Search NASA⌕ Search

SEARCH · Search NASA

Results for “cracking temperature”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Influence of hydrogen environments on crack growth in Inconel 718

The effect of hydrogen environments on sustained-load and cyclic-load crack growth in Inconel 718 was investigated using fracture-mechanics-type specimens. The sustained-load crack growth was determined to be a function of heat-treatment condition, temperature, and hydrogen pressure. The threshold stress intensity for subcritical crack growth was independent of hydrogen pressure at pressures greater than 21 MN/sq m (3000 psi). The cyclic-load crack growth rate in Inconel 718 at low and moderate stress intensity ranges increased with increasing hydrogen pressure. Decreasing the cyclic frequency from 1.0 to 0.1 Hz considerably increased the cyclic crack growth rate at 0.069 MN/sq m (10 psi) and at 68.9 MN/sq m (10,000 psi) hydrogen pressure. A series of measurements performed between 1.0 and 0.1 Hz showed that the crack growth rate increased as a complex function of the time per cycle.

Walter, R. J.↗

Hydrogen-enhanced fatigue crack growth in Ti-6Al-4V ELI weldments.

The effects of a hydrogen environment on the fatigue crack growth rates in Ti-6Al-4V ELI (STA) and weld material were determined in the temperature range of ambient to -200 F. The hydrogen environment resulted in an acceleration of the crack growth rate and a change in the fracture mode for both materials in the temperature range of ambient to -100 F. At -200 F, there was no significant difference between the crack growth rates obtained in helium and hydrogen gas. The degree of hydrogen-enhanced crack growth was found to be dependent on the crack tip stress-intensity range, temperature, and microstructure of the material. The data are consistent with an embrittlement mechanism involving hydrogen diffusing ahead of the crack front.

Pittinato, G. F.↗

Application of Sol-Gel Method as a Protective Layer on a Specular Reflective Surface for Secondary Reflector in a Solar Receiver

Highly-specular reflective surfaces that can withstand elevated-temperatures are desirable for many applications including reflective heat shielding in solar receivers and secondary reflectors, which can be used between primary concentrators and heat collectors. A high-efficiency, high-temperature solar receiver design based on arrays of cavities needs a highly-specular reflective surface on its front section to help sunlight penetrate into the absorber tubes for effective flux spreading. Since this application is for high-temperature solar receivers, this surface needs to be durable and to maintain its optical properties through the usable life. Degradation mechanisms associated with elevated temperatures and thermal cycling, which include cracking, delamination, corrosion/oxidation, and environmental effects, could cause the optical properties of surfaces to degrade rapidly in these conditions. Protected mirror surfaces for these applications have been tested by depositing a thin layer of SiO2 on top of electrodeposited silver by means of the sol-gel method. To obtain an effective thin film structure, this sol-gel procedure has been investigated extensively by varying process parameters that affect film porosity and thickness. Endurance tests have been performed in a furnace at 150 degrees C for thousands of hours. This paper presents the sol-gel process for intermediate-temperature specular reflective coatings and provides the long-term reliability test results of sol-gel protected silver-coated surfaces.

14 SOLAR ENERGY↗

Effect of temperature on microstructure and mechanical properties of ECAPed (TiB + La2O3)/Ti-6Al-4V composites

Highlights: • Dynamic recrystallization resulted in ultrafine grains near TiB interface region. • Tensile strength of ECAPed composites increased by up to 18%. • The average aspect ratio of TiB reduced with increasing ECAP temperature. • Interface debonding of TiB led to crack propagation and low ductility. TiB short fibers and La{sub 2}O{sub 3} particles reinforced titanium matrix composites (TMCs) were successfully equal-channel angular pressed (ECAPed) at 600 °C–900 °C. The effect of ECAP temperature on the microstructure and mechanical properties of the TMCs was investigated. The results indicated that dislocation tangling formed cell structures in matrix at lower ECAP temperature. In contrast, continuous dynamic recrystallization occurred at higher ECAP temperature, and promoted the formation of numerous new ultrafine grains. The average aspect ratio of TiB short fibers decreased with increasing ECAP temperature, which induced interfacial debonding. The tensile strength of TMCs ECAPed at 800 °C was up to 1128 MPa, which was 18% higher than the as-received composites. Interfacial debonding led TiB short fibers in low aspect ratios disabled to bear load, while the formation of ultrafine grains increased the strength of TMCs. The coupling of these two factors resulted in little effect of ECAP temperature on the tensile strength. However, the elongation of ECAPed TMCs generally decreased due to the loss of strain hardening capacity. Stress concentration tended to occur around the tips of TiB short fibers due to the interfacial debonding and cause crack propagation. It led to the premature fracture and low ductility.

36 MATERIALS SCIENCE↗

Type IV failure in weldment of creep resistant ferritic alloys: I. Micromechanical origin of creep strain localization in the heat affected zone

Creep strength enhanced ferritic (CSEF) steels containing 9-12wt% chromium have been extensively used in fossil-fuel-fired power plants. Despite their excellent creep resistance at high temperatures, premature failures (especially Type IV cracking) are often found in the fine-grained heat affected zone (HAZ) or intercritical HAZ of the welded components. This failure mode is preceded by the strain localization in the HAZ, as measured by the Digital Image Correlation (DIC) technique. The present work aims to develop a finite-element based computational method to determine the micromechanical and microstructural origin of the strain localization phenomenon. We construct a two-dimensional digital microstructure based on the actual microstructure of ferritic steel weldments by using the Voronoi-tessellation method, to account for the effects of its large grain-size gradients. A mechanism-based finite element method is developed for modeling the high temperature deformation resulting from a synergy of thermally activated dislocation movements, diffusional flow and grain boundary sliding. The numerical results agree well with the strain measurements by our DIC technique, particularly revealing the effect of pre-welding tempering on the evolution of strain localization in HAZ of creep resistant steel weldments. It is found that the diffusional creep with dependence on grain sizes, dislocation creep with dependence on material strength, and more importantly, grain boundary sliding, contribute synergistically to the creep strain accumulation in the HAZ, and their relative degree of significance is quantified. The creep rupture life will be investigated in the companion paper.

36 MATERIALS SCIENCE↗

Fracture analysis of various cracked configurations in sheet and plate materials

A two-parameter fracture criterion was derived which relates the linear-elastic stress-intensity factor at failure, the elastic nominal failure stress, and two material parameters. The fracture criterion was used previously to analyze fracture data for surface- and through-cracked sheet and plate specimens under tensile loading. The fracture criterion was applied to center-crack tension, compact, and notch-band fracture specimens made of steel, titanium, or aluminum alloy materials tested at room temperature. The fracture data included a wide range of crack lengths, specimen widths, and thicknesses. The materials analyzed had a wide range of tensile properties. Failure stresses calculated using the criterion agreed well (plus or minus 10 percent) with experimental failure stresses. The criterion was also found to correlate fracture data from different specimen types (such as center-crack tension and compact specimens), within plus or minus 10 percent for the same material, thickness, and test temperature.

Newman, J. C., Jr.↗

Fracture analysis of various cracked configurations in sheet and plate materials

A two-parameter fracture criterion has been derived which relates the linear-elastic stress-intensity factor at failure, the elastic nominal failure stress, and two material parameters. The fracture criterion was applied to center-crack tension, compact, and notch-bend fracture specimens made of steel, titanium, or aluminum alloy materials tested at room temperature. The fracture data included a wide range of crack lengths, specimen widths, and thicknesses. The materials analyzed had a wide range of tensile properties. Failure stresses calculated using the criterion agreed well (plus or minus 10 percent) with experimental failure stresses. The criterion was also found to correlate fracture data from different specimen types (such as center-crack tension and compact specimens), within plus or minus 10 percent for the same material, thickness, and test temperature.

Newman, J. C., Jr.↗

Correlation of deformation mechanisms with the tensile and compressive behavior of NiAl and NiAl(Zr) intermetallic alloys

To identify the mechanisms controlling strength and ductility in powder-extruded NiAl and NiAl + 0.05 at. pct Zr, tensile and compressive testing was performed from 300 to 1300 K for several grain sizes. Grain size refinement significantly increased yield stress in both alloys and, in some cases, slightly lowered the ductile-to-brittle transition temperature (DBTT), although no room-temperature tensile ductility was observed even in the finest grain size specimens. The small Zr addition increased the DBTT and changed the low-temperature fracture mode from intergranular in NiAl to a combination of intergranular and transgranular in the Zr-doped alloy. Scanning electron microscopy of compression specimens deformed at room temperature revealed the presence of grain-boundary cracks in both alloys. These cracks were due to the incompatibility of strain in the polycrystalline material, owing to the lack of five independent slip systems. The tendency to form grain-boundary cracks, in addition to the low fracture stress of these alloys, contributed to the lack of tensile ductility at low temperatures.

Bowman, R. R.↗

MODELING SOLIDIFICATION-INDUCED STRESSES IN CERAMIC WASTE FORMS CONTAINING NUCLEAR WASTES

The goal of this work is to produce a ceramic waste form (CWF) that permanently occludes radioactive waste. This is accomplished by absorbing radioactive salts into zeolite, mixing with glass frit, heating to a molten state 915 C to form a sodalite glass matrix, and solidifying for long-term storage. Less long term leaching is expected if the solidifying cooling rate doesn’t cause cracking. In addition to thermal stress, this paper proposes that a stress is formed during solidification which is very large for fast cooling rates during solidification and can cause severe cracking. A solidifying glass or ceramic cylinder forms a dome on the cylinder top end. The temperature distribution at the time of solidification causes the stress and the dome. The dome height, “the length deficit,” produces an axial stress when the solid returns to room temperature with the inherent outer region in compression, the inner in tension. Large tensions will cause cracking of the specimen. The temperature deficit, derived by dividing the length deficit by the coefficient of thermal expansion, allows solidification stress theory to be extended to the circumferential stress. This paper derives the solidification stress theory, gives examples, explains how to induce beneficial stresses, and compares theory to experimental data.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Edge crack growth of thermally aged graphite/polyimide composites

Laminates of Celion 6000/LARC-160 and Celion 6000/PMR-15 graphite/polyimide composite materials were aged in air at temperatures of 202, 232, 260 and 288 C for various times up to 15,000 hours. Three unidirectional specimen types were studied: short beam shear (SBS), flexure, and 153 mm square panels. The interior region of the square panels exhibited little or no property degradation, whereas both laminate materials degraded and cracked preferentially at the specimen edge perpendicular to the fibers. Using a dye penetrant, the specimens were X-rayed and the crack depth measured as a function of time and temperature. A time temperature superposition of the crack data was successfully performed using an Arrhenius form for the shift factor. A direct correlation was found for edge crack depth and SBS strength for the LARC-160 laminates but the correlation for PMR-15 laminates was more complex.

Nelson, J. B.↗

In Situ Guided Wave Structural Health Monitoring System

Aircraft engine rotating equipment operates at high temperatures and stresses. Noninvasive inspection of microcracks in those components poses a challenge for nondestructive evaluation. A low-cost, low-profile, high-temperature ultrasonic guided wave sensor was developed that detects cracks in situ. The transducer design provides nondestructive evaluation of structures and materials. A key feature of the sensor is that it withstands high temperatures and excites strong surface wave energy to inspect surface and subsurface cracks. The sol-gel bismuth titanate-based surface acoustic wave (SAW) sensor can generate efficient SAWs for crack inspection. The sensor is very thin (submillimeter) and can generate surface waves up to 540 C. Finite element analysis of the SAW transducer design was performed to predict the sensor behavior, and experimental studies confirmed the results. The sensor can be implemented on structures of various shapes. With a spray-coating process, the sensor can be applied to the surface of large curvatures. It has minimal effect on airflow or rotating equipment imbalance, and provides good sensitivity.

Zhao, George↗

Hotspot formation due to shock-induced pore collapse in 1,3,5,7-tetranitro-1,3,5,7-tetrazoctane (HMX): Role of pore shape and shock strength in collapse mechanism and temperature

The shock to detonation transition in heterogeneous high energy density solids starts with the spatial localization of mechanical energy into so-called hotspots that form due to the interaction between the leading wave and microstructural features and defects. We used large-scale molecular dynamics to characterize the hotspots resulting from the shock-induced collapse of cylindrical voids and elongated cracks focusing on the effect of shock strength, defect shape, and size. The temperature fields resulting from the collapse of cracks elongated along the shock direction show significantly higher sensitivity to both shock strength and size than cylindrical voids. Cracks 80 nm in length result in temperatures almost three times higher than voids 80 nm in diameter, reaching values corresponding to the ideal case of isentropic recompression of a gas. The molecular dynamics trajectories reveal the atomic origin of this contrasting behavior. While circular voids undergo a transition from viscoelastic pore collapse to a hydrodynamic regime with increasing shock strength, shock focusing in elongated cracks results in jetting and vaporization which, upon recompression, leads to increased heating.

36 MATERIALS SCIENCE↗

Thermal decomposition of expanded polystyrene in a pebble bed reactor to get higher liquid fraction yield at low temperatures

Expanded polystyrene is one of the polymers produced in large quantities due to its versatile application in different fields. This polymer is one of the most intractable components in municipal solid waste. Disposal of polymeric material by pyrolysis or catalytic cracking yields valuable hydrocarbon fuels or monomers. Literature reports different types of reactors and arrangements that have uniform temperatures during pyrolysis and catalytic cracking. The present study focuses on reducing the temperature to maximize the quantity of styrene monomer in the liquid product. A bench scale reactor has been developed to recover the styrene monomer and other valuable chemicals. Experiments were carried under partial oxidation and vacuum conditions in the temperature range of 300-500 deg. C. In the pyrolysis optimization studies, the best atmospheric condition was determined to be vacuum, the pyrolysis temperature should be 500 deg. C, yield of liquid product obtained was 91.7% and yield of styrene obtained was 85.5%. In the characterization studies, distillation and IR spectroscopy experiments were carried out. The remaining of the liquid product comprises of benzene, ethyl benzene, and styrene dimers and trimers.

54 ENVIRONMENTAL SCIENCES↗

Fracture dynamics in implanted silicon

Crack propagation in implanted silicon for thin layer transfer is experimentally studied. The crack propagation velocity as a function of split temperature is measured using a designed optical setup. Interferometric measurement of the gap opening is performed dynamically and shows an oscillatory crack “wake” with a typical wavelength in the centimetre range. The dynamics of this motion is modelled using beam elasticity and thermodynamics. The modelling demonstrates the key role of external atmospheric pressure during crack propagation. A quantification of the amount of gas trapped inside pre-existing microcracks and released during the fracture is made possible, with results consistent with previous studies.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Thermal fatigue performance of integrally cast automotive turbine wheels

Fluidized bed thermal fatigue testing was conducted on 16 integrally cast automotive turbine wheels for 1000-10,000 (600 sec total) thermal cycles at 935/50 C. The 16 wheels consisted of 14 IN-792 + 1% Hf and 2 gatorized AF2-1DA wheels; 6 of the IN-792 + Hf wheels contained crack arrest pockets inside the blade root flange. Temperature transients during the thermal cycling were measured in three calibration tests using either 18 or 30 thermocouples per wheel. Thermal cracking based on crack length versus accumulated cycles was greatest for unpocketed wheels developing cracks in 8-13 cycles compared to 75-250 cycles for unpocketed wheels. However, pocketed wheels survived up to 10,000 cycles with crack lengths less than 20 mm, whereas two unpocketed wheels developed 45 mm long cracks in 1000-2000 cycles.

Humphreys, V. E.↗

High-temperature low cycle fatigue behavior of a gray cast iron

The strain controlled low cycle fatigue properties of the studied gray cast iron for engine cylinder blocks were investigated. At the same total strain amplitude, the low cycle fatigue life of the studied material at 523 K was higher than that at 423 K. The fatigue behavior of the studied material was characterized as cyclic softening at any given total strain amplitude (0.12%–0.24%), which was attributed to fatigue crack initiation and propagation. Moreover, this material exhibited asymmetric hysteresis loops due to the presence of the graphite lamellas. Transmission electron microscopy analysis suggested that cyclic softening was also caused by the interactions of dislocations at 423 K, such as cell structure in ferrite, whereas cyclic softening was related to subgrain boundaries and dislocation climbing at 523 K. Micro-analysis of specimen fracture appearance was conducted in order to obtain the fracture characteristics and crack paths for different strain amplitudes. It showed that the higher the temperature, the rougher the crack face of the examined gray cast iron at the same total strain amplitude. Additionally, the microcracks were readily blunted during growth inside the pearlite matrix at 423 K, whereas the microcracks could easily pass through pearlite matrix along with deflection at 523 K. The results of fatigue experiments consistently showed that fatigue damage for the studied material at 423 K was lower than that at 523 K under any given total strain amplitude. - Highlights: • The low cycle fatigue behavior of the HT250 for engine cylinder blocks was investigated. • TEM investigations were conducted to explain the cyclic deformation response. • The low cycle fatigue cracks of HT250 GCI were studied by SEM. • The fatigue life of the examined material at 523 K is higher than that at 423 K.

36 MATERIALS SCIENCE↗

Effects of loading rate and temperature on dynamic fracture of ceramic matrix composites

A hybrid experimental-numerical procedure was used to determine the dynamic fracture initiation toughnesses and the dynamic stress intensity factors of alumina, TiB2-particulate/SiC-matrix, and SiC(w)/Al2O3-matrix composites at room and elevated temperatures under static and impact loadings. The dynamic fracture initiation toughnesses at room and elevated temperatures were greater than the corresponding static fracture toughness. The crack velocity versus the dynamic stress intensity factor relations showed minor differences due to temperature changes but significant differences due to the change in loading rates.

Yang, K. H.↗