FePtCu alloy thin films: Morphology, L1{sub 0} chemical ordering, and perpendicular magnetic anisotropy

Rapid thermal annealing was applied to transform sputter-deposited Fe{sub 51}Pt{sub 49}/Cu bilayers into L1{sub 0} chemically ordered ternary (Fe{sub 51}Pt{sub 49}){sub 100-x}Cu{sub x} alloys with (001) texture on amorphous SiO{sub 2}/Si substrates. It was found that for thin film samples, which were processed at 600 Degree-Sign C for 30 s, the addition of Cu strongly favors the L1{sub 0} ordering and (001) texture formation. Furthermore, it could be revealed by transmission electron microscopy and electron backscatter diffraction that the observed reduction of the ordering temperature with Cu content is accompanied by an increased amount of nucleation sites forming L1{sub 0} ordered grains. The change of the structural properties with Cu content and annealing temperature is closely related to the magnetic properties. While an annealing temperature of 800 Degree-Sign C induces strong perpendicular magnetic anisotropy (PMA) in binary Fe{sub 51}Pt{sub 49} films, the addition of Cu systematically reduces the PMA. However, due to the enhancement of both the A1-L1{sub 0} phase transformation and the development of the (001) texture with increasing Cu content, lowering of the annealing temperature leads to a shift of the maximum perpendicular magnetic anisotropy towards alloys with higher Cu content. Thus, for an annealing temperature of 600 Degree-Sign C, the highest perpendicular magnetic anisotropy energy is found for the (Fe{sub 51}Pt{sub 49}){sub 91}Cu{sub 9} alloy. The smooth surface morphology, adjustable PMA, and high degree of intergranular exchange coupling make these films suitable for post-processing required for specific applications such as for sensorics or magnetic data storage.

36 MATERIALS SCIENCE↗

Structural Characterization of Nb Films Deposited by ECR Plasma Energetic Deposition on Crystalline Insulators

An energetic condensation thin film coating technique with an electron cyclotron resonance (ECR) induced plasma ion source is used to deposit Nb thin films on crystalline insulating substrates, such as a-plane and c-plane sapphire (Al2O3) and on magnesium oxide, MgO (100), (110) and (111). Heteroepitaxial Nb films were produced by ECR deposition with regulated substrate temperature. The residual resistance ratio (RRR) of about 1 micron thick films reach unprecedented values (350 - 450) on (11-20) sapphire substrates. The epitaxial relationship of Nb/crystalline substrate is found to be strongly influenced by the substrate bias voltage (adding to the initial Nb+ kinetic energy), the substrate crystalline orientation, and heating conditions. At low substrate temperature, the Nb films demonstrated non-epitaxial crystalline textures, revealed by XRD Pole Figure technique and Electron Backscattering Diffraction (EBSD). The texture might be caused by ?Volmer-Weber? growth mode, i.e. island growth, at low surface adatom mobility. This study shows that the film?s crystal structural character has great impact on its RRR/Tc value, which in turn is related to the electron-mean-free-path of radio-frequency superconductivity. The knowledge learned from this research sheds some light on how to coat low-defect density Nb thin films on SRF cavity-preferred metallic substrates, such as Cu.

Zhao, X.↗

NSUF RTE completion report for 23-4780: Microstructural Defect Induced Thermal Conductivity Reduction in Uranium Nitride and Thorium Nitride

Uranium nitride (UN) is known to have a higher thermal conductivity than traditional oxide fuels, which could lead to a more efficient energy transport and lower local temperature during its lifetime. But the thermal transport performance of UN in extreme environments has not been systematic studied. This study investigated the irradiation induced microstructural defects in UN and the impacts on thermal conductivity. The samples were produced by spark plasma sintering at University of Texas-San Antonio (UTSA), Los Alamos National Laboratory (LANL), and Idaho National Laboratory (INL). Thermal conductivity of UN before and after 2MeV proton irradiation were measured by using laser metrology at INL in a temperature range of 77-295K. Thermal conductivity measurements in this wide, cryogenic temperature range is critical to understand the phonon scattering mechanisms between the thermal energy carrier, phonons, and different types of irradiation-induced defects. In order to ensure the measurements were conducted in the same grains and minimize the impact of the local heterogeneities, the measurement locations were highlighted by fiducial marks using the focused ion beam (FIB) with grain orientation identified using the electron backscatter diffraction (EBSD) at the Center of Advanced Energy Studies (CAES). Irradiation experiment was conducted at the Ion Beam Laboratory at Texas A&M University (TAMU). A total of 6 samples were irradiated with different irradiation doses and temperatures. After irradiation, the microstructure was characterized by using Transmission Electron Microscope (TEM) at CAES (also in the FIB marks).

36 - MATERIALS SCIENCE↗

Three-dimensional analysis by serial sectioning of cubic zirconia sinters

Three-dimensional electron backscatter diffraction technique was used for the characterization of grain boundary geometry and pore morphology in cubic zirconia. A set of three samples composed of cubic yttria stabilized zirconia, sintered under different conditions was investigated. Analysis of grain boundaries and pore structure was carried out in a dual-beam scanning electron microscope. For each sample, a volume of 15·10{sup 3} μm{sup 3} was investigated. The results of three-dimensional microstructure analysis were compared to the results derived from regular, two-dimensional maps of the area of 2500 µm{sup 2}. Based on two-dimensional and three-dimensional data the average grain diameter, number of grains, average number of neighbors and porosity were calculated. The average grain diameter varied in the range from 2.39 µm to 2.91 µm and from 3.00 µm to 3.79 µm, while the level of porosity varied in the range from 1.22% to 1.77% and from 1.30% to 5.61% for two-dimensional and three-dimensional data, respectively. The analysis of grain boundary networks revealed a strong dependence between grain boundary density and sample preparation parameters. The parameters of the sintering process affected also the size and distribution of pores. The comparison of the results of 2D and 3D materials characterization revealed significant differences in the values of calculated microstructure parameters.

36 MATERIALS SCIENCE↗

Microstructure of selective laser melted CM247LC nickel-based superalloy and its evolution through heat treatment

The selective laser melting of high temperature alloys is of great interest to the aerospace industry as it offers the prospect of producing more complex geometries than can be achieved with other manufacturing methods. In this study, the microstructure of the nickel-based superalloy, CM247LC, has been characterised following selective laser melting and after a post deposition heat treatment below the γ′ solvus temperature. In the as-deposited state, scanning electron microscopy with electron backscatter diffraction revealed a fine, cellular microstructure with preferential alignment of 〈001〉 along the build direction. A high dislocation density was seen at the periphery of the cells, indicating substantial localised deformation of the material. Fine primary MC carbides were also observed in the inter-cellular regions. High-resolution transmission electron microscopy identified the occurrence of very fine γ′ precipitates, approximately 5 nm in diameter, dispersed within the gamma phase. After heat treatment, the elongated cell colonies were observed to partially coalesce, accompanied by a decrease in dislocation density, producing columnar grains along the build direction. Cuboidal γ′ precipitates approximately 500 nm in diameter were observed to form in the recrystallised grains, accompanied by larger γ′ precipitates on the grain boundaries.

36 MATERIALS SCIENCE↗

BiFeO{sub 3}/La{sub 0.7}Sr{sub 0.3}MnO{sub 3} heterostructures deposited on spark plasma sintered LaAlO{sub 3} substrates

Multiferroic BiFeO{sub 3} (BFO)/La{sub 0.7}Sr{sub 0.3}MnO{sub 3} heterostructured thin films were grown by pulsed laser deposition on polished spark plasma sintered LaAlO{sub 3} (LAO) polycrystalline substrates. Both polycrystalline LAO substrates and BFO films were locally characterized using electron backscattering diffraction, which confirmed the high-quality local epitaxial growth on each substrate grain. Piezoforce microscopy was used to image and switch the piezo-domains, and the results are consistent with the relative orientation of the ferroelectric variants with the surface normal. This high-throughput synthesis process opens the routes towards wide survey of electronic properties as a function of crystalline orientation in complex oxide thin film synthesis.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Engineering of Nanoscale Heterogeneous Transition Metal Dichalcogenide–Au Interfaces

Engineering the transition metal dichalcogenide (TMD)–metal interface is critical for the development of two-dimensional semiconductor devices. By directly probing the electronic structures of WS 2 –Au and WSe 2 –Au interfaces with high spatial resolution, we delineate nanoscale heterogeneities in the composite systems that give rise to local Schottky barrier height modulations. Photoelectron spectroscopy reveals large variations (>100 meV) in TMD work function and binding energies for the occupied electronic states. Characterization of the composite systems with electron backscatter diffraction and scanning tunneling microscopy leads us to attribute these heterogeneities to differing crystallite orientations in the Au contact, suggesting an inherent role of the metal microstructure in contact formation. Here we then leverage our understanding to develop straightforward Au processing techniques to form TMD–Au interfaces with reduced heterogeneity. Our findings illustrate the sensitivity of TMDs’ electronic properties to metal contact microstructure and the viability of tuning the interface through contact engineering.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Characterization of Subsurface Microstructural Alterations Induced by Hard Turning of Inconel 718

Conventional machining especially hard turning is commonly used in aerospace industry to produce the final shape of cylindrical parts. However, the process generates damages and microstructural alterations on the surface and at the subsurface layer, in particular the cracking of hard carbides particles. The present paper focuses on investigating the probable mechanisms responsible for carbide cracking and the formation of a softened layer at a depth between 10 and 30 µm below the machined surface. Advanced techniques, such as laser confocal microscopy and field emission gun scanning electron microscope equipped with in situ picoindenter and electron backscatter diffraction, were used to characterize and analyze the evolution of the microstructure in the affected layer and propose the possible governing mechanisms for the observations.

36 MATERIALS SCIENCE↗

Epitaxial growth of CdTe thin film on cube-textured Ni by metal-organic chemical vapor deposition

CdTe thin film has been grown by metalorganic chemical vapor deposition (MOCVD) on Ni(100) substrate. Using x-ray pole figure measurements we observed the epitaxial relationship of {111}CdTe// {001}Ni with [110]CdTe//[010]Ni and [112] CdTe//[100]Ni. The 12 diffraction peaks in the (111) pole figure of CdTe film and their relative positions with respect to the four peak positions in the (111) pole figure of Ni substrate are consistent with four equivalent orientational domains of CdTe with three to four superlattice match of about 0.7% in the [110] direction of CdTe and the [010] direction of Ni. The electron backscattered diffraction (EBSD) images show that the CdTe domains are 30 degrees orientated from each other.

GIARE, C↗

Development of Fe-9Cr Alloy via High-Energy Ball Milling and Spark Plasma Sintering

Iron and chromium powders were mixed and mechanically alloyed via high-energy ball milling for different time durations (2–20 h) to produce an alloy powder with a nominal composition of Fe-9Cr (wt.%). The milled Fe-9Cr powders were analyzed using scanning electron microscopy (SEM), x-ray diffraction (XRD) and transmission electron microscopy (TEM) to understand the impact of ball milling (BM) time on the characteristics of the milled powder. The optimized milled powder samples were then consolidated via spark plasma sintering (SPS) for different dwell times and temperatures. The density of consolidated samples was found to reach a maximum of 98%. Microstructural characterization of the SPS samples were performed using XRD, SEM, TEM and electron backscatter diffraction. This study highlights the principles and importance of high-energy BM and SPS of Fe-9Cr model alloy for the future development of more complex oxide dispersion-strengthened alloys for various applications including advanced nuclear reactor applications.

36 MATERIALS SCIENCE↗

Nanoindentation Investigation of Chloride-Induced Stress Corrosion Crack Propagation in an Austenitic Stainless Steel Weld

Transgranular chloride-induced stress corrosion cracking (TGCISCC) is a mounting concern for the safety and longevity of arc welds on austenitic stainless steel (AuSS) nuclear waste storage canisters. Recent studies have shown the key role of crystallography in the susceptibility and propagation of TGCISCC in SS weldments. Given that crystallography underlies mechanical heterogeneities, the mechanical-crystallographic relationship during TGCISCC growth must be understood. In this study, welded SS 304L coupons are loaded in four-point bend fixtures and then boiled in magnesium chloride to initiate TGCISCC. Nanoindentation mapping is paired with scanning electron microscopy (SEM) electron backscatter diffraction (EBSD) to understand the correlation between grain orientation, grain boundaries, and hardening from TGCISCC propagation. The nanoindentation hardness of individual grains is found to not be a controlling factor for TGCISCC propagation. However, intragranular hardness is generally highest immediately around the crack due to localized strain hardening at the crack tip. This work shows that nanoindentation techniques can be useful in understanding CISCC behaviors when paired with electron microscopy.

36 MATERIALS SCIENCE↗

Transmission Electron Microscopy of Magnetite Plaquettes in Orgueil

Magnetite sometimes takes the form of a plaquette - barrel-shaped stack of magnetite disks - in carbonaceous chondrites (CC) that show evidence of aqueous alteration. The asymmetric nature of the plaquettes caused Pizzarello and Groy to propose magnetite plaquettes as a naturally asymmetric mineral that can indroduce symmetry-breaking in organic molecules. Our previous synchrotron X-ray computed microtomography (SXRCT) and electron backscatter diffraction (EBSD) analyses of the magnetite plaquettes in fifteen CCs indicate that magnetite plaquettes are composed of nearly parallel discs, and the crystallographic orientations of the discs change around a rotational axis normal to the discs surfaces. In order to further investigate the nanostructures of magnetite plaquettes, we made two focused ion beam (FIB) sections of nine magnetite plaquettes from a thin section of CI Orgueil for transmission electron microscope (TEM) analysis. The X-ray spectrum imaging shows that the magnetite discs are purely iron oxide Fe3O4 (42.9 at% Fe and 57.1 at% O), which suggest that the plaquettes are of aqueous origin as it is difficult to form pure magnetite as a nebular condensate. The selected area electron diffraction (SAED) patterns acquired across the plaquettes show that the magnetite discs are single crystals. SEM and EBSD analyses suggest that the planar surfaces of the magnetite discs belong to the {100} planes of the cubic inverse spinel structure, which are supported by our TEM observations. Kerridge et al. suggested that the epitaxial relationship between magnetite plaquette and carbonate determines the magnetite face. However, according to our TEM observation, the association of magnetite with porous networks of phyllosilicate indicates that the epitaxial relationship with carbonate is not essential to the formation of magnetite plaquettes. It was difficult to determine the preferred rotational orientation of the plaquettes due to the symmetry of the cubic structure, however, we are able to observe small but consistent rotational orientation across several discs within a plaquette.

Chan, Q. H. S.↗

Understanding the Mechanism of Dynamic Recrystallization During High-Temperature Deformation in Nb-1Zr-0.1C Alloy

In the present investigation, a systematic study of the evolution of microstructure and crystallographic texture during hot deformation of Nb-1Zr-0.1C was carried out in the temperature range 1773-1973 K (1500-1700 °C) at different strain rates of 0.001, 0.01 and 0.1 s{sup −1}. The aim was to examine the mechanisms of dynamic recovery and recrystallization in a high-temperature range. A detailed microstructural analysis of the deformed samples was performed using the electron backscatter diffraction technique to study the occurrence and nature of various dynamic restoration processes; the different regimes of dynamic recovery and recrystallization were identified. The orientations of the dynamically recrystallized grains were found to be (001) .

36 MATERIALS SCIENCE↗

High dislocation density of tin induced by electric current

A dislocation density of as high as 10{sup 17} /m{sup 2} in a tin strip, as revealed by high resolution transmission electron microscope, was induced by current stressing at 6.5 x 10{sup 3} A/ cm{sup 2}. The dislocations exist in terms of dislocation line, dislocation loop, and dislocation aggregates. Electron Backscattered Diffraction images reflect that the high dislocation density induced the formation of low deflection angle subgrains, high deflection angle Widmanstätten grains, and recrystallization. The recrystallization gave rise to grain refining.

36 MATERIALS SCIENCE↗

Short communication on Kinetics of grain growth and particle pinning in U-10 wt.% Mo

Samples of a U-10Mo alloy was annealed at temperatures ranging from 700 °C to 900°C for periods lasting up to 24 hours. Annealed microstructures were examined using Electron Backscattered Diffraction (EBSD) to obtain average grain sizes and grain size distributions. From the temporal evolution of the average grain size, the activation energy of grain growth was determined to be 172.4 ± 0.961 kJ/mol. Grain growth over the annealing period stagnated after a period of 1 to 4 hours. This stagnation is apparently caused by the pinning effect of second-phase particles in the materials. In conclusion, back-scattered electron imaging (BSE) was used to confirm that these particles do not appreciably coarsen or dissolve during annealing at the aforementioned temperatures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced electromechanical coupling in Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-PbTiO{sub 3} <001>{sub C} radially textured cylinders

We demonstrate Pb(Mg{sub 1/3}Nb{sub 2/3})O{sub 3}-PbTiO{sub 3} cylinders with ∼98% <100>{sub C} texture along the radial direction. A giant enhancement in the magnitude of electromechanical coupling factor (k{sub 31} = k{sub h} = 0.60, and k{sub l} = 0.7) was obtained for textured cylinder, and d{sub 31} × g{sub 31} was measured to be 6766 × 10{sup −15} m{sup 2}/N which is 3–6 times higher than that of commercial Pb(Zr,Ti)O{sub 3} compositions. The crystallographic grain orientation in the textured cylinder was visualized by electron backscatter diffraction, and the domain structure was characterized by piezoresponse force microscopy. Using these results, we explain the mechanism for this enhanced performance of radially textured piezoelectrics.

36 MATERIALS SCIENCE↗

Effect of Annealing Treatment on Mechanical and Magnetic Softening Behaviors of Cold Rolled Interstitial-Free Steel

The recovery and recrystallization behaviors of low-carbon interstitial-free steel are investigated at different annealing temperatures (200-690 °C) through correlation between the changes in magnetic parameters (coercivity and r.m.s. voltage), hardness, tensile strength and high-angle grain boundary fractions (HAB). Magnetic parameters and tensile strength show a significant change within recovery region (200-500 °C), while the hardness variation is very minimal at this temperature region. On the other hand, the hardness is abruptly changed compared to magnetic properties at higher annealing temperature (550-640 °C). The grain boundary characteristics and microtexture evolution occurring at recrystallization regime are evaluated by orientation imaging microscopy (OIM) and orientation distribution function (ODF) through electron backscattered diffraction (EBSD). The increase in recrystallization fraction noticeably affects microtexture property, justifying with the strengthening of γ-fiber, weakening of α-fiber and disappearance of rotated cube component with increasing annealing temperatures.

36 MATERIALS SCIENCE↗

Characterization of Static Recrystallization of a Ni-Cr-Mo-Based C276 Superalloy in Two-Stage Isothermal Compression

In order to clarify the microstructure evolution characteristics during holding period after slight degree of deformation for a Ni-Cr-Mo-based C276 superalloy, two-stage isothermal compression tests have been performed at the temperature range of 1000-1150 °C and the strain rate range of 0.1-5 s{sup −1}. The stress–strain curves and microstructure observation infer that both static recovery (SRV) and static recrystallization (SRX) took place during the holding period when the specimens were deformed at 1100-1150 °C and only SRV occurred in the specimens that deformed at the temperatures lower than 1100 °C. The softening effects increase with the increasing temperature and deformation degree, while the influence of strain rate seems less pronounced because of the limited stored energy resulted from the small deformation. The grain boundary characteristics, analyzed using electron backscatter diffraction technique, indicate that high densities of twins and Σ3 grain boundaries form associated with the nucleation and growth of SRX grains. Finally, the recrystallization during and after deformation, i.e., dynamic recrystallization, SRX and metadynamic recrystallization, was discussed concurrently.

36 MATERIALS SCIENCE↗