Search NASA⌕ Search

SEARCH · Search NASA

Results for “PITTING CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

534 records · Page 30

Evaluation of Erosion of the Dummy “EE” Plate 19 in YA Type ATR Fuel Element During Reactor PALM Cycles

Advanced Test Reactor (ATR) Cycle 153B-1 was a 14-day, high-power, powered axial locator mechanism (PALM) operating cycle that completed on April 12, 2013. Cycle 153B-1 was a typical operating cycle for the ATR, and did not result in any unusual plant transients. ATR was started up and shut down as scheduled. The PALM drive physically moves the selected experiments into and out of the core to simulate reactor startup and heat up, and shutdown and cooldown transients, while the reactor remains in steady-state conditions. However, after the cycle was over, when the fuel elements were removed from the core and inspected, several thousand flow-assisted erosion pits and “horseshoeing” defects were readily observed on the surface of the several YA-type fuel elements (these are aluminum “dummy” plates that contain no fuel). In order to understand these erosion phenomena, a thermal-hydraulic model of coolant channel 20 on a YA-M fuel element was generated. The boundaries of the model were the aluminum EE plate of a YA-M fuel element and a beryllium reflector block with 13 horizontal saw cuts which represented regions of zero flow. The heat generated in fuel plates 1 through 18 was modeled to be passing through the aluminum EE plate. The coolant channel 20 width was set at 0.058 in. (58 mils). It was established that the horizontal saw cuts had a significant effect on the temperature of the coolant. The flow, which was expected to vary linearly with gradual heating of the coolant as it passed through the channel, was extremely turbulent. The temperature rise, which was expected to be a smooth “S” curve, was represented by a series temperature rise “humps,” which occurred at each horizontal saw cut in the beryllium reflector block. Each of the 13 saw cuts had a chamfered edge which resulted in the coolant flow being re-directed as a jet across the coolant channel into the surface of the EE plate, which explained the temperature rise and the observed scalloping and pitting degradation on the YA-M fuel elements. In the case of scalloping (horseshoeing) a surprising similarity of that defect to those appearing on aluminum plate rolled in over-lubrication conditions, were established. In turn, this made us think that the principal feature responsible for the appearance of these defects, was horizontal cuts in the beryllium reflector block created to arrest the propagation of large vertical crack(s) in Be in PALM cycles with higher overall fluence. This assumption was fully confirmed by the results of thermo-hydraulic simulations. The neutronics data for these modeling experiments were provided using advanced irradiation simulations (MCNP, HELIOS). In the case of pitting erosion the following corrective measures were proposed based upon the results of JMatPro v.8.2 modeling (TTT- and CCT-diagrams): change the fabrication process by adding blister anneal before program anneal, immediately after cold rolling of AA6061plate. This step will allow achieving complete recrystallization, eliminating of strengthening due to metastable precipitates, and reduce the possibility of forming sharp microstructural features upon the surface.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

The Stress Corrosion Resistance and the Cryogenic Temperature Mechanical Behavior of 18-3 Mn (Nitronic 33) Stainless Steel Parent and Welded Material

The ambient and cryogenic temperature mechanical properties and the ambient temperature stress corrosion results of 18-3 Mn (Nitronic 33)stainless steel, longitudinal and transverse, as received and as welded (TIG) material specimens manufactured from 0.063 inch thick sheet material, were described. The tensile test results indicate an increase in ultimate tensile and yield strengths with decreasing temperature. The elongation remained fairly constant to -200 F, but below that temperature the elongation decreased to less than 6.0% at liquid hydrogen temperature. The notched tensile strength (NTS) for the parent metal increased with decreasing temperature to liquid nitrogen temperature. Below -320 F the NTS decreased rapidly. The notched/unnotched (N/U) tensile ratio of the parent material specimens remained above 0.9 from ambient to -200 F, and decreased to approximately 0.65 and 0.62, respectively, for the longitudinal and transverse directions at liquid hydrogen temperature. After 180 days of testing, only those specimens exposed to the salt spray indicated pitting and some degradation of mechanical properties.

Montano, J. W.↗

Measurements and mechanisms of localized aqueous corrosion in aluminum-lithium-copper alloys

Summary information is included for electrochemical aspects of stress corrosion cracking in alloy 2090 and an introduction to the work to be initiated on the new X2095 (Weldalite) alloy system. Stress corrosion cracking (SCC) was studied in both S-T and L-T orientations in alloy 2090. A constant load TTF test was performed in several environments with a potentiostatically applied potential. In the same environments the electrochemical behavior of phases found along subgrain boundaries was assessed. It was found that rapid failure due to SCC occurred when the following criteria was met: E(sub BR,T1) is less than E(sub applied) is less than E(sub Br, matrix phase). Although the L-T orientation is usually considered more resistant to SCC, failures in this orientation occurred when the stated criteria was met. This may be due to the relatively isotropic geometry of the subgrains which measure approximately 12 to 25 microns in diameters. Initial studies of alloy X2095 includes electrochemical characterization of three compositional variations each at three temperatures. The role of T(sub 1) dissolution in SCC behavior is addressed using techniques similar to those used in the research of 2090 described. SCC susceptibility is also studied using alternate immersion facilities at Reynolds Metals Corporation. Pitting is investigated in terms of stability, role of precipitate phases and constituent particles, and as initiation sites for SCC. In all research endeavors, attempts are made to link electrochemistry to microstructure. Previous work on 2090 provides a convenient basis for comparison since both alloys contain T(sub 1) precipitates but with different distributions. In 2090 T(sub 1) forms preferentially on subgrain boundaries whereas in X2095 the microstructure appears to be more homogeneous with finer T(sub 1) particles. Another point for comparison is the delta prime strengthening phase found in 2090 but absent in X2095.

Wall, Douglas↗

241-AY-102 Leak detection pit drain line visual inspection - 15678

In October 2012, Washington River Protection Solutions LLC (WRPS) determined that waste had leaked into the annulus of Tank 241-AY-102. WRPS conducted an extensive review of Tank AY-102 and increased both inspection and monitoring of the tank; however, the precise cause and location of the leak could not be determined. In parallel with the leak in the primary tank, the Tank AY-102 leak detection pit (LDP) was accumulating water through the drain system external to the secondary tank liner. Liquid collecting in the LDP is suspected to be from water intrusion and collects at a rate such that the LDP must be pumped routinely. Following a routine pumping event on June 20, 2013, elevated radiation dose rates were noted on the transfer hose and surface contamination readings were found on the transfer pump when it was removed from the Tank AY-102 LDP. These two field readings suggested that tank waste from a secondary liner breach could be leaking into the LDP. As a result, WRPS initiated a plan to ascertain the integrity of the secondary tank liner including a robotic inspection of the LDP. To perform the robotic visual inspection, a custom robotic crawler with a deployment device was designed, built, and operated by IHI Southwest for WRPS to inspect the 6 in (152 mm) leak detection pit drain line. To ensure success when deployed in the field, the inspection equipment was demonstrated at both the IHI facility in Denver, Colorado, and the Hanford Site using full scale piping mockups. On November 20, 2013 WRPS inspected the 6 in (152 mm) diameter drain line. The deployment device successfully attached to the drain line, and the crawler entered the drain line and traversed to within approximately 7 ft (2.1 m) of the central sump located under the center of the tank before losing traction. Crawler performance was satisfactory, and the quality of the camera image and lighting provided sufficient detail to document the current condition of the visible regions of the pipe. The inspection showed that the majority of the drain line was dry. Two wet areas were observed, a portion of the line nearest the LDP and a portion near the center of the tank. The portion nearest the LDP was under water prior to pumping on November 14, 2013. Although sediment and debris were seen during the inspection, it is believed to be construction debris and corrosion products. No material was found in the inspection that looked like tank waste or the material seen in the Tank AY-102 annulus (i.e., no greenish or yellowish deposits or dark fluids, dried salt deposits, or crystalline material). The contamination levels seen on the crawler were consistent with past values seen on LDP pumping equipment. Sampling and analysis of the recovered residues from the crawlers did not find material consistent with tank waste. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Current understanding of environment-induced cracking of steam turbine steels (Reprinted from Proceedings of the CORROSION/2007 research topical symposium 'Advances in Environmentally Assisted Cracking', 2007)

An overview is given of the current knowledge and understanding of environment-induced cracking of steam turbine discs and blades. There has been extensive research on this theme, though our ability to predict the impact of environmental variables on service life is still constrained because early research had focused on environments that were not always representative of condensates formed in service. More recent research has yielded insight into the evolution of damage from pits and has provided more detailed long crack growth rates, but the growth of cracks in the short crack regime is largely undetermined. For coal-fired plants, the advent of two-shifting (switching on- and off-load on a daily basis) will lead to a reduction in remnant life due to transients in stress and environment. Since the number of cycles is small, the impact of load cycling is predicted to be modest. However, there may be an effect of the transient exposure to oxygen off-load on the subsequent crack growth rate on-load, and this also needs to be accounted for in life assessment.

20 FOSSIL-FUELED POWER PLANTS↗

Ultrasonic Examination of Double-Shell Tank 241-AP-107 Examination Completed February 2008

AREVA Federal Services LLC (AFS), under a contract from CH2M HILL Hanford Group (CH2M HILL), has performed an ultrasonic examination of selected portions of Double-Shell Tank 241-AP-107. The purpose of this examination was to provide information that could be used to evaluate the integrity of the wall of the primary tank. The requirements for the ultrasonic examination of Tank 241-AP-107 were to detect, characterize (identify, size, and locate), and record measurements made of any wall thinning, pitting, or cracks that might be present in the wall of the primary tank. Any measurements that exceed the requirements set forth in the Engineering Task Plan (ETP), RPP-Plan-34301 (Castleberry 2007) and summarized on page 1 of this document, are to be reported to CH2M HILL and the Pacific Northwest National Laboratory (PNNL) for further evaluation. Under the contract with CH2M HILL, all data is to be recorded on electronic media and paper copies of all measurements are provided to PNNL for third-party evaluation. PNNL is responsible for preparing a report(s) that describes the results of the AFS ultrasonic examinations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Lawrence Livermore National Laboratory (LLNL) Experimental Test Site (Site 300) Salinity Evaluation and Minimization Plan for Cooling Towers and Mechanical Equipment Discharges

This document was created to comply with the Central Valley Regional Water Quality Control Board (CVRWQCB) Waste Discharge Requirement (Order No. 98-148). This order established new requirements to assess the effect of and effort required to reduce salts in process water discharged to the subsurface. This includes the review of technical, operational, and management options available to reduce total dissolved solids (TDS) concentrations in cooling tower and mechanical equipment water discharges at Lawrence Livermore National Laboratory's (LLNL's) Experimental Test Site (Site 300) facility. It was observed that for the six cooling towers currently in operation, the total volume of groundwater used as make up water is about 27 gallons per minute and the discharge to the subsurface via percolation pits is 13 gallons per minute. The extracted groundwater has a TDS concentration of 700 mg/L. The cooling tower discharge concentrations range from 700 to 1,400 mg/L. There is also a small volume of mechanical equipment effluent being discharged to percolation pits, with a TDS range from 400 to 3,300 mg/L. The cooling towers and mechanical equipment are maintained and operated in a satisfactory manner. No major leaks were identified. Currently, there are no re-use options being employed. Several approaches known to reduce the blow down flow rate and/or TDS concentration being discharged to the percolation pits and septic systems were reviewed for technical feasibility and cost efficiency. These options range from efforts as simple as eliminating leaks to implementing advanced and innovative treatment methods. The various options considered, and their anticipated effect on water consumption, discharge volumes, and reduced concentrations are listed and compared in this report. Based on the assessment, it was recommended that there is enough variability in equipment usage, chemistry, flow rate, and discharge configurations that each discharge location at Site 300 should be considered separately when deciding on an approach for reducing the salt discharge to the subsurface. The smaller units may justify moderate changes to equipment, and may benefit from increased cleaning frequencies, more accurate and suitable chemical treatment, and sources of make up water and discharge re-use. The larger cooling towers would be more suitable for automated systems where they don't already exist, re-circulation and treatment of blow down water, and enhanced chemical dosing strategies. It may be more technically feasible and cost efficient for the smaller cooling towers to be replaced by closed loop dry coolers or hybrid towers. There are several potential steps that could be taken at each location to reduce the TDS concentration and/or water use. These include: sump water filtration, minimization of drift, accurate chemical dosing, and use of scale and corrosion coupons for chemical calibration. The implementation of some of these options could be achieved by a step-wise approach taken at two representative facilities. Once viable prototype systems have been proven in the field, systematic implementation should proceed for the remaining systems, with cost, desired reduction, and general feasibility taken into consideration for such systems.

54 ENVIRONMENTAL SCIENCES↗

The effect of zinc additions on the environmental stability of Alloy 8090 (Al-Li-Cu-Mg-Zr)

Stress corrosion cracking (SCC) remains a problem in both Al-Li and conventional Al heat treatable alloys. It has recently been found that relatively small additions (less than or approximately 1 wt-percent) of Zn can dramatically improve the SCC performance of alloy 8090 (Al-Li-Cu-Mg-Zr). Constant load time to failure experiments using cylindrical tensile samples loaded between 30 and 85 percent of TYS indicate improvements of orders of magnitude over the baseline 8090 for the Zn-containing alloys under certain aging conditions. However, the toughnesses of the alloys were noticeably degraded due to the formation of second phase particles which primarily reside on grain and subgrain boundaries. EDS revealed that these intermetallic particles were Cu and Zn rich. The particles were present in the T3 condition and were not found to be the result of quench rate, though their size and distribution were. At 5 hours at 160 C, the alloys displayed the greatest susceptibility to SCC but by 20 hours at 160 C the alloys demonstrated markedly improved TTF lifetimes. Aging past this time did not provide separable TTF results, however, the alloy toughnesses continued to worsen. Initial examination of the alloys microstructures at 5 and 20 hours indicated some changes most notably the S' and delta' distributions. A possible model by which this may occur will be explored. Polarization experiments indicated a change in the trend of E(sub BR) and passive current density at peak aging as compared to the baseline 8090. Initial pitting experiments indicated that the primary pitting mechanism in chloride environments is one occurring at constituent (Al-Fe-Cu) particles and that the Cu and Zn rich boundary precipitates posses a breakaway potential similar to that of the matrix acting neither anodic or cathodic in the first set of aerated 3.5 w/o NaCl experiments. Future work will focus on the identification of the second phase particles, evaluation of K(sub 1SCC) and plateau da/dt via both DCB and slow strain rate techniques. A lower Zn content variant will be examined in the near future in hopes of optimizing toughness, density and SCC performance.

Kilmer, Raymond J.↗

Thrust Stand Measurements Using Alternative Propellants in the Microwave Assisted Discharge Inductive Plasma Accelerator

Storable propellants (for example water, ammonia, and hydrazine) are attractive for deep space propulsion due to their naturally high density at ambient interplanetary conditions, which obviates the need for a cryogenic/venting system. Water in particular is attractive due to its ease of handling and availability both terrestrially and extra-terrestrially. While many storable propellants are reactive and corrosive, a propulsion scheme where the propellant is insulated from vulnerable (e.g. metallic) sections of the assembly would be well-suited to process these otherwise incompatible propellants. Pulsed inductive plasma thrusters meet this criterion because they can be operated without direct propellant-electrode interaction. During operation of these devices, electrical energy is capacitively stored and then discharged through an inductive coil creating a time-varying current in the coil that interacts with a plasma covering the face of the coil to induce a plasma current. Propellant is accelerated and expelled at a high exhaust velocity (O(10-100 km/s)) by the Lorentz body force arising from the interaction of the magnetic field and the induced plasma current. While this class of thruster mitigates the life-limiting issues associated with electrode erosion, many pulsed inductive plasma thrusters require high pulse energies to inductively ionize propellant. The Microwave Assisted Discharge Inductive Plasma Accelerator (MAD-IPA) is a pulsed inductive plasma thruster that addressees this issue by partially ionizing propellant inside a conical inductive coil before the main current pulse via an electron cyclotron resonance (ECR) discharge. The ECR plasma is produced using microwaves and a static magnetic field from a set of permanent magnets arranged to create a thin resonance region along the inner surface of the coil, restricting plasma formation, and in turn current sheet formation, to a region where the magnetic coupling between the plasma and the theta-pinch coil is high. The use of a conical theta-pinch coil also serves to provide neutral propellant containment and plasma plume focusing that is improved relative to the more common planar geometry of the Pulsed Inductive Thruster (PIT). In this paper, we describe thrust stand measurements performed to evaluate the specific impulse and thrust efficiency of the MAD-IPA for a variety of propellants. Propellants tested include both widely-used, non-reactive noble gases like argon, and rarely-used propellants such as water, hydrazine and ammonia. Dependencies of impulse data on propellant species are discussed in the context of the current sheet formation and electromagnetic plasma acceleration processes.

Hallock, Ashley K.↗

Analysis of erosion/corrosion data for high-level waste pipelines at Hanford - 15519

Washington River Protection Solutions (WRPS) has implemented a fitness-for-service program which will evaluate the degraded condition of the tank farm waste transfer system. The Tank Farms Waste Transfer System Fitness-for-Service Requirements and Recommendations, includes a requirement to inspect primary piping, encasements, and jumpers for corrosion/erosion. The 242-A Evaporator pump room was upgraded by adding instrumentation to the feed and return jumpers, prior to running the next campaign. As part of this upgrade, several jumpers were removed for disposal and a total of five jumpers were selected for ultrasonic thickness (UT) inspection. The jumpers selected were the following: 18-4, C-4 and 5, J-13A, 13-K, and 19-5. All of these jumpers will be removed permanently except for jumper 19-5 which will be reinstalled for further service. As part of this study, several jumpers from the AW-02E Feed Pit were also removed for disposal and two were selected for UT inspection. The jumpers selected were the 1-4 and B-2 which were packaged and sent to the 222-S Laboratory for UT assessments. This paper includes details of each jumper as well as the estimated remaining useful life (ERUL), if applicable, for its components based on the wall thinning measured in elbows and straight sections. The jumper's ultrasonic thickness measurements are plotted and trends are assessed based on the volume of fluid transferred or time of service. Variability in thickness is generally evaluated in two approaches, radially around the circumference of the pipe or component and longitudinally along the length. The paper also explains the analysis procedure for evaluating the different components. In particular, issues related to thinning from manufacturing different types of elbows (long radius, five diameter bend radius) are presented. Analysis techniques are developed for elbows that differentiate thinning from erosion/corrosion and manufacturing which is critical for this analysis. Results demonstrate that in most components, the thickness measurements are still greater than the manufactured nominal thickness. For the cases in which the thickness is below the nominal thickness, the ERUL well exceeds the life needed for servicing the Waste Treatment Plant. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Determination of Erosion/Corrosion Rates in Hanford Tank Farms Radioactive Waste Transfer System Pipelines

The twenty-eight double-shell underground radioactive waste storage tanks at the U. S. Department of Energy’s Hanford Site near Richland, WA are interconnected by the Waste Transfer System network of buried steel encased pipelines and pipe jumpers in below-grade pits. The pipeline material is stainless steel or carbon steel in 51 mm to 152 mm (2 in. to 6 in.) sizes. The pipelines carry slurries ranging up to 20 volume percent solids and supernatants with less than one volume percent solids at velocities necessary to prevent settling. The pipelines, installed between 1976 and 2011, were originally intended to last until the 2028 completion of the double-shell tank storage mission. The mission has been subsequently extended. In 2010 the Tank Operating Contractor began a systematic evaluation of the Waste Transfer System pipeline conditions applying guidelines from API 579-1/ASME FFS-1 (2007), Fitness-For-Service. Between 2010 and 2014 Fitness-for-Service examinations of the Waste Transfer System pipeline materials, sizes, and components were completed. In parallel, waste throughput histories were prepared allowing side-by-side pipeline wall thinning rate comparisons between carbon and stainless steel, slurries and supernatants and throughput volumes. The work showed that for transfer volumes up to 6.1E+05 m 3 (161 million gallons), the highest throughput of any pipeline segment examined, there has been no detectable wall thinning in either stainless or carbon steel pipeline material regardless of waste fluid characteristics or throughput. The paper describes the field and laboratory evaluation methods used for the Fitness-for-Service examinations, the results of the examinations, and the data reduction methodologies used to support Hanford Waste Transfer System pipeline wall thinning conclusions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Determination of Erosion/Corrosion Rates in Hanford Tank Farms Radioactive Waste Transfer System Pipelines - 16395

The twenty-eight double-shell underground radioactive waste storage tanks at the U.S. Department of Energy's Hanford Site near Richland, WA are interconnected by the Waste Transfer System network of buried steel encased pipelines and pipe jumpers in below-grade pits. The pipeline material is stainless steel or carbon steel in 51 mm to 152 mm (2 in. to 6 in.) sizes. The pipelines carry slurries ranging up to 20 volume percent solids and supernatants with less than one volume percent solids at velocities necessary to prevent settling. The pipelines, installed between 1976 and 2011, were originally intended to last until the 2028 completion of the double-shell tank storage mission. The mission has been subsequently extended. In 2010 the Tank Operating Contractor began a systematic evaluation of the Waste Transfer System pipeline conditions applying guidelines from API 579-1/ASME FFS-1 (2007), Fitness-For- Service. Between 2010 and 2014 Fitness-for-Service examinations of the Waste Transfer System pipeline materials, sizes, and components were completed. In parallel, waste throughput histories were prepared allowing side-by-side pipeline wall thinning rate comparisons between carbon and stainless steel, slurries and supernatants and throughput volumes. The work showed that for transfer volumes up to 6.1 E+05 m{sup 3} (161 million gallons), the highest throughput of any pipeline segment examined, there has been no detectable wall thinning in either stainless or carbon steel pipeline material regardless of waste fluid characteristics or throughput. The paper describes the field and laboratory evaluation methods used for the Fitness-for-Service examinations, the results of the examinations, and the data reduction methodologies used to support Hanford Waste Transfer System pipeline wall thinning conclusions. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗