A Micromechanics Finite Element Model for Studying the Mechanical Behavior of Spray-On Foam Insulation (SOFI)

A micromechanics model has been constructed to study the mechanical behavior of spray-on foam insulation (SOFI) for the external tank. The model was constructed using finite elements representing the fundamental repeating unit of the SOFI microstructure. The details of the micromechanics model were based on cell observations and measured average cell dimensions discerned from photomicrographs. The unit cell model is an elongated Kelvin model (fourteen-sided polyhedron with 8 hexagonal and six quadrilateral faces), which will pack to a 100% density. The cell faces and cell edges are modeled using three-dimensional 20-node brick elements. Only one-eighth of the cell is modeled due to symmetry. By exercising the model and correlating the results with the macro-mechanical foam behavior obtained through material characterization testing, the intrinsic stiffness and Poisson s Ratio of the polymeric cell walls and edges are determined as a function of temperature. The model is then exercised to study the unique and complex temperature-dependent mechanical behavior as well as the fracture initiation and propagation at the microscopic unit cell level.

Ghosn, Louis J.↗

Geologic Mapping of the Guinevere Planitia Quadrangle of Venus

The Guinevere Planitia quadrangle of Venus (0-25degN, 300-330deg) covers a lowland region east of Beta Regio and west of Eistla Regio, including parts of Guinevere and Undine Planitiae. The V-30 quadrangle is dominated by low-lying plains interpreted to be of volcanic origin and exhibiting numerous wrinkle ridges. Using Pioneer Venus, Goldstone, and Arecibo data, previous investigators have described radar bright, dark, and mottled plains units in the Guinevere Planitia region, as well as arcuate fracture zones and lineament belt segments that define the Beta-Eistla deformation zone [1-5]. Magellan SAR images show that volcanic landforms compose the majority of the surface units in V-30 [6-7]. The quadrangle contains parts of four major volcanoes: Atanua (9degN, 307deg), Rhpisunt (3degN, 302deg), Tuli (13degN, 314deg), and Var (3degN, 316deg) Montes, and three coronae: Hulda (12degN, 308deg), Madderakka (9degN, 316deg), and Poloznitsa (1degN, 303deg). Seymour crater, located at 18degN, 327deg, is associated with extensive crater outflow deposits.

Crown, David A.↗

AERoBOND Project Summary

Under NASA’s Convergent Aeronautics Solutions (CAS) project, the Adhesive-Free Bonding of Complex Composites (AERoBOND) project investigated off-stoichiometric epoxy polymers for fast, reliable assembly of epoxy matrix composite structures. The project goal was to demonstrate feasibility of the AERoBOND joining method by demonstrating mechanical properties greater than 80% of conventional co-cured materials while reducing structure weight by 1%. The project consisted of three convergent research areas: material and process development, systems analysis, and material and process modeling. Material and process development was the largest component of AERoBOND with approximately 6 FTE and 1WYE of support to formulate and characterize new resins, prepare carbon fiber prepregs, fabricate laminates, measure mechanical properties, analyze failure results, and select material and process improvements. The systems analysis activity estimated the potential reduction in part count and aircraft weight by comparing models of composite wing boxes with no fasteners (co-cured structure), fasteners in major joints (co-cured stringers), and fasteners in all joints. The materials and process modeling activity included a molecular model of the AERoBOND materials system to predict mechanical properties of resins with offset stoichiometry and a process model to predict the effect of resin formulation and processing conditions on the extent of mixing and degree of cure in a finished joint. As the number of airline passenger trips doubles in the next 20 years (IATA/Tourism Economics Air Passenger Forecasts, April 2019), the increased demand for new commercial aircraft is now the single greatest technical challenge to the airframe manufacturing industry. To meet efficiency requirements, new aircraft must be fabricated primarily from high performance structural composites, but manufacturing processes are inherently slow with the largest bottleneck attributed to assembly and installation of fasteners (NASA/TM–2019-220428). Manufactures of commercial transport aircraft are compelled to install more than 100,000 redundant fasteners into bonded joints to prevent failures due to unpredictable weak bonds. In structural adhesive bonds, the interface between adherend and adhesive is nearly two-dimensional making it susceptible to minute quantities of contamination, which can cause weak bonds. Currently, bond strength assessment is only possible through destructive testing (i.e., breaking the joint). For these reasons, regulatory organizations such as the Federal Aviation Administration (FAA) often require redundant load paths in secondary-bonded, primary-structures to alleviate concerns with bond performance. The AERoBOND process enables reflow of matrix resin during assembly to eliminate the material discontinuity at the interface, thereby eliminating the dependence of mechanical performance on interfacial adhesion. The AERoBOND joint is equivalent to the interlaminar region obtained during a co-cure process, so joint performance depends on the cohesive properties of the matrix resin. Conventional co-cured structures, although too costly and complex for large-scale manufacturing, are trusted by manufacturers and regulators, and are certified for flight with few or no redundant fasteners.Systems analysis performed on a composite wing model at the scale of a single-aisle commercial transport aircraft indicated that >20,000 redundant fasteners per wing could be eliminated by implementing the AERoBOND joining method. A total weight reduction of 15% was predicted in a wing box by eliminating fasteners and thinning components that must no longer support localized fastener loads and accommodate fastener dimensions. Interlaminar shear fracture toughness measured by the end-notched flexure test was greater than 1 kJ/m2 (nearly 140% of the co-cured benchmark property), which is greatly in excess of the project goals for mechanical properties. Testing was planned to measure interlaminar tensile fracture toughness as well as interlaminar tensile and shear strengths using the same AERoBOND configuration, but was delayed due to closure of LaRC facilities during the COVID-19 pandemic. The AERoBOND process model is partially validated and available for experimental use. It allows the user to input AERoBOND process parameters such as material composition, laminate configuration, and cure cycle to predict the final cure state of the AERoBOND joint. A preliminary, multi-scale material model was developed to predict AERoBOND joint mechanical properties (stiffness and strength) based on the cure state of the joint provided by the process model. The timing for transition of this technology within NASA is excellent as NASA initiates new enduring projects to address composites manufacturing rate challenges. AERoBOND technology is well suited to AAVP/AATT objectives for rapid manufacturing of a composite wing. A minimal effort (1 FTE/$15k procurement/0 WYE) is proposed in FY21 to continue a minor mechanical testing effort and maintain a SAA with ASX composites to develop commercial quality prepreg material. An RFI with the composites industry is suggested to quantify the technology gap between the current TRL and the TRL needed for transition to industry. A moderate effort [3-4 FTE/$150k/1 WYE (~$115k)] is proposed in FY22 for the “high rate composites manufacturing” project currently in planning. The partnership with ASX Composites will be expanded to produce material for sub-element/element-scale “panel-off” activities. Industry partnerships with airframe manufacturers is an expected component to explore damage tolerance and environmental stability. Further development of multi-scale modeling tools (process model, meso-scale model, and molecular model) is planned to enhance and deliver tools for rapid manufacturing infusion.

Frank Louis Palmieri↗

Fracture technology for brittle materials

Ceramics materials have the potential for use in high-temperature, fuel-efficient engines. However, because these materials are brittle, their fracture characteristics must be well documented prior to their application. Thus Lewis is working to understand the fracture and strength properties of brittle ceramic and ceramic matrix materials. An understanding of fracture properties aids both designers who are attempting to design high-temperature structures and materials scientists who seek to design more temperature-resistant materials. Both analytical and experimental approaches to fracture analysis are being taken. Methods for testing fracture toughness, crack growth resistance, and strength are being developed. The failure mechanisms at both room and elevated temperatures are also being investigated. Such investigations aid materials scientists in developing better high-temperature materials. Of concern is the anisotropy of ceramic materials and the experimental verification of ceramic design codes that will allow brittle material behavior to be accurately predicted at high temperature.

Salem, Jonathan A.↗

Measured Fluid Flow in an Active H2O-CO2 Geothermal Well as an Analog to Fluid Flow in Fractures on Mars: Preliminary Report

Water in the Earth's crust generally contains dissolved gases such as CO2. Models for both 'Blue Mars' (H2O-driven processes) and 'White Mars' (CO2-driven processes) predict liquid H2O with dissolved CO2 at depth. The fate of dissolved CO2 as this mixture rises toward the surface has not been quantitatively explored. Our approach is a variation on NASA's 'Follow the Water' as we 'Follow the Fluid' from depth to the surface in hydrothermal areas on Earth and extrapolate our results to Mars. This is a preliminary report on a field study of fluid flow in a producing geothermal well. For proprietary reasons, the name and location of this well cannot be revealed, so we have named it 'Earth1' for this study.

Kieffer, Susan W.↗

Assessment of metabolic bone diseases by quantitative computed tomography

Advances in the radiologic sciences have permitted the development of numerous noninvasive techniques for measuring the mineral content of bone, with varying degrees of precision, accuracy, and sensitivity. The techniques of standard radiography, radiogrammetry, photodensitometry, Compton scattering, neutron activation analysis, single and dual photon absorptiometry, and quantitative computed tomography (QCT) are described and reviewed in depth. Results from previous cross-sectional and longitudinal QCT investigations are given. They then describe a current investigation in which they studied 269 subjects, including 173 normal women, 34 patients with hyperparathyroidism, 24 patients with steroid-induced osteoporosis, and 38 men with idiopathic osteoporosis. Spinal quantitative computed tomography, radiogrammetry, and single photon absorptiometry were performed, and a spinal fracture index was calculated on all patients. The authors found a disproportionate loss of spinal trabecular mineral compared to appendicular mineral in the men with idiopathic osteoporosis and the patients with steroid-induced osteoporosis. They observed roughly equivalent mineral loss in both the appendicular and axial regions in the hyperparathyroid patients. The appendicular cortical measurements correlated moderately well with each other but less well with spinal trabecular QCT. The spinal fracture index correlated well with QCT and less well with the appendicular measurements. Knowledge of appendicular cortical mineral status is important in its own right but is not a valid predictor of axial trabecular mineral status, which may be disproportionately decreased in certain diseases. Quantitative CT provides a reliable means of assessing the latter region of the skeleton, correlates well with the spinal fracture index (a semiquantitative measurement of end-organ failure), and offers the clinician a sensitive means of following the effects of therapy.

Minerals/analysis↗

Global Failure Modes in Composite Structures

Composite materials provide well-known advantages for space and aeronautical applications in terms of strength and rigidity to weight ratios and other mechanical properties. As a consequence, their use has experienced a constant increase in the past decades and it is anticipated that this trend will be maintained in the near future. At the same time, being these materials relatively new compared to metals, and having failure characteristics completely different from them, their damage growth and their failure mechanisms are not as well understood in a predictive sense. For example, while in metals fracture produces "clean" cracks with their well defined analytically stress fields at the crack tip, composite fracture is a more complex phenomenon. Instead of a crack, we confront a "damage zone" that may include fiber breakage, fiber microbuckling, fiber pullout, matrix cracking, delamination, debonding or any combination of all these different mechanisms. These phenomena are prevalent in any failure process through an aircraft structure, whether one addresses a global failure such as the ripping of a fuselage or wing section, or whether one is concerned with the failure initiation near a thickness change at stringers or other reinforcement. Thus the topic that has been under consideration has wide application in any real structure and is considered an essential contribution to the predictive failure analysis capability for aircraft containing composite components. The heterogeneity and the anisotropy of composites are not only advantageous but essential characteristics, yet these same features provide complex stress fields, especially in the presence of geometrical discontinuities such as notches, holes or cutouts or structural elements such as stiffeners, stringers, etc. To properly address the interaction between a damage/crack front and a hole with a stringer it is imperative that the stress and deformation fields of the former be (sufficiently well) characterized. The question of "scaling" is an essential concern in any structural materials investigation. For example, experiments in the past have shown that the "strength" of a composite depends on hole size. As a consequence the validity of traditional fracture mechanics concepts applied to composite materials failure must be questioned. The size of the fibers, the dimensions of the laminae, etc. together with the fact that, because of the layered anisotropy, the stress field is no longer two-dimensional, prevent the otherwise obviously confident use of "similarity concepts". Therefore, the question needs to be raised of whether in composites "size matters or not", i.e., whether the results obtained in a laboratory using small coupons are truly representative of the situation involving a full scale component.

Knauss, W. G.↗

Mechanical Properties of Air Plasma Sprayed Environmental Barrier Coating (EBC) Materials

Development work in Environmental Barrier Coatings (EBCs) for Ceramic Matrix Composites (CMCs) has focused considerably on the identification of materials systems and coating architectures to meet application needs. The evolution of these systems has occurred so quickly that modeling efforts and requisite data for modeling lag considerably behind development. Materials property data exists for many systems in the bulk form, but the effects of deposition on the critical properties of strength and fracture behavior are not well studied. We have plasma sprayed bulk samples of baseline EBC materials (silicon, ytterbium disilicate) and tested the mechanical properties of these materials to elicit differences in strength and toughness. We have also endeavored to assess the mixed-mode fracture resistance, Gc, of silicon in a baseline EBC applied to SiCSiC CMC via four point bend test. These results are compared to previously determined properties of the comparable bulk material.

Ceramic Matrix Composites (CMC's)↗

Fracture analysis of surface and through cracks in cylindrical pressure vessels

A previously developed fracture criterion was applied to fracture data for surface- and through-cracked cylindrical pressure vessels to see how well the criterion can correlate fracture data. Fracture data from the literature on surface cracks in aluminum alloy, steel, and epoxy vessels, and on through cracks in aluminum alloy, titanium alloy steel, and brass vessels were analyzed by using the fracture criterion. The criterion correlated the failure stresses to within + or - 10 percent for either surface or through cracks over a wide range of crack size and vessel diameter. The fracture criterion was also found to correlate failure stresses to within + or - 10 percent for flat plates (center-crack or double-edge-crack tension specimens) and cylindrical pressure vessels containing through cracks.

Newman, J. C., Jr.↗

A study of damage zones or characteristic lengths as related to the fracture behavior of graphite/epoxy laminates

Uniaxial tensile tests conducted on a variety of graphite/epoxy laminates, containing narrow rectangular slits, square or circular holes with various aspect ratios are discussed. The techniques used to study stable crack or damage zone growth--namely, birefringence coatings, COD gages, and microscopic observations are discussed. Initial and final fracture modes are discussed as well as the effect of notch size and shape, and laminate type on the fracture process. Characteristic lengths are calculated and compared to each other using the point, average and inherent flaw theories. Fracture toughnesses are calculated by the same theories and compared to a boundary integral equation technique. Finite width K-calibration factors are also discussed.

Yeow, Y. T.↗

The fracture behavior of graphite/epoxy laminates

The results of uniaxial tensile tests conducted on a variety of graphite/epoxy laminates containing narrow rectangular slits and square or circular holes with various aspect ratios are discussed. The techniques used to study stable-crack or damage-zone growth - namely, birefringence coatings, COD gages, and microscopic observations are discussed. Initial and final-fracture modes are discussed as well as the effect of notch size and shape and laminate type on the fracture process. Characteristic lengths are calculated using the point, average and inherent flaw theories and comparisons with observations are discussed. Further, the effect of flaw geometry on stress states and deformations is assessed.

Yeow, Y. T.↗

Multilayer Pressure Vessel Materials Testing and Analysis

To provide NASA a comprehensive suite of materials strength, fracture toughness and crack growth rate test results for use in remaining life calculations for aging multilayer pressure vessels, Southwest Research Institute (R) (SwRI) was contracted in two phases to obtain relevant material property data from a representative vessel. This report describes Phase 1 of this effort which includes a preliminary material property assessment as well as a fractographic, fracture mechanics and fatigue crack growth analyses of an induced flaw in the outer shell of a representative multilayer vessel that was subjected to cyclic pressure test. SwRI performed this Phase 1 effort under contract to the Digital Wave Corporation in support of their contract to Jacobs ATOM for the NASA Ames Research Center.

Cardinal, Joseph W.↗

Fracture analysis of surface and through-cracks in cylindrical pressure vessels

A previously developed fracture criterion was applied to surface- and through-cracked cylindrical pressure vessels to see how well the criterion can correlate fracture data. Fracture data from the literature on surface cracks in aluminum alloy, steel, and epoxy vessels and on through cracks in aluminum alloy, titanium alloy, steel, and brass vessels were analyzed using the fracture criterion. The criterion correlated the failure stresses to within + or - 10 percent for either surface or through cracks over a wide range of crack size and vessel diameter. The fracture criterion was also found to correlate failure stresses from flat plates (center-crack or double-edge-crack tension specimens) and cylindrical pressure vessels containing through - cracks within + or - 10 percent.

Newman, J. C., Jr.↗

A New Energy Source for Organic Synthesis in Europa's Surface Ice

Colored regions on Jupiter's satellite Europa and other icy bodies in the outer Solar System may be contaminated by organic macromolecular solid material that is produced when surface ices are exposed to electrical energy. Hypervelocity meteorite impacts and fracture release tidal and tectonic stresses in icy crusts in the form of electrical discharges, which provide the energy for in situ synthesis of the organic solids. We report measurements of electrical discharge, light emission, and magnetic phenomena in hypervelocity impacts into ice with projectiles with V approx. 5 km/s. Part of the projectile's kinetic energy is converted into electrical potential, while the mechanical disruption of the impact also releases stress energy as light, heat, electrical, and magnetic fields as secondary emissions. These newly recognized energy sources suggest that the dark material in the area of impact craters are tholins generated from the energy of the impacts and that well up from the fracture zone. Large pools of liquid water would persist under the meteorite crater for thousands of years, with the potential for prebiotic chemistry to take place at an accelerated rate due to energy pumped in from the secondary emissions.

Borucki, Jerome G.↗

On the strength of oceanic fracture zones and their influence on the intraplate stress field

We use the locations and source mechanisms of oceanic intraplate earthquakes to test the hypothesis that the strength of oceanic fracture zones is less than that of normal oceanic lithosphere. The 77 earthquakes selected for the study have well-determined focal mechanisms and epicenters in regions where fracture zones are well mapped. We have search for dependence of faulting style, fault orientation, or principal stress direction on the distance from the nearest fracture zone. If fracture zones were generally weaker than the surrounding lithosphere, one of the principal horizontal stresses would be oriented nearly perpendicular to the fracture zone; we find no evidence that principal stresses near fracture zones are oriented preferentially in this manner. There is a slight tendency for earthquakes to occur near fracture zones, and patterns of fault orientation and sense of slip support the view that differential cooling and horizontal contraction on fracture zones may contribute seismogenic stress.

Bergman, Eric A.↗

Influence of fretting on flexural fatigue of 304 stainless steel and mild steel

Fretting fatigue experiments conducted on 304 stainless steel using a flexural fatigue test arrangement with bolted on fretting pads demonstrated that fatigue life is reduced by at least a factor of 10 in the 265 to 334 MPa (38,500 - to 48,500 psi) nominal flexural fatigue stress range. In addition, experiments in which the fretting pads were removed after selected numbers of cycles, followed by continued flexural fatigue without fretting show that continued fretting beyond 50,000 cycles does not significantly further reduce fatigue life of 304 stainless steel at 317 MPa (46,000 psi). Microscopic examination of the fretted contact areas revealed fracture initiation sites as well as numerous cracks that did not propagate to failure. Flexural fretting fatigue experiments performed on mild steel showed an insensitivity of fatigue life to the incidence of fretting under flexural stress conditions of from 162 to 217 MPa (23,500 to 31,500 psi).

Bill, R. C.↗

Acoustic emission characterization using AE (parameter) delay

The acoustic emission (AE) parameter delay concept is defined as that particular measured value of a parameter at which a specified baseline level of cumulative AE activity is reached. The parameter can be from any of a broad range of elastic, plastic, viscoelastic, and fracture mechanics parameters, as well as their combinations. Such parameters include stress, load, strain, displacement, time, temperature, loading cycle, unloading stress, stress intensity factor, strain energy release rate, and crack tip plasticity zone size, while the AE activity may be AE event counts, ringdown counts, energy, event duration, etc., as well as their combinations. Attention is given to examples for the AE parameter delay concept, together with various correlations.

Williams, J. H., Jr.↗

A Review of the CTOA/CTOD Fracture Criterion: Why it Works

The CTOA/CTOD fracture criterion is one of the oldest fracture criteria applied to fracture of metallic materials with cracks. During the past two decades, the use of elastic-plastic finite-element analyses to simulate fracture of laboratory specimens and structural components using the CTOA criterion has expanded rapidly. But the early applications were restricted to two-dimensional analyses, assuming either plane-stress or plane-strain behavior, which lead to generally non-constant values of CTOA, especially in the early stages crack extension. Later, the non-constant CTOA values were traced to inappropriate state-of-stress (or constraint) assumptions in the crack-front region and severe crack tunneling in thin-sheet materials. More recently, the CTOA fracture criterion has been used with three-dimensional analyses to study constraint effects, crack tunneling, and the fracture process. The constant CTOA criterion (from crack initiation to failure) has been successfully applied to numerous structural applications, such as aircraft fuselages and pipelines. But why does the "constant CTOA" fracture criterion work so well? This paper reviews the results from several studies, discusses the issues of why CTOA works, and discusses its limitations.

Newman, J. C., Jr.↗