At least 559 records · Page 31

Corrosion and repassivation of Super 13Cr stainless steel in artificial 1D pit electrodes at elevated temperature

Repassivation behavior of Super 13Cr martensitic stainless steel was investigated using a one-dimensional artificial pit electrode in deaerated NaCl solutions at 85 °C. Critical potentials for pit repassivation (E crit ) were measured by downward potential scans. E crit and the final current density (i f ) at the end of the scan can be correlated to the pit repassivation, showing that repassivation is more probable with smaller i f and higher E crit . Pit repassivation at a constant potential was correlated with if and average current density (i avg ). A combination of lower i f and i avg suggests a higher probability for pit repassivation.

36 MATERIALS SCIENCE↗

Critical pitting temperature of selective laser melted 316L stainless steel: A mechanistic approach

In this work, the critical pitting temperature (CPT) of selective laser melted (SLM) 316 L stainless steel in 1.0 M NaCl was measured and compared with a commercial wrought alloy. Potentiostatic measurements determined a mean CPT value of 16 ± 0.7 °C, 27.5 ± 0.8 °C and 31 ± 1 °C for the wrought alloy, the SLM alloy normal to the build direction and parallel to the build direction, respectively. The lead-in pencil electrode technique was used to study the pit chemistry of the two alloys and to explain the higher CPT values observed for the SLM alloy. A lower critical current density required for passivation in a simulated pit solution was measured for the SLM alloy. Moreover, the ratio of the critical concentration to saturated concentration of dissolving metal cations was found to be higher for the SLM alloy, which was related to its different salt film properties, possibly as a result of the SLM’s distinct microstructure.

36 MATERIALS SCIENCE↗

Hydrogen embrittlement of additively manufactured austenitic stainless steel 316 L

Additive manufacturing (AM) is a promising means of production of austenitic stainless steel (SS) parts for hydrogen service. The hydrogen embrittlement resistance of SS 316 L parts manufactured by powder-bed-fed selective laser melting (SLM) and directed energy deposition (DED) was examined using slow strain rate tensile testing. The influence of the hierarchical AM microstructures on mechanical response, microstructural evolution, and void formation were analyzed using multiscale electron microscopy. Furthermore, the presence of hydrogen reduced ductility in as-built DED materials, but did not significantly influence the response in as-built SLM material or heat-treated materials. Microstructural features driving these different responses are discussed.

36 MATERIALS SCIENCE↗

Oxidation kinetics and microstructure evolution of high Mn stainless-steel alloy in CO 2 at 700 °C

Oxidation kinetics and scale formation were examined in 21–2N Stainless Steel alloys in a CO 2 environment at 700 °C. Several characterization techniques were used to identify the morphology, crystallographic structure, and chemical composition of the oxide scale formation during exposures up to 1925 h. High manganese content played an important role in homogenous oxide scale formation of Mn 3 O 4 and MnCr 2 O 4 at the scale/gas and scale/alloy interfaces and as an FCC stabilizer in the alloy. Depletion of Mn resulted in an FCC to BCC phase transformation at the scale/alloy interface. No carburization was observed, indicating that the oxide layer is preventing carbon uptake.

36 MATERIALS SCIENCE↗

Discovering the nanoscale origins of localized corrosion in additive manufactured stainless steel 316L by liquid cell transmission electron microscopy

Here, we use liquid cell scanning transmission electron microscopy (STEM) to directly characterize the nanoscale origins of corrosion initiation in Additive manufacturing (AM) 316 L stainless steel. Under applied anodic potentials, we found that the dislocation cellular boundaries were preferentially corroded and that regions of localize corrosion occurred along the cellular boundaries. We directly observed the earliest stages of corrosion by controlling the biasing parameters to decelerate the corrosion processes. The results show that highly localized corrosion occurs via inclusion dissolution along dislocation cell boundaries. More widespread corrosion initiates at the dislocation cell boundaries and spreads throughout the dislocation networks.

36 MATERIALS SCIENCE↗

Effect of tellurium concentration on the corrosion and mechanical properties of 304 stainless steel in molten FLiNaK salt

In this study, the effect of Te concentration in molten FLiNaK salt on the corrosion and mechanical properties of 304 stainless steel was investigated. The corrosion depth of samples after the immersion tests for 48 h at 600 °C decreased with increasing Te concentration. Likewise, the sample after the immersion test containing 1.0 wt% of Te (1.0 wt% Te sample) showed less reduction in mechanical properties than the 0.1 wt% Te sample. We hypothesize that the condition for a Cr-oxide layer that has the protective property is fulfilled underneath the Ni-Fe rich layer which is formed by the selective leaching of Cr.

36 MATERIALS SCIENCE↗

Influence of carbon nanotubes on microstructure and corrosion performance of additively manufactured 316L stainless steel

For this study, laser powder bed fusion (LPBF) was performed on feedstock-modified 316L stainless steel powder with 1 and 2 vol% carbon nanotubes (CNT). The corrosion resistance was evaluated following cyclic potentiodynamic polarization tests conducted in 0.6 M NaCl at room temperature, 35 and 50 °C, and immersion tests in 6 % FeCl 3 . The CNT addition has increased the pitting potential and decreased number of pits formed during immersion in FeCl 3 solution, which could be attributed to Mn-Si-O nano inclusions refinement and segregation of chromium around the inclusions. The observed corrosion behavior was correlated with the altered microstructure due to CNT addition.

36 MATERIALS SCIENCE↗

Understanding a novel form of intergranular corrosion of stainless steel 316L exposed to molten LiCl-Li 2 O-Li

We report stainless steel 316 L exposed to LiCl-Li2O molten salt containing Li metal for 500 and 1000 h experiences deep intergranular attack and bulk void formation. This degradation is due to a synergistic corrosion mechanism, different than other forms of molten salt corrosion, where Cr and Mn oxides and carbides form along grain boundaries and are dissolved by Li metal. Synchrotron transmission X-ray microscopy 3D imaging is used to show corrosion morphology and Cr enrichment and depletion in a novel format that has not previously been used for bulk corrosion samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Corrosion mechanism of cold forged 316 stainless steel in molten FLiNaK salt

This study examined how cold forging (CF) affects the corrosion of 316 stainless steel (SS) in molten FLiNaK salt at 700 °C for 48 h. CF samples had two corrosion areas: one near the top and another displaying intergranular corrosion (IGC). Samples with lower CF (5–30 %) showed more IGC, while the 50 % CF sample had less IGC but the shallowest corrosion depth. This was due to the increased number of grain boundaries, which raised the potential corrosion initiation sites, and certain grain boundaries promoting chromium dissolution, thus enhancing IGC.

FLiNaK↗

Corrosion of 316 L stainless steel under the natural circulation of molten NaCl-MgCl 2 salt

The corrosion behavior of 316 L stainless steel (SS) was studied via the natural circulation of molten eutectic NaCl-MgCl 2 salt through a microloop. The post-corrosion tested 316 L SS microloop sections were characterized with microscopy techniques to determine the microstructural and microchemical changes that occurred at the alloy/salt interface. It was found that 316 L SS showed heterogeneous dissolution at the hot-leg, whereas deposition of corrosion products occurred at the cold-leg. For the first time, experimentally obtained molten salt flow-induced corrosion of 316 L SS results were combined with computational thermodynamic-kinetic models to validate the dissolution and deposition in terms of elemental compositional changes at the alloy/salt interface. The thermodynamic-kinetic modeling predicted that the heterogeneous dissolution of Cr and Fe from the hot-leg section of 316 L SS persisted throughout the salt circulation. The model also estimated that, despite Cr deposition starting earlier than Fe, the total redeposition of Fe is expected to be significantly greater than that of Cr over the circulation of salt. Furthermore, the modeling accurately predicted the subsurface enrichment of Mo which is attributed to the reduced Cr activity and the relatively higher diffusion rate of Mo within the alloy matrix. Here, the agreement between modeling and experimental results confirms that Fe chlorides dissolve at the hot-leg and subsequently deposit at the cold-leg due to activity changes driven by the thermal gradient. By contrast, Cr was not detected in the cold-leg deposits, which is attributed to its weaker temperature dependence on activity, limiting its redeposition under these conditions.

36 - MATERIALS SCIENCE↗

Mechanistic transition of stainless steel 304L corrosion in MgCl 2 phase change material under thermal cycling

Magnesium chloride (MgCl 2 )-based molten salt phase change materials (PCMs) are promising candidates for thermal energy storage (TES) owing to their advantageous thermophysical properties, however, their high corrosivity in the molten state limits material compatibility. In this study, the corrosion behavior of 304?L stainless steel (SS304L) exposed to MgCl2 PCM was investigated as a function of thermal cycling (up to 9000 cycles) relevant to PCM-based TES systems. Microstructural changes and elemental redistribution at the alloy-salt interface under thermal cycling conditions were characterized using synchrotron-based X-ray fluorescence (XRF) and scanning electron microscopy coupled with energy dispersive X-ray spectroscopy (SEM-EDS). Results show that corrosion is governed by selective Cr-dissolution and elemental diffusion near the interface and grain boundaries. A clear transition in the dominant corrosion mechanism is observed with increasing thermal cycles. Surface corrosion is the dominant mechanism up to 1000 cycles, whereas intergranular corrosion becomes the primary degradation mode beyond 2000 cycles. These mechanistic changes are interpreted in terms of evolving interfacial chemistry, microstructure and the diffusion-driven redistribution of alloying elements.

36 MATERIALS SCIENCE↗

High-temperature chromium diffusion in austenitic stainless steel: Ab initio molecular dynamics simulations

Chromium self-diffusion through stainless steel (SS) matrix and along grain boundaries is an important mechanism controlling SS structural materials corrosion. For this work, Cr diffusion in austenitic SS was simulated using canonical ab initio molecular dynamics with realistic models of type-316 SS bulk, with and without Cr vacancies, and a low-energy Σ3 twin boundary typically observed at active corrosion sites. Cr self-diffusion coefficients at 750 and 850 °C calculated using Einstein’s diffusion equation are 4.2 × 10 –6 and 8.1 × 10 –6 Å 2 ps –1 in pristine bulk, 3.8 × 10 –3 and 5.5 × 10 –3 Å 2 ps –1 in bulk including Cr vacancies, and 9.5 × 10 –2 and 1.0 × 10 –1 Å 2 ps –1 at a Σ3[1 1 1]60° twin boundary.

36 MATERIALS SCIENCE↗

Fatigue behavior and modeling for additive manufactured 304L stainless steel: The effect of surface roughness

The fatigue strength of additively manufactured metallic parts in their as-built surface condition is mainly dominated by the surface roughness. Post-processing is often inevitable to reduce surface roughness effects even though post-processing diminishes the main advantage of additive manufacturing, which is net-shaped direct-to-service production. This work investigates the underlying mechanisms responsible for fatigue failure of additively manufactured 304L stainless steel parts in as-built and machined/polished surface conditions. Both strain- and force-controlled, fully reversed fatigue tests were conducted to gain a comprehensive understanding of surface roughness effects on fatigue behavior. The sensitivity to surface roughness is shown to be dependent on the control mode, with stress-based fatigue tests showing greater sensitivity than strain-based fatigue tests. Moreover, the fatigue life estimation for as-built specimens was performed based on surface roughness parameters as well as the fatigue properties of the specimens in machined/polished surface condition of the material without using any fatigue data of specimens in as-built surface condition. Accordingly, the effect of surface roughness on the fatigue behavior could be estimated reasonably well in both strain-life and stress-life approaches.

36 MATERIALS SCIENCE↗

On the influence of test speed and environment in the fatigue life of small diameter nitinol and stainless steel wire

Here, to better understand the complex interplay of speed and environment on metals commonly used in implants, rotary bend fatigue tests were conducted on stainless steel and nitinol wires. A range of alternating strains was tested to create ε-N curves at two speeds (physiologic and accelerated) and in three environments (deionized water at body temperature, phosphate buffered saline at body temperature, and laboratory air at ambient room temperature). Results indicate that speed and environment can affect the observed fatigue life in nuanced ways. An electropotential monitoring technique was demonstrated to characterize fatigue crack growth which may be useful in future investigations.

36 MATERIALS SCIENCE↗

Influence of stacking fault energy and hydrogen on deformation mechanisms in high Mn austenitic steels during in-situ tensile testing

High Mn austenitic steels are considered an economical alloy system for hydrogen storage and transport applications. This study used stacking fault energy (SFE) as a design parameter to achieve hydrogen embrittlement (HE)-resistant high Mn austenitic alloys. The role of hydrogen on the deformation mechanisms of low (29 mJ/m 2 ) and high SFE (49 mJ/m 2 ) alloys was evaluated through in-situ neutron diffraction during tensile loading. Hydrogen-precharging increased yield strength, partly due to hydrogen-induced lattice distortion (i.e., solute strengthening). Hydrogen accelerated the increase in defect density, including dislocations and stacking faults. The formation of planar deformation structures (twins and stacking faults), relative to dislocations, plays a critical role in promoting hydrogen-assisted fracture. The stacking fault frequency parameter obtained from neutron diffraction quantifies planar deformation tendencies, correlated with HE sensitivity. The higher SFE alloy exhibited greater resistance to HE, associated with the reduced propensity to form stacking faults and twins upon deformation in the hydrogen-precharged condition.

High Mn austenitic steel↗

Interplay between hydrogen, temperature, and character angle on dissociated dislocation energies in Fe–Ni–Cr austenitic stainless steels

Dislocation energy has an important role in the mechanical performance of structural metals. While dislocation energies cannot be fully obtained from continuum theories due to the contribution of the dislocation core, they have been calculated via atomistic simulations in elemental metals. However, constraints on the local atomic environments have prevented the use of such approaches in systems that incorporate alloying or interstitial solutes. In this work, we develop robust molecular dynamics methods to resolve these issues through a geometric construction of dislocation dipoles and the calculation of time-averaged energies. Furthermore, we apply these methods to calculate dislocation energies (including core energies) in an Fe 70 Ni 11 Cr 19 austenitic steel at a variety of character angles, hydrogen concentrations, temperatures, and dipole spacings. The resulting highly converged energies show an excellent agreement with continuum expressions. Overall, hydrogen concentrations up to 1.0 % do not have a significant effect on the elastic parameters and dislocation energy. The methods and insights derived in this work have the potential to facilitate the calculation of dislocation energies in a wide range of systems, and to guide our understanding of hydrogen embrittlement.

Alloyed systems↗

Crystal plasticity modeling of strain-induced martensitic transformations to predict strain rate and temperature sensitive behavior of 304 L steels: Applications to tension, compression, torsion, and impact

This paper advances crystallographically-based Olson-Cohen (direct γ → α’) and deformation mechanism (indirect γ→ε→α’) phase transformation models for predicting strain-induced austenite to martensite transformation. Here, the advanced transformation models enable predictions of not only strain-path sensitive, but also of strain-rate and temperature sensitive deformation of polycrystalline stainless steels (SSs). The deformation of constituent grains in SSs is modeled as a combination of anisotropic elasticity, crystallographic slip, and phase transformation, while the hardening is based on the evolution of dislocation density and explicit shifts in phase fractions. Such grain-scale deformation is implemented within the meso-scale elasto-plastic self-consistent (EPSC) homogenization model, which is coupled with the implicit finite element (FE) method to provide a constitutive response at each FE integration point for solving boundary value problems at the macro-scale. Parameters pertaining to the hardening and transformation models within FEEPSC are calibrated and validated on a suite of data including flow curves and phase fractions for monotonic compression, tension, and torsion as a function of strain-rate and temperature for wrought and additively manufactured (AM) SS304L. To illustrate the potential and accuracy of the integrated multi-level FE-EPSC simulation framework, geometry, mechanical response, phase fractions, and texture evolution are simulated during gas-gun impact deformation of a cylinder and quasi-static tension of a notched specimen made of AM SS304L. Details of the simulation framework, comparison between experimental and simulation results, and insights from the results are presented and discussed.

304L steels↗

Accelerated creep profiling: a high-throughput thermal- and stress-gradient approach applied to additive and wrought stainless steel

Here, this study investigates logarithmic creep behavior at temperatures near room temperature in wrought and additively manufactured (AM) 316 L austenitic stainless steel. A novel high-throughput (HiTp) methodology employed thermal gradients to obtain stress- and temperature-dependence of creep behavior. The findings, based on 104 two-week creep tests, reveal significant differences in creep response between wrought and AM materials. Compared to the wrought material, the AM material exhibited a higher activation energy and a lower activation volume. These differences were attributed to the materials’ distinct microstructural features, e.g., dislocation cell structures and precipitate distributions, which alter the susceptibility to dislocation glide creep, particularly at stresses below the yield stress. The HiTp methodology provides both an accelerated determination of low-temperature creep mechanisms, offering critical data for the design and optimization of alloys in near-ambient, high stress applications.

316 L Stainless steel↗