Electrostatic Separation Of Layers In Thermal Insulation

Layers in multilayer insulation charged to keep them separated by electrostatic repulsion, eliminating need for spacer nets. Removal of spacer nets reduces conduction of heat between layers. Insulation in question type used to slow leakage of heat into Dewar flasks containing liquid helium. Proposal originally applied to insulation in cryogenic cooling subsystems of infrared-detector systems in outer space, also appears applicable to small panels of insulation for terrestrial cryogenic equipment, provided layers contained in evacuated spaces and weight of each layer small fraction of electrostatic force upon it.

Bhandari, Pradeep↗

Mechanically and thermally robust microporous copolymer separators for lithium ion batteries

Next generation, multifunctional separators can enhance energy storage, power, and safety performance of lithium ion batteries but must be simple to fabricate and incorporate with existing roll-to-roll manufacturing. Here, this study presents a strategy to facilely prepare these separators using UV-initiated polymerization-induced phase separation (PIPS), wherein microporous polymer separators are fabricated directly from constituent monomers and ethylene carbonate (EC) porogen. This enables a wide compositional design space as co-monomers with specific chemical functionality can be readily incorporated into the PIPS precursor mixture. Herein, 1,4-butanediol diacrylate (BDDA) was copolymerized with poly(ethylene glycol) diacrylate (PEGDA) to increase the acrylate conversion in the photopolymerization and improve mechanical properties. By tuning the ratio of PEGDA and EC, separators with high porosity (41.3%) and effective ionic conductivity (2.09 mS cm –1 ) were prepared. Inclusion of PEGDA was essential to increasing the elastic modulus to > 345 MPa, which is required for cell assembly by roll-to-roll manufacturing. All separators prepared were shown to enable reversible cycling of lithium metal/LiNi 0.5 Mn 0.3 Co 0.2 O 2 half-cells for 100 cycles. Unlike conventional polyolefin separators, which were shown to melt at 160 °C and shrink by up to 29.8% at elevated temperatures, the PIPS separators possess exceptional, safety-enhancing thermomechanical properties, undergoing no phase transitions or thermal shrinkage.

25 ENERGY STORAGE↗

Thermally driven surface phase separation in intermetallic alloys

Intermetallic compounds are widely recognized for their high-temperature phase stability and resistance to composition and structural changes. However, we reveal athermally activated bulk-to-surface mass exchange mechanism that drives surface phase separation, resulting in the formation of surface precipitates with distinct composition andstructure from the bulk matrix. Using the archetypal β-NiAl system, we show that asymmetries in vacancy formation energies between Ni and Al atoms induce preferential Ni segregation to the surface, forming Ni-rich γ'-Ni 3 Al precipitates. By integrating in-situ electron microscopy, synchrotron X-ray absorption spectroscopy and first-principles computational modeling, we establish a direct mechanistic connection between bulk thermal defect dynamics, surface compositional evolution, and phase segregation behavior. This bulk-surface coupling mechanism can be a driver of surface phase separation in multicomponent alloys under thermal stress. In conclusion, these results refine the thermodynamic boundaries of intermetallic stability and provide insights into managingthe performance and durability of intermetallic alloys for demanding high-temperature applications.

36 MATERIALS SCIENCE↗

Pore Aperture Control Toward Size‐Exclusion‐Based Hydrocarbon Separations

Abstract Metal–organic frameworks (MOFs) have been proposed as a promising material for non‐thermal chemical separations owing to their high structural diversity and tunability. Here, we report the synthesis of a zinc‐based MOF containing a three‐dimensional (3D) linker, bicyclo[2.2.2]octane‐1,4‐dicarboxylic acid, with high thermal stability towards the separation of hexane isomers. The incorporation of the 3D linker enhances the structural stability and provides well‐defined pore apertures/channels with sub‐Ångstrom precision. This precision allowed for the separation of similarly sized hexane isomers based on subtle differences in their kinetic diameters. Multi‐component liquid phase batch experiments confirmed the separation of hexanes mixture into linear, monobranched, and dibranched isomers. This work represents a significant milestone in the construction of stable Zn‐based MOFs and the incorporation of 3D linkers as a potential solution to challenging separations.

Lal, Bhajan↗

Pore Aperture Control Toward Size‐Exclusion‐Based Hydrocarbon Separations

Metal–organic frameworks (MOFs) have been proposed as a promising material for non-thermal chemical separations owing to their high structural diversity and tunability. Here, we report the synthesis of a zinc-based MOF containing a three-dimensional (3D) linker, bicyclo[2.2.2]octane-1,4-dicarboxylic acid, with high thermal stability towards the separation of hexane isomers. The incorporation of the 3D linker enhances the structural stability and provides well-defined pore apertures/channels with sub-Ångstrom precision. This precision allowed for the separation of similarly sized hexane isomers based on subtle differences in their kinetic diameters. Multi-component liquid phase batch experiments confirmed the separation of hexanes mixture into linear, monobranched, and dibranched isomers. This work represents a significant milestone in the construction of stable Zn-based MOFs and the incorporation of 3D linkers as a potential solution to challenging separations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High Temperature Degradation Mechanisms in Polymer Matrix Composites

Polymer matrix composites are increasingly used in demanding structural applications in which they may be exposed to harsh environments. The durability of such materials is a major concern, potentially limiting both the integrity of the structures and their useful lifetimes. The goal of the current investigation is to develop a mechanism-based model of the chemical degradation which occurs, such that given the external chemical environment and temperatures throughout the laminate, laminate geometry, and ply and/or constituent material properties, we can calculate the concentration of diffusing substances and extent of chemical degradation as functions of time and position throughout the laminate. This objective is met through the development and use of analytical models, coupled to an analysis-driven experimental program which offers both quantitative and qualitative information on the degradation mechanism. Preliminary analyses using a coupled diffusion/reaction model are used to gain insight into the physics of the degradation mechanisms and to identify crucial material parameters. An experimental program is defined based on the results of the preliminary analysis which allows the determination of the necessary material coefficients. Thermogravimetric analyses are carried out in nitrogen, air, and oxygen to provide quantitative information on thermal and oxidative reactions. Powdered samples are used to eliminate diffusion effects. Tests in both inert and oxidative environments allow the separation of thermal and oxidative contributions to specimen mass loss. The concentration dependency of the oxidative reactions is determined from the tests in pure oxygen. Short term isothermal tests at different temperatures are carried out on neat resin and unidirectional macroscopic specimens to identify diffusion effects. Mass loss, specimen shrinkage, the formation of degraded surface layers and surface cracking are recorded as functions of exposure time. Geometry effects in the neat resin, and anisotropic diffusion effects in the composites, are identified through the use of specimens with different aspect ratios. The data is used with the model to determine reaction coefficients and effective diffusion coefficients. The empirical and analytical correlations confirm the preliminary model results which suggest that mass loss at lower temperatures is dominated by oxidative reactions and that these reaction are limited by diffusion of oxygen from the surface. The mechanism-based model is able to successfully capture the basic physics of the degradation phenomena under a wide range of test conditions. The analysis-based test design is successful in separating out oxidative, thermal, and diffusion effects to allow the determination of material coefficients. This success confirms the basic picture of the process; however, a more complete understanding of some aspects of the physics are required before truly predictive capability can be achieved.

Cunningham, Ronan A.↗

High Temperature Degradation Mechanisms in Polymer Matrix Composites

Polymer matrix composites are increasingly used in demanding structural applications in which they may be exposed to harsh environments. The durability of such materials is a major concern, potentially limiting both the integrity of the structures and their useful lifetimes. The goal of the current investigation is to develop a mechanism-based model of the chemical degradation which occurs, such that given the external chemical environment and temperatures throughout the laminate, laminate geometry, and ply and/or constituent material properties, we can calculate the concentration of diffusing substances and extent of chemical degradation as functions of time and position throughout the laminate. This objective is met through the development and use of analytical models, coupled to an analysis-driven experimental program which offers both quantitative and qualitative information on the degradation mechanism. Preliminary analyses using coupled diffusion/reaction model are used to gain insight into the physics of the degradation mechanisms and to identify crucial material parameters. An experimental program is defined based on the results of the preliminary analysis which allows the determination of the necessary material coefficients. Thermogravimetric analyses are carried out in nitrogen, air, and oxygen to provide quantitative information on thermal and oxidative reactions. Powdered samples are used to eliminate diffusion effects. Tests in both inert and oxidative environments allow the separation of thermal and oxidative contributions to specimen mass loss. The concentration dependency of the oxidative reactions is determined from the tests in pure oxygen. Short term isothermal tests at different temperatures are carried out on neat resin and unidirectional macroscopic specimens to identify diffusion effects. Mass loss, specimen shrinkage, the formation of degraded surface layers and surface cracking are recorded as functions of exposure time. Geometry effects in the neat resin, and anisotropic diffusion effects in the composites, are identified through the use of specimens with different aspect ratios. The data is used with the model to determine reaction coefficients and effective diffusion coefficients. The empirical and analytical correlations confirm the preliminary model results which suggest that mass loss at lower temperatures is dominated by oxidative reactions and that these reaction are limited by diffusion of oxygen from the surface. The mechanism-based model is able to successfully capture the basic physics of the degradation phenomena under a wide range of test conditions. The analysis-based test design is successful in separating out oxidative, thermal, and diffusion effects to allow the determination of material coefficients. This success confirms the basic picture of the process; however, a more complete understanding of some aspects of the physics are required before truly predictive capability can be achieved.

Cunningham, Ronan A.↗

Thermal Analysis of Cryogenic Hydrogen Liquid Separator

During launch for the new Space Launch System (SLS) liquid hydrogen is bleed through the engines during replenish, pre-press, and extended pre-press to condition the engines prior to launch. The predicted bleed flow rates are larger than for the shuttle program. A consequence of the increased flow rates is having liquif hydrogen in the vent system, which the facilities was never designed to handle. To remedy the problem a liquid separator is being designed in the system to accumulated the liquid propellant and protect the facility flare stack (which can only handle gas). The attached document is a presentation of the current thermalfluid analysis performed for the separator and will be presented at the Thermal and Fluid Analysis Workshop (NASA workshop) next week in Cleveland, Ohio.

liquid separator↗

Resistance heater rod and method of making such

A resistive heater capable of delivering heat loads on the same order as those produced by in-pile nuclear fuel experiments. The heater rod provides the energy for high-temperature steady-state testing, as well as the power needed to simulate the transient pulse in the Transient Reactor Test Loop (TRTL) system. The resistive heater includes a removable housing, two or more thermal conductors in the housing; and one or more stabilizers coupled to the two or more thermal conductors to keep the two or more thermal conductors separated to avoid shorting, wherein the two or more thermal conductors are coupled to the housing via an inert gas (e.g., Helium). The two or more thermal conductors comprise a material with substantially zero infrared spectrum (e.g., sapphire, silica, or glass).

LaBrier, Daniel↗

Tuning gas separation performance of polyimide membranes with macrocyclic crown ether units

Membrane-based gas separation is an energy-efficient alternative to conventional thermally-driven separation processes. However, polymer membranes face the permeability-selectivity trade-off challenge, which stems from the broad size distribution of free volume voids. Here, this study reports a molecular design strategy to address this challenge through incorporating macrocyclic crown ether (CE) moieties into the backbone of Matrimid® polyimide, a commercial gas separation membrane. A series of CE-containing Matrimid®-like copolyimides were synthesized with systematically varied CE molar contents ranging from 3 to 20%. These copolyimides formed ductile, defect-free thin films suitable for membrane fabrication. Gas permeation tests revealed a non-monotonic relationship between permeability/selectivity and CE content. Notably, the copolyimide with only 5% CE demonstrated a 61% increase in CO 2 /CH 4 selectivity and a 13% increase in CO 2 permeability relative to pristine Matrimid®. Higher CE contents did not yield further performance improvements, which is likely due to the competing effects of chain packing disruption and π–π interactions among CE moieties at high content. This hypothesis was supported by wide-angle X-ray scattering (WAXS) analysis, density measurements, and fractional free volume calculations. These findings highlight the potential of macrocyclic crown ether incorporation strategies in fine tuning the microstructure of commercial polyimide gas separation membranes to surpass the traditional permeability-selectivity trade-off.

CO2 separation↗

Progress Report on Performance of A709 and G91 Steels in Sodium

Specimens in six different processing and heat treatment conditions of A709 H58776 were exposed to sodium at 550, 600, and 650°C, respectively for various exposure times. G91 base metal was tested in sodium at 550, 600, and 650°C, and G91 weldment at 550 and 600°C, respectively. Parallel thermal aging experiments were conducted on G91 and A709 to obtain thermal aging data for comparison with sodium exposure results to separate the thermal and sodium effects. The corrosion data obtained on A709 steel continue to show low corrosion rates, which indicate good compatibility of A709 with sodium when oxygen content is controlled. G91 has also shown acceptable corrosion rates over the temperature range of 550-650°C in sodium. Thermal aging or sodium exposures reduced the tensile strength, uniform elongation, and total elongation for A709 ESR, AOD specimens. These specimens consistently showed higher yield stress and tensile strength and lower uniform and total elongations after sodium exposure than after thermal aging under comparable testing conditions. It implies that there was an additional effect of sodium exposure that gave rise to an increase in tensile strength of A709. Dynamic strain aginginduced flow serrations were completely removed by either thermal aging or sodium exposure at 650°C, which imply that carbon or nitrogen in solution was removed from the solution and formed precipitates during aging or sodium exposures. The tensile data ruled out the possibility of decarburization under the sodium exposure conditions. The HOMO specimens behaved somewhat differently from the ESR and AOD specimens in sodium. While thermal aging and sodium exposures at 550 and 600°C decreased the yield stress and the ultimate tensile strength of G91, there was virtually no additional effect resulting from sodium exposures at these two temperatures. In contrast, sodium exposures at 650°C had a drastic effect on the yield stress and the ultimate tensile strength of G91. It is suggested that G91 experienced decarburization in the 650°C sodium environments. Carbon concentrations in sodium in the SMT-1 and SMT-2 loops were determined by a foil equilibration method. The estimated carbon concentration was in the range of 0.8-1.2 ppm in the SMT-1 loop and 0.3-0.7 ppm in the SMT-2 loop. The carbon activity in sodium in the SMT-2 loop was estimated to be 0.03-0.08 at 600°C, and 0.08-0.2 at 550°C. The carbon activity in sodium at 650°C in the SMT-1 loop was 0.04-0.07. Equilibrium simulation of the carburization – decarburization processes was conducted for A709 and G91 steels exposed in sodium environments at temperatures of 550-700°C. The carbon activity-concentration relationship for G91 was re-evaluated by considering four phases in G91, i.e. bcc ferrite, M 23 C 6 , NbC and VC carbides. It was found that the carburization-decarburization process in G91 steel was dictated by M 23 C 6 carbides at high carbon activities, while NbC carbides dominated the process at low carbon activities. Formation of NbC increases the decarburization resistance of G91 steel. It remains to be understood whether the decarburization resistance provided by MC carbides in G91 can be maintained during long-term operations of SFRs. The carbon concentration-activity relationship for A709 was calculated based on the equilibrium of fcc-austenite and M 23 C 6 carbide phase. The calculations showed that A709 decarburizes at 650°C in the SMT-1 loop environments, which is different from the experimental findings. The carbon concentration-activity relationship in A709 was further evaluated by considering four phases, including fcc-austenite, M 23 C 6 , NbC, and TiC carbide phases. TiC is the most stable carbides among the three carbide phases. The carburization-decarburization process in A709 is dictated by M 23 C 6 carbides at high carbon activities and by TiC at low carbon activities. Formation of TiC increases the decarburization resistance of A709 steel. Because of the complexity of the precipitation process in A709 during sodium exposures, detailed characterization of precipitates in sodium-exposed specimens and improved thermodynamic models are needed to understand the carburization-decarburization behavior of A709. Kinetic analysis of carbon transfer will be investigated for G91 and A709 in future work.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Sodium Exposure Tests of A709 Steel (FY2020 Progress Report)

Sodium exposure tests were conducted on the first commercial heat, H58776 of A709 steel. Six different processing and heat treatment conditions were investigated, including three processing conditions, namely, Argon-Oxygen-Decarburization (AOD), Electro-slag Remelting (ESR), and Electro-slag Remelting with subsequent homogenization (HOMO), and two heat treatment conditions, i.e. solution annealing at 1100°C (SA1100°C) or 1150°C (SA1150°C). Specimens of AOD-SA1100°C, AOD-SA1150°C, ESR-SA1100°C, ESR-SA1150°C, HOMO-SA1100°C, and HOMO-SA1150°C were tested in sodium at 650°C and for times up to 10,152 h. Specimens in the AOD-SA1100°C and AOD-SA1150°C conditions were also tested in sodium at 550 and 600°C. Parallel thermal aging experiments were carried out for comparison with sodium exposure tests to separate the thermal and sodium effects. It was found that A709 H58776 generally showed a weight loss after sodium exposures at 650°C except a few data points of the ESR-SA1100°C specimens. The corrosion rate showed large variations in the initial stage and decreased with increasing exposure time. Long-term exposure tests are needed to determine its steady-state corrosion rate. The AOD-SA1100°C and HOMO-SA1100°C specimens showed similar tensile responses after thermal or sodium exposures at 650°C. The yield stress increased, the ultimate tensile strength decreased, and the uniform and total elongations were reduced after thermal or sodium exposures. A longer exposure time had a minimal effect on the tensile strength but further reduced the tensile ductility. The sodium-exposed specimens had higher tensile strength than the thermally-aged specimens. In contrast, the ESR-SA1100°C specimens showed an increase in the yield stress and the ultimate tensile strength after thermal or sodium exposures at 650°C and ~10,000 h. The AOD-SA1150°C and ESR-SA1150°C specimens showed similar tensile behavior after thermal or sodium exposures at 650°C.Thermal or sodium exposures at 650°C increased the yield stress, decreased the ultimate tensile strength, and reduced uniform and total elongations. There were minimal differences in tensile properties between the sodium-exposed and thermally-aged specimens after an ~3000 h exposure. After an exposure for ~10,000 h the sodium-exposed specimens showed higher yield stress and ultimate tensile strength and lower uniform and total elongations than the thermally-aged specimens. For the HOMO-SA1150°C specimens, thermal or sodium exposures at 650°C significantly increased the yield stress but had a minimal effect on the ultimate tensile strength. Both uniform and total elongations were significantly reduced at an exposure time of ~3,000 h, and they were further reduced after an exposure of ~10,000 h. The sodium-exposed specimens had lower tensile ductility than the thermally-aged specimens. Before exposure, the stress-strain curves of the specimens in all six processing-heat treatment conditions showed serrations indicating the dynamic aging effect at 650°C. Thermal aging or sodium exposures at 650°C after ~10,000 h completely removed the serrations of the flow curves in A709 H58776, indicating strong precipitation during thermal or sodium exposures. Longer-term sodium exposure tests are needed to determine the steady-state corrosion rates in sodium for A709 H58776 and fully understand the influence of sodium exposures on its mechanical performance.

36 MATERIALS SCIENCE↗

Tree Canopy Characterization for EO-1 Reflective and Thermal Infrared Validation Studies: Rochester, New York

The tree canopy characterization presented herein provided ground and tree canopy data for different types of tree canopies in support of EO-1 reflective and thermal infrared validation studies. These characterization efforts during August and September of 2001 included stem and trunk location surveys, tree structure geometry measurements, meteorology, and leaf area index (LAI) measurements. Measurements were also collected on thermal and reflective spectral properties of leaves, tree bark, leaf litter, soil, and grass. The data presented in this report were used to generate synthetic reflective and thermal infrared scenes and images that were used for the EO-1 Validation Program. The data also were used to evaluate whether the EO-1 ALI reflective channels can be combined with the Landsat-7 ETM+ thermal infrared channel to estimate canopy temperature, and also test the effects of separating the thermal and reflective measurements in time resulting from satellite formation flying.

Ballard, Jerrell R., Jr.↗