Search NASA⌕ Search

SEARCH · Search NASA

Results for “microstructure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 541 records · Page 30

Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing↗

Overcoming Anode Instability in Solid‐State Batteries through Control of the Lithium Metal Microstructure

Abstract Enabling the lithium metal anode (LMA) in solid‐state batteries (SSBs) is the key to developing high energy density battery technologies. However, maintaining a stable electrode–electrolyte interface presents a critical challenge to high cycling rate and prolonged cycle life. One such issue is the interfacial pore formation in LMA during stripping. To overcome this, either higher stack pressure or binary lithium alloy anodes are used. Herein, it is shown that fine‐grained ( d = 20 µm) polycrystalline LMA can avoid pore formation by exploiting the microstructural dependence of the creep rates. In a symmetric cell set‐up, i.e., LiǀLi 6.25 Al 0.25 La 3 Zr 2 O 12 (LLZO)ǀLi, fine‐grained LMA achieves > 11.0 mAh cm −2 compared to ≈ 3.6 mAh cm −2 for coarse‐grained LMA ( d = 295 µm) at 0.1 mA cm −2 and at moderate stress of 2.0 MPa. Smaller diffusion lengths (≈ 20 µm) and higher diffusivity pathway along dislocations ( D d ≈ 10 −7 cm 2 s −1 ), generated during cell fabrication, result in enhanced viscoplastic deformation in fine‐grained polycrystalline LMA. The electrochemical performances corroborate well with estimated creep rates. Thus, microstructural control of LMA can significantly reduce the required stack pressure during stripping. These results are particularly relevant for “anode‐free” SSBs wherein both the microstructure and the mechanical state of the lithium are critical parameters.

25 ENERGY STORAGE↗

Reactive Carbide‐Based Synthesis and Microstructure of NASICON Sodium Metal All Solid‐State Electrolyte

Reactive carbide precursor-based synthesis of NASICON-type NZSP (Na 1+x Zr 2 Si x P 3-x O 12 ) solid-state electrolyte (SSE) is demonstrated, in contrast to the established oxide-based approach. Exothermic decomposition of ZrC and SiC in air homogenizes microstructure, yielding 98% compact density after conventional sintering at 1200 °C. Quantitative stereology demonstrates that significant microstructural differences are present. Compacts of carbide-derived Carb-NZSP are 98% dense with a secondary zirconium oxide (ZrO 2 ) volume fraction of 0.2% ± 0.3%, versus 93% dense and 3% ± 1% for oxide-derived baseline. For Carb-NZSP, the secondary glassy phosphate phase is agglomerated, while for baseline, it is dispersed and percolated. Electrochemical testing combined with post-mortem analysis demonstrates how microstructural control of secondary phases is critical for dendrite suppression: Carb-NZSP critical current density (CCD) is 3.1 ± 0.8 mA cm −2 at 0.1 mAh cm −2 , versus 1.0 ± 0.7 mA cm −2 at 0.1 mAh cm −2 . Cryogenic focused ion beam (cryo-FIB) analysis demonstrates that in both materials, the porous 2D sheet-like sodium metal dendrites propagate around and subsume NZSP grains, likely following a path enriched with glassy phase and with porosity. Dendrites also flow around isolated zirconia particles. Phase field simulation reveals deflection of dendrites by mechanically tough zirconia, while brittle glassy phase accelerates dendrite growth, especially when finely distributed.

36 MATERIALS SCIENCE↗

Comparison of the Microstructure and Flux Pinning Properties of Polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} Containing Zn{sub 0.95}Mn{sub 0.05}O or Al{sub 2}O{sub 3} Nanoparticles

Here we compare the microstructure and flux pinning properties of polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} (Y-123 or YBCO) containing either Al{sub 2}O{sub 3} or Zn{sub 0.95}Mn{sub 0.05}O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticles were added up to a concentration of 0.1 wt%. The crystal structure, microstructure, electrical and magnetic properties were analyzed using X-ray diffraction, scanning electron microscopy and transmission electron microscopy (TEM), and electrical resistivity and DC magnetization measurements, respectively. TEM observations showed that the addition of Zn{sub 0.95}Mn{sub 0.05}O resulted in a high density of fine twins and a variety of interacting microstructures, while Al{sub 2}O{sub 3} addition resulted in a high density of Al-rich nanoscale inhomogeneities embedded in the Y-123 matrix. Flux pinning forces were determined, and predominant pinning mechanisms in the prepared samples were proposed. We evaluated the superconducting properties of YBCO considering the effects of adding insulating or magnetic nanoparticles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Impact of Defects in Powder Feedstock Materials on Microstructure of 304L and 316L Stainless Steel Produced by Additive Manufacturing

Recent work in both 304L and 316L stainless steel produced by additive manufacturing (AM) has shown that in addition to the unique, characteristic microstructures formed during the process, a fine dispersion of sub-micron particles, with a chemistry different from either the powder feedstock or the expected final material, are evident in the final microstructure. Such fine-scale features can only be resolved using transmission electron microscopy (TEM) or similar techniques. The present paper uses electron microscopy to study both the initial powder feedstock and microstructures in final AM parts. Special attention is paid to the chemistry and origin of these nanoscale particles in several different metal alloys, and their impact on the final build. Finally, comparisons to traditional, wrought material will be made.

36 MATERIALS SCIENCE↗

A Review on Friction Stir Processing of Titanium Alloy: Characterization, Method, Microstructure, Properties

In the past two decades, friction stir processing (FSP) technology has received considerable attention. FSP can be used to adjust and control the microstructure of materials, including eliminating defects, destroying dendrites and controlling fractions in the second stage, and is therefore widely used in titanium and its alloys for biomedical, aerospace and automotive applications. This article comprehensively reviews the methods of studying FSP, the microstructure evolution of materials and the summary of material properties. It begins with the introduction of the FSW system, characterization, structure and elemental analysis, and simulation and performance testing methods, and then introduces the microstructure evolution mechanism of various titanium materials and discusses in detail the material properties of titanium alloy, namely hardness and wear resistance, elasticity and plasticity, corrosion resistance and biocompatibility. Finally, this review presents unresolved issues and outstanding challenges in FSP technology and reveals the direction of this emerging field of research.

36 MATERIALS SCIENCE↗

Effect of Bainitic Microstructure on Ballistic Performance of Armour Steel Weld Metal Using Developed High Ni-Coated Electrode

Welding of armour steel has gained significant importance during the past few years as recent civilian and military requirements demand weld metal properties matching with base metal having good ballistic performance along with high strength and toughness at − 40 °C as per specification. The challenge of armour steel welding therefore lies in controlling the weld metal composition which is strongly dependent on welding electrode/consumables, resulting in desired weld microstructure consisting of lower bainite along with retained austenite. The performance of butt-welded armour steel joints produced by the developed electrodes was evaluated using tensile testing, ballistic testing, impact toughness at room temperature and subzero temperature. Microstructures of weld metals are exclusively characterized by x-ray diffraction technique, scanning electron microscope and transmission electron microscopy with selected area diffraction pattern. Experimental results show that weld metal with relatively lower carbon, higher manganese and lower nickel content was attributed to lower bainite with film type of retained austenite may be considered as a most covetable microstructure for armour steel weld metal.

36 MATERIALS SCIENCE↗

The Prediction of Microstructure Evolution of 6005A Aluminum Alloy in a P-ECAP Extrusion Study

Finite element modeling (FEM) was applied for predicting the recrystallized structure in extruded 6005 aluminum alloy, and simulated results were experimentally validated. First, microstructure evolution of 6005 aluminum alloy during deformation was studied by means of isothermal compression test, where the processing parameters were chosen to reproduce the typical industrial conditions. Second, microstructure evolution was analyzed, and the obtained information was used to fit a dynamic recrystallization model implementing inside the DEFORM-3D FEM code environment. FEM of deformation of 6005 aluminum has been established and validated by microstructure comparison. Finally, the obtained dynamic recrystallization model was applied to tube extrusion by using a portholes-equal channel angular pressing die. The finite element analysis results showed that coarse DRX grains occur in the extruded tube at higher temperature and in the extruded tube at the faster speed of the stem. The test results showed material from the front end of the extruded tube has coarse grains (60 μm) and other extruded tube has finer grains (20 μm).

36 MATERIALS SCIENCE↗

Microstructural Characterization, Mechanical Properties, and Corrosion Resistance of Dental Co-Cr-Mo-W Alloys Manufactured by Selective Laser Melting

In this paper, the microstructure, mechanical properties, and corrosion resistance of the dental Co-Cr-Mo-W alloys fabricated by selective laser melting (SLM) were systematically investigated and correlated. The microstructure of the SLM group (SG) specimens is composed of extremely fine columnar crystals, exhibiting supersaturated and homogeneous character. The matrix mainly consists of face-centered-cubic (FCC) cobalt solid solutions, and minimal hexagonal-close-packed (HCP) cobalt solid solutions. Mechanical test results showed that the 0.2% yield strength of SG was 775 ± 7 MPa, and the ultimate tensile strength was 1118 ± 25 MPa. The elongation of SG was 8.28 ± 0.4%, and the microhardness of SG was 476 ± 10 HV. All of these values largely exceeded the cast group (CG) specimens. The high strength is attributed to their fine columnar crystals and supersaturated matrices. The fewer content from the HCP phase and a lack of intermetallic compounds or eutectic contribute to the high ductility. Furthermore, a higher E{sub corr}, lower I{sub corr} were acquired for better corrosion resistance compared to cast specimens, due to even less composition segregation and more microstructural homogeneity.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Al-Mg-Sc-Zr Alloy Variable Polarity Plasma Arc Welding Joint

Al-Mg-Sc-Zr alloy plates were welded by variable polarity plasma arc welding (VPPAW) with Sc-containing filler wire. The microstructure and mechanical properties were investigated. Results show that the weld zone and heat-affected zone (HAZ) are narrow due to the high concentrated heat input of VPPAW. Primary Al{sub 3}(Sc,Zr) particles are nice nucleating sites for α-Al, which can significantly refine the grains of α-Al, helping the weld zone maintain an outstanding strength. The unmelted Al{sub 3}(Sc,Zr) precipitates of the base metal aggregated near the fusion boundary result in the formation of a fine equiaxed grains zone, which improves the bonding degree between the weld zone and the base metal. The Al{sub 3}(Sc,Zr) precipitates in the HAZ have excellent inhibition effect on recrystallization. According to the observed microhardness distribution and microstructure characteristics, the microstructure model of welded joint is obtained. The fractured position of welded joint locates in the weld zone. The tensile strength of the welded joint without reinforcing rib is 330 MPa. The welding coefficient reaches 74%.

36 MATERIALS SCIENCE↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

Processing, As-Cast Microstructure and Wear Characteristics of a Monotectic Al-Bi-Cu Alloy

Ternary Al-based monotectic alloys have a good combination of wear resistance and mechanical strength. While self-lubricating soft elements guarantee an adequate wear resistance, the modification with third elements can increase the ability to support load. In the present investigation, a collection of microstructures is generated through transient directional solidification of the Al-3.2wt.%Bi-3.0wt.%Cu alloy. Samples with different Bi spacing have been subjected to micro-adhesive wear ball tests. A relationship linking the wear volume, V, the microstructural spacing and the test time is proposed for Bi spacing higher than 16 μm, according to which V decreases with the decrease in Bi spacing. It is observed that wider and deeper grooves emerged on the surface of the samples related to more refined Bi and Al{sub 2}Cu phases, that is, associated with Bi spacing and Bi diameter lower than 16 and 2.4 μm, respectively. A reverse trend is noted for these finer microstructures, for which V increases with further decrease in Bi spacing. This can be caused by the detachment of the very fine and less cohesive Al{sub 2}Cu lamellas as the Al{sub 2}O{sub 3} oxide breaks up forming debris, with the presence of these lamellas as loose debris at the interface acting as third-body abrasives.

36 MATERIALS SCIENCE↗

Study on the Hot Deformation Behavior and Microstructure Evolution of Cu-Cr-In Alloy

Based on the hot compressive tests in the temperature range of 700-900 °C and strain rate range of 0.01-10 s{sup −1}, the hot deformation behavior of a Cu-Cr-In alloy was investigated. The true stress–strain curves of the alloy were obtained, and a constitutive equation for the alloy was established by the method of equivalent stress. The processing maps were constructed based on the constitutive equation, and the microstructural evolutions were analyzed and correlated with the processing maps. The results show that the true stress of the alloy increased with decreasing strain rate and decreased with increasing temperature. The microstructures of the alloy deformed under different conditions were in good accordance with the processing maps results. According to the processing maps and the microstructures of the alloy with true strains of 0.4 and 0.8, the optimal hot deformation conditions lie in the range of 850-900 °C and strain rate range of 0.01-0.1 s{sup −1}.

36 MATERIALS SCIENCE↗

A Study of Microstructure Evolution During Creep of 9Cr-1Mo Steel Using Ultrasonic and Hardness Measurements

In this work, microstructural changes during creep of 9Cr-1Mo steel were characterized using ultrasonic and hardness measurements. The creep testing of this steel was firstly performed at 873 K under the initial stresses of 160 and 175 MPa, respectively. Then, eight specimens under each stress level were prepared by the interrupted tests to simulate various creep states. Subsequently, two parameters of ultrasonic attenuation and velocity were introduced by the ultrasonic testing. Experiment results showed that regardless of the stresses, the ultrasonic attenuation experiences a peak at about 20% of the creep rupture time and a minimum value at about 50%, showing a strong correlation between ultrasonic attenuation and the creep life fraction. In addition to a slight increase during the primary creep, the ultrasonic velocity exhibits a significant change during the tertiary creep. Based on the analysis of microstructure changes, it indicated that the ultrasonic attenuation is significantly sensitive to the dynamic changes of the dislocation. In contrast, the velocity is mainly related to the evolution of precipitates. The Vickers hardness decreases monotonously during the creep process and presents a linear relation with the inverse of average diameter of M{sub 23}C{sub 6} carbides during the secondary and tertiary creep. Accordingly, it suggested that the present ultrasonic and hardness measurements provided a convenient tool to evaluate the microstructure evolution during creep degradation of heat-resistant steels.

36 MATERIALS SCIENCE↗

Microstructure and Properties of Mn-Cu-Based Damping Alloys Prepared by Ball Milling and Hot-Press Sintering

A Mn-Cu-based damping alloy with a nominal composition of 70Mn-24Cu-3Zn-3Al (at.%) was prepared by ball milling of pure elemental powders and subsequent hot-press sintering of powder mixture at 750 and 825 °C for 2 h. For comparison, this alloy was also prepared by induction melting technology and then homogenized at 850 °C for 24 h. Further, they were aged at 430 °C for 2 h. The microstructure, damping capacity and microhardness of the hot-press-sintered and induction-melted alloys have been investigated. The results show that the microstructure of the powder mixture upon ball milling mainly comprises convoluted composite particles containing α-Mn and γ-Cu phases, and isolated α-Mn ones around. The high compactness of the alloys is obtained after hot-press sintering (94.8 and 98.6% at 750 and 825 °C, respectively). At a holding temperature of 750 °C, the microstructure of the alloy is primarily composed of γ-MnCu, γ-CuMn and α-Mn grains. With increasing the target temperature to 825 °C, the single γ-MnCu solid solution has been formed in the alloy by diffusion of Mn etc. into γ-Cu lattices. The hot-press-sintered alloys (especially at 825 °C) possess relatively high damping capacity although which is still lower than that of induction-melted one. In contrast, the microhardness of the hot-press-sintered alloys (especially at 750 °C) is obviously higher than that of the induction-melted one.

36 MATERIALS SCIENCE↗

Effect of Forging on Microstructure, Mechanical Properties and Acoustic Emission Characteristics of Al Alloy (2014): 10 wt.% SiC{sub p} Composite

In this paper a systematic study has been undertaken to study the effect of forging on microstructure, mechanical properties and acoustic emission (AE) characteristics of Al alloy (2014)—10 wt.% SiC metal-matrix composites. Hammer forging was carried out at a temperature of 470 °C in an open die, with a deformation ratio of 3.5:1. Microstructural analyses were carried out at three different positions of forged billet. Significant material flow was observed in the sample taken from the sides of the forged billet, but no appreciable material flow was observed at the center of the forged billet. The microstructural characterization showed that forging resulted in cracking of SiC particles in Al alloy (2014)—10 wt.% SiC composite. The AE results during forging showed an increase in AE signal intensity during the initial yielding period and a subsequent decrease in the intensity of AE signals with sudden burst at the end of the forging. The plastic deformation at room temperature was less ductile in nature but at high temperature, appreciable ductility was observed. The FESEM micrographs of fracture surfaces of the tensile specimens showed appreciable clustering of SiC particles during plastic deformation both at room and high temperature.

36 MATERIALS SCIENCE↗

Laser 3D Printing of Fe-Based Bulk Metallic Glass: Microstructure Evolution and Crack Propagation

This work presents a comprehensive study of microstructure evolution, crack development and hardness performance of Fe-based bulk metallic glass parts processed by laser 3D printing. The combination of a low scan speed and high energy density generates a low temperature gradient, leading to supercooling and the formation of coarse dendrite and cellular crystal microstructure. Columnar dendrites grow in a single direction with large stress, and cracks are easily formed between the dendrites. The stress intensity factor (SIF) caused by the crack surface tension is small, the crack healing effect is weak, and it is difficult to prevent crack propagation. Cellular grain growth is uniform and more easily accommodates the strain, preventing crack initiation and propagation. In contrast, use of a high scan speed with low energy input produces a fine and uniform dendrite or even nanocrystalline, microstructure with microcracks. The SIF caused by the crack surface tension is large, and the crack healing effect is strong and prevents crack initiation and propagation. For low energy density, the hardness of the sample is similar to the hardness of the cast amorphous. This result indicates that the printing sample retained some amorphous characteristics.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of a SiO{sub 2} Ceramic and TC4 Alloy Joint Brazed with a Nanocomposite Filler

Vacuum brazing of TC4 alloy and SiO{sub 2} ceramic was achieved using a nano-AgCuNi braze alloy. The melting temperature of nano-AgCu powders was analyzed by differential scanning calorimeter. Furthermore, the effects of the Ni content on the microstructure and mechanical properties of the joints were studied. The results showed that the melting temperature of the nano-AgCu filler was 774 °C. A decrease in the melting temperature of 6 °C was observed, compared with the general AgCu filler, and this decrease enabled the interfacial reaction of the joint to begin earlier. The typical interfacial microstructure of the TC4/nano-AgCuNi/SiO{sub 2} ceramic joint brazed at 950 °C for 10 min was TC4/α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure/Ti{sub 2}(Cu,Ni) compound with α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure/Ti{sub 4}O{sub 7} + TiSi{sub 2}/SiO{sub 2} ceramics. The homogeneous microstructure of α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure primarily existed in the diffusion layer. Additionally, the refined α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure created via a eutectic reaction and Ti{sub 2}(Cu,Ni) compound was distributed in the brazing seam. The Ni content could influence the formation of Ti-Cu-Ni ternary intermetallic compounds (IMCs). An increase in Ni led to an increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure in the brazing seam. The shear strength of the brazed joints first increased and then decreased with the increase in the nano-Ni content, and the optimal shear strength of 30.1 MPa was achieved at 10 wt.% Ni. The increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure and the decrease in brittle compounds enhanced the shear strength of the joint. Fracture analysis of the joints brazed at 950 °C for 10 min indicated that the cracks mainly occurred in SiO{sub 2} ceramic.