In situ variable temperature X-ray diffraction studies on the transformations of nano-precursors to La-Ni-O phases
In situ variable temperature XRD (VT-XRD) measurements on the transformation of nano-precursors to La-Ni-O phases are presented. Experimental results showed that LaNiO{sub 3} and La{sub 2}NiO{sub 4} phases were formed at ca. 700 deg. C via the reaction of La{sub 2}O{sub 3} and NiO (from the initial nano-precursors), where a relatively low temperature of 700 deg. C was found for the synthesis of La{sub 2}NiO{sub 4}. The formation of La{sub 3}Ni{sub 2}O{sub 7} at higher temperature (up to 1150 deg.C) appeared to proceed through a further reaction of La{sub 2}NiO{sub 4} with unreacted NiO, whilst the formation of La{sub 4}Ni{sub 3}O{sub 10} (at 1075 deg. C) proceeded via a further decomposition of LaNiO{sub 3}. Although phase pure La{sub 3}Ni{sub 2}O{sub 7} and La{sub 4}Ni{sub 3}O{sub 10} were not directly obtained under the processing conditions herein, the results of this study allow for a better understanding of formation pathways, particularly for the higher order La-Ni-O phases. - Graphical abstract: In situ variable temperature XRD showing the phase formation pathway of La{sub n+1}Ni{sub n}O{sub 3n+1} at evaluated temperatures. Highlights: > In situ VT-XRD was utilized to study the pathways for La{sub n+1}Ni{sub n}O{sub 3n+1} formations. > LaNiO{sub 3} and La{sub 2}NiO{sub 4} phases were formed via the reaction of La{sub 2}O{sub 3} and NiO, respectively. > La{sub 3}Ni{sub 2}O{sub 7} phase was formed via further reaction of La{sub 2}NiO{sub 4} phase with unreacted NiO. > La{sub 4}Ni{sub 3}O{sub 10} phase was formed via further decomposition of LaNiO{sub 3} phase.