling CO 2 storage are influenced by the morphological and mineralogical heterogeneities of these materials. In this context, delineating the interactions of highly acidic solutions such as wet supercritical CO 2 on shales with varying mineralogy is crucial to inform the stability of caprock seal for CO 2 storage and enhancements in permeability for fluid transport, reactivity, and storage. The feedback chemical effects associated with the interactions of acidic solutions on the morphologies and mineralogies of shales have not been extensively investigated. These insights are crucial for assessing temporal changes in the reactivity and the fate of the fluids in subsurface environments. In this study, we investigate the effect of 1M HCl solution on the chemistry and morphology of three different shale samples with varying carbonate, clay and silica contents. An increase in the amorphous content, from 37% to 41.3%, of silica-rich and carbonate/clay lean shale is noted due to reactions with an acidic solution which is attributed to the dissolution of Si-bearing phases such as clays, accompanied by SiO 2 precipitation. In shales bearing high content of clays and carbonates, significant increase in the pore volumes and surface areas are noted. Non-monotonic changes in the micron-scale porosity of silica rich–carbonate/clay lean (e.g., Mowry shale) are noted using in-situ X-ray microtomography experiments. Due to the initial mobilization of silica and dissolution of carbonate/clay phases, the total porosity slightly increases from 6.7% to 10.7% followed by a decrease to similar to 4% caused by SiO 2 reprecipitation. In conclusion, these findings suggest that even though silica is less reactive in acidic environments, the changes in the amorphous and crystalline content due to dissolution and reprecipitation alter the porosity and fluid flow paths.

04 OIL SHALES AND TAR SANDS↗

Optimizing Porous Transport Layer Porosity for Proton Exchange Membrane Water Electrolysis

An empirical model is presented that describes anode-side losses related to porous transport layer (PTL) morphology in proton exchange membrane water electrolysis (PEMWE). The model is based on an advanced voltage breakdown analysis that links various overpotentials to PTL morphology. Custom Ti PTLs, spanning uncommonly low porosities (22 - 31%), were fabricated and analyzed with X-ray CT to obtain pore and particle size distributions. Particle size distributions were consistent across samples with an average particle diameter of 12.0?..mu..m, whereas average pore diameters ranged from 6.0 to 7.0?..mu..m. The PTLs were tested in standard PEMWE cell assemblies with anode catalyst loadings of 0.1 mgIr cm-2 to obtain polarization curves, electrochemical impedance spectra, and augmented Tafel analysis. The PTL-dependent anode side losses were deconvoluted and assigned to excess utilization, concentration, ion transport resistance, and electrical contact resistance overpotentials. The data and model reveal an optimal 20 - 28% PTL porosity region where utilization and contact resistance overpotentials are minimized without triggering concentration and ion transport losses related to water deprivation. The optimal PTL porosity depends on the operating current density and is demonstrated at realistic PEMWE water flow rates to establish PTL design guidance for operation at scale.

08 HYDROGEN↗

Site specific porosity-thermal performance correlations in neutron irradiated U-10Zr fuel

In this work, we present a site-specific three-dimensional analysis of porosity evolution in neutron-irradiated U–10Zr metallic fuel using high-resolution synchrotron X-ray tomography. Focused ion beam cubic lift-outs from four radial positions—fuel center, middle, edge, and fuel-cladding interaction (FCCI) zones—were imaged, reconstructed, and segmented to quantify pore volume, density, morphology, and pore connectivity. Porosity increased modestly from 5.5% at the center to 10.5% at the edge, yet pore number density increased by over two orders of magnitude in the fuel portion near the FCCI interface (from 4.8 x 10 4 to 6.0 x 10 6 pores/mm 3 ). Morphological classification revealed a progression from small spherical pores at the center to equiaxed and tortuous networks at the periphery, with enhanced orientation along the radial direction. Connectivity and permeability analysis reveal that the FCCI region maintains dense, highly interconnected pores despite a moderate volume fraction, enabling rapid fission gas transport and lanthanide migration. Effective thermal conductivity models incorporating sodium logging confirm that these site-specific pore features critically influenced heat transport during reactor irradiation. These findings demonstrate that pore topology—not just porosity fraction—controls thermal performance and thermal pathways in U–10Zr fuels, impacting fuel thermal performance in a reactor.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗