Search NASA⌕ Search

SEARCH · Search NASA

Results for “vapor pressure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Effusion Cell Measurements of the Vapor Pressure of Cobalt at Temperatures up to 2000K; Comparisons with Iron and Nickel

It has become increasingly clear over the past decade that high temperature processes played important roles in the Primitive Solar Nebula. Unfortunately, basic data, such as the vapor pressures of Fe, Ni, Co or SiO have not been measured over the appropriate temperature range (near T approx. 2000K), but must be extrapolated from lower temperature measurements often made more than 50 years ago. The extrapolation of the available data to higher temperatures can be quite complex (e.g., see [1] for SiO vapor pressures) and can depend on other factors such as the oxygen fugacity or the presence of hydrogen gas not accounted for in the original measurements. Moreover, modern technology has made possible more accurate measurements of such quantities over a wider temperature range. We have acquired a commercial Thermo-Cahn Thermogravimetric system capable of vacuum operation to 1700C and measurement of a 10g change in sample mass using up to a 100g sample, with microgram accuracy. With this new system we have initiated a series of basic vapor pressure measurements on simple metals such as Fe[2] and Ni[3] with the intention to extend such measurements to more complex systems once we gain sufficient experience.

Nuth, J. A.↗

The effect of relative humidity and temperature on the response of stomatal conductance to vapor pressure deficit in tropical trees

Understanding how leaf gas exchange responds to changes in vapor pressure deficit (VPD) is key to predicting tropical forest resilience to climate change. Stomata regulate leaf water and CO2 diffusion, and respond to changes in temperature and relative humidity (RH), two drivers of VPD. At high temperatures, the cuticular pathway may also become significant and participate in the overall leaf conductance. Here, we measured gas exchange under light and dark conditions to investigate the stomatal and cuticular responses to temperature and RH on detached branches in five tropical tree species. Leaf conductance in the dark, when stomata are essentially closed, was not markedly impacted by temperature and RH, suggesting a minimal response of the cuticular pathway to these conditions. We compared six steady-state conductance models incorporating different effects of photosynthesis and evaporative demand on stomatal control. All models performed well (residual standard deviation, σ, < 0.025 mol m-2 s-1), but the best-fitting model (σ = 0.017 mol m-2 s-1) used a nonlinear relationship between photosynthesis and stomatal conductance and incorporated RH rather than vapor pressure difference. All models overestimated the steady-state conductance at high RH. Furthermore, leaf conductance immediately increased after a decrease in RH (wrong-way response), but not after an increase in leaf temperature. This suggests that the mechanisms underlying stomatal response to VPD need further investigation. The non-linear coupling between photosynthetic rate and stomatal conductance indicates a sharper physiological response than previously acknowledged.

Lamour, Julien↗

Measurement of partial vapor pressures of salt mixtures via combined horizontal transpiration and thermogravimetric analysis

A method combining thermogravimetric analysis (TGA) and horizontal transpiration with elemental analysis via inductively coupled plasma mass spectrometry or ion chromatography enabled calculation of partial pressures of individual salts in molten mixtures. TGA quantified total mass loss, while transpiration identified vapor-phase composition. Furthermore, two chloride (NaCl-MgCl 2 , NaCl-MgCl 2 + UCl 3 ) salts and one mixed halide (LiCl-LiF + Li 2 O) salt were analyzed at 750 °C and 550 °C, respectively. NaCl and MgCl 2 vapor pressures were 2.19–2.61 × 10 -4 atm and 2.47–2.48 × 10 -5 atm (dependent upon the identity of the invesitgated mixture); UCl 3 was 1.42 × 10 -7 atm. LiCl and LiF vapor pressures at 550 °C were 1.53 × 10 -6 and 6.32 × 10 -6 atm, respectively. Additionally, the TGA method was validated against values from the literature for unary LiCl and LiF.

36 MATERIALS SCIENCE↗

Low vapor pressure braze alloys for thermionic energy converters

Preliminary results in the use of some low-vapor-pressure braze alloys are reported; these are binary alloys of refractory metals (Th, Zr, Hf, Ru, Nb, Ir, Mo, Ta, Os, Re, W) with vapor pressures below 0.1 nanotorr at 1500 K or 10 microtorr at 2000 K. The melting point minima or eutectics of the alloys range from 1510 K to above 3000 K. Melting points and surface wetting on a Ta base are given. Results are presented on brazing of Ir, LaB6, Nb, Re, W, and ZrO2 (with 22 wt % Zr) into a Ta base or a Nb-1% Zr base. The results are applicable in electrode screening programs for thermionic cesium diodes.

Bair, V. L.↗

Accurate determination of the vapor pressure of potassium using optical absorption

The vapor pressure of potassium has been measured in absorption using a CW tunable laser and calibrated against the accurate radiative lifetime of the 4s-4p doublet of potassium. An accurate value of 20,850 + or - 30 cal/mol for the heat of vaporization (from the liquid phase) at the melting point was determined.

Shirinzadeh, B.↗

Low vapor pressure braze alloys for thermionic energy converters

The evaluation of cesium diode electrode materials called for braze fillers with very low vapor pressures and a wide range of melting points. Binary alloys of low vapor pressure refractory metals were chosen to fill this need. These alloys of Th, Zr, Hf, Ru, Nb, Ir, Mo, Ta, Os, Re, and W have reported melting point minima or eutectics from 1,510 K to above 3,000 K. Preliminary data are compiled on the use of several of these braze alloys. Melting points and surface wetting on a Ta base are given. Results of brazing Ir, LaB6, Nb, Re, W, and Zr-22 wt % ZrO2 materials into Ta and Nb-1% Zr bases are presented. Current braze usage is summarized.

Bair, V. L.↗

Pluto's atmosphere - Models based on refraction, inversion, and vapor-pressure equilibrium

Viking spacecraft radio-occultation measurements indicate that, irrespective of substantial differences, the polar ice cap regions on Mars have inversions similar to those of Pluto, and may also share vapor pressure equilibrium characteristics at the surface. This temperature-inversion phenomenon occurs in a near-surface boundary layer; surface pressure-temperature may correspond to the vapor-pressure equilibrium with CH4 ice, or the temperature may be slightly higher to match the value derived from IRAS data.

Eshleman, Von R.↗

Stomatal closure as a driver of minimum leaf conductance declines at high temperature and vapor pressure deficit in Quercus

Abstract Rising global temperatures and vapor pressure deficits (VPDs) are increasing plant water demand and becoming major drivers of large-scale plant mortality. Controlling transient leaf water loss after stomatal closure (minimum stomatal conductance [gmin]) is recognized as a key trait determining how long plants survive during soil drought. Yet, substantial uncertainty remains regarding how gmin responds to elevated temperatures and VPD and the underlying mechanisms. We measured gmin in 24 Quercus species from temperate and Mediterranean climates to determine whether gmin was sensitive to a coupled temperature and VPD increase. We also explored mechanistic links to phenology, climate, evolutionary history, and leaf anatomy. We found that gmin in all species exhibited a nonlinear negative temperature and VPD dependence. At 25 °C (VPD = 2.2 kPa), gmin varied from 1.19 to 8.09 mmol m−2 s−1 across species but converged to 0.57 ± 0.06 mmol m−2 s−1 at 45 °C (VPD = 6.6 kPa). In a subset of species, the effect of temperature and VPD on gmin was reversible and linked to the degree of stomatal closure, which was greater at 45 °C than at 25 °C. Our results show that gmin is dependent on temperature and VPD, is highly conserved in Quercus species, and is linked to leaf anatomy and stomatal behavior.

Zailaa, Joseph (ORCID:000000019103190X)↗

Initial Measurement of the Vapor Pressures of Simple Refractory Materials: Cu and Fe

It has become increasingly clear over the past decade that high temperature processes played important roles in the Primitive Solar Nebula. Unfortunately, basic data, such as the vapor pressures of iron or SiO have not been measured over the appropriate temperature range (near T approximately equal to 2000K), but must be extrapolated from lower temperature measurements often made more than 50 years ago. The extrapolation of the available data to higher temperatures can be quite complex and can depend on other factors such as the oxygen fugacity or the presence of hydrogen gas. Moreover, modern technology has made possible more accurate measurements of such quantities over a wider temperature range. We recently acquired a commercial Thermo-Cahn Thermogravimetric system capable of vacuum operation to 1700 C and measurement of mass change with microgram accuracy in a 100g sample or smaller. In this paper, we will report our progress in learning to make vapor pressure measurements using this system.

Nuth, Joseph A., III↗