Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Friction Stir Lap Welding of Magnesium Alloy to Steel: A Preliminary Investigation

An initial study was made to evaluate the feasibility of joining Magnesium alloy AZ31 sheet to galvanized steel sheet in lap configuration using friction stir welding (FSW). Two different automotive sheet steels were used for comparative evaluation of the dissimilar joining potential; a 0.8mm thick, electro galvanized (EG) mild steel, and a 1.5mm thick hot dipped galvanized (HDG) high-strength, low-alloy steel (HSLA). These steels were joined to 2.33mm thick AZ31B magnesium sheet. A single FSW tool design was used for both dissimilar welds, and process parameters were kept the same. Average peak load for the AZ31-1.5 mm steel weld joint in lap shear mode was found to be 6.3 ± 1.0 kN. For the AZ31-0.8 mm steel weld, joint strength was 5.1 ± 1.5 kN. Microstructural investigation indicates melting of the Zn coating at the interface and subsequent alloying with the Mg sheet resulting in formation of solidified Zn-Mg alloy layer at AZ31/steel interface.

36 MATERIALS SCIENCE↗

A Novel Shim-Assisted Resistance Spot Welding Process to Improve Weldability of Medium-Mn Transformation-Induced Plasticity Steel

Medium-Mn transformation-induced plasticity steels have great potential to significantly reduce vehicle weight and improve fuel economy due to their outstanding combination of high strength and excellent ductility. One bottleneck to the application is their poor weldability resulting from their high Mn contents. In this paper, three resistance spot welding set-ups, including no shim, an interstitial-free steel shim at the faying interface (shim-in) and shims against the electrodes (shim-out), were incorporated to investigate the weldability of Fe-7Mn-0.14C medium-Mn steel. Tensile-shear, cross-tension, and microhardness tests were used to evaluate the mechanical properties of the welds. Experimental results demonstrated that the failure mode of the welds transitioned from the interfacial fracture in the case of no shim to the desired nugget pull-out fracture in the shim-out set-up, resulting in dramatical improvements in both peak loads and their corresponding extensions during the tensile-shear and cross-tension tests. In contrast, the shim-in set-up made no improvement. What can contribute to such improvement was then discussed on the basis of observed morphologies and microstructures of welds.

36 MATERIALS SCIENCE↗

Experimental Study and Fractal Analysis on the Anisotropic Performance of Explosively Welded Interfaces of 304 Stainless Steel/245 Carbon Steel

The mechanical anisotropy of an explosive welding composite plate made of 304 stainless steel/245 steel was studied through shear experiments performed on explosively welded wavy interfaces along several orientation angles. The results indicated that the strength and the fracture energy of samples significantly varied with the orientation angles. The fracture surfaces of all samples were observed using a scanning electron microscope and through three-dimensional structure microscopy. The periodic features of all the fracture surfaces were clearly shown in different fracture modes. The fractal dimension of the fracture surfaces was calculated based on the fractal geometry by the box-counting method in MATLAB. The cohesive element model was used to analyze the fracture energy according to the physical dependence of the fractal dimension on thermodynamic entropy and interface separation energy. The fracture energy was an exponential function of the fractal dimension value, which was in good agreement with the experimental results. All results were validated for effective use in the application of anisotropy analysis to the welded interface and structural optimization of explosively welded composite plates.

36 MATERIALS SCIENCE↗

Joining sheet aluminum AA6061-T4 to cast magnesium AM60B by vaporizing foil actuator welding: Input energy, interface, and strength

Dissimilar joining of sheet aluminum AA6061-T4 to cast magnesium AM60B was achieved by vaporizing foil actuator welding (VFAW). Three input energy levels were used (6, 8, and 10 kJ), and as a trend, higher input energies resulted in progressively higher flyer velocities, more pronounced interfacial wavy features, larger weld zones, higher peel strengths, and higher peel energies. In all cases, weld cross section revealed a soundly bonded interface characterized by well-developed wavy features and lack of voids and continuous layers of intermetallic compounds (IMCs). At 10 kJ input energy, flyer speed of 820 m/s, peel strength of 22.4 N/mm, and peel energy of 5.2 J were obtained. In lap-shear, failure occurred in AA6061- T4 flyer at 97% of the base material’s peak tensile load. Peel samples failed along the weld interface, and the AM60B-side of the fracture surface showed thin, evenly-spaced lines of Al residuals which had been torn out of the base AA6061-T4 in a ductile fashion and transferred over to the AM60B side, indicating very strong AA6061-T4/AM60B bond in these areas. Furthermore, this work demonstrates VFAW’s capability in joining dissimilar lightweight metals such as Al/Mg, which is expected to be a great enabler in the ongoing push for vehicle weight reduction.

36 MATERIALS SCIENCE↗

A potential emerging issue concerning repair welding of out-of-core PWR components involving tritium exposure and 3 He retention

This paper identifies a potential but previously unrecognized risk of helium-induced embrittlement and cracking during repair welding of out-of-core pressurized water reactor (PWR) components exposed to tritium-contaminated coolant. While previous weldability concerns centered on 4 He accumulation in neutron-irradiated alloys located within the in-core or near-core regions, new measurements show that 3 He generated by tritium decay can accumulate in out-of-core components. Because hydrogen isotopes readily diffuse to grain boundaries and become trapped there, significant 3 He generation at grain boundaries may lead to cracking during weld repairs. Initial data from far-below-core PWR flux thimble tubes confirm the presence of 3 He levels above known cracking thresholds for repair welds. In conclusion, these findings indicate that out-of-core regions should be considered when defining safe weld repair windows in reactors operating for 60–100 years.

Extended PWR lifetimes↗

Formation mechanism of linear friction welded Ti-6Al-4V alloy joint based on microstructure observation

The microstructure of the linear friction welded Ti-6Al-4V titanium alloy joint was investigated by optical microscope, scanning electronic microscope and transmission electron microscope. Results show that the dynamic recovery and recrystallization resulting from the intensive plastic deformation and fast heating and cooling processes during linear friction welding account for the superfine {alpha} + {beta} grains in the weld center. Fine {alpha} grains distribute in the {beta} matrix or at the boundaries of {beta} grains. A mass of dislocations networks and metastructures present within the {alpha} and {beta} grains. - Research Highlights: {yields} TEM is employed in the analysis. {yields} The dynamic recovery is the main mechanism in thermal deformation of TC4. {yields} Superfine grains in the weld result from dynamic recovery and dynamic recrystallizaion, but the recrystallization is inadequate.

36 MATERIALS SCIENCE↗

The problem of intermixing of metals possessing no mutual solubility upon explosion welding (Cu-Ta, Fe-Ag, Al-Ta)

On the basis of the results obtained for joints of dissimilar metals such as copper-tantalum and iron-silver, the reason of immiscible suspensions mixing upon explosion welding has been cleared out. It has been found that the interface (plain or wavy) is not smooth and contains inhomogeneities, namely, cusps and local melting zones. The role of granulating fragmentation providing partitioning of initial materials as a main channel of input energy dissipation has been revealed. It has been shown that in joints of metals possessing normal solubility the local melting zones are true solutions, but if metals possess no mutual solubility the local melting zones are colloidal solutions. Realization of either emulsion or suspension variant takes place. The results can be used in the development of new joints of metals possessing no mutual solubility. - Highlights: Black-Right-Pointing-Pointer Immiscible pairs Ta/Cu and Fe/Ag are welded successfully by explosive welding. Black-Right-Pointing-Pointer Fragmentation provides for partitioning as the main energy dissipation channel. Black-Right-Pointing-Pointer Immiscible metals form colloidal solid solutions during solidification. Black-Right-Pointing-Pointer Melting and boiling temperatures ratio determines the colloidal solution type. Black-Right-Pointing-Pointer Local melting zones being in suspension form enhance welds hardening.

36 MATERIALS SCIENCE↗

Understanding the solidification and microstructure evolution during CSC-MIG welding of Fe–Cr–B-based alloy

The present is a study of the solidification and microstructure of Fe–28.2%Cr–3.8%B–1.5%Si–1.5%Mn (wt.%) alloy deposited onto a 1020 plain carbon steel substrate using the controlled short-circuit metal inert gas welding process. The as-solidified alloy was a metal matrix composite with a hypereutectic microstructure. Thermodynamic calculation based on the Scheil–Gulliver model showed that a primary (Cr,Fe){sub 2}B phase formed first during solidification, followed by an eutectic formation of the (Cr,Fe){sub 2}B phase and a body-centered cubic Fe-based solid solution matrix, which contained Cr, Mn and Si. Microstructure analysis confirmed the formation of these phases and showed that the shape of the (Cr,Fe){sub 2}B phase was irregular plate. As the welding heat input increased, the weld dilution increased and thus the volume fraction of the (Cr,Fe){sub 2}B plates decreased while other microstructural characteristics were similar. - Highlights: • We deposit Fe–Cr–B-based alloy onto plain carbon steel using the CSC-MIG process. • We model the solidification behavior using thermodynamic calculation. • As deposited alloy consists of (Cr,Fe){sub 2}B plates embedded in Fe-based matrix. • We study the effect of the welding heat input on the microstructure.

36 MATERIALS SCIENCE↗

Microstructural characterisation of friction stir welding joints of mild steel to Ni-based alloy 625

In this study, 6-mm-thick mild steel and Ni-based alloy 625 plates were friction stir welded using a tool rotational speed of 300 rpm and a travel speed of 100 mm·min{sup −1}. A microstructural characterisation of the dissimilar butt joint was performed using optical microscopy, scanning and transmission electron microscopy, and energy dispersive X-ray spectroscopy (XEDS). Six different weld zones were found. In the steel, the heat-affected zone (HAZ) was divided into three zones and was composed of ferrite, pearlite colonies with different morphologies, degenerated regions of pearlite and allotriomorphic and Widmanstätten ferrite. The stir zone (SZ) of the steel showed a coarse microstructure consisting of allotriomorphic and Widmanstätten ferrite, degenerate pearlite and MA constituents. In the Ni-based alloy 625, the thermo-mechanically affected zone (TMAZ) showed deformed grains and redistribution of precipitates. In the SZ, the high deformation and temperature produced a recrystallised microstructure, as well as fracture and redistribution of MC precipitates. The M{sub 23}C{sub 6} precipitates, present in the base material, were also redistributed in the stir zone of the Ni-based alloy. TMAZ in the steel and HAZ in the Ni-based alloy could not be identified. The main restorative mechanisms were discontinuous dynamic recrystallisation in the steel, and discontinuous and continuous dynamic recrystallisation in the Ni-based alloy. The interface region between the steel and the Ni-based alloy showed a fcc microstructure with NbC carbides and an average length of 2.0 μm. - Highlights: • Comprehensive microstructural characterisation of dissimilar joints of mild steel to Ni-based alloy • Friction stir welding of joints of mild steel to Ni-based alloy 625 produces sound welds. • The interface region showed deformed and recrystallised fcc grains with NbC carbides and a length of 2.0 μm.

36 MATERIALS SCIENCE↗

Characterization of bond line discontinuities in a high-Mn TWIP steel pipe welded by HF-ERW

In this work, the microstructure and defects in a high-frequency electrical resistance welded (HF-ERW) pipe of high-Mn twinning-induced plasticity (TWIP) steel were characterized. The microstructure of the base metal and the bond line were examined using both optical microscopy and scanning electron microscopy. The features of the bond line were similar to those of conventional steel. Simultaneously, the circumferential ductility was evaluated via a flaring test. It was concluded that the deterioration of the circumferential ductility in a high-Mn TWIP steel pipe was caused by irregular shaped oxide defects and a penetrator that had been formed during welding. Specifically, the penetrator, which is composed of MnO and Mn{sub 2}SiO{sub 4}, was found to be the most influential on the circumferential ductility of the welded pipe. The penetrator was analyzed using both an electron probe micro analyzer and transmission electron microscopy, and the formation sequence of the penetrator was evaluated. - Highlights: •This study focused on applying the HF-ERW process to the seam welding of expandable pipe using TWIP steels. •For improvement of the circumferential ductility, deterioration factors were characterized. •Penetrator which would mainly deteriorate the circumferential ductility consisted of round MnO and Mn{sub 2}SiO{sub 4}. •Metallurgical evidence of existing theory regarding the mechanism of defect formation during the HF-ERW was characterized.

36 MATERIALS SCIENCE↗

Effect of micromorphology at the fatigue crack tip on the crack growth in electron beam welded Ti-6Al-4V joint

In this paper, we describe experiments on welded joints of Ti-6Al-4V alloy specimens exhibiting fatigue characteristics in the base metal (BM), hot affected zone (HAZ) and fuse zone (FZ). The effect of micromorphology on crack propagation at the tip of the fatigue crack in joints formed by electron beam welding was investigated using an optical microscope, transmission electron microscope and other methodologies. The results demonstrated that the fatigue crack originated in and propagated along α/β boundaries in the BM. In the HAZ, the fatigue crack occurred at the boundary between martensite laths, and propagated through most irregular-equiaxed α phases and a few martensite laths. In the FZ, the fatigue crack originated at the boundaries between the fine crushing phases among martensite laths, and propagated along a majority of α/β boundaries and several narrow martensite laths. The electron beam welded joint of Ti-6Al-4V alloy showed instances of zigzag fatigue cracks that increased in degree from lowest in the HAZ, moderate in the FZ to greatest in the BM. Conversely, fatigue crack growth rate (FCGR) was greatest in the HAZ, less in the FZ and slowest in the BM. - Highlights: •Ti-6Al-4V welded joint exhibits different fatigue characteristics. •The fatigue crack propagates along α/β boundaries in the BM. •The fatigue crack propagates through α phases and martensite laths in the HAZ. •The fatigue crack propagates along α/β boundaries and martensite laths in the FZ. •Fatigue crack growth rate is fastest in the HAZ, less in the FZ, slowest in the BM.

36 MATERIALS SCIENCE↗

Defect features, texture and mechanical properties of friction stir welded lap joints of 2A97 Al-Li alloy thin sheets

1.4 mm 2A97 Al-Li alloy thin sheets were welded by friction stir lap welding using the stirring tools with different pin length at different rotational speeds. The influence of pin length and rotational speed on the defect features and mechanical properties of lap joints were investigated in detail. Microstructure observation shows that the hook defect geometry and size mainly varies with the pin length instead of the rotational speed. The size of hook defects on both the advancing side (AS) and the retreating side (RS) increased with increasing the pin length, leading to the effective sheet thickness decreased accordingly. Electron backscatter diffraction analysis reveals that the weld zones, especially the nugget zone (NZ), have the much lower texture intensity than the base metal. Some new texture components are formed in the thermo-mechanical affected zone (TMAZ) and the NZ of joint. Lap shear test results show that the failure load of joints generally decreases with increasing the pin length and the rotational speed. The joints failed during the lap shear tests at three locations: the lap interface, the RS of the top sheet and the AS of the bottom sheet. The fracture locations are mainly determined by the hook defects. - Highlights: • Hook defect size mainly varies with the pin length of stirring tool. • The proportion of LAGBs and substructured grains increases from NZ to TMAZ. • Weld zones, especially the NZ, have the much lower texture intensity than the BM. • Lap shear failure load and fracture location of joints is relative to the hook defects.

36 MATERIALS SCIENCE↗

Comparative study of microstructure and properties of low-alloy-steel/nickel-based-alloy interfaces in dissimilar metal weld joints prepared by different GTAW methods

Highlights: • Number of type I and type II boundaries: H-DMWJ > C-DMWJ > W-DMWJ. • Width carbon depleted zones and carbon enriched zones: H-DMWJ > C-DMWJ > W-DMWJ. • Type I and type II boundaries are susceptible to SCC and cracked during mechanical bending. • C-DMWJ has the best performance while H-DMWJ has the worst one. - Abstract: Low-alloy-steel/buttering (or welding) metal interfaces in safe-end dissimilar metal weld joints (DMWJs) at nuclear power plants are weak parts. To optimize the quality of the safe-end DMWJs used for the construction of domestic nuclear power plants and to improve the welding productivity, a series of DMWJs in full-size have been manufactured by using different gas tungsten arc welding (GTAW) methods. The microstructure, chemical composition distribution and local properties across the SA508/52(M) interfaces in these DMWJs are studied. The high heat input and long high temperature duration during hot-wire GTAW process promote the carbon diffusion and grain boundary migration and hence the DMWJ by hot-wire GTAW has the largest amount of type I and type II boundaries and the widest carbon depleted zones and carbon enriched zones, which resulting in the worst performance among the DMWJs in simulated primary water. Type I and type II boundaries are high angle random grain boundaries (RGBs) and Cr-depleted zones are found along type II boundaries resulting in their high susceptibility to SCC. In addition, these boundaries are prone to be cracked during mechanical bending process.

36 MATERIALS SCIENCE↗

Microstructural evolution and hardness response in the laser beam welded joints of pure titanium during recrystallization and grain growth

Highlights: • The LABs and high local misorientations indicate the existence of plastic strains in the as-welded HAZ and FZ. • During heat treatment the recrystallization occurs in the HAZs, decreasing plastic strains, but it doesn't appear in the FZs. • The coarse and unstrained grains gradually replace the fine and strained ones in the HAZs during recrystallization. • The decrease of plastic strains in the HAZs during recrystallization causes the descent of average hardness values based on the strain strengthening. - Abstract: Microstructural evolution and hardness response in the laser beam welded joints of pure titanium during recrystallization and grain growth were investigated by means of electron backscatter diffraction and hardness measurement. The low-angle boundaries (LABs) and high local misorientations, in the as-welded heat affected zone (HAZ) and fusion zone (FZ), indicate the existence of plastic strains caused by the plastic strains due to the thermal stress and the non-equilibrium phase transformations. The recrystallization occurs in the HAZs during heat treatment, but the grain growth after recrystallization does not appear under the heat treatment conditions. Moreover as a result of the slightly high impurity contents in the as-welded FZ, no distinct recrystallization is found in the FZs in this work. During recrystallization in the HAZs, the coarse and unstrained grains with equiaxed shape and smooth boundary gradually consume the fine and strained ones with irregular shape and serrate boundary. Meanwhile, the LABs disappear and the low local misorientations replace the high ones in the modified grains. The recrystallization during heat treatment causes the decrease of plastic strains in the HAZs, which reflects on the descent of average hardness values based on the strain strengthening.

36 MATERIALS SCIENCE↗

Macroscale property assessment and indentation characteristics of thick section friction stir welded AA 5083

The spatial gradients in microstructure have been proven to be effective in optimizing the performance of components, and several techniques have been developed to achieve this microstructure. Nevertheless, the local microstructural modification methods inevitably result in the formation of gradient microstructure leading to a variation in the property. Herein this work systematically investigates the effect of gradient microstructure formed during thick section friction stir weld Al5083 alloy on its mechanical properties. A novel macro-indentation technique, profilometer-based indentation plastometry (PIP), is utilized to capture the variation in the mechanical properties in the feedstock (rolled plate) and weld region. The feedstock exhibited a gradient microstructure owing to different stress states during rolling. Additionally, the stirring of the tool resulted in a complex material flow pattern producing a microstructure gradient in the weld region. The aspect ratio of the grains was identified as the primary factor causing variation in indentation response in the feedstock. In contrast, variation in the grain size in the weld region resulted in property variation. Overall, the stir zone has a lower yield strength (158±4MPa) than the base material (173±3MPa). In addition, microstructure heterogeneity in the stir zone resulted in lower elongation than the base material.

36 MATERIALS SCIENCE↗

Building A Simulation Model For The Prediction Of Temperature Distribution In Pulsed Laser Spot Welding Of Dissimilar Low Carbon Steel 1020 To Aluminum Alloy 6061

This paper describes the development of a computer model used to analyze the heat flow during pulsed Nd: YAG laser spot welding of dissimilar metal; low carbon steel (1020) to aluminum alloy (6061). The model is built using ANSYS FLUENT 3.6 software where almost all the environments simulated to be similar to the experimental environments. A simulation analysis was implemented based on conduction heat transfer out of the key hole where no melting occurs. The effect of laser power and pulse duration was studied.Three peak powers 1, 1.66 and 2.5 kW were varied during pulsed laser spot welding (keeping the energy constant), also the effect of two pulse durations 4 and 8 ms (with constant peak power), on the transient temperature distribution and weld pool dimension were predicated using the present simulation. It was found that the present simulation model can give an indication for choosing the suitable laser parameters (i.e. pulse durations, peak power and interaction time required) during pulsed laser spot welding of dissimilar metals.

36 MATERIALS SCIENCE↗

Full-Field Strain Measurement On Titanium Welds And Local Elasto-Plastic Identification With The Virtual Fields Method

One of the main problems in welding is the microstructural transformation within the area affected by the thermal history. The resulting heterogeneous microstructure within the weld nugget and the heat affected zones is often associated with changes in local material properties. The present work deals with the identification of material parameters governing the elasto--plastic behaviour of the fused and heat affected zones as well as the base material for titanium hybrid welded joints (Ti6Al4V alloy). The material parameters are identified from heterogeneous strain fields with the Virtual Fields Method. This method is based on a relevant use of the principle of virtual work and it has been shown to be useful and much less time consuming than classical finite element model updating approaches applied to similar problems. The paper will present results and discuss the problem of selection of the weld zones for the identification.

36 MATERIALS SCIENCE↗

Numerical simulation of linear fiction welding (LFW) processes

Solid state welding processes are becoming increasingly important due to a large number of advantages related to joining ''unweldable'' materials and in particular light weight alloys. Linear friction welding (LFW) has been used successfully to bond non-axisymmetric components of a range of materials including titanium alloys, steels, aluminum alloys, nickel, copper, and also dissimilar material combinations. The technique is useful in the research of quality of the joints and in reducing costs of components and parts of the aeronautic and automotive industries.LFW involves parts to be welded through the relative reciprocating motion of two components under an axial force. In such process the heat source is given by the frictional forces work decaying into heat determining a local softening of the material and proper bonding conditions due to both the temperature increase and the local pressure of the two edges to be welded. This paper is a comparative test between the numerical model in two dimensions, i.e. in plane strain conditions, and in three dimensions of a LFW process of AISI1045 steel specimens. It must be observed that the 3D model assures a faithful simulation of the actual threedimensional material flow, even if the two-dimensional simulation computational times are very short, a few hours instead of several ones as the 3D model. The obtained results were compared with experimental values found out in the scientific literature.

36 MATERIALS SCIENCE↗