Effect of wheel speed and annealing temperature on microstructure and texture evolution of Ni{sub 45}Mn{sub 36.6}In{sub 13.4}Co{sub 5} ribbon

Ni{sub 45}Mn{sub 36.6}In{sub 13.4}Co{sub 5} magnetic shape memory alloy was successfully produced as preferentially textured ribbon by melting spinning with different wheel speed. X-ray diffraction (XRD) and electron back scatter diffraction (EBSD) were used to study structure and texture evolution of these melt-spun ribbons. The thickness of melt-spun ribbon is 42 μm, 65 μm and 30 μm depending on wheel speed of 1 0 m/s, 15 m/s and 20 m/s, respectively. Density of α fiber texture (〈100〉//ND) vary with wheel speed changes, and is most intensive in the ribbon with wheel speed of 15 m/s. Grains of the ribbons grow after being annealed at 873 K, 973 K, 1073 K and 1173 K, recrystallization was not observed in ribbons after being annealed at 873 K but occurred in ribbons after being annealed at higher temperatures. The α fiber texture becomes weaker to some extent after annealing at different temperatures, due to new recrystallization texture formed at the process of annealing. - Highlights: •Sectional part of shape memory ribbon is firstly investigated by EBSD method. •Thickness and texture of ribbons vary with wheel speed. •Annealing temperature affect texture and microstructure evolution greatly. •Recrystallization textures were observed in ribbons after being annealed.

36 MATERIALS SCIENCE↗

Formation of {332}<113>β twins from parent {130}<310>α″ plastic twins in a full α″ Ti-Nb alloy by annealing

Highlights: • The solution-treated, deformed and annealed structures of a full α″ martensitic Ti-23Nb (at.%) alloy have been investigated. • The self-accommodated feature of the α″ martensites is presented by EBSD. • The martensites transform into β phase after annealing and the β phase is retained to room temperature by furnace-cooling. • Direct evidence is given for the formation of {332}{sub β} twins from {130}{sub α″} plastic twins by ex-situ EBSD observations. • A possible {351}<1 1-bar 2>{sub α″} twinning in α″ phase that corresponds to {332}<11 3-bar >{sub β} is proposed. - Abstract: The solution-treated (ST), deformed and subsequently annealed microstructures of a full α″ martensitic Ti-23Nb at.% alloy have been investigated by optical micrograph (OM), X-ray diffraction (XRD) and electron back-scattered diffraction (EBSD). The results show that both the self-accommodated α″ martensites in ST sample and re-orientated martensitic structure and plastic {130}{sub α″} twins in the Deformed sample fully transformed into the β phase with a small amount of the ω phase by annealing. The ex-situ EBSD measurements showed that the {332}{sub β} twins occur in the Annealed sample, which correspond to the {130}{sub α″} plastic twins of the α″ phase in the Deformed sample, and thus give a direct evidence that the {332}{sub β} twins in the β phase form from the reverse martensitic transformation of the {130}{sub α″} plastic twins in the α″ phase. Moreover, it's also expected from EBSD results that in addition to {130}<3 1-bar 0>{sub α″}, the possible <{351}<1 1-bar 2>{sub α″} twinning system of the α″ phase corresponds to the {332}<11 3-bar >{sub β} twinning of the β phase.

36 MATERIALS SCIENCE↗

Understanding and Predicting Metallic Whisker Growth and its Effects on Reliability (LDRD Final Report)

Tin (Sn) whiskers are conductive Sn filaments that grow from Sn-plated surfaces, such as surface finishes on electronic packages. The phenomenon of Sn whiskering has become a concern in recent years due to requirements for lead (Pb)-free soldering and surface finishes in commercial electronics. Pure Sn finishes are more prone to whisker growth than their Sn-Pb counterparts and high profile failures due to whisker formation (causing short circuits) in space applications have been documented. At Sandia, Sn whiskers are of interest due to increased use of Pb-free commercial off-the-shelf (COTS) parts and possible future requirements for Pb-free solders and surface finishes in high-reliability microelectronics. Lead-free solders and surface finishes are currently being used or considered for several Sandia applications. Despite the long history of Sn whisker research and the recently renewed interest in this topic, a comprehensive understanding of whisker growth remains elusive. This report describes recent research on characterization of Sn whiskers with the aim of understanding the underlying whisker growth mechanism(s). The report is divided into four sections and an Appendix. In Section 1, the Sn plating process is summarized. Specifically, the Sn plating parameters that were successful in producing samples with whiskers will be reviewed. In Section 2, the scanning electron microscopy (SEM) of Sn whiskers and time-lapse SEM studies of whisker growth will be discussed. This discussion includes the characterization of straight as well as kinked whiskers. In Section 3, a detailed discussion is given of SEM/EBSD (electron backscatter diffraction) techniques developed to determine the crystallography of Sn whiskers. In Section 4, these SEM/EBSD methods are employed to determine the crystallography of Sn whiskers, with a statistically significant number of whiskers analyzed. This is the largest study of Sn whisker crystallography ever reported. This section includes a review of previous literature on Sn whisker crystallography. The overall texture of the Sn films was also analyzed by EBSD. Finally, a short Appendix is included at the end of this report, in which the X-Ray diffraction (XRD) results are discussed and compared to the EBSD analyses of the overall textures of the Sn films. Sections 2, 3, and 4 have been or will be submitted as stand-alone papers in peer-reviewed technical journals. A bibliography of recent Sandia Sn whisker publications and presentations is included at the end of the report.

36 MATERIALS SCIENCE↗

Microstructural analysis on cleavage fracture in pearlitic steels

Microstructural features controlling cleavage fracture in pearlitic structures were investigated by means of scanning electron microscopy and electron backscattered diffraction. It was found that pearlite block size corresponds well to the cleavage facet size, and a single cleavage facet usually contains multiple pearlite colonies. Pearlite block size and cleavage facet size decrease with the refinement of prior austenite grain size, while pearlite colony size only changes slightly. The cleavage crack can largely deflect at block boundaries rather than at colony boundaries. Pearlite block can act as the dominant substructure on cleavage crack propagation in pearlitic steels. - Highlights: •The cleavage crack propagation path in pearlitic structures was analyzed by EBSD. •Pearlite block boundaries can effectively hinder the crack propagation. •Pearlite block size corresponds well to the cleavage facet size. •A single cleavage facet usually contains multiple pearlite colonies.

36 MATERIALS SCIENCE↗

Electron Beam Welding of Nimonic 80A Superalloy: Microstructure Evolution and EBSD Study After Aging Heat Treatment

The purpose of this research was to evaluate integrity and microstructure changes of the electron beam-welded Nimonic 80A and the base metal after aging heat treatment process, i.e., 700 °C/72 h/air cooling. Here, microstructure, microhardness and tensile were investigated by various tools, i.e., scanning electron microscope with energy-dispersive spectroscopy and electron backscatter diffraction, x-ray diffraction analysis and Vickers hardness. Evaluation of microstructure shows that the weld zone mainly consists of columnar dendrites. The effect of aging heat treatment on the microstructure morphology and phase structure is very limited. Also, it was observed that there are obvious segregation and precipitates in intracrystalline and along the grain boundaries after aging heat treatment. Electron backscatter diffraction results show that the weld zone and base metal have a clear difference in the grain boundary characterization and kernel average misorientation at room temperature and after aging heat treatment, which leads to a difference in microhardness of the weld zone. In addition, the relationship between microhardness and tensile strength is discussed.

36 MATERIALS SCIENCE↗

Secondary carbides in high chromium cast irons: An alternative approach to their morphological and spatial distribution characterization

Highlights: • Systematic characterization of second phase particles by combining a variety of techniques • Comparison of morphological parameters obtained from SEM, BSE, etching+CLSM and EBSD • Quantitative analysis and degree of distribution of secondary carbides • Particle size, distribution and morphology from image analysis of CLSM, SEM and EBS images - Abstract: Secondary carbides precipitated in high chromium cast irons during thermal treatments were characterized by means of different characterization techniques, including scanning electron microscopy, energy dispersive X-ray spectroscopy, electron backscattered diffraction and a combination of chemical etching with confocal scanning laser microscopy. This set of techniques provides a full morphological, chemical and crystallographic description of the analysed phases. This work evaluated different methods for optimizing the image acquisition for a further image analysis (IA) based on the threshold binarization. Finally, the carbide size, distribution and morphology were determined after IA of the images acquired by aforementioned characterization techniques. Although the different techniques report some dispersion in the value for the average particle size, the particle inter-spacing and aspect ratio meet within the error value. The proposed characterization methodology provides statistically reliable data for a further evaluation of related physical properties in composites.

36 MATERIALS SCIENCE↗

Role of deformation temperature on the evolution and heterogeneity of texture during equal channel angular pressing of magnesium

Investigations on texture evolution and through-thickness texture heterogeneity during equal channel angular pressing (ECAP) of pure magnesium at 200 °C, 150 °C and room temperature (RT) was carried out by neutron, high energy synchrotron X-ray and electron back-scatter diffraction. Irrespective of the ECAP temperature, a distinctive basal (B) and pyramidal (C{sub 2}) II type of fibers forms. The texture differs in the bottom 1 mm portion, where the B-fiber is shifted ~ 55° due to negative shear attributed to friction. - Highlights: • ECAP of magnesium was carried out at 200 °C, 150 °C and room temperature. • Microstructure and micro-texture evolution was examined using EBSD in FEG–SEM. • Bulk-texture was studied using neutron diffraction and compared with micro-texture. • Through thickness texture heterogeneity was observed by synchrotron radiation. • Changes in these parameters with respect to deformation temperature are discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure development in a high-nickel austenitic stainless steel using EBSD during in situ tensile deformation

Highlights: • The number of low angle boundaries increases significantly at strains ≥ 9.5%. • Grain rotation was observed to lead to grain subdivision and even fragmentation. • Annealing twins deform due to accumulation of dislocations near their boundaries. • No deformation twins were observed and deformation took place by dislocation slip. - Abstract: Plastic deformation of surface grains has been observed by electron backscatter diffraction technique during in situ tensile testing of a high-nickel austenitic stainless steel. The evolution of low- and high-angle boundaries as well as the orientation changes within individual grains has been studied. The number of low-angle boundaries and their respective misorientation increases with increasing strain and some of them also evolve into high-angle boundaries leading to grain fragmentation. The annealing twin boundaries successively lose their integrity with increasing strain. The changes in individual grains are characterized by an increasing spread of orientations and by grains moving towards more stable orientations with <111> or <001> parallel to the tensile direction. No deformation twins were observed and deformation was assumed to be caused by dislocation slip only.

36 MATERIALS SCIENCE↗

Effect of cold deformation on the recrystallization behavior of FePd alloy at the ordering temperature using electron backscatter diffraction

In this study, the evolution of the recrystallization texture and microstructure was investigated after annealing of 50% and 90% cold-rolled FePd alloy at 530 °C. The FePd alloy was produced by vacuum arc melting in an atmosphere of 97% Ar and 3% H{sub 2}. The specimens were cold rolled to achieve 50% and 90% reduction in thickness. Electron backscatter diffraction measurements were performed on the rolling direction–normal direction section. With increased deformation from 50% to 90%, recrystallized texture transition occurs. For the 50% cold-rolled alloy, the preferred orientation is (0 1 0) [11 0 1], which is close to the cubic orientation after 400 h of annealing. For the 90% cold-rolled alloy, the orientation changes to (0 5 4) [22–4 5] after 16 h of annealing. - Highlights: • Texture and microstructure in cold-rolled FePd alloy was investigated during annealing using EBSD. • The recrystallized texture of 50% cold-rolled FePd is (0 1 0) [11 0 1] at 530 °C for 400 hours. • The recrystallized texture of 90% cold-rolled FePd is changed to (0 5 4) [22–4 5] at 530 °C after 16 hours.

36 MATERIALS SCIENCE↗

Three-dimensional EBSD characterization of thermo-mechanical fatigue crack morphology in compacted graphite iron

In cylinder heads made of compacted graphitic iron (CGI), heating and cooling cycles can lead to localized cracking due to thermo-mechanical fatigue (TMF). To meticulously characterize the complex crack path morphology of CGI under TMF condition, in relation to microstructural features and to find out how and by which mechanisms the cracks predominantly develop, three-dimensional electron back scattering diffraction (EBSD) was employed. Based on the precise quantitative microstructural analysis, it is found that graphite particles not only play a crucial role in the crack initiation, but also are of primary significance for crack propagation, i.e. crack growth is enhanced by the presence of graphite particles. Furthermore, the density of graphite particles on the fracture plane is more than double as high as in any other arbitrary plane of the structure. The obtained results did not indicate a particular crystallographic preference of fracture plane, i.e. the crystal plane parallel to the fracture plane was nearly of random orientation. - Highlights: • Crystallographic features of a thermo-mechanical fatigue (TMF) crack were studied. • Wide-field 3D EBSD is used to characterize the TMF crack morphology. • Data processing was applied on a large length scale of the order of millimeters. • Graphite density in the fracture plane is much higher than any other random plane. • It is revealed that crack growth is enhanced by the presence of graphite particles.

36 MATERIALS SCIENCE↗

Relationship between morphologies and orientations of Cu{sub 6}Sn{sub 5} grains in Sn3.0Ag0.5Cu solder joints on different Cu pads

The morphologies and orientations of Cu{sub 6}Sn{sub 5} intermetallic compounds in the Sn3.0Ag0.5Cu solder joints both on polycrystalline and single crystal Cu pads under different peak reflow temperatures and times above liquids were investigated. The relationship between Cu{sub 6}Sn{sub 5} grain orientations and morphologies was clarified. At the interface of Sn3.0Ag0.5Cu/polycrystalline Cu pad, scalloped Cu{sub 6}Sn{sub 5} intermetallic compounds formed at 250 °C and roof shape Cu{sub 6}Sn{sub 5} formed at 300 °C. Both scalloped Cu{sub 6}Sn{sub 5} and roof shape Cu{sub 6}Sn{sub 5} had a preferred orientation of (0001) plane being parallel to polycrystalline Cu pad surface. Besides, the percentage of large angle grain boundaries increased as the peak reflow temperature rose. At the interface of Sn3.0Ag0.5Cu/(111) single crystal Cu pad, the Cu{sub 6}Sn{sub 5} intermetallic compounds were mainly scallop-type at 250 °C and were prism type at 300 °C. The prismatic Cu{sub 6}Sn{sub 5} grains grew along the three preferred directions with the inter-angles of 60° on (111) single crystal Cu pad while along two perpendicular directions on (100) single crystal Cu pad. The orientation relationship between Cu{sub 6}Sn{sub 5} grains and the single crystal Cu pads was investigated by electron backscatter diffraction technology. In addition, two types of hollowed Cu{sub 6}Sn{sub 5} intermetallic compounds were found inside the joints of polycrystalline Cu pads. The long hexagonal Cu{sub 6}Sn{sub 5} strips were observed in the joints reflowing at 250 °C while the hollowed Cu{sub 6}Sn{sub 5} strips with the ‘▪’ shape cross-sections appeared at 300 °C, which was attributed to the different grain growth rates of different Cu{sub 6}Sn{sub 5} crystal faces. - Highlights: • The orientation of interfacial Cu{sub 6}Sn{sub 5} grains was obtained by EBSD technology. • Two types of hollowed Cu{sub 6}Sn{sub 5} strips were found at different temperatures. • The formation mechanism of hollowed Cu{sub 6}Sn{sub 5} was elaborated based on Bravais law. • The relationship between Cu{sub 6}Sn{sub 5} grain orientations and morphologies was clarified.

36 MATERIALS SCIENCE↗

Residual-stress-induced grain growth of twinned grains and its effect on formability of magnesium alloy sheet at room temperature

A magnesium alloy sheet was subjected to in-plane compression along with a vertical load to avoid buckling during compression. Pre-compressed specimens machined from the sheet were annealed at different temperatures and the changes in microstructure and texture were observed using electron back scattered diffraction (EBSD). Twinned grains preferentially grew during annealing at 300 °C, so that a strong texture with the < 0001 > direction parallel to the transverse direction developed. EBSD analysis confirmed that the friction caused by the vertical load induced inhomogeneous distribution of residual stress, which acted as an additional driving force for preferential grain growth of twinned grain during annealing. The annealed specimen showed excellent formability. - Highlights: • A magnesium alloy sheet subjected to in-plane compression under a vertical load • The vertical load induced inhomogeneous distribution of the residual stress. • The residual stress acted as an additional driving force for grain growth. • The annealed specimen with strong non-basal texture showed excellent formability.

36 MATERIALS SCIENCE↗

Evolution of microstructure and microtexture during hot deformation in an advanced P/M nickel base superalloy

Highlights: • Microstructural evolution of PM superalloy sensitive to temperature and strain rate. • Highest DRX with finer grained structure at higher temperatures and strain rates. • Dominance of DDRX showed by serrated grain boundaries and misorientation gradient. • Weak microtextural evolution inclined towards [110] fiber compression texture seen. In the present study, the effect of hot deformation parameters on the microstructural evolution is investigated for an experimental powder metallurgy nickel superalloy. The hot isostatically pressed (HIPed) alloy is isothermally hot compressed at constant true strain rate over wide temperatures (1000 °C, 1050 °C, 1100 °C, 1150 °C) and strain rates (0.001 s{sup −1}, 0.01 s{sup −1}, 0.1 s{sup −1}, 1 s{sup −1}) regimes. Electron Back-Scattered Diffraction (EBSD) characterization of the hot deformed samples is carried out to evaluate the microstructural evolution, grain boundary characteristics, and microtextural behaviour. The strong dependence of dynamic recrystallization characteristics on the hot deformation conditions is divulged through EBSD derived colour inverse pole figure maps endorsed by grain/twin boundary characteristics and misorientation gradient. Dynamic recrystallization (DRX) is maximized at higher deformation temperatures, whereas limited DRX is observed at lower deformation temperatures, especially at higher strain rates. The dominance of discontinuous dynamic recrystallization (DDRX) is manifested through bulged/serrated grain boundaries resulting in the formation of necklace microstructure corroborated by grain boundary cumulative misorientation gradient. Although random microtexture is revealed in both deformed and recrystallized microstructures, the tendency towards the formation of 110 fiber compression texture is apparently evident.

36 MATERIALS SCIENCE↗

Correlative characterization of primary particles formed in as-cast Al-Mg alloy containing a high level of Sc

Primary particles formed in as-cast Al-5Mg-0.6Sc alloy and their role in microstructure and mechanical properties of the alloy were investigated using optical microscopy (OM), scanning electron microscopy (SEM), electron back-scatter diffraction (EBSD) and tensile testing. It was found that primary particles due to a close orientation to matrix could serve as the potent heterogeneous nucleation sites for α-Al during solidification and thus impose a remarkable grain refinement effect. Eutectic structure consisted of layer by layer of ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ and cellular-dendritic substructure were simultaneously observed at the particles inside, indicating that these particles could be identified as the eutectics rather than individual Al{sub 3}Sc phase. A calculating method, based on EBSD results, was introduced for the spatial distribution of these particles in matrix. The results showed that these eutectic particles randomly distributed in matrix. In addition, the formation of primary eutectic particles significant improved the strength of the Al-Mg alloy in as-cast condition, which is ascribed to the structural evolution from coarse dendrites to prefect fine equiaxed grains. On the other hand, these large-sized particles due to the tendency to act as the microcrack sources could cause a harmful effect in the ductility of Al-Mg-Sc alloy. - Highlights: •Primary particles exhibit an ‘Al{sub 3}Sc + α-Al + Al{sub 3}Sc + ⋯’ multilayer feature with a cellular-dendritic mode of growth. •EBSD analyses the mechanism of grain refinement and the distribution of primary particles in α-Al matrix. •A computational method was presented to calculate the habit planes of primary particles.

36 MATERIALS SCIENCE↗

Analysis of the extent of interphase precipitation in V-HSLA steels through in-situ characterization of the γ/α transformation

In-situ characterization techniques have been applied to elucidate the influence of γ/α transformation upon the extent of interphase precipitation in a low-carbon, vanadium-HSLA steel. Electron Back-scattered diffraction analyses of the γ/α orientation relationship with continuous cooling at 2 and 10 K/s suggest that the proportion of ferrite likely to hold interphase precipitation varies little with cooling rate. However, TEM analyses show that the interphase precipitation refines with increasing cooling rate in this cooling range. With cooling rates in excess of 20 K/s, interphase precipitation is increasingly suppressed due to the increasingly diffusional-displacive nature of the Widmanstätten γ/α transformation that is activated. The present study illustrates that the extent and dimensions of interphase precipitation can be controlled through controlled cooling. - Highlights: • In-situ characterization of γ/α transformation • EBSD characterization of γ/α transformation orientation relationship • Extent of interphase precipitation can be controlled through controlled cooling.

36 MATERIALS SCIENCE↗

Effect of short-range order on microstructure, texture and strain hardening of cold drawn Cu-10 at.%Mn alloy

Highlights: • Excluding the effect of stacking fault energy, short-range order effect is discussed solely. • Short-range order is beneficial for twinning and slip planarity. • Short-range order promotes the formation of <111> fiber texture. • Strain hardening improving by short-range order. - Abstract: The aim of the present study is to investigate the effect of short-range order (SRO) on the microstructural evolution and mechanical property of Cu-10 at.%Mn alloy during cold drawing deformation. Characterization of the cold drawn Cu-10 at.%Mn alloy samples were performed using transmission electron microscope (TEM) and electron back scattering diffraction (EBSD), and their hardness were also tested. The results show that SRO is beneficial for both twinning and the transition of dislocation glide from wavy slip to planar slip at the low strains. At the high strains, the wavy slip generates due to the destruction of SRO. SRO increases the volume fraction of <111> texture component and the critical strain threshold. Moreover, the presence of SRO significantly improves strain hardening by combining the effects of dislocation, deformation twinning and texture hardening, which results in a significant increase of hardness.

36 MATERIALS SCIENCE↗

Effects of V addition on recrystallization resistance of 7150 aluminum alloy after simulative hot deformation

The effects of different V contents (0.01 to 0.19 wt.%) on the recrystallization resistance of 7150 aluminum alloys during post-deformation heat treatment were investigated. The microstructural evolutions at as-cast, as-homogenized conditions and after post-deformation annealing were studied using optical, scanning electron and transmission electron microscopes and using the electron backscattered diffraction technique. The precipitation of Al{sub 21}V{sub 2} dispersoids was observed in alloys containing 0.11 to 0.19 wt.% V after homogenization. The dispersoids were mainly distributed in the dendrite cells, and the precipitate-free zones occurred in the interdendritic regions and near grain boundaries. V addition could significantly enhance the recrystallization resistance during post-deformation annealing, particularly in the presence of a great number of Al{sub 21}V{sub 2} dispersoids. Recrystallized grain growth was effectively restricted because of the dispersoid pinning effect. The alloy containing 0.15 wt.% V exhibited the highest recrystallization resistance amongst all V-containing alloys studied. - Highlights: • Investigated the effect of V level on microstructure and flow stress of 7150 alloys • Characterized microstructures using optical microscopy, SEM, TEM and EBSD • Described the precipitation behavior of V-dispersoids in the dendritic structure • Studied the V effect on recrystallization resistance during post heat treatment • V addition greatly enhanced the recrystallization resistance during annealing.

36 MATERIALS SCIENCE↗

Multiscale mechanical behavior and microstructure evolution of extruded magnesium alloy sheets: Experimental and crystal plasticity analysis

Highlights: • Experimental stress-strain responses were reproduced by CPFE simulation based on Voronoi grains on three strain paths. • Textures predicted by simulation were in accordance with the ones measured by EBSD at the strain of 0.085. • Deformation heterogeneity in slip-dominated cases was found more significant than that in twin-favored case. • For slip-dominated cases, both high m′ value and high SFs in adjacent grains are responsible for strain localization. - Abstract: A phenomenological crystal plasticity finite element (CPFE) model based on Voronoi grains was applied to reproduce basic deformation features of a hot-extruded magnesium alloy sheet under various strain paths. Corresponding experimental investigations, including mechanical tests, electron back scattered diffraction (EBSD) measurements and optical observation, were also carried out as either a validation or a supplement of the numerical results. Predicted average stress-strain responses and texture evolution are in good accordance with measured ones. Furthermore, deformation heterogeneity at the mesoscopic and intergranular scale were investigated based on the proposed model. At the mesoscale, the heterogeneity in the slip-dominated cases tends to develop continuously, whereas the heterogeneity is retarded in twin-favored deformation. At the intergranular scale, it is concluded from the slip-dominated case that a high slip-transfer parameter and high Schmid factors (SFs) of principal slip systems in adjacent grains could accommodate higher local strain.

36 MATERIALS SCIENCE↗