Corrosion Effects of Calcium Chloride Injection for Mercury Control on the Pollution Control Equipment

In response to the Clean Air Mercury Rule (CAMR) of 2005, Black Hills Power (BHP) initiated testing of a calcium chloride (CaCl{sub 2}) injection method in their Wygen 1 (Gillette, WY) coal-fired power plant to help lower mercury emissions. In 2006, Babcock & Wilcox (B&W) was contracted to test their CaCl{sub 2} technology in-situ by adding a CaCl{sub 2} solution onto the raw, pre-pulverized coal during normal operation of Wygen 1. Follow-up tests were conducted by BHP in 2007. Data were collected from these two time periods and analyzed by a collaborative investigation team from Western Research Institute (WRI) and the University of Wyoming (UW) to see if there were any effects on the current air pollution control systems. During a CaCl{sub 2} injection period in 2007, corrosion was monitored in the flue and recycle ash system by placing corrosion coupons in strategic locations to test if corrosion was enhanced by the CaCl{sub 2} injection. While the CaCl{sub 2} produced a reduction in stack mercury levels, there was some evidence of beneficial impacts on the removal of SO{sub 2} from the flue gas during CaCl{sub 2} injection. Data on NOx remained inconclusive. It was also discovered that corrosion was enhanced significantly in the Spray Drier Absorber (SDA) vessel and corresponding outlet ductwork during CaCl{sub 2} injections. Further studies are being carried out in the field and lab to better understand the corrosive effects of CaCl{sub 2} to help formulate operation controls to manage the increased corrosion rates.

01 COAL, LIGNITE, AND PEAT↗

Characterization of Encapsulated Corrosion Inhibitors for Environmentally Friendly Smart Coatings

Research efforts are under way to replace current corrosion inhibitors with more environmentally friendly alternatives. However, problems with corrosion inhibition efficiency, coating compatibility and solubility have hindered the use of many of these materials as simple pigment additives.This paper will present technical details on how the Corrosion Technology Lab at NASAs Kennedy Space Center (KSC) has addressed these issues by encapsulating environmentally friendly inhibitors into organic and inorganic microparticles and microcapsules. The synthetic process for polymer particles was characterized and post-synthesis analysis was performed to determine the interactions between the inhibitors and the encapsulation material. The pH-controlled release of inhibitors from various particle formulations in aqueous base was monitored and compared to both electrochemical and salt immersion accelerated corrosion experiment. Furthermore, synergistic corrosion inhibition effects observed during the corrosion testing of several inhibitor combinations will be presented.

Environmentally Friendly↗

Validation of the Modelling of Corrosion Driven Expansion in Grouted Waste-forms - 16125

One of the current preferred solutions for the disposal of Intermediate Level radioactive waste in the UK is grout encapsulation inside steel boxes for long term storage. These boxes are then to be entombed in a Geological Disposal Facility once one is available. However, both prior to and during geological disposal, waste contents can react with the water present in the encapsulant grout and begin to corrode. This corrosion product occupies a larger volume (by several hundred percent) than the original material and the corrosion occurs over the course of decades and centuries, long after the encapsulant grout has set and hardened. The expanding waste then creates stresses in the encapsulant causing both it and the surrounding box to deform and, in extreme circumstances, and after long times, for the structural integrity of the box to fail. This behaviour needs to be quantified before the box can be approved for use as any excessive deformation could lead to a loss of containment or, since the boxes are stacked on top of each other, to a significant accident in the stores. Due to the long timescales involved, physical testing of the phenomenon in full scale is impossible. Instead, a combination of chemical modelling and finite element analysis is used to predict the extent of the corrosion in the waste and its effect of the integrity of the box. There are a number of difficulties in modelling the corrosion-driven expansion and subsequent deformation of the boxes. Although the corrosion occurs over a very long time scale, the event is highly non-linear and dynamic. All of the material models, including the steel and grout are non-linear. The deformation is in the order of 10s of centimetres, well beyond the static elastic range. Finally, the components must be allowed to move relative to each other which involve a lot of part to part contacts. This means that simple static modelling, which would solve quite quickly, cannot be used. Instead a dynamic analysis code, LS-DYNA, has been used to expand the product over time to simulate the corrosion-driven expansion. This software is generally used for modelling car crashes or scenarios where waste containers have been dropped. The analyses therefore include a significant inertial component. This paper will detail the NNL's approach to modelling this long-term, quasi-static phenomenon in the dynamic, impact oriented software code LS-DYNA. It will cover the problems inherent in this approach, the errors that it creates as well as the tests and solutions that NNL worked on in order to overcome them and be confident that the solution could be validated. This work will ultimately be used to determine the maximum inventory which can be stored in each box based on the waste content and the potential extent of expansion as well as any modification that could be made to the box design or the processing streams that may improve the storage solution. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Chemistry Envelope for the Determination of Pitting Corrosion Susceptibility - 19554

Liquid radioactive wastes at the Hanford and Savannah River sites are stored in large underground carbon steel tanks. The high-level wastes are processed in several of the tanks and then transferred by piping to other site facilities for further processing before they are stabilized in a vitrified or grout waste form. Based on waste removal and processing schedules, many of the tanks, will be required to be in service for times exceeding the initial intended life (i.e., greater than 60 years). Until the waste is removed from storage, transferred, and processed, the materials and structures of the tanks must maintain a confinement function by providing a barrier to the environment and by maintaining acceptable structural stability during design basis events, which include loadings from both normal service and abnormal (e.g., earthquake) conditions. Administrative programs are in place to mitigate potential corrosion mechanisms and thereby maintain the structural and leak integrity functions of these waste tanks throughout their intended service life. Waste chemistry and temperature control are the means by which corrosion degradation of the waste tanks is minimized. Chemistry controls are based on in-situ coupon tests, waste tank experience, and laboratory testing. These requirements comprise the technical standards for corrosion control. The standards are utilized then as guidelines for operational procedures. The present waste chemistry controls for the Hanford DSTs were established in the 1980's in response to tank failures caused by stress corrosion cracking (SCC) at the DOE Savannah River Site (SRS). Portions of the SRS chemistry limits, which were developed at the Savannah River National Laboratory (SRNL) were coupled with corrosion testing results from Pacific Northwest National Laboratories (PNNL) and adopted for corrosion control of the double-shell tank (DST) waste at the Hanford Site. Since that time, the temperatures of the waste in the DSTs have decreased to less than 50 deg. C in most cases as the radioactive material has decayed. As a consequence, new chemistry controls were formulated for SCC in 2010. This testing however, did not address that potential for pitting in the supernatant and at the liquid-air interface. Indeed, initial tests indicated that the inhibitor requirements for SCC would be insufficient for the prevention of pitting. In addition to lower waste temperatures, future retrieval and process changes may impact the DST waste chemistry. Initial projections suggest that the waste chemistry of the DSTs may shift to a broader range of pH and higher aggressive anion concentrations (e.g., chloride, sulfate, etc.) than the wastes that are presently stored. Additionally, processes within the vitrification facility may result in streams that are returned to the tank farm for evaporation. These streams may also contain high concentrations of aggressive species. SRNL investigated the propensity for pitting of the carbon steel waste tanks at current and projected DST waste chemistries. A statistically designed series of tests provided a pitting factor that relates the ratio of the inhibitor species to the aggressive species and the probability of observing pitting. An acceptable pitting factor was determined and was utilized for the development of a new chemistry envelope. The new chemistry envelope was compared to the envelope that was established for SCC and was determined to be bounding. Validation of the new chemistry envelope was performed via model simulations and comparison with historical experimental results and approaches to establishing chemistry envelopes. The new chemistry envelope will eventually be part of an overall assessment of the condition of the tanks and any changes made to the overall structural integrity program for the Hanford DSTs. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

THE SENSITIVITY OF CARBON STEELS' SUSCEPTIBILITY TO LOCALIZED CORROSION TO THE PH OF NITRATE BASED NUCLEAR WASTES

The Hanford tank reservation contains approximately 50 million gallons of liquid legacy radioactive waste from cold war weapons production, which is stored in 177 underground storage tanks. The tanks will be in use until waste processing operations are completed. The wastes tend to be high pH (over 10) and nitrate based. Under these alkaline conditions carbon steels tend to be passive and undergo relatively slow uniform corrosion. However, the presence of nitrate and other aggressive species, can lead to pitting and stress corrosion cracking. This work is a continuation of previous work that investigated the propensity of steels to suffer pitting and stress corrosion cracking in various waste simulants. The focus of this work is an investigation of the sensitivity of the steels' pitting and stress corrosion cracking susceptibility tosimulant pH. Previous work demonstrated that wastes that are high in aggressive nitrate and low in inhibitory nitrite are susceptible to localized corrosion. However, the previous work involved wastes with pH 12 or higher. The current work involves wastes with lower pH of 10 or 11. It is expected that at these lower pHs that a higher nitrite-to-nitrate ratio will be necessary to ensure tank integrity. This experimental work involved both electrochemical testing, and slow strain rate testing at either the free corrosion potential or under anodic polarization. The results of the current work will be discussed, and compared to work previously presented.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of CO 2 and H 2 S on Corrosion of Martensitic Steels in Brines at Low Temperature

Corrosion studies were conducted for martensitic carbon steels in 5 wt% NaCl brine solutions at 4°C and 10 MPa (1,450 psi). These studies simulated different subsurface environments relevant to Arctic drilling. Here, two high-strength martensitic carbon steels, S-135 and UD-165, were studied in three different environments: (1) a CO 2 -NaCl-H 2 O solution with a CO 2 :H 2 O molar ratio of 0.312 in the whole system, (2) an H 2 S-NaCl-H 2 O solution with an H 2 S:H 2 O molar ratio of 3.12 × 10 –4 , and (3) a CO 2 -H 2 S-NaCl-H 2 O solution with the same acid gas to water ratios as environments 1 and 2. Results from the CO 2 +H 2 S mixed environment indicated that sour corrosion mechanism was dominant when the CO 2 :H 2 S molar ratio was 1,000. This impact of a small amount of H 2 S on the corrosion mechanism could be attributed to the specific adsorption of H 2 S on the steel surface. Electrochemical and mass loss measurements showed a distinct drop in the corrosion rate (CR) by more than one order of magnitude when transitioning from sweet to sour corrosion. This inhibiting effect on CR was attributed to the formation of a protective sulfide thin film. Tafel analyses of the anodic reaction showed that the Bockris mechanism was unlikely in the conditions tested. As a result, when comparisons were made between modeled and experimental CRs, good agreement was found in the CO 2 -only and H 2 S-only environments, but not in the CO 2 +H 2 S environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of Microadding Amine Surfactant on Erosion-Corrosion Wear of Structural Steel in NPP

Corrosion processes, specifically, erosion-corrosion, are one of the causes of damage occurring in NPP equipment during operation. Measures are taken to prevent erosion-corrosion wear of thermal-power equipment and pipelines. One such measure is the development and adoption of water chemistry regimes that are capable of forming a protective fi lm on a metal surface. Octadecylamine is one such reagent. The results of laboratory tests and industrial experiments studying the effect of octadecylamine on the development of erosion-corrosion wear of NPP equipment are presented. The octadecylamine-hydrazine water chemistry regime at octadecylamine concentration 0.5 mg/dm{sup 3} reduces the rate of erosion-corrosion wear by about 15-fold. The positive effect of micro-additions of octadecylamine is confirmed by direct erosion-corrosion studies performed at the Kola NPP.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Probabilistic modeling of the corrosion of steel structures in marine water-development works

Considering that corrosion takes place as a random process over time, a a probabilistic approach was utilized in this paper. The corrosion of metallic sheet piling employed in the fascia wall of a bulwerk is considered as an example. A stochastic model is constructed on the base of a modified Weibull distribution function with consideration of parameters of the corrosion process as a function of time. One of the factors defining the corrosion rate of the sheet piling is the degree of access of a section of the wall to the zone of variable water level, or the underwater zone. The type of corrosion-continuous or local-is another factor. The accuracy of corrosion prediction in the underwater zone is higher than that in the zone of variable water level.

36 MATERIALS SCIENCE↗

Atmospheric Corrosion Behavior and Mechanism of a Ni-Advanced Weathering Steel in Simulated Tropical Marine Environment

Corrosion behavior of Ni-advanced weathering steel, as well as carbon steel and conventional weathering steel, in a simulated tropical marine atmosphere was studied by field exposure and indoor simulation tests. Meanwhile, morphology and composition of corrosion products formed on the exposed steels were surveyed through scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction. Results indicated that the additive Ni in weathering steel played an important role during the corrosion process, which took part in the formation of corrosion products, enriched in the inner rust layer and promoted the transformation from loose γ-FeOOH to dense α-FeOOH. As a result, the main aggressive ion, i.e., Cl{sup −}, was effectively separated in the outer rust layer which leads to the lowest corrosion rate among these tested steels. Thus, the resistance of Ni-advanced weathering steel to atmospheric corrosion was significantly improved in a simulated tropical marine environment.

36 MATERIALS SCIENCE↗

Effect of Surface Treatment on Bio-corrosion in Aluminum Alloy 2024-T3

Bio-corrosion is one of the major problems faced in any engineering/aerospace industry. The present study focuses on understanding the effect of surface treatment on AA2024-T3 on bio-corrosion in aircraft fuel tanks. The microbial attack on aluminum alloy (2024-T3) in aircraft fuel tanks by Pseudomonas aeruginosa was studied. Substrates with (1) chromate-free surface treatment (anodization; 2) Ormosil coatings doped with inhibitors/derivatives known for antimicrobial properties were evaluated for their bio-corrosion protection efficiency as compared to bare coupons. The coupons were immersed in aviation fuel spiked with the test culture. The changes in chemical parameters of test solution like pH were monitored periodically. A probable relationship between number of organisms, changes in pH and the extracellular protein (hypothesized to be produced by organisms) were evaluated. Our studies indicated that pH did not appear to play a crucial role in biofilm formation. Surface morphology of bare and anodized AA2024-T3 coupons before and after electrochemical impedance studies (EIS) was analyzed using FE-SEM. Anodized samples with least i{sub corr} value of (0.075 × 10{sup −6} A cm{sup −2}) and corrosion rate of (0.12 × 10{sup −2} mm/y) after 60 days showed distinct corrosion protection than bare and the coated samples. Additional evidence in support of corrosion protection efficiency of anodized was obtained by the biofilm barrier efficiency of 98.94%.

36 MATERIALS SCIENCE↗

Welding Heat Input Influence on UNS S82441 Lean Duplex Stainless Steel Corrosion Resistance Assessed by Scanning Vibrating Electrode Technique (SVET)

The precipitation of the intermetallic phases can impair mechanical and corrosion properties. In the case of lean duplex stainless steels, they present solidification mode as primary ferrite, with austenite precipitation in the solid state, during cooling. This means the heat-affected zone balanced microstructure can be changed during the welding by the cooling rate, which is associated to the welding heat input, the thickness of the plate and the physical properties of the material. This work intends to present the influence of welding heat input on the corrosion resistance of UNS S82441 lean duplex stainless steel. The gas metal arc welding process was used to make the weld beads, using ER2209 as filler metal, which characterizes a dissimilar welded joint. The corrosion resistance of these specimens was analyzed through scanning vibrating electrode technique. It was observed that welding heat input variation distinctly influences corrosion in different zones of the weld beads over the specimen exposure time. The weld bead under intermediate welding heat input showed the highest corrosion rate and the one under the highest welding heat input, the lowest corrosion rate intensity.

36 MATERIALS SCIENCE↗

Effects of Solution Treatment on Microstructure Transformation, Tensile and Exfoliation Corrosion Properties of 7136 Aluminum Alloy

The effects of solution treatment on microstructure transformation and tensile properties of 7136 aluminum alloys were investigated by means of scanning electron microscopy, electron backscatter diffraction, differential scanning calorimeter, x-ray diffraction and tensile test, electrochemical evaluations, exfoliation corrosion tests, respectively. The results indicate that solution treatment had a significant effect on the microstructure transformation and tensile properties. Soluble constituents of 7136 aluminum alloys were more likely to form the η(MgZn{sub 2}) phase rather than the S(Al{sub 2}CuMg) phase. With increasing the solution temperature, the η phase was re-dissolved into the α(Al) matrix gradually. After solution treatment of 475 °C/1 h, the η phase was completely dissolved into the matrix, with insoluble Fe-rich phases remained. The dissolution of η phase would increase the strength and the corrosion resistance of the alloys. When continuing to increase the solution temperature, the recrystallized fraction increased obviously, resulting in the decrease in the strength and the corrosion resistance. Consequently, the strength and the corrosion resistance of the alloys increased firstly and then decreased with the increase in solution temperature. After solution treatment of 475 °C/1 h, the tensile strength and yield strength of the aged alloy reached their peaks, 738 and 715 MPa, respectively. The elongation of the alloy solution treated at 475 °C/1 h reached 11.2%, and its exfoliation corrosion rating got EB level. Furthermore, after the double-stage solution treatment of 450 °C/1 h + 475 °C/1 h, the recrystallized fraction decreased, resulting in a slight increase to 12.6% of the elongation, a slight increase in the corrosion resistance and a slight decrease in the strength.

36 MATERIALS SCIENCE↗

Effects of the Addition of Micro-amounts of Calcium on the Corrosion Resistance of Mg-0.1Mn-1.0Zn-xCa Biomaterials

Magnesium alloys have good biocompatibility and degradability, which are considered ideal characteristics of biomedical implants. However, there are few studies on the influence of the addition of micro-amounts of Ca on magnesium alloys. In this work, the effects of adding micro-amounts of Ca on the microstructure, mechanical properties, and corrosion properties of Mg-0.1Mn-1.0Zn-xCa (x = 0.1, 0.2, and 0.3 wt.%) alloys were investigated. The results reveal that the grain size of the alloy decreased and the yield strength and elongation both increased with increasing Ca concentrations. Corrosion tests in Kokubo simulated body fluid showed that the in vitro immersion rate first slowed down and then increased (6.395 → 6.283 → 6.395 mm/year) with increasing Ca concentrations. This phenomenon was due to the addition of Ca causing grain refinement, which slowed the corrosion rate and generated an Mg{sub 2}Ca phase to accelerate corrosion. The second-phase Mg{sub 2}Ca precipitated at the grain boundary and acted as a cathode, and the metal magnesium phase acted as an anode to form a primary battery, which caused corrosion of the magnesium phase and accelerated the corrosion rate.

36 MATERIALS SCIENCE↗

Effects of Zr Ion Implantation on Surface Mechanical Properties and Corrosion Resistance of Pure Magnesium

Zirconium (Zr) was implanted into pure Mg by metal vapor vacuum arc (MEVVA) at the dose of 2 × 10{sup 16} ions/cm{sup 2} at room temperature. The surface characteristics of Zr-implanted Mg were analyzed by the Stopping and Range of Ions in Matter software (SRIM) and x-ray photoelectron spectroscopy (XPS), the surface nanohardness and tribological behavior were measured through nanoindentation and a friction-abrasion testing machine, and the corrosion resistance of Zr-implanted Mg was evaluated by electrochemical measurement and immersion test in simulated body fluid (SBF). The results demonstrated that a gradient modified layer composed of MgO, Mg(OH){sub 2}, ZrO{sub 2} and Zr was formed on the near surface of pure Mg and the nanohardness of pure Mg was improved by 48%. Furthermore, the Zr-implanted Mg exhibited a more positive corrosion potential of − 1.43 V (versus SCE) and a lower corrosion current density of 19.9 μA/cm{sup 2}, and localized corrosion was effectively retarded during 24 h immersion in SBF, suggesting that the corrosion resistance of pure Mg was remarkably improved after Zr ion implantation. The mechanisms of surface strengthening and improved corrosion resistance were also discussed in this paper.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Annealed Steels with Different Carbon Contents (0.002, 0.17, 0.43 and 0.7% C) in Freely Aerated 3.5% NaCl Solution

Four annealed carbon steels with different carbon contents (0.002, 0.17, 0.43, and 0.7% C), consisting of ferrite, ferrite-pearlite and fully pearlite microstructures, were selected to understand the corrosion behavior of carbon steel as a function of carbon content in freely aerated 3.5% NaCl solution. Dynamic polarization, electrochemical impedance and linear polarization methods were used. The corrosion rate obtained from the different carbon steels was found to increase greatly from ultra-low carbon steel (0.002%) to low carbon steel (0.17%) due to the presence of pearlite in the low carbon steel. However, the increase in corrosion rate was marginal with the increase in carbon content from low carbon (0.17%) to medium (0.43% C) and high carbon steels (0.7% C). The mirostrucural evolution of the steels before and after polarization test without etching as observed by scanning electron microscopy could show that the corrosion behavior of the steels with the presence of pearlite was due to the combined effect from % pearlite, interlamellar spacing and cementite/ferrite area ratio in pearlite. Pearlite morphology also led to the differential corrosion within the pearlite colony in all the steels except the steel with 0.002% C. Catalytic activity of cementite on enhancing oxygen reduction reaction attributes to the higher corrosion rates in case of the steels with the presence of pearlite.

36 MATERIALS SCIENCE↗

Investigation of Corrosion of 304 Stainless, Inconel 625, and Haynes 230 in a Chloride-Salt-Based Thermal Storage Medium

One of the critical challenges for latent heat thermal energy storage systems in concentrating solar power applications is corrosion of metallic alloys as containment and heat transfer fluid tube materials in corrosive salts at high temperatures. In this study, the effects of MgCl 2 on the corrosion of stainless steel 304, Inconel 625, and Haynes 230 alloys were investigated through embedded metal samples in the graphite foam/MgCl 2 storage medium. Four experimental testing modules were fabricated, and experimental tests were conducted under controlled environment by heating the testing modules to and keeping them at 750 °C for 100, 200, 500, and 1000 h. The estimated corrosion rates based on the weight losses for stainless steel 304, Inconel 625, and Haynes 230 were 94, 9, and 8 μm/year, respectively. The fitted equations for the loss of the thickness as functions of the exposure time show that the corrosion rates decrease with the exposure time. Additionally, the results on the corrosion zones or depths and chromium segregation ranges of the experimental samples are also presented.

36 MATERIALS SCIENCE↗

Corrosion of Mild Steel Buried Underground for 3 Years in Different Soils of Varying Textures

The effect of moisture content and soil texture on the corrosion behavior of mild steel coupons buried for 3 years in different soils was estimated from weight loss measurements and electrochemical techniques such as Tafel plots and electrochemical impedance spectroscopy. The results showed that the rate of corrosion and intensity of corrosion attack significantly depend on the soil’s moisture content and on the soil type. Corrosion was found to be severe in clayey soil compared to that in mixed and sandy soils. Morphological analysis of the corroded specimens performed using optical microscopy and scanning electron microscopy showed the presence of amorphous oxides and low-intense crystalline phases of goethite and hematite on the surface of the mild steel coupons, indicating only the initial stage of corrosion. It is concluded from this study that mild steel undergoes only less intense surface-level corrosion in 3 years when buried underground.

36 MATERIALS SCIENCE↗

Corrosion Response of Ni-19Cr-5Fe in Molten NaCl-MgCl 2 Salt

Ni-based alloys are strong candidates for use in high-temperature molten salt reactors due to their superior corrosion resistance and mechanical stability compared to stainless steels. In this study, the static corrosion behavior of a Ni-19Cr-5Fe model alloy was systematically evaluated in a purified molten NaCl-MgCl 2 salt at 700°C for 30, 240, and 500 h. Post-exposure analyses were conducted to assess microstructural evolution, corrosion depth, and elemental depletion profiles. Corrosion rates, quantified by chromium depletion depth, followed an inverse power-law trend with increasing exposure time, indicating diffusion-limited kinetics. This trend is attributed to limitations in mass transport in the static salt and to the progressive local depletion of reactive chromium species. Coupled electron backscatter diffraction and energy dispersive X-ray spectroscopy analysis further revealed that the grain boundary character significantly influences corrosion susceptibility: high-angle grain boundaries exhibited pronounced Cr depletion and pitting, while low-angle and Σ3 boundaries remained comparatively resistant. These results offer valuable insight into the role of microstructure in corrosion processes and reinforce the importance of time-dependent material evaluation in molten salt environments relevant to advanced reactor designs.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗