Biaxial constitutive modelling and testing of a single crystal superalloy at elevated temperatures

A viscoplastic constitutive model for single crystal superalloys is developed from crystallographic slip theory. The model is applied to the tension and torsion deformation behavior of the single crystal superalloy PWA 1480 at 871 C (1600 F). Both octahedral and cube slip behavior are needed to model the deformation behavior of single crystal superalloys at elevated temperature.

Walker, K. P.↗

Effect of tensile mean stress on fatigue behavior of single-crystal and directionally solidified superalloys

Two nickel base superalloys, single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf, were studied in view of the potential usage of the former and usage of the latter as blade materials for the turbomachinery of the Space Shuttle main engine. The baseline zero mean stress (ZMS) fatigue life (FL) behavior of these superalloys was established, and then the effect of tensile mean stress (TMS) on their FL behavior was characterized. A stress range based FL prediction approach was used to characterize both the ZMS and TMS fatigue data. In the past, several researchers have developed methods to account for the detrimental effect of tensile mean stress on the FL for polycrystalline engineering alloys. These methods were applied to characterize the TMS fatigue data of single crystal PWA 1480 and directionally solidified MAR-M 246 + Hf and were found to be unsatisfactory. Therefore, a method of accounting for the TMS effect on FL, that is based on a technique proposed by Heidmann and Manson was developed to characterize the TMS fatigue data of these superalloys. Details of this method and its relationship to the conventionally used mean stress methods in FL prediction are discussed.

Kalluri, Sreeramesh↗

Effects of Hydrogen Annealing, Sulfur Segregation and Diffusion on the Cyclic Oxidation Resistance of Superalloys: a Review

This review is based on the phenomenon of improved oxide scale adhesion for desulfurized superalloys. The proposed adhesion mechanism involves sulfur interfacial segregation and scale-metal bond weakening. Sulfur surface segregation on superalloys is examined as a function of temperature and sulfur content and related to classical behavior predicted by the McLean isotherm. Effective desulfurization to less than 1 ppmw can be accomplished by hydrogen annealing and is governed by sulfur diffusion kinetics in nickel. Hydrogen annealing results in excellent cyclic oxidation resistance for a number of advanced superalloys. The concept of a critical sulfur content is discussed in terms of practical annealing conditions and section thicknesses.

Smialek, J. L.↗

Effects of hydrogen annealing, sulfur segregation and diffusion on the cyclic oxidation resistance of superalloys: A review

This review is based on the phenomenon of improved oxide scale adhesion for desulfurized superalloys. The proposed adhesion mechanism involves sulfur interfacial segregation and scale-metal bond weakening. Sulfur surface segregation on superalloys is examined as a function of temperature and sulfur content, and is related to the classical behavior predicted by the McLean isotherm. Effective desulfurization to less than 1 ppmw can be accomplished by hydrogen annealing and is described by sulfur diffusion kinetics in nickel. Hydrogen annealing results in excellent cyclic oxidation resistance for a number of advanced superalloys. The concept of a critical sulfur content is discussed in terms of practical annealing conditions and section thicknesses.

Smialek, J. L.↗

Soft Computing Methods in Design of Superalloys

Soft computing techniques of neural networks and genetic algorithms are used in the design of superalloys. The cyclic oxidation attack parameter K(sub a), generated from tests at NASA Lewis Research Center, is modelled as a function of the superalloy chemistry and test temperature using a neural network. This model is then used in conjunction with a genetic algorithm to obtain an optimized superalloy composition resulting in low K(sub a) values.

Cios, K. J.↗

Soft computing methods in design of superalloys

Soft computing techniques of neural networks and genetic algorithms are used in the design of superalloys. The cyclic oxidation attack parameter K(sub a), generated from tests at NASA Lewis Research Center, is modeled as a function of the superalloy chemistry and test temperature using a neural network. This model is then used in conjunction with a genetic algorithm to obtain an optimized superalloy composition resulting in low K(sub a) values.

Cios, K. J.↗

Effect of Crystal Orientation on Fatigue Failure of Single Crystal Nickel Base Turbine Blade Superalloys

High Cycle Fatigue (HCF) induced failures in aircraft gas-turbine engines is a pervasive problem affecting a wide range of components and materials. HCF is currently the primary cause of component failures in gas turbine aircraft engines. Turbine blades in high performance aircraft and rocket engines are increasingly being made of single crystal nickel superalloys. Single-crystal Nickel-base superalloys were developed to provide superior creep, stress rupture, melt resistance and thermomechanical fatigue capabilities over polycrystalline alloys previously used in the production of turbine blades and vanes. Currently the most widely used single crystal turbine blade superalloys are PWA 1480/1493 and PWA 1484. These alloys play an important role in commercial, military and space propulsion systems. PWA1493, identical to PWA1480, but with tighter chemical constituent control, is used in the NASA SSME (Space Shuttle Main Engine) alternate turbopump, a liquid hydrogen fueled rocket engine. Objectives for this paper are motivated by the need for developing failure criteria and fatigue life evaluation procedures for high temperature single crystal components, using available fatigue data and finite element modeling of turbine blades. Using the FE (finite element) stress analysis results and the fatigue life relations developed, the effect of variation of primary and secondary crystal orientations on life is determined, at critical blade locations. The most advantageous crystal orientation for a given blade design is determined. Results presented demonstrates that control of secondary and primary crystallographic orientation has the potential to optimize blade design by increasing its resistance to fatigue crack growth without adding additional weight or cost.

Arakere, Nagaraj K.↗

Fretting Stresses in Single Crystal Superalloy Turbine Blade Attachments

Single crystal nickel base superalloy turbine blades are being utilized in rocket engine turbopumps and turbine engines because of their superior creep, stress rupture, melt resistance and thermomechanical fatigue capabilities over polycrystalline alloys. Currently the most widely used single crystal nickel base turbine blade superalloys are PWA 1480/1493 and PWA 1484. These alloys play an important role in commercial, military and space propulsion systems. High Cycle Fatigue (HCF) induced failures in aircraft gas turbine and rocket engine turbopump blades is a pervasive problem. Blade attachment regions are prone to fretting fatigue failures. Single crystal nickel base superalloy turbine blades are especially prone to fretting damage because the subsurface shear stresses induced by fretting action at the attachment regions can result in crystallographic initiation and crack growth along octahedral planes. Furthermore, crystallographic crack growth on octahedral planes under fretting induced mixed mode loading can be an order of magnitude faster than under pure mode I loading. This paper presents contact stress evaluation in the attachment region for single crystal turbine blades used in the NASA alternate Advanced High Pressure Fuel Turbo Pump (HPFTP/AT) for the Space Shuttle Main Engine (SSME). Single crystal materials have highly orthotropic properties making the position of the crystal lattice relative to the part geometry a significant factor in the overall analysis. Blades and the attachment region are modeled using a large-scale 3D finite element (FE) model capable of accounting for contact friction, material orthotrophy, and variation in primary and secondary crystal orientation. Contact stress analysis in the blade attachment regions is presented as a function of coefficient of friction and primary and secondary crystal orientation, Stress results are used to discuss fretting fatigue failure analysis of SSME blades. Attachment stresses are seen to reach peak values at locations where fretting cracks have been observed. Fretting stresses at the attachment region are seen to vary significantly as a function of crystal orientation. Attempts to adapt techniques used for estimating fatigue life in the airfoil region, for life calculations in the attachment region, are presented. An effective model for predicting crystallographic crack initiation under mixed mode loading is required for life prediction under fretting action.

Arakere, Nagaraj K.↗

Computational Thermodynamic Study to Predict Complex Phase Equilibria in the Nickel-Base Superalloy Rene N6

A previous study by Ritzert et al. on the formation and prediction of topologically closed packed (TCP) phases in the nickel-base superalloy Rene' N6 is re-examined with computational thermodynamics. The experimental data on phase distribution in forty-four alloys with a composition within the patent limits of the nickel-base superalloy Rene' N6 provide a good basis for comparison to and validation of a commercial nickel superalloy database used with ThermoCalc. Volume fraction of the phases and partitioning of the elements are determined for the forty-four alloys in this dataset. The baseline heat treatment of 400 h at 1366 K was used. This composition set is particularly interesting since small composition differences lead to dramatic changes in phase composition. In general the calculated values follow the experimental trends. However, the calculations indicated no TCP phase formation when the experimental measurements gave a volume percent of TCP phase less than 2 percent. When TCP phases were predicted, the calculations under-predict the volume percent of TCP phases by a factor of 2 to 8. The calculated compositions of the gamma and gamma' phases show fair agreement with the measurements. However, the calculated compositions of the P Phase do not agree with those measured. This may be due to inaccuracies in the model parameters for P phase and/or issues with the microprobe analyses of these phases. In addition, phase fraction diagrams and sigma and P phase solvus temperatures are calculated for each of the alloys. These calculations indicate that P phase is the primary TCP phase formed for the alloys considered here at 1366 K. Finally, a series of isopleths are calculated for each of the seven alloying elements. These show the effect of each alloying element on creating TCP phases.

Copland, Evan H.↗

Superalloy Foams for Aeroshell Applications

Current thermal protection systems for reentry from space, such as that employed on the space shuttle, rely on ceramic tiles with ultra-low conductivity. These materials provide excellent thermal protection but are extremely fragile, easily degraded by environmental attack, and carry no structural loads. Future thermal protection systems being proposed in NASAs MITAS Program will attempt to combine thermal protection with improved durability and structural capability without significant increases in vehicle weight. This may be accomplished by combining several materials in a layered structure to obtain the desired function for aeroshell applications. One class of materials being considered for inclusion in this concept are high temperature metal foam. The objective of this paper was to fabricate low density, superalloy foams and conduct limited testing to evaluate their thermal and structural capabilities. Superalloys were chosen for evaluation as they possesses good strength and excellent environmental endurance over a wide range of temperatures. Utilizing superalloys as low density foams, with porosity contents greater than 90%, minimizes weight and thermal conductivity.

Gayda, John↗

Superalloy Lattice Block Structures

In their simplest form, lattice block panels are produced by direct casting and result in lightweight, fully triangulated truss-like configurations which provide strength and stiffness [2]. The earliest realizations of lattice block were made from A1 and steels, primarily under funding from the US Navy [3]. This work also showed that the mechanical efficiency (eg., specific stiffness) of lattice block structures approached that of honeycomb structures [2]. The lattice architectures are also less anisotropic, and the investment casting route should provide a large advantage in cost and temperature capability over honeycombs which are limited to alloys that can be processed into foils. Based on this early work, a program was initiated to determine the feasibility of extending the high temperature superalloy lattice block [3]. The objective of this effort was to provide an alternative to intermetallics and composites in achieving a lightweight high temperature structure without sacrificing the damage tolerance and moderate cost inherent in superalloys. To establish the feasibility of the superalloy lattice block concept, work was performed in conjunction with JAMCORP, Inc. Billerica, MA, to produce a number of lattice block panels from both IN71 8 and Mar-M247.

Whittenberger, J. D.↗

Strengthening Precipitate Morphologies Fully Quantified in Advanced Disk Superalloys

Advanced aviation gas turbine engines will require disk superalloys that can operate at higher temperatures and stresses than current conditions. Such applications will be limited by the tensile, creep, and fatigue mechanical properties of these alloys. These mechanical properties vary with the size, shape, and quantity of the gamma precipitates that strengthen disk superalloys. It is therefore important to quantify these precipitate parameters and relate them to mechanical properties to improve disk superalloys. Favorable precipitate morphologies and practical processing approaches to achieve them can then be determined. A methodology has been developed at the NASA Lewis Research Center to allow the comprehensive quantification of the size, shape, and quantity of all types of gamma precipitates.

Gabb, Timothy P.↗

Compatibility of Niobium Alloys and Superalloys in a Flowing He-Xe Power Conversion System

Proposed concepts for an ambitious mission to explore Jupiter's three icy moons place significant demands on the various spacecraft systems. There are many challenges related to the high output power conversion systems being considered, and one example is the need to ensure system compatibility at all levels. The utilization of appropriate materials for component structures is important to ensuring long mission life. Refractory metal alloys have attractive high-temperature properties in inert environments, but these alloys are sometimes susceptible to contamination. Potential material compatibility issues exist between refractory metal candidates and more conventional alloys. Nb-1Zr has long been considered one of the most well characterized refractory alloys that is well suited for elevated-temperature use and liquid-metal compatibility. However, previous studies have suggested that niobium alloys can not co-exist in a closed system with traditional stainless steels or superalloys due to transport of contaminants. The relevance of this information to a proposed power conversion system is discussed. Also, experiments and fundamental calculations are being performed to determine contamination transport from candidate superalloys to Nb-1Zr in a closed system with an inert carrier gas. Potential protective schemes are explored to ensure system level compatibility between the refractory alloy Nb-1Zr and a nickel-based superalloy.

Bowman, Cheryl L.↗

Initial Mechanical Testing of Superalloy Lattice Block Structures Conducted

The first mechanical tests of superalloy lattice block structures produced promising results for this exciting new lightweight material system. The testing was performed in-house at NASA Glenn Research Center's Structural Benchmark Test Facility, where small subelement-sized compression and beam specimens were loaded to observe elastic and plastic behavior, component strength levels, and fatigue resistance for hundreds of thousands of load cycles. Current lattice block construction produces a flat panel composed of thin ligaments arranged in a three-dimensional triangulated trusslike structure. Investment casting of lattice block panels has been developed and greatly expands opportunities for using this unique architecture in today's high-performance structures. In addition, advances made in NASA's Ultra-Efficient Engine Technology Program have extended the lattice block concept to superalloy materials. After a series of casting iterations, the nickel-based superalloy Inconel 718 (IN 718, Inco Alloys International, Inc., Huntington, WV) was successfully cast into lattice block panels; this combination offers light weight combined with high strength, high stiffness, and elevated-temperature durability. For tests to evaluate casting quality and configuration merit, small structural compression and bend test specimens were machined from the 5- by 12- by 0.5-in. panels. Linear elastic finite element analyses were completed for several specimen layouts to predict material stresses and deflections under proposed test conditions. The structural specimens were then subjected to room-temperature static and cyclic loads in Glenn's Life Prediction Branch's material test machine. Surprisingly, the test results exceeded analytical predictions: plastic strains greater than 5 percent were obtained, and fatigue lives did not depreciate relative to the base material. These assets were due to the formation of plastic hinges and the redundancies inherent in lattice block construction, which were not considered in the simplified computer models. The fatigue testing proved the value of redundancies since specimen strength was maintained even after the fracture of one or two ligaments. This ongoing test program is planned to continue through high-temperature testing. Also scheduled for testing are IN 718 lattice block panels with integral face sheets, as well as specimens cast from a higher temperature alloy. The initial testing suggests the value of this technology for large panels under low and moderate pressure loadings and for high-risk, damage-tolerant structures. Potential aeropropulsion uses for lattice blocks include turbine-engine actuated panels, exhaust nozzle flaps, and side panel structures.

Krause, David L.↗

Effects of High-Temperature Exposures on the Fatigue Life of Disk Superalloys Examined

Tests used to characterize the low-cycle-fatigue resistance of disk superalloys are usually performed at cyclic frequencies of 0.33 Hz or faster. However, service conditions for disks in some aerospace and land-based gas turbine engines can produce major cycle periods extending from minutes to hours and days. Over a service life, this can produce total service times near the maximum temperature that exceed 100 hr for aerospace applications and 100,000 hr for land-based applications. Such time-dependent effects of realistic mission cycles on fatigue resistance can be significant in superalloy disks, and need to be considered for accurate disk life prediction. The purpose of this study at the NASA Glenn Research Center was to examine the effects of extended exposures and extended cycle periods on the fatigue resistance of two disk superalloys. Current alloy Udimet 720 (Special Metals Corporation, Huntington, WV) disk material was provided by Solar Turbines/Caterpillar Co., and advanced alloy ME3 was provided by the NASA Ultra-Efficient Engine Technologies (UEET) Project, in powder-metallurgy-processed, supersolvus heat-treated form. Fatigue specimens were fully machined and exposed in air at temperatures of 650 to 704 C for extended times. Then, they were tested using conventional fatigue tests with a total strain range of 0.70 percent and a minimum-to-maximum strain ratio of zero to determine the effects of prior exposure on fatigue resistance. Subsequent tests with extended dwells at minimum strain in each fatigue cycle were performed to determine cyclic exposure effects.

Gabb, Timothy P.↗

NASA and Superalloys: A Customer, a Participant, and a Referee

NASA has had a long history of research and development in the field of superalloys. These efforts have continued today, where the latest advancements in turbine disk and blade technologies are being developed Although NASA does support military flight systems, it s predominant role is in supporting civilian air transportation systems, and thus has goals for improving fuel efficiency, emissions, noise, and safety of today s aircraft. NASA has traditionally served several distinct but complimentary roles as participants in multi-disciplinary research teams, as customers who fund research and development efforts at industry and universities, and as referees who can address broad issues that affect the entire aeronautics community. Because of our longer range viewpoint, we can take on higher risk, higher reward research topics. NASA can also serve as an intermediary between the basic research performed primarily at universities and the development efforts emphasized by industry. By interacting with individual companies, NASA can identify areas of general interest and problems common to a large portion of the aeronautics community, and devise programs aimed at solving these problems. In space missions, NASA is a direct customer responsible for developing vehicles. In the case of the Space Shuttle, NASA has worked with various contractors to design and build numerous components out of superalloys. Another fascinating area for the use of superalloys is in power systems for long life applications in space. Potential missions include providing electric power for deep space missions, surface rovers, including lunar and Mars, and stationary power generators on the lunar surface.

Nathal, Michael V.↗

NASA and Superalloys: A Customer, a Participant, and a Referee

NASA has had a long history of research and development in the field of superalloys. These efforts have continued today, where the latest advancements in turbine disk and blade technologies are being developed. Although NASA does support military flight systems, its predominant role is in supporting civilian air transportation systems, and thus has goals for improving fuel efficiency, emissions, noise, and safety of today s aircraft. NASA has traditionally served several distinct but complimentary roles as participants in multi-disciplinary research teams, as customers who fund research and development efforts at industry and universities, and as referees who can address broad issues that affect the entire aeronautics community. Because of our longer range viewpoint, we can take on higher risk, higher reward research topics. NASA can also serve as an intermediary between the basic research performed primarily at universities and the development efforts emphasized by industry. By interacting with individual companies, NASA can identify areas of general interest and problems common to a large portion of the aeronautics community, and devise programs aimed at solving these problems. In space missions, NASA is a direct customer responsible for developing vehicles. In the case of the Space Shuttle, NASA has worked with various contractors to design and build numerous components out of superalloys. Another fascinating area for the use of superalloys is in power systems for long life applications in space. Potential missions include providing electric power for deep space missions, surface rovers, including lunar and Mars, and stationary power generators on the lunar surface.

Nathal, Michael V.↗

A New Approach of Designing Superalloys for Low Density

New low-density single-crystal (LDS) alloy, have bee. developed for turbine blade applications, which have the potential for significant improvements in the thrust-to-weight ratio over current production superalloys. An innovative alloying strategy was wed to achieve alloy density reductions, high-temperature creep resistance, microstructural stability, and cyclic oxidation resistance. The alloy design relies on molybdenum as a potent. lower-density solid-solution strengthener in the nickel-based superalloy. Low alloy density was also achieved with modest rhenium levels tmd the absence of tungsten. Microstructural, physical mechanical, and environmental testing demonstrated the feasibility of this new LDS superalloy design.

MacKay, Rebecca A.↗