Search NASA⌕ Search

SEARCH · Search NASA

Results for “defect evolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

In situ microstructural evolution in face-centered and body-centered cubic complex concentrated solid-solution alloys under heavy ion irradiation

This study characterizes the microstructural evolution of single-phase complex concentrated solid-solution alloy (CSA) compositions under heavy ion irradiation with the goal of evaluating mechanisms for CSA radiation tolerance in advanced fission systems. Three such alloys, Cr 18 Fe 27 Mn 27 Ni 28 , Cr 15 Fe 35 Mn 15 Ni 35 , and equimolar NbTaTiV, along with reference materials (pure Ni and E90 for the Cr-FeMnNi family and pure V for NbTaTiV) were irradiated at 50 K and 773 K with 1 MeV Kr ++ ions to various levels of displacements per atom (dpa) using in-situ transmission electron microscopy. Cryogenic irradiation resulted in small defect clusters and faulted dislocation loops as large as 12 nm in face-centered cubic (FCC) CSAs. With thermal diffusion suppressed at cryogenic temperatures, defect densities were lower in all CSAs than in their less compositionally complex reference materials indicating that point defect production is reduced during the displacement cascade stage. High temperature irradiation of the two FCC CSA resulted in the formation of interstitial dislocation loops which by 2 dpa grew to an average size of 27 nm in Cr 18 Fe 27 Mn 27 Ni 28 and 10 nm in Cr 15 Fe 35 Mn 15 Ni 35 . This difference in loop growth kinetics was attributed to the difference in Mn-content due to its effect on the nucleation rate by increasing vacancy mobility or reducing the stacking-fault energy.

36 MATERIALS SCIENCE↗

Mechanisms of Skyrmion and Skyrmion Crystal Formation from the Conical Phase

Real-space topological magnetic structures such as skyrmions and merons are promising candidates for information storage and transport. However, the microscopic mechanisms that control their formation and evolution are still unclear. In this work, using in situ Lorentz transmission electron microscopy, we demonstrate that skyrmion crystals (SkXs) can nucleate, grow, and evolve from the conical phase in the same ways that real nanocrystals form from vapors or solutions. More intriguingly, individual skyrmions can also “reproduce” by division in a mitosis-like process that allows them to annihilate SkX lattice imperfections, which is not available to crystals made of mass-conserving particles. Combined string method and micromagnetic calculations show that competition between repulsive and attractive interactions between skyrmions governs particle-like SkX growth, but nonconservative SkX growth appears to be defect mediated. Our results provide insights toward manipulating magnetic topological states by applying established crystal growth theory, adapted to account for the new process of skyrmion mitosis.

36 MATERIALS SCIENCE↗

Early self-organization of fission gas bubble superlattice formation in neutron-irradiated monolithic U-10Mo fuels

Self-organization of defect superlattices in far-from-equilibrium systems presents a promising way to mitigate swelling concerns in nuclear materials. The gas bubble superlattice (GBS) is a highly ordered, three-dimensional complex defect structure that can retain fission gasses in Uranium-Molybdenum (U-Mo) fuels. Transmission electron microscopy (TEM) investigation of monolithic U-10Mo fuel irradiated to 1.15 × 10 21 fissions/cm 3 and 1.30 × 10 21 fissions/cm 3 revealed that early-stage ordering preferentially occurs at the grain boundaries (GB) and that the critical bubble size for complete ordering is ~3 nm. Once formed at the GB, the GBS extends towards the grain interior; however, the spread in distance from the GB varies likely depending on the type and strength of the GB sink. TEM results also showed a possible correlation between the growth and evolution of the intragranular disordered bubbles and large dislocation networks. The fission product distribution in and outside of the GBS was also investigated confirming the presence of xenon in the GBS, as well as other fission products including cesium, barium, lanthanum, and cerium.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multi-pronged approach to improving carbon utilization by cyanobacterial cultures

The goal of this project was to increase the efficiency of carbon utilization by a Synechocystis biofuel production strain in a photobioreactor system by at least 50% using a multi-pronged approach that combined the best features of both biological and physicochemical CO 2 capture technologies to: 1) increase rates and extent of CO 2 absorption into the culture medium by addition of biocompatible amine solvents and a nanobubble gas delivery system, and 2) increase cellular rates of inorganic carbon uptake and carbon fixation through genetic engineering. In addition, the project plan included evaluating the use of fermentation effluent gases as a CO 2 source and demonstrating performance under outdoor conditions in closed-pond photobioreactor systems. These combined efforts would be guided by integrated technoeconomic and life-cycle analyses. Both physicochemical CO 2 capture technologies explored proved to be successful. The amine solvent monoethanolamine (MEA) was found to be biocompatible with a Synechocystis laurate production strain. Using an adaptive evolution strategy, an MEA-tolerant laurate production strain was developed that showed significantly increased carbon utilization over the parent strain. To our knowledge this was the first time nanobubble (NB) technology had been used as a carbon delivery system for algae production and it also proved quite successful as a proof of concept. Solutions containing CO 2 nanobubbles (Nano-BG11) at concentrations significantly higher than the aqueous CO 2 concentrations achieved with gas sparging were successfully generated and characterized with regard to bubble size (nm), concentration (NB/L), and pH stability as per project plan. Growth studies proved challenging. However, once the source of a puzzling growth defect was found and remedied Synechocystis was able to grow somewhat better in Nano-BG11 than in standard BG11 medium.

09 BIOMASS FUELS↗

Entropy-Driven Structural Evolution in Ceramic Oxides

High-entropy ceramics, with five or more elements randomly occupying the same cation crystallographic sites, offer vast compositional diversity and unique properties for material design and applications. However, for many dissimilar elements, entropic stabilization cannot overcome the enthalpic barrier to cation substitution. As a result, most high-entropy ceramics incorporate only a few similar elements, limiting the in-depth exploration of the effect of entropy on ceramic properties. Here, we first use density functional theory to model fluorite crystal structures composed of 1-10 elements and then experimentally present practical fluorite oxide nanostructures containing 1, 3, 8, and 15 metals, as well as a record-breaking 25-element high-entropy ceramic incorporating a diverse palette of rare-earth, transition, alkaline, p-block, and noble metals. As entropy increases, structural and configurational disorder in the solid solution rises, altering structural features such as lattice distortion, crystallinity, homogeneity, defect density, and thermal stability. This research provides new insights and understanding of the role of entropy in stabilizing compositionally complex ceramics.

Liu, Shuo↗

Resolving atomic transport through iron oxide under irradiation using isotopic tracers

Structural materials in nuclear environments are exposed to complex and harsh conditions, including high temperatures, corrosive solutions, and irradiation. Material stability and likewise degradation are fundamentally controlled by atomic transport mechanisms. Here, we investigate the influence of radiation-induced, non-equilibrium point defect populations on mass transport within model oxide systems using isotopic tracers and atom probe tomography. An isotopically labelled hematite (a-Fe2O3) film was synthesized with 16O- and 18O-rich layers (>30nm and 10 nm, respectively) sequentially deposited via molecular beam epitaxy. One region of the film was proton irradiated to ~0.1 dpa at 450°C, and regions outside the beam spot provided a non-irradiated control of thermal annealing only. 3D APT was used to directly visualize the elemental and O-isotopic redistribution following both thermal and combined thermal and irradiation conditions. Complementary scanning transmission electron microscopy (STEM) was also employed to study the microstructural evolution. Error function fits of the 18O-concentration profiles enabled quantification of diffusion coefficients.

isotopic tracers, diffusion, proton irradiation, h↗

Pseudospectral Landau-Lifshitz description of magnetization dynamics

Magnetic materials host a wealth of nonlinear dynamics, textures, and topological defects. This is possible due to the competition between strong nonlinearity and dispersion, which act at the atomic scale, as well as long-range interactions. However, these features are difficult to study analytically and numerically because of the vastly different temporal and spatial scales involved. Here, in this work, we present a pseudospectral approach for the Landau-Lifshitz equation that invokes energy and momentum conservation embodied in the magnon dispersion relation to accurately describe both atomic and continuum limits. Furthermore, this approach enables analytical study at every scale. We show the applicability of this model in both the continuum and atomic limit by investigating modulational instability and ultrafast evolution of magnetization due to transient grating, respectively, in a one-dimensional ferromagnetic chain with perpendicular magnetic anisotropy. This model provides the possibility of grid-independent multiscale numerical approaches that will enable the description of singularities within a single framework.

1-dimensional spin chains↗

In-situ irradiation-induced studies of grain growth kinetics of nanocrystalline UO 2

The thermal conductivity of UO 2 fuel needs to be high enough to dissipate the heat generated from the fission reaction. Since grain size affects thermal conductivity and grain size can evolve with irradiation, it is critical to understand in-reactor UO 2 grain growth. Most studies of grain growth in UO 2 are based on thermally driven processes at elevated temperatures. However, studies have shown that grain growth can occur even at cryogenic temperatures by ballistic processes. Such irradiation-induced grain growth in UO 2 is yet to be studied. Advanced in-situ Kr ion irradiation and transmission electron microscopy were systematically performed on nanocrystalline UO 2 thin films at temperatures ranging from 50 K to 1073 K; grain growth was observed at all temperatures. A combination of manual and machine learning techniques was used to measure and plot grain size evolution against irradiation fluence at various irradiation temperatures. The machine learning method has significantly improved the analysis efficiency and reduced human labors. The grain diameter data were fitted using classical grain growth and thermal spike models to describe grain growth kinetics with and without irradiation effect. Grain growth during low temperature irradiation (≤ 475 K) can be well described by the thermal spike model. Above 475 K, there were additional thermally assisted processes that further accelerate the grain growth. At the highest irradiation temperature about 1075 K, both irradiation-induced dislocation loops and cavities/bubbles were observed to form in the UO 2 . In this report, the effects of irradiation-induced defects on grain growth kinetics are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A microstructural signature of the coesite-quartz transformation: New insights from high-pressure experiments and EBSD

Ultra-high pressure (UHP) metamorphism is difficult to identify in continental crust as few petrological barometers are suitable for dominantly felsic lithologies. In such cases, burial to extreme depths is commonly identified through the preservation of coesite, a high-pressure polymorph of SiO 2 that typically forms at depths exceeding ∼ 100 km (i.e., > 2 GPa pressure). Unfortunately, coesite readily transforms to quartz upon exhumation, meaning that UHP terranes may often be overlooked. While some studies have suggested that quartz may inherit an orientation signature indicative of former coesite, both the specific nature of this signature and the conditions favouring its development remain uncertain. Here, to address this problem, we combine electron backscatter diffraction analysis of natural and experimental samples to explore microstructural evolution across the coesite-quartz phase transformation. We demonstrate that neighbouring domains of quartz commonly feature an 84 ± 4° rotation of [c] axes around the pole of a common {m} plane. This orientation relationship is a product of epitaxy, whereby the {$11\bar{2}2$} Japan twin plane in quartz nucleates on the (010) plane in coesite. In supercell simulations, the nucleation of Japan twins can be explained by the energetically favourable alignment of quartz tetrahedra on parental coesite tetrahedra. Through experiments, we demonstrate that this signature emerges over a broad range of conditions, regardless of the availability of nucleation sites (e.g., grain boundaries) or the density of crystal lattice defects (e.g., dislocations). Overall, our work provides a quantitative and unambiguous tool for identifying UHP terranes from quartz in isolation.

Coesite↗

Capture efficiency and bias from the defect dynamics near grain boundaries in BCC Fe using mesoscale simulations

The capture efficiency describes the capability of a sink, such as a grain boundary (GB), dislocation, and void, to absorb point defects (PDs). The bias defines the difference in capture efficiency between the absorption of a vacancy and dumbbell at a sink. Complete kinetic information on PDs, including diffusion barriers and diffusion orientations, as well as accurate saddle points, are needed to determine the capture efficiency and bias at a sink accurately, which is computationally demanding. Here, in the present study, the Self-Evolving Atomistic Kinetic Monte Carlo (SEAKMC) method was used to investigate the defect dynamics of PDs near different types of grain boundaries (GBs) (with both $\langle$100$\rangle$ and $\langle$110$\rangle$ families) accurately in body-centered cubic (BCC) iron (Fe). The capture efficiency, sink strength, and bias factor of different types of GBs were determined in Fe, which, different from traditional rate theory estimation, showed a distinct capture efficiency, sink strength, and bias in different GBs. The results demonstrate a strong positive correlation between the capture efficiency and the GB strain width, instead of the GB misorientation, GB energy, or GB-PD binding energy, which have been investigated previously. This work provides valuable insight into the radiation-induced microstructural evolution of GBs.

36 MATERIALS SCIENCE↗

NiGa 2 O 4 interfacial layers in NiO/Ga 2 O 3 heterojunction diodes at high temperature

NiO/Ga 2 O 3 heterojunction diodes have attracted attention for high-power applications, but their high temperature performance and reliability remain underexplored. Here, we report the time evolution of the electrical properties in the widely studied p-NiO/n-Ga 2 O 3 heterojunction diodes and formation of NiGa 2 O 4 interfacial layers at high temperatures. Results of our thermal cycling experiment show an initial leakage current increase which stabilizes after sustained thermal load, due to reactions at the NiO–Ga 2 O 3 interface. High-resolution TEM microstructure analysis of the devices after thermal cycling indicates that the NiO–Ga 2 O 3 interface forms a ternary compound at high temperatures, and thermodynamic calculations suggest the formation of the spinel NiGa 2 O 4 layer between NiO and Ga 2 O 3 . First-principles defect calculations find that NiGa 2 O 4 shows low p-type intrinsic doping and hence can serve to limit electric field crowding at the interface. Vertical NiO/ Ga 2 O 3 diodes with intentionally grown 5 nm thin spinel-type NiGa 2 O 4 interfacial layers show an excellent device ON/OFF ratio of >10 10 (± 3 V), V ON of ~1.9 V, and increased breakdown voltage of ~1.2 kV for an initial unoptimized 300 lm diameter device. These p–n heterojunction diodes are promising for high-voltage, high temperature applications.

30 DIRECT ENERGY CONVERSION↗

In-situ hydrogen microstructural characterization of Si heterojunction passivation: Addressing V OC degradation and mitigation pathways

Si heterojunction (SHJ) solar cells have demonstrated record efficiency >27%, approaching the theoretical limit of ≈ 29%, primarily due to best surface/interface defect passivation provided by deposited thin layers of hydrogenated amorphous silicon (a-Si:H). Such excellent surface/interface passivation reduces recombination loss and result in >100 mV improvement of cell open circuit voltage (V OC ) to ≈ 750 mV, thus the cell efficiency. However, fielded SHJ modules exhibit loss of V OC and hence efficiency over time in years, presumably due to degradation related to a-Si:H layers. This adversely affects the technology’s market acceptance, and levelized cost of energy (LCOE). It is hypothesized that the origin of a-Si:H degradation is somehow related to the presence of weak Si–Si bonds and hydrogen in a-Si:H films. The objective of this project is to test this hypothesis by directly measuring chemical and structural changes occurring within SHJ component layers and solar cells. This is achieved by developing an innovative in-situ Fourier transform infrared (FTIR) spectrometry apparatus to monitor hydrogen microstructural changes occurring within amorphous silicon and decipher hydrogen evolution kinetics over time when samples are exposed to heat and/or light stress. These in-situ measured hydrogen microstructural changes are correlated to the changes in effective minority carrier lifetime (τ eff ), implied V OC (iV OC ), surface recombination velocity (S), and cell V OC . These mechanistic understandings will provide critical guidance to mitigate the V OC -driven degradation of SHJ solar cell performance. Passivation optimization and degradation analysis of individual SHJ component structures were achieved through systematic deposition of three symmetric structures and the completed SHJ solar cell structure. The three symmetric structures used were intrinsic a-Si:H [(i)a-Si:H] layers in a bilayer structure, intrinsic and p-type doped stacked layers [(i-p)a-Si:H] representing the front heterojunction in the SHJ cell, and intrinsic and n-typed doped stacked layers [(i-n)a-Si:H] representing the back-side back surface field (BSF) in the SHJ cell. State-of-the-art passivation qualities are demonstrated by a champion iV OC of 740 mV for the (i)a-Si:H layers, and the (i-n)a-Si:H symmetric structure. A 725 mV iV OC is observed for the (i-p)a-Si:H symmetric structure. These symmetric passivated SHJ component structures were subsequently subjected to different accelerated lifetime (ALT) stressors to identify which conditions contribute the most to iV OC degradation. Degradation of the thin (10 nm) (i)a-Si:H passivation layers without any additional overlying layers is minimal; complexity of this study arises due to unavoidable surface oxidation of (i)a-Si:H layer during most of the stress application, which is likely irrelevant for a full SHJ cell configuration with overlying protective layers. The iV OC degradation of symmetric structures is found to occur primarily at the (i-p)a-Si:H passivation stack under dark heat stress with associated hydrogen loss from the (p)a-Si:H layer. An activation energy for increase in S (defect creation) of 0.65 eV can be correlated to the activation energy of ≈ 0.4 eV for hydrogen loss from the (i-p)a-Si:H stack. This also suggests the presence of weakly bonded hydrogen in the (p)a-Si:H films, which effuses out of the film stack at such low activation energy. When light and heat stress are applied together, similar hydrogen loss from (i-p)a-Si:H stack is observed, however, does not appreciably degrade iV OC or increase S. This is an important result and departure from direct correlation between hydrogen loss and defect creation. This perhaps indicates additional defect chemistries or annealing that might be occurring in the presence of light requiring further detailed defect measurements. The full SHJ cell structure used for this project is depicted in Fig.1(d). SHJ cells with an initial V OC ≈ 700 mV were fabricated and subjected to similar ALT stress conditions. Cell V OC is found to degrade the most under dark heat stress and is confirmed by observed hydrogen migration out of the (i-p)a-Si:H stack. However, hydrogen cannot escape from the cell stack, it accumulates near the (p)a-Si:H/ITO contact interface, where ITO acts as a barrier preventing hydrogen loss. Furthermore, light-heat combined stress does not degrade V OC appreciably, confirming the occurrence of a defect annealing process.

14 SOLAR ENERGY↗

Strong Fermi-level pinning at metal contacts to halide perovskites

The performance of halide perovskite-based electronic and optoelectronic devices is often related to interfacial charge transport. To shed light on the underlying physical and chemical properties of CH 3 NH 3 PbI 3 (MAPbI 3 ) in direct contact with common electrodes Al, Ti, Cr, Ag, and Au, the evolution of interfacial properties and Fermi level pinning is systematically studied. Given a unique experimental facility, pristine interfaces without any exposure to ambient air were prepared. We observe aggregation of substantial amounts of metallic lead (Pb 0 ) at the metal/MAPbI 3 interface, resulting from the interfacial reaction between the deposited metal and iodine ions from MAPbI 3 . It is found that the Schottky barrier height at the metal/MAPbI 3 interface is independent of the metal work function due to strong Fermi level pinning, possibly due to the metallic Pb 0 aggregates, which act as interfacial trap sites. The charge neutrality level of MAPbI 3 is consistent with the energy level of Pb 0 -related defects, indicating that Pb 0 interfacial trap states can be nonradiative recombination sites. Here this work underlines that control of chemical bonding at interfaces is a key factor for designing future halide perovskite-based devices.

36 MATERIALS SCIENCE↗

Effect of surface steps on chemical ordering in the subsurface of Cu(Au) solid solutions

Atomic steps are typically assumed to only influence surface phenomena of solids. In contrast, in this paper we show, using in-situ atomic-resolution electron microscopy observations and atomistic modeling, the pronounced effect from surface stepsin inducing compositional and structural evolution in the subsurface of a Cu(Au) solid solution. We find that Au surface segregation results in a stacked sequence of Cu-Au ordered phases in the subsurface. The presence of a monatomic step at the surface induces the formation of an anti-phase boundary that extends from the surface step to deeper layers by maintaining the same composition profile associated with each terrace. The bunching of surface steps induces chemical disordering of the Cu-Au ordered phases in the subsurface region of the bunched steps. These results demonstrate the instant propagation of surface dynamics of atomic steps into the subsurface region and can find broader applicability in utilizing surface defects to tune the composition and structure in the subsurface of alloys.

36 MATERIALS SCIENCE↗

Computational modeling of grain boundary segregation: A review

Nearly all metals, alloys, ceramics, and their associated composites are polycrystalline in nature, with grain boundaries that separate well-defined crystalline regions that influence materials properties. In all but the most pure elemental systems, intentional solutes or impurities are present and can segregate to, or less commonly away from, the grain boundaries, in turn influencing boundary behavior, their stability, and associated materials properties. In some cases, grain-boundary segregation can also trigger “phase-like” structural transitions that dramatically alter the essential nature of the boundary. With the development of advanced electron microscopy techniques, researchers can directly observe grain-boundary structures and segregation with atomic precision. Despite such spatial resolution, the underlying mechanisms governing grain-boundary segregation remain difficult to characterize. As a result, computational modeling techniques such as density functional theory, molecular dynamics, mesoscale phase-field, continuum defect theory, and others are important complementary tools to experimental observations for studying grain-boundary segregation behavior. In conclusion, these computational methods offer the ability to explore the underlying formation mechanisms of grain-boundary segregation, elucidate complex segregation behavior, and provide insights into solutions to effectively controlling microstructure.

36 MATERIALS SCIENCE↗

Transforming an Ionic Conductor into an Electronic Conductor via Crystallization: In Situ Evolution of Transference Numbers and Structure in (La,Sr)(Ga,Fe)O 3–x Perovskite Thin Films

Mixed-conducting perovskites are workhorse electrochemically active materials, but typical high-temperature processing compromises their catalytic activity and chemo-mechanical integrity. Low-temperature pulsed laser deposition of amorphous films plus mild thermal annealing is an emerging route to form homogeneous mixed conductors with exceptional catalytic activity, but little is known about the evolution of the oxide-ion transport and transference numbers during crystallization. Here the coupled evolution of ionic and electronic transport behavior and structure in room-temperature-grown amorphous (La,Sr)(Ga,Fe)O 3-x films as they crystallize is explored. In situ ac-impedance spectroscopy with and without blocking electrodes, simultaneous capturing-synchrotron-grazing-incidence X-ray diffraction, dc polarization, transmission electron microscopy, and molecular dynamics simulations to evaluate isothermal and non-isothermal crystallization effects and the role of grain boundaries on transference numbers is combined. Ionic conductivity increases by ≈2 orders of magnitude during crystallization, with even larger increases in electronic conductivity. Consequently, as crystallinity increases, LSGF transitions from a predominantly ionic conductor to a predominantly electronic conductor. The roles of evolving lattice structural order, microstructure, and defect chemistry are examined. Grain boundaries appear relatively nonblocking electronically but significantly blocking ionically. The results demonstrate that ionic transference numbers can be tailored over a wide range by tuning crystallinity and microstructure without having to change the cation composition.

36 MATERIALS SCIENCE↗

A non-melting additive approach to structural repair of aluminum aircraft fastener holes

The damage to fastener holes in aerospace aluminum structures presents significant challenges for aircraft durability, and conventional bushing methods for repairing oversized holes often fall short due to the lack of metallurgical bonding and limited edge distance availability. This study investigates additive friction stir deposition, a non-melting additive process, as a viable alternative for the structural repair of aerospace fastener holes. The repair process, demonstrated on AA7050 (Al-Zn-Mg-Cu-Zr) hole structures, involves filling oversized holes with new material and machining to restore the original hole size. The repaired hole coupons are defect-free and exhibit good fatigue performance under fully reversed tension-compression loading (R = -1). At a nominal stress amplitude of 123.5 MPa, the average number of cycles to failure is 12,666 for unrepaired baseline coupons and 17,372 for effectively repaired coupons. Restoring complex geometries without compromising fatigue performance has been difficult in aerospace applications; this study marks the first demonstration of additive repair that consistently outperforms the unrepaired baseline coupons. Notably, the result is achieved through a low-energy, cost-effective solution without the need for post-repair heat treatment. Except for a few outliers, the post-repair fatigue performance generally remains inferior to that of undamaged, pristine coupons, likely due to precipitate evolution in AA7050 caused by the thermomechanical processing nature of additive friction stir deposition. This evolution weakens the repair region and the adjacent base material, leading to faster crack initiation and growth compared to the properly aged base material, AA7050-T7451.

36 MATERIALS SCIENCE↗