Search NASA⌕ Search

SEARCH · Search NASA

Results for “POWER FACTOR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Recirculating Th2 cells induce severe thymic dysfunction via IL-4/STAT6 signaling pathway

Highlights: • Th2 cell is the most powerful factor in the inhibition of T cell development. • The effect caused by Th2 cells is principally due to the direct action of IL-4. • IL-4/STAT6 signaling is a major contributor to the ruins of T cell development. • The effect has a positive significance associated with thymic involution. Thymic involution happened early in life, but a certain ratio of activated CD4{sup +} T cells will persistently recirculate into the thymus from the periphery and it have been suggested to be able to inhibit the development of embryonic thymocytes. Our present study was aimed to elucidate the specific mechanism how activated CD4{sup +} T cells could influence upon developing thymocytes by using fetal thymic organ culture (FTOC) and kidney capsule transplantation. Our results demonstrated that Th2 cells were found to play a fundamental role in the inhibition of embryonic thymocyte development since a very low concentration of Th2 cells could obviously reduce the total number of thymocytes. And this effect was not tenable in other Th cell type. Notably, IL-4, the major cytokine secreted by Th2 cells, was suggested the key factor playing the inhibition role. In addition to reduced cell population, the proportion of double positive (DP) T cells was also heavily decreased. Furthermore, we demonstrated that it was the downstream effector signal transducer and activator of transcription 6 (STAT6) of IL-4 partially manipulate this inhibition. Together, these findings reveal a novel influence of Th2 cells re-entering the thymus on thymic involution.

60 APPLIED LIFE SCIENCES↗

Cost-efficient copper-nickel alloy for active cooling applications

It is recently proposed that active (Peltier) and passive (conductive) cooling could be combined to design highly-efficient thermal conductors as active heat sinks. Here we study the potential of low-cost copper-nickel alloys for active cooling applications. We show that for this application, copper-nickel alloys prepared using industrial-grade powders to lower the manufacturing cost, are as good as copper-nickel alloys made out of high purity metals. Furthermore, directed energy deposition, a type of additive manufacturing, can produce copper-nickel alloys which have about 10 percent lower thermoelectric power factor compared to mechanical-alloying methods but have larger thermal conductivity values, hence, possessing similar effective thermal conductivity values, reaching 403 W m -1 K -1 at 390K. Much larger values are expected at higher temperatures. The usage of additive manufacturing enables complex geometries and large-scale production.

36 MATERIALS SCIENCE↗

Thermoelectric Properties of Au- Containing Type-I Clathrates Ba8AuxGa16-3xGe30+2x

Type I clathrates, with compositions based on Ba8Ga16Ge30, are a class of promising thermoelectric materials due to their intrinsically low thermal conductivity. It has been demonstrated previously that the thermoelectric performance can be improved by transition metal substitution of the framework atoms. In this study, the effects of Au substitution for Ga/Ge on thermal and electrical transport properties of type I clathrate compounds have been investigated. Polycrystalline samples with a large range of Au content have been synthesized using conventional solid state techniques with the actual compositions of resulting materials approximately following Zintl-Klemm rules. The charge carrier type changes from electrons (n) to holes (p) as the Au content increases. The Seebeck coefficient (S) and power factor (S2/ where is the electrical resistivity) were improved by Au substitution and the resulting overall thermoelectric properties were enhanced by Au substitution with a thermoelectric figure of merit ZT ~ 0.63 at temperature T = 740 K for the composition Ba8Au5.47Ge39.96. The results presented herein show that Au-containing type I clathrates are promising p-type thermoelectric materials for high temperature applications.

Clathrates↗

Enhanced Thermoelectric Properties of Cu 2 ZnSnSe 4 with Ga-doping

Gallium doped Cu 2 ZnSnSe 4 quaternary chalcogenides with and without excess Cu were synthesized by elemental reaction and densified using hot pressing in order to investigate their high temperature thermoelectric properties. The resistivity, , and Seebeck coefficient, S, for these materials decrease with increased Ga-doping while both mobility and effective mass increase with Ga doping. The power factor (S 2 /ρ) therefore increases with Ga-doping. The highest thermoelectric figure of merit (ZT = 0.39 at 700 K) was obtained for the composition that had the lowest thermal conductivity. Our results suggest an approach to achieving optimized thermoelectric properties and are part of the continuing effort to explore different quaternary chalcogenide compositions and structure types, as this class of materials continues to be of interest for thermoelectrics applications.

36 MATERIALS SCIENCE↗

Effects of aluminum content on thermoelectric performance of Al x CoCrFeNi high-entropy alloys

Introducing a non-regular distribution in the mass and bonding by including distinctly different elements can reduce the phonon transport even within structurally well-ordered materials. These distributions are a quality of all high-entropy alloys (HEAs), however the inclusion of aluminum in Al x CoCrFeNi is particularly impactful due to the large mismatch in atomic mass with other components. The resultant low phonon conductivity is a requirement for high thermoelectric performance, motivating the investigation of the effects of Al content on phonon transport as well as other thermoelectric properties. This work examines the phonon and electron transport and thermoelectric conversion properties with various Al contents (0 ≤ x Al ≤ 2) in this Cantor alloy using first-principles calculations, molecular dynamics, and semi-classical Boltzmann transport theory. The calculated phonon density of states and thermoelectric properties present reasonable agreements with experiments, including neutron scattering. A large reduction of phonon conductivity (k L ) is observed even with low x Al s, which we attribute to effective phonon scatterings by the large mass mismatch. However, its temperature dependence is not significant, demonstrating a minor contribution of interphonon scattering. In contrast, electrical conductivity (σ) and Seebeck coefficient (S) increase with temperature at higher x Al s with body-centered cubic structures. Therefore, the thermoelectric figure of merit (ZT) of Al x CoCrFeNi HEAs is enhanced by increasing the Al content mainly due to the increase of the thermoelectric power factor (σS 2 ) at high temperatures, while at low temperatures the phonon-scattering enhancement by mass mismatch is also important.

36 MATERIALS SCIENCE↗

Synthesis of poly(3,4-ethylenedioxythuophene) derivatives using three-armed conjugated cross-linker and its thermoelectric properties

Conducting polymer based thermoelectric systems are very effective at harvesting electricity from waste heat with low-temperature gradients relative to environmental temperature. However, although various studies concerning the doping effect exist, there are insufficient reports on the effect of the change in polymer chain structure on the thermoelectric properties. Here we demonstrate different poly(3,4-ethylenedioxythiophene) (PEDOT)-derivative chain structures (such as linear, two-dimensional, co-polymer), by varying the amount of three-armed conjugated cross-linker (1,3,5-tri(2-thienyl)-benzene (TTB)). Further, at a small amount of TTB addition (until 0.5 mM), the electrochemical charge transport of the PEDOT films increased without shift of the UV–Vis absorbing property. However, from higher than 0.5 mM TTB, electrochemical charge transport decreased with blue shift of the UV–Vis absorbing curve. Moreover, the power factor of the PEDOT-derivative films without TTB to a small amount of TTB (0.5 mM) was improved from (27.03 to 49.43) µWm -1 K -2 , and at higher than 0.5 mM TTB concentration, was diminished, respectively, because a small amount of TTB enhanced the π–π interaction of the polymer chains without disrupting the conjugation, while excess TTB molecules blocked conjugation of the polymer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Enhanced thermoelectric properties of bismuth sulfide polycrystals prepared by mechanical alloying and spark plasma sintering

Bismuth sulfide powders were synthesized by mechanical alloying (MA) and then consolidated by spark plasma sintering (SPS) technique. In order to improve the electrical transport properties of bismuth sulfides, the carrier concentration was optimized by modifying chemical composition of sulfur through producing sulfur vacancies, and the carrier mobility was enhanced by a two-step SPS as a hot-forging process through increasing grain orientation. The electrical resistivity of bismuth sulfides was reduced to 10{sup -4} from 10{sup -2} {omega} m by optimizing sulfur content, and further lowered by hot-forging, whereby the power factor was significantly increased from 91 to 254 {mu}W/mK{sup 2}. The hot-forged Bi{sub 2}S{sub 2.90} sample showed the highest ZT=0.11 (at 523 K), which is higher than the reported value. The present work revealed that bismuth sulfide compounds as a promising candidate of thermoelectric materials can be synthesized by a simple process. - Abstract: Electrical properties of bismuth sulfides were improved by optimizing carrier concentration through modifying compositions of sulfur and enhancing carrier mobility through SPSed hot-forging. The ZT value of 0.11 was obtained, which is the maximum reported so far . Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of Rh on the thermoelectric performance of the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler alloys

We show that Rh substitution at the Co site in Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} (0<=x<=1) half-Heusler alloys strongly reduces the thermal conductivity with a simultaneous, significant improvement of the power factor of the materials. Thermoelectric properties of hot-pressed pellets of several compositions with various Rh concentrations were investigated in the temperature range from 300 to 775 K. The Rh 'free' composition shows n-type conduction, while Rh substitution at the Co site drives the system to p-type semiconducting behavior. The lattice thermal conductivity of Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} alloys rapidly decreased with increasing Rh concentration and lattice thermal conductivity as low as 3.7 W/m*K was obtained at 300 K for Zr{sub 0.5}Hf{sub 0.5}RhSb{sub 0.99}Sn{sub 0.01}. The drastic reduction of the lattice thermal conductivity is attributed to mass fluctuation induced by the Rh substitution at the Co site, as well as enhanced phonon scattering at grain boundaries due to the small grain size of the synthesized materials. - Graphical abstract: Significant reduction of the lattice thermal conductivity with increasing Rh concentration in the p-type Zr{sub 0.5}Hf{sub 0.5}Co{sub 1-x}Rh{sub x}Sb{sub 0.99}Sn{sub 0.01} half-Heusler materials prepared by solid state reaction at 1173 K.

36 MATERIALS SCIENCE↗

Improvement of the thermoelectric properties of [Bi{sub 1.68}Ca{sub 2}O{sub 4-{delta}}]{sup RS}[CoO{sub 2}]{sub 1.69} cobaltite by chimie douce methods

[Bi{sub 1.68}Ca{sub 2}O{sub 4-{delta}}]{sup RS}[CoO{sub 2}]{sub 1.69} has been obtained by different chimie douce methods and uniaxially or isostatically pressed. The influence of these parameters on the thermoelectric properties has been investigated. Contrary to the Seebeck coefficient, which remains unchanged, the electrical conductivity is greatly modified. In particular, spray-drying synthesis followed by uniaxial pressing results in an electrical conductivity two times larger than in the case of conventional solid state synthesis. Our results suggest that a narrow particle size distribution is beneficial to the thermoelectric properties of the layered compounds. The spray-drying technique seems to be promising to improve the electrical conductivity of layered materials. Moreover, this method presents other advantages (homogeneous samples and less energetic processing) which could be interesting to the future manufacturing of thermoelectric devices. - Graphical abstract: Small particles and narrow size distribution is obtained for spray-drying [Bi{sub 1.68}Ca{sub 2}O{sub 4}]{sup RS}[CoO{sub 2}]{sub 1.69} cobaltate. The power factor is boosted up two times compared with the conventional solid state method.

36 MATERIALS SCIENCE↗

p-Type thermoelectric properties of the oxygen-deficient perovskite Ca{sub 2}Fe{sub 2}O{sub 5} in the brownmillerite structure

Brownmillerite calcium ferrite was synthesized in air at 1573 K and thermoelectric properties (direct current electrical conductivity {sigma}, Seebeck coefficient {alpha}, thermal conductivity {kappa}, thermal expansion {alpha}{sub L}) were measured from 373 to 1050 K in air. Seebeck coefficient was positive over all temperatures indicating conduction by holes, and electrical properties were continuous through the Pnma-Imma phase transition. Based on the thermopower and conductivity activation energies as well as estimated mobility, polaron hopping conduction was found to dominate charge transport. The low electrical conductivity, <1 S/cm, limits the power factor ({alpha}{sup 2{sigma}}), and thus the figure of merit for thermoelectric applications. The thermal conductivity values of {approx}2 W/mK and their similarity to Ruddlesden-Popper phase implies the potential of the alternating tetrahedral and octahedral layers to limit phonon propagation through brownmillerite structures. Bulk linear coefficient of thermal expansion ({approx}14x10{sup -6} K{sup -1}) was calculated from volume data based on high-temperature in situ X-ray powder diffraction, and shows the greatest expansion perpendicular to the alternating layers. - Graphical abstract: Representative microstructure of Ca{sub 2}Fe{sub 2}O{sub 5} samples used for thermoelectrical measurements.

36 MATERIALS SCIENCE↗

Beneficial effect of Se substitution on thermoelectric properties of Co{sub 4}Sb{sub 11.9-x}Te{sub x}Se{sub 0.1} skutterudites

Skutterudite-based compounds, Co{sub 4}Sb{sub 12-x-y}Te{sub x}Se{sub y} (x=0.4, 0.5, 0.6 and y=0.0, 0.1), are synthesized by the solid state reaction and the spark plasma sintering methods, and their structure and the thermoelectric properties have been investigated systematically. It is found that Se doping results in decrease of the lattice parameter and refinement of the particle size compared with those of Se-free samples. The Se-doped samples do not yield a certain increase in the power factor, but show a significant depression in the lattice thermal conductivity. The highest dimensionless figure of merit ZT=1.09 is achieved at 800 K for the Co{sub 4}Sb{sub 11.3}Te{sub 0.6}Se{sub 0.1} compound, which is improved by 15% compared with that of Te alone doped Co{sub 4}Sb{sub 11.4}Te{sub 0.6} compound at the corresponding temperature. - Graphical abstract: The Te and Se co-doped Co{sub 4}Sb{sub 11.9-x}Te{sub x}Se{sub 0.1} skutterudites show amazingly lower thermal conductivity ({kappa}) and lattice thermal conductivity ({kappa}{sub L}) compared with those of Co{sub 4}Sb{sub 12-x}Te{sub x} skutterudites. Highlights: Black-Right-Pointing-Pointer Te and Se co-doped Co{sub 4}Sb{sub 12-x-y}Te{sub x}Se{sub y} compounds have been synthesized by the solid state reaction method. Black-Right-Pointing-Pointer Doping of Se resulted in decrease of the lattice parameter and refinement of the particle size. Black-Right-Pointing-Pointer The co-doped skutterudites show amazingly lower lattice thermal conductivity. Black-Right-Pointing-Pointer Co-doping with Te and Se is an attractive approach to enhance the TE performance of skutterudites.

36 MATERIALS SCIENCE↗

High thermoelectric performance of In, Yb, Ce multiple filled CoSb{sub 3} based skutterudite compounds

Filling voids with rare earth atoms is an effective way to lowering thermal conductivity which necessarily enhances thermoelectric properties of skutterudite compounds. Yb atom is one of the most effective species among the rare earth atoms for filling the voids in the skutterudite structure due to a large atomic mass, radius and it is intermediate valence state. In this work, we aim to find the best filling partners for Yb using different combinations of Ce and In as well as to optimize actual filling fraction in order to achieve high values of ZT. The traditional method of synthesis relying on melting-annealing and followed by spark plasma sintering was used to prepare all samples. The thermoelectric properties of four samples of Yb{sub 0.2}In{sub 0.2}Co{sub 4}Sb{sub 12}, Yb{sub 0.2}Ce{sub 0.15}Co{sub 4}Sb{sub 12}, Yb{sub 0.2}Ce{sub 0.15}In{sub 0.2}Co{sub 4}Sb{sub 12}, and Yb{sub 0.3}Ce{sub 0.15}In{sub 0.2}Co{sub 4}Sb{sub 12} (nominal) were examined based on the Seebeck coefficient, electrical conductivity, thermal conductivity, and Hall coefficient. Hall coefficient and Seebeck coefficient signs confirm that all samples are n-type skutterudite compounds. Carrier density increases with the increasing Yb+Ce content. A high power factor value of 57.7 {mu}W/K{sup 2}/cm for Yb{sub 0.2}Ce{sub 0.15}Co{sub 4}Sb{sub 12} and a lower thermal conductivity value of 2.82 W/m/K for Yb{sub 0.2}Ce{sub 0.15}In{sub 0.2}Co{sub 4}Sb{sub 12} indicate that small quantities of Ce with In may be a good partner to Yb to reduce the thermal conductivity further and thus enhance the thermoelectric performance of skutterudites. The highest ZT value of 1.43 was achieved for Yb{sub 0.2}Ce{sub 0.15}In{sub 0.2}Co{sub 4}Sb{sub 12} triple-filled skutterudite at 800 K. - Graphical abstract: Thermoelectric figure of merit of Yb{sub x}In{sub y}Ce{sub z}Co{sub 4}Sb{sub 12} (0{<=}x,y,z{<=}0.18 actual) compounds versus temperature. Highlights: Black-Right-Pointing-Pointer TE properties of Yb,In,Ce multiple-filled Yb{sub x}In{sub y}Ce{sub z}Co{sub 4}Sb{sub 12} skutterudites were investigated. Black-Right-Pointing-Pointer Thermal conductivity is strongly suppressed by multiple filling of Yb, Ce and In. Black-Right-Pointing-Pointer Small amounts of Ce and In with Yb are beneficial for the enhancement of TE performance. Black-Right-Pointing-Pointer The highest ZT=1.43 was achieved with Yb{sub 0.07}In{sub 0.094}Ce{sub 0.065}Co{sub 4}Sb{sub 11.92} at 800 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Prospects of nanostructures Bi{sub 1-x}Sb{sub x} for thermoelectricity

It has been predicted that surface states of topological insulators have large a thermopower and also ultrahigh mobilities. The authors report results of a magneto-thermoelectric investigation of single crystal Bi{sub 1-x}Sb{sub x} nanowires in a glass cover with diameters ranging from 90 nm to 5 {mu}m. The wide-ranging antimony concentration enabled us to study the effect of nanowire dimensionality in the semimetal, semi-conductor and gapless regimes. Quantum size effects in Bi-2 at%Sb nanowires, which are shown in temperature dependences of resistance R(T) and thermopower {alpha}(T) for the diameters significantly higher than the critical diameter for pure Bi-wires, are observed. The thermopower in weak magnetic fields, reaches values +400 {mu}V/K at T=20-40 K. Power factor {alpha}{sup 2}{sigma} depending on diameter of wires, structure, temperature and magnetic field is calculated. In connection with topological insulators, we will discuss the surface effect in the thermoelectric properties that we observe. - Graphical abstract: Temperature dependences of resistance R{sub T}/R{sub 300}(T) (a) for Bi-2 at%Sb wires various diameters d: 1-d=300 nm, 2-d=400 nm, 3-d=600 nm, 4-d=1600 nm. Inset (a) SEM cross sectional image of the 650 nm Bi-2 at%Sb wire (clear) in glass envelope (gray). The magnetic field dependences thermopower (H Double-Vertical-Line {Delta}T) (b) Bi-2 at%Sb wires, with different diameters: (1). d=300 nm, (2). d=400 nm, (3). d=600 nm, T=26 K. Highlights: Black-Right-Pointing-Pointer SMSC transition in semimetal Bi-Sb wires due to the quantum size effect is observed. Black-Right-Pointing-Pointer In Bi-6 at%Sb wires alloys has been realized the gapless (GL) state. Black-Right-Pointing-Pointer In the area GS state abnormal growth thermopower in magnetic fields is found out. Black-Right-Pointing-Pointer Semiconductor Bi{sub 1-x} Sb{sub x} nanowires manifest properties of the topological insulators.

36 MATERIALS SCIENCE↗

Fabrication of large sintered pellets of Sb-doped n-type Mg{sub 2}Si using a plasma activated sintering method

Sb is known to be the most stable n-type dopant in Mg{sub 2}Si, whereas the reproducibility and sintering scalability of Sb-doped Mg{sub 2}Si has proved to be difficult. We have developed a metallic binder for the Sb-doped Mg{sub 2}Si sintering process. A remarkable benefit of the binder is that it enables us to reproducibly fabricate large sintered Sb-doped Mg{sub 2}Si pellets up to 30 mm in diameter with no internal cracks. For binder contents of 3-7 wt%, the observed power factor and thermal conductivity were identical to that of conventional Sb-doped samples, while excess binder degraded the TE properties. The binder mixture also plays a part in increasing the yield in the production of TE legs, up to 82% for 5 wt% Ni incorporation, as well as improving the hardness of the sintered sample. Incorporation of 5 wt% Ni binder affected an increase in the ZT value up to 0.97. - Graphical abstract: The sample of 30 mm in diameter is fabricated by using a Ni binder. Highlights: Black-Right-Pointing-Pointer We have developed a metallic binder for the Sb-doped Mg{sub 2}Si sintering process. Black-Right-Pointing-Pointer Sb-doped Mg{sub 2}Si pellets up to 30 mm in diameter with no internal cracks. Black-Right-Pointing-Pointer Incorporation of 5 wt% Ni binder affected an increase in the ZT value up to 0.97.

36 MATERIALS SCIENCE↗

The effect of structural vacancies on the thermoelectric properties of (Cu₂Te){sub 1–x}(Ga₂Te₃) x

We have studied the effects of structural vacancies on the thermoelectric properties of the ternary compounds (Cu₂Te) 1–x (Ga₂Te₃) x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75), which are solid solutions found in the pseudo-binary phase diagram for Cu₂Te and Ga₂Te₃, and possesses tunable structural vacancy concentrations. This materials system is not suitable due to the cost and scarcity of the constituent elements, but the vacancy behavior is well understood and will provide a valuable test case for other systems more suitable from the standpoint of cost and abundance of raw materials, which also possesses these vacancy features, but whose structural characterization is lacking at this stage. We find that the nominally defect free phase CuGaTe₂ possess the highest ZT (ZT=S²T/ρκ, where S is the Seebeck coefficient and ρ is the electrical resistivity κ is the thermal conductivity and T is the absolute temperature) which approaches 1 at 840 K and seems to continuously increase above this temperature. This result is due to the unexpectedly low thermal conductivity found for this material at high temperature. The low thermal conductivity was caused by strong Umklapp (thermally resistive scattering processes involving three phonons) phonon scattering. We find that due to the coincidentally strong scattering of carriers by the structural defects that higher concentrations of these features lead to poor electrical transport properties and decreased ZT. - Graphical abstract: Thermal conductivity and zT as a function of temperature for a series of compounds of the type (Cu₂Te) 1–x (Ga₂Te₃)x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75). Highlights: • All the samples show p-type semiconducting behavior in the temperature dependence of the Seebeck and Hall coefficients. • The increased carrier concentration and the introduction of vacancies diminish the carrier mobility and power factor. • The low temperature k decreases significantly as the Ga₂Te₃ content increases due to increasing point defects. • The highest ZT ~ 1.0 at 840 K among the samples in this study was found in CuGaTe₂, which contains no vacancies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transport properties of the SnBi{sub 2}Te{sub 4}–PbBi{sub 2}Te{sub 4} solid solution

We report on the electrical and thermal transport properties of the Sn{sub 1−x}Pb{sub x}Bi{sub 2}Te{sub 4} series and we discuss the potential of these materials for thermoelectric conversion applications. From the evolution of the XRD patterns, we can confidently conclude that a complete solid solution exists between SnBi{sub 2}Te{sub 4} and PbBi{sub 2}Te{sub 4}, with no miscibility gap. A crossover from p-type conduction in Sn-rich samples to n-type conduction in Pb-rich ones has been observed, with a transition between x=0.3 and 0.4. A concomitant increase of the electrical resistivity and of the Seebeck coefficient has been observed in the solid solution, which leads to almost constant values of the thermoelectric power factor. Moreover, the thermal conductivity is slightly reduced in the solid solution. The best figure of merit ZT values at room temperature have been observed for p-type Sn{sub 0.8}Pb{sub 0.2}Bi{sub 2}Te{sub 4} with ZT=0.25 and for n-type Sn{sub 0.3}Pb{sub 0.7}Bi{sub 2}Te{sub 4} with ZT=0.15. - Graphical abstract: Seebeck coefficient in (Pb/Sn)Bi{sub 2}Te{sub 4} solid solution. - Highlights: • A complete solid solution exists between PbBi{sub 2}Te{sub 4} and SnBi{sub 2}Te{sub 4.} • A crossover between p-type and n-type is observed for 0.3<Pb fraction <0.4. • The lattice thermal conductivity is hardly reduced in the solid solution.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Transport properties and thermal behavior of YbMnSb 2 semimetal above room temperature

Single crystals of ytterbium manganese diantimonide, YbMnSb 2 have been grown from a high-temperature reaction of the elements, employing molten Sb as self-flux. This phase crystallizes in the tetragonal centrosymmetric space group P4/nmm (No. 129) and adopts the ZrCuSiAs structure type. Here, the structure consists of Sb-based square nets and PbO-type layers formed by fused [MnSb 4/4 ] tetrahedra. YbMnSb 2 is stable under ambient atmosphere and incongruently melts at a temperature of ca. 1120 K. In the temperature range from 300 K to 450 K, the electrical resistivity of the as-grown single-crystalline material is as low as 3.2 mΩ cm, while its thermopower is as high as 180 μV/K. As such, YbMnSb 2 shows promise for thermoelectric applications in the mid-temperature region, with an estimated power factor of 0.85–0.95 mW/(m K 2 ).