Search NASA⌕ Search

SEARCH · Search NASA

Results for “silicone elastomer”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Characterization of Adhesives for Attaching Reusable Surface Insulation on Space Shuttle Vehicles

An extensive development and testing program on adhesive systems shows that: (1) A closed cell silicone rubber sponge bonded to substrates with thin bond lines of glass filled adhesive exhibits density and modulus values approximately one third that of solid silicone adhesives; (2) utilization of glass or phenolic microballoons as fillers in silicone adhesives reduces density but increases moduli of the vulcanized materials; (3) the silicone elastomer based adhesives appear to be complex systems rather than homogeneous, isotropic materials. Tensile, shear, and compression properties plotted versus temperature verify this conjecture; and (4) constant strain-stress relaxation tests on glass-filled adhesive show that stress relaxation is most pronounced near the glass transition temperature.

Owen, H. P.↗

Bonding of reusable surface insulation with low density silicone foams

The development and evaluation of a reduced density, high reliable foamed bond strain isolation system for attaching reusable surface insulation to the space shuttle structure are reported. Included are data on virgin materials as well as on materials that received 100 cycles of exposure to 650 F for approximately 20 minutes per cycle. Room temperature vulcanizing silicon elastomers meet all the requirments for an adhesive bonding system.

Hiltz, A. A.↗

Interaction of gases with ablative composites. II - Water

An investigation was conducted to study the sorption of water on two ablative composites and their components as a function of pressure and temperature. A pressure range from 0.001 to 10 torr and a temperature range from 25 to 35 C were considered in the investigation. It was found that the sorption of water vapor by the ablative composites and their components varied directly with pressure. The components of the ablative composites included phenolic spheres, cork, a carbon-glass fiber mixture, glass spheres, silica fibers, and a silicone elastomer.

Honeycutt, R. H., III↗

Evaluation of the energy transfer in the char zone during ablation. Part 2: In-depth response of ablative composites, volume 1

The decomposition of ablative composites is described along with the transport phenomena of pyrolysis gases which result from the decomposition of these plastics as they flow through the porous char of char-forming ablators. The pyrolysis products are those formed by the thermal degradation of nylon-phenolic resin and silicone elastomer composites. Emphasis is placed on the nature and extent of chemical reactions of the pyrolysis products and the char, along with the energy absorbed by the combined pyrolysis and char zone. Chemical reactions with thermodynamically consistent kinetic data are determined in order to develop a realistic analysis for predicting the thermal performance of ablative heat shields.

Pike, R. W.↗

Advanced solid electrolyte cell for CO2 and H2O electrolysis

A solid electrolyte cell with improved sealing characteristics was examined. A tube cell was designed, developed, fabricated, and tested. Design concepts incorporated in the tube cell to improve its sealing capability included minimizing the number of seals per cell and moving seals to lower temperature regions. The advanced tube cell design consists of one high temperature ceramic cement seal, one high temperature gasket seal, and three low temperature silicone elastomer seals. The two high temperature seals in the tube cell design represent a significant improvement over the ten high temperature precious metal seals required by the electrolyzer drum design. For the tube cell design the solid electrolyte was 8 mole percent yttria stabilized zirconium oxide slip cast into the shape of a tube with electrodes applied on the inside and outside surfaces.

Shumar, J. W.↗

Improved Cure-in-Place Silicone Adhesives

Two improved cure-in-place silicone-elastomer-based adhesives have low thermal expansion and low thermal conductivity. Adhesives are flexible at low temperature and withstand high temperatures without disintegrating. New ablative compounds were initially developed for in-flight repair of insulating tile on Space Shuttle orbiter. Could find use in other applications requiring high-performance adhesives, such as sealants for solar collectors.

Blevins, C. E.↗

Synthesis of aminosilane and aromatic diamine intermediates for polymerization

The preparation of monomers for use in a study to improve properties of epoxy polymers and silicone elastomers is described. Various approaches to the solution of the synthesis of aminosilane and diamine curing agents were examined. Ortho-, meta-, and para-substituted diamines where X is CH2, C(CH3)2, O, S, NH, or SO2 and n = 0, 1, 2, and 3 were investigated.

Mcmanus, S. P.↗

Molding Compound For Inspection Of Internal Contours

Material clean, sets rapidly, and easy to use. Silicone elastomer, Citrocon or equivalent, commonly used in dentistry, in combination with mold-release agent (Also see MFS-29240), speeds and facilitates making of impressions of interior surfaces so surface contours examined. Elastomer easily moved around in cavity until required location found.

Adams, Jim↗

Reducing Seal Adhesion in Low Impact Docking Systems

Silicone elastomers, used in seals for airlocks or other sealing surfaces in space, are sticky in their as-received condition. Because of the sticking, a greater force may be needed to separate the mating surfaces. If the adhesion is sufficiently high, a sudden unpredicted movement of the spacecraft during undocking, vibration, or uneven release could pull off the seal, resulting in a damage that would have to be repaired before another docking. The damaged seal can result in significant gas leakage and possibly in a catastrophic mishap impacting the safety of the crew. It is also possible that a compromised seal could result in a delayed but sudden gas leak that could put the crew at unexpected risk. This is especially of concern for androgynous seals, which have identical mating surfaces on both sides for interchangeability and redundancy. Such seals typically have elastomer-on-elastomer sealing surfaces. To reduce sticking, one could use release agents such as powders and lubricants, but these can be easily removed and transferred to other surfaces, causing uneven sealing and contamination. Modification of the elastomer surface to make a more slippery and less sticky surface that is integral with the bulk elastomer would be more desirable.

Banks, Bruce A.↗

Adjusting Permittivity by Blending Varying Ratios of SWNTs

A new composite material of singlewalled carbon nanotubes (SWNTs) displays radio frequency (0 to 1 GHz) permittivity properties that can be adjusted based upon the nanotube composition. When varying ratios of raw to functionalized SWNTs are blended into the silicone elastomer matrix at a total loading of 0.5 percent by weight, a target real permittivity value can be obtained between 70 and 3. This has particular use for designing materials for microwave lenses, microstrips, filters, resonators, high-strength/low-weight electromagnetic interference (EMI) shielding, antennas, waveguides, and low-loss magneto-dielectric products for applications like radome construction.

Tour, James M.↗

Validation of Test Methods for Air Leak Rate Verification of Spaceflight Hardware

As deep space exploration continues to be the goal of NASAs human spaceflight program, verification of the performance of spaceflight hardware becomes increasingly critical. Suitable test methods for verifying the leak rate of sealing systems are identified in program qualification testing requirements. One acceptable method for verifying the air leak rate of gas pressure seals is the tracer gas leak detector method. In this method, a tracer gas (commonly helium) leaks past the test seal and is transported to the leak detector where the leak rate is quantified. To predict the air leak rate, a conversion factor of helium-to-air is applied depending on the magnitude of the helium flow rate. The conversion factor is based on either the molecular mass ratio or the ratio of the dynamic viscosities. The current work was aimed at validating this approach for permeation-level leak rates using a series of tests with a silicone elastomer O-ring. An established pressure decay method with constant differential pressure was used to evaluate both the air and helium leak rates of the O-ring under similar temperature and pressure conditions. The results from the pressure decay tests showed, for the elastomer O-ring, that neither the molecular flow nor the viscous flow helium-to-air conversion factors were applicable. Leak rate tests were also performed using nitrogen and argon as the test gas. Molecular mass and viscosity based helium-to-test gas conversion factors were applied, but did not correctly predict the measured leak rates of either gas. To further this study, the effect of pressure boundary conditions was investigated. Often, pressure decay leak rate tests are performed at a differential pressure of 101.3 kPa with atmospheric pressure on the downstream side of the test seal. In space applications, the differential pressure is similar, but with vacuum as the downstream pressure. The same O-ring was tested at four unique differential pressures ranging from 34.5 to 137.9 kPa. Up to six combinations of upstream and downstream pressures for each differential pressure were compared. For a given differential pressure, the various combinations of upstream and downstream dry air pressures did not significantly affect the leak rate. As expected, the leak rate of the O-ring increased with increasing differential pressure. The results suggested that the current leak test pressure conditions, used to verify spacecraft sealing systems with elastomer seals, produce accurate values even though the boundary conditions do not model the space application.

helium leak detector↗

Space Environment's Effects on Seal Materials

A Low Impact Docking System (LIDS) is being developed by the NASA Johnson Space Center to support future missions of the Crew Exploration Vehicle (CEV). The LIDS is androgynous, such that each system half is identical, thus any two vehicles or modules with LIDS can be coupled. Since each system half is a replica, the main interface seals must seal against each other instead of a conventional flat metal surface. These sealing surfaces are also expected to be exposed to the space environment when vehicles are not docked. The NASA Glenn Research Center (NASA GRC) is supporting this project by developing the main interface seals for the LIDS and determining the durability of candidate seal materials in the space environment. In space, the seals will be exposed to temperatures of between 50 to 50 C, vacuum, atomic oxygen, particle and ultraviolet radiation, and micrometeoroid and orbital debris (MMOD). NASA GRC is presently engaged in determining the effects of these environments on our candidate elastomers. Since silicone rubber is the only class of seal elastomer that functions across the expected temperature range, NASA GRC is focusing on three silicone elastomers: two provided by Parker Hannifin (S0-899-50 and S0-383-70) and one from Esterline Kirkhill (ELA-SA-401). Our results from compression set, elastomer to elastomer adhesion, and seal leakage tests before and after various simulated space exposures will be presented.

deGroh, Henry C., III↗

Ultra-High-Molecular-Weight Silphenylene/Siloxane Elastomers

Elastomers enhance thermal and mechancial properties. Capable of performing in extreme thermal/oxidative environments and having molecular weights above 10 to the sixth power prepared and analyzed in laboratory experiments. Made of methylvinylsilphenylene-siloxane terpolymers, new materials amenable to conventional silicone-processing technology. Similarly formulated commercial methyl-vinyl silicones, vulcanized elastomers exhibit enhance thermal/oxidative stability and equivalent or superior mechanical properties.

Hundley, N. H.↗

NASA Tech Briefs, Februrary 2013

Topics covered include: Measurements of Ultra-Stable Oscillator (USO) Allan Deviations in Space; Gaseous Nitrogen Orifice Mass Flow Calculator; Validation of Proposed Metrics for Two-Body Abrasion Scratch Test Analysis Standards; Rover Low Gain Antenna Qualification for Deep Space Thermal Environments; Automated, Ultra-Sterile Solid Sample Handling and Analysis on a Chip; Measuring and Estimating Normalized Contrast in Infrared Flash Thermography; Spectrally and Radiometrically Stable, Wideband, Onboard Calibration Source; High-Reliability Waveguide Vacuum/Pressure Window; Methods of Fabricating Scintillators With Radioisotopes for Beta Battery Applications; Magnetic Shield for Adiabatic Demagnetization Refrigerators (ADR); CMOS-Compatible SOI MESFETS for Radiation-Hardened DC-to-DC Converters; Silicon Heat Pipe Array; Adaptive Phase Delay Generator; High-Temperature, Lightweight, Self-Healing Ceramic Composites for Aircraft Engine Applications; Treatment to Control Adhesion of Silicone-Based Elastomers; High-Temperature Adhesives for Thermally Stable Aero-Assist Technologies; Rockballer Sample Acquisition Tool; Rock Gripper for Sampling, Mobility, Anchoring, and Manipulation; Advanced Magnetic Materials Methods and Numerical Models for Fluidization in Microgravity and Hypogravity; Data Transfer for Multiple Sensor Networks Over a Broad Temperature Range; Using Combustion Synthesis to Reinforce Berms and Other Regolith Structures; Visible-Infrared Hyperspectral Image Projector; Three-Axis Attitude Estimation With a High-Bandwidth Angular Rate Sensor Change_Detection.m; AGATE: Adversarial Game Analysis for Tactical Evaluation; Ionospheric Simulation System for Satellite Observations and Global Assimilative; Modeling Experiments (ISOGAME); An Extensible, User- Modifiable Framework for Planning Activities; Mission Operations Center (MOC) - Precipitation Processing System (PPS) Interface Software System (MPISS); Automated 3D Damaged Cavity Model Builder for Lower Surface Acreage Tile on Orbiter; Mixed Linear/Square-Root Encoded Single-Slope Ramp Provides Low-Noise ADC with High Linearity for Focal Plane Arrays; RUSHMAPS: Real-Time Uploadable Spherical Harmonic Moment Analysis for Particle Spectrometers; Powered Descent Guidance with General Thrust-Pointing Constraints; X-Ray Detection and Processing Models for Spacecraft Navigation and Timing; and Extreme Ionizing-Radiation-Resistant Bacterium

Source record↗

Comparison of Adhesion and Retention Forces for Two Candidate Docking Seal Elastomers

To successfully mate two pressurized vehicles or structures in space, advanced seals are required at the interface to prevent the loss of breathable air to the vacuum of space. A critical part of the development testing of candidate seal designs was a verification of the integrity of the retaining mechanism that holds the silicone seal component to the structure. Failure to retain the elastomer seal during flight could liberate seal material in the event of high adhesive loads during undocking. This work presents an investigation of the force required to separate the elastomer from its metal counter-face surface during simulated undocking as well as a comparison to that force which was necessary to destructively remove the elastomer from its retaining device. Two silicone elastomers, Wacker 007-49524 and Esterline ELASA-401, were evaluated. During the course of the investigation, modifications were made to the retaining devices to determine if the modifications improved the force needed to destructively remove the seal. The tests were completed at the expected operating temperatures of -50, +23, and +75 C. Under the conditions investigated, the comparison indicated that the adhesion between the elastomer and the metal counter-face was significantly less than the force needed to forcibly remove the elastomer seal from its retainer, and no failure would be expected.

Hartzler, Brad D.↗

Space Environment Effects on Silicone Seal Materials

A docking system is being developed by the NASA to support future space missions. It is expected to use redundant elastomer seals to help contain cabin air during dockings between two spacecraft. The sealing surfaces are exposed to the space environment when vehicles are not docked. In space, the seals will be exposed to temperatures between 125 to -75 C, vacuum, atomic oxygen, particle and ultraviolet radiation, and micrometeoroid and orbital debris (MMOD). Silicone rubber is the only class of space flight-qualified elastomeric seal material that functions across the expected temperature range. NASA Glenn has tested three silicone elastomers for such seal applications: two provided by Parker (S0899-50 and S0383-70) and one from Esterline (ELA-SA-401). The effects of atomic oxygen (AO), UV and electron particle radiation, and vacuum on the properties of these three elastomers were examined. Critical seal properties such as leakage, adhesion, and compression set were measured before and after simulated space exposures. The S0899-50 silicone was determined to be inadequate for extended space seal applications due to high adhesion and intolerance to UV, but both S0383-70 and ELA-SA-401 seals were adequate.

deGroh, Henry C., III↗

Removing overcoatings from microcircuits

Silicone resin of elastomer overcoatings are removed more quickly from microcircuit chips with hot concentrated sulfuric acid. Process takes few minutes as compared to day or two, using commercial solvents based on toluene, xylene, and like. Overcoatings are removed to expose circuit for failure analysis.

Belcher, J. G., Jr.↗

Determination of Silicon in Hydrazine

Inductively coupled plasma-mass spectrometry (ICP-MS) is a highly sensitive technique sometimes used for the trace determination of silicon at a mass-to-charge (m/z) ratio of 28, the most abundant natural isotope of silicon. Unfortunately, ICP-MS is unable to differentiate between other sources of m/z 28 and false positive results for silicon will result when other sources of m/z 28 are present. Nitrogen was a major source of m/z 28 and contributes to the m/z 28 signal when hydrazine sample or nitric acid preservative is introduced into the plasma. Accordingly, this work was performed to develop a sample preparation step coupled with an ICP-MS analysis that minimized non-silicon sources of m/z 28. In the preparatory step of this method, the hydrazine sample was first decomposed predominately to nitrogen gas and water with copper-catalyzed hydrogen peroxide. In the analysis step, ICP-MS was used without nitric acid preservative in samples or standards. Glass, a potential source of silicon contamination, was also avoided where possible. The method was sensitive, accurate, and reliable for the determination of silicon in monopropellant grade hydrazine (MPH) in AF-E-332 elastomer leaching tests. Results for silicon in MPH were comparable to those reported in the literature for other studies.

McClure, Mark B.↗