Search NASA⌕ Search

SEARCH · Search NASA

Results for “depth profiling”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 559 records · Page 31

Positron Annihilation Studies In Polymer Nano-Composites

Positron annihilation spectroscopy coupled with a variable mono-energy positron beam has been applied to study nanoscale polymeric nanocomposites. New information about multilayer depth profiles and structures, interfacial free-volume and open space properties have been obtained in polystyrene/carbon nano fiber composites. The S parameter in Doppler Broadening Energy Spectra combined slow positron beam is used to quantitatively represent the free volume, open spaces, and interactions in the interface between polystyrene matrix and carbon nanofibers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Imaging laser analysis of building materials - practical examples

The Laser induced Breakdown Spectroscopy (LIBS) is supplement and extension of standard chemical methods and SEM- or Micro-RFA-applications for the evaluation of building materials. As a laboratory method LIBS is used to gain color coded images representing composition, distribution of characteristic ions and/or ingress characteristic of damaging substances. To create a depth profile of element concentration a core has to be taken and split along the core axis. LIBS was proven to be able to detect all important elements in concrete, e. g. Chlorine, Sodium or Sulfur, which are responsible for certain degradation mechanisms and also light elements like lithium or hydrogen. Practical examples are given and a mobile system for on-site measurements is presented.

36 MATERIALS SCIENCE↗

Effects of ozone exposure on 'Golden' papaya fruit by photoacoustic phase-resolved method: Physiological changes associated with carbon dioxide and ethylene emission rates during ripening

This work addresses the effects of ozone activity on the physiology of 'Golden' papaya fruit. Depth profile analysis of double-layer biological samples was accomplished using the phase-resolved photoacoustic spectroscopy. The feasibility of the method was demonstrated by singling out the spectra of the cuticle and the pigment layers of papaya fruit. The same approach was used to monitor changes occurring on the fruit during ripening when exposed to ozone. In addition, one has performed real time studies of fluorescence parameters and the emission rates of carbon dioxide and ethylene. Finally, the amount of pigments and the changes in waxy cuticle have been monitored. Results indicate that a fruit deliberately subjected to ozone at a level of 6 ppmv underwent ripening sooner (at least 24-48 h) than a fruit stored at ambient conditions. Moreover, ozone caused a reduction in the maximum quantum yield of photosynthetic apparatus located within the skin of papaya fruit.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-resolution x-ray diffraction investigation of relaxation and dislocations in SiGe layers grown on (001), (011), and (111) Si substrates

This work presents a detailed characterization, using high-resolution x-ray diffraction, of multilayered Si{sub 1-x}Ge{sub x} heterostructures grown on (001), (011), and (111) Si substrates by reduced pressure chemical vapor deposition. Reciprocal space mapping has been used to determine both the strain and Ge concentration depth profiles within each layer of the heterostructures after initially determining the crystallographic tilt of all the layers. Both symmetric and asymmetric reciprocal space maps were measured on each sample, and the evaluation was performed simultaneously for the whole data set. The ratio of misfit to threading dislocation densities has been estimated for each individual layer based on an analysis of diffuse x-ray scattering from the defects.

36 MATERIALS SCIENCE↗

Characterization of Vacancy Defects in Carbon Ion Irradiated Graphite Using Positrons

Highly Oriented Pyrolytic Graphite samples are irradiated with 200 keV Carbon ions to fluences of 10{sup 14} and 10{sup 15} C{sup +} ions/cm{sup 2}. Depth resolved Doppler lineshape S-parameter exhibited large increase in peak damage regions of the sample, indicating the existence of irradiation induced vacancy defects. The depth profile of the defect region has been deduced from the analysis of the experimental data. It is found that divacancies are the dominant defects in the irradiated samples.

36 MATERIALS SCIENCE↗

Influence of crystal orientation and ion bombardment on the nitrogen diffusivity in single-crystalline austenitic stainless steel

The nitrogen diffusivity in single-crystalline AISI 316L austenitic stainless steel (ASS) during ion nitriding has been investigated at different crystal orientations ((001), (110), (111)) under variations of ion flux (0.3-0.7 mA cm{sup -2}), ion energy (0.5-1.2 keV), and temperature (370-430 deg. C). The nitrogen depth profiles obtained from nuclear reaction analysis are in excellent agreement with fits using the model of diffusion under the influence of traps, from which diffusion coefficients were extracted. At fixed ion energy and flux, the diffusivity varies by a factor up to 2.5 at different crystal orientations. At (100) orientation, it increases linearly with increasing ion flux or energy. The findings are discussed on the basis of atomistic mechanisms of interstitial diffusion, potential lattice distortions, local decomposition, and ion-induced lattice vibrational excitations.

36 MATERIALS SCIENCE↗

Novel 4{pi} Detection System for the Measurement of the {sup 6}Li(n,{alpha}){sup 3}H Reaction Cross Section

A dedicated one-dimensional Time Projection Chamber (1D-TPC) was designed and produced at IRMM to determine the {sup 6}Li(n,{alpha}){sup 3}H cross section in the 0.4-2.8 MeV energy range, aiming at 5% accuracy. The basic TPC components were a twin gridded ionisation chamber (GIC) with interwired electrodes and fast digitisation of the anode and cathode signals. The energy of both reaction products emitted from a thin {sup 6}LiF sample at the common TPC cathode was measured. A Kr(97%)CO{sub 2}(3%) mixture was used as the detector gas at a pressure up to 3.5 bar. A {sup 238}U sample mounted on the cathode of an ionisation chamber without grid was used as the neutron flux monitor. Special care was taken to reduce the experimental sources of uncertainty. The beam-monitor {sup 238}U sample was characterised at IRMM by low-geometry {alpha}-counting with an accuracy of 0.1%. A {sup 6}Li sample was produced at IRMM by vacuum evaporation of {sup 6}LiF onto transparent aluminium backing. The number of {sup 6}Li atoms will be measured via Thermal Neutron Depth Profiling with an expected accuracy of 2% with respect to an IRMM Standard Reference Material. First test measurements were performed using a monoenergetic neutron beam produced by the T(p,n){sup 3}He reaction at the IRMM 7 MV Van de Graaff accelerator. The experimental method and preliminary results are presented.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Nano-structural Characteristics of N-doped ZnO Thin Films and Fabrication of Film Bulk Acoustic Resonator Devices

N-doped ZnO thin films (ZnO:N) with c-axis preferred orientation were prepared on p-Si(100) wafers, using an RF magnetron sputter deposition. For ZnO deposition, N{sub 2}O gas was employed as a dopant source and various deposition conditions such as N{sub 2}O gas fraction and RF power were applied. In addition, the film bulk acoustic resonator (FBAR) devices with three kinds of top electrodes patterns were fabricated by using the N-doped ZnO thin films as the piezoelectric layers. The depth profiles of the nitrogen [N] atoms incorporated into the ZnO thin films were investigated by an Auger Electron Spectroscopy (AES) and the nano-scale structural characteristics of the N-doped ZnO (ZnO:N) thin films were also investigated by a scanning electron microscope (SEM) technique. The fabricated resonators were evaluated by measuring the return loss (S{sub 11}) characteristics using a probe station and E8361A PNA Network Analyzer.

36 MATERIALS SCIENCE↗

Contactless monitoring of Ge content and B concentration in ultrathin single and double layer Si{sub 1-x}Ge{sub x} epitaxial films using multiwavelength micro-Raman spectroscopy

Non-contact monitoring of Ge content and B concentration in single and double Si{sub 1-x}Ge{sub x} epitaxial layers on Si(100) device wafers was attempted using high-resolution, multiwavelength micro-Raman spectroscopy. The Ge content and B concentration determined by secondary ion mass spectroscopy (SIMS) depth profiling showed very strong correlation with the position and full-width-at-half-maximum of the Si-Si peak from the Si{sub 1-x}Ge{sub x} epitaxial layers as determined by Raman measurements. High resolution X-ray diffraction (HRXRD) characterization was done for all wafers to determine Ge and B sensitivity and form comparisons with Raman and SIMS analysis. The non-destructive, in-line monitoring of Ge content and B concentration of single and double Si{sub 1-x}Ge{sub x} epitaxial layers with thickness ranging from 5 {approx} 120 nm, on small area monitoring pads, was successfully demonstrated by multiwavelength micro-Raman spectroscopy during epitaxial process optimization, material property verification, and quality control applications.

36 MATERIALS SCIENCE↗

Magnetic and electronic properties of the interface between half metallic Fe{sub 3}O{sub 4} and semiconducting ZnO

We have investigated the magnetic depth profile of an epitaxial Fe{sub 3}O{sub 4} thin film grown directly on a semiconducting ZnO substrate by soft x-ray resonant magnetic reflectometry (XRMR) and electron energy loss spectroscopy (EELS). Consistent chemical profiles at the interface between ZnO and Fe{sub 3}O{sub 4} are found from both methods. Valence selective EELS and XRMR reveal independently that the first monolayer of Fe at the interface between ZnO and Fe{sub 3}O{sub 4} contains only Fe{sup 3+} ions. Besides this narrow 2.5 A interface layer, Fe{sub 3}O{sub 4} shows magnetic bulk properties throughout the whole film making highly efficient spin injection in this system feasible.

36 MATERIALS SCIENCE↗

Growth of AlN/SiC/AlN quantum wells on Si(111) by molecular beam epitaxy

AlN/SiC/AlN quantum well structures have been grown on Si(111) by molecular beam epitaxy at 700 deg. C. The microstructure is single-crystal wurtzite AlN and cubic SiC with stacking sequence disorder. Depth profiles taken by Auger electron spectroscopy indicate that the ratio of Si to C is about 5:4. Layers with lower carbon content exhibit regions with five-fold superstructures. Fourier transform infrared spectroscopy confirms the presence of Al-N and Si-C bonds. Our work demonstrates the feasibility of a low-temperature synthesis route for epitaxial SiC and AlN/SiC heterostructures on Si.

36 MATERIALS SCIENCE↗

Strain control of AlGaN/GaN high electron mobility transistor structures on silicon (111) by plasma assisted molecular beam epitaxy

This paper reports on the use of plasma assisted molecular beam epitaxy of AlGaN/GaN-based high electron mobility transistor structures grown on 4 in. Si (111) substrates. In situ measurements of wafer curvature during growth proved to be a very powerful method to analyze the buffer layer's thickness dependent strain. The Ga/N ratio at the beginning of growth of the GaN buffer layer is the critical parameter to control the compressive strain of the entire grown structure. An engineered amount of compressive strain must be designed into the structure to perfectly compensate for the tensile strain caused by differences in the thermal expansion coefficient between the epi-layer and substrate during sample cool down from growth temperatures. A maximum film thickness of 4.2 {mu}m was achieved without the formation of any cracks and a negligible bow of the wafers below 10 {mu}m. Measurement of the as-grown wafers revealed depth profiles of the charge carrier concentration comparable to values achieved on SiC substrates and mobility values of the two dimensional electron gas in the range 1230 to 1350 cm{sup 2}/Vs at a charge carrier concentration of 6.5-7 10{sup 12}/cm{sup 2}. First results on processed wafers with 2 {mu}m thick buffer layer indicate very promising results with a resistance of the buffer, measured on 200 {mu}m long contacts with 15 {mu}m pitch, in the range of R > 10{sup 9}{Omega} at 100 V and breakdown voltages up to 550 V.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of ion source configuration and its operation parameters on the target sputtering and implantation process

In the work, investigation of the features and operation regimes of sputter enhanced ion-plasma source are presented. The source is based on the target sputtering with the dense plasma formed in the crossed electric and magnetic fields. It allows operation with noble or reactive gases at low pressure discharge regimes, and, the resulting ion beam is the mixture of ions from the working gas and sputtering target. Any conductive material, such as metals, alloys, or compounds, can be used as the sputtering target. Effectiveness of target sputtering process with the plasma was investigated dependently on the gun geometry, plasma parameters, and the target bias voltage. With the applied accelerating voltage from 0 to 20 kV, the source can be operated in regimes of thin film deposition, ion-beam mixing, and ion implantation. Multi-component ion beam implantation was applied to {alpha}-Fe, which leads to the surface hardness increasing from 2 GPa in the initial condition up to 3.5 GPa in case of combined N{sub 2}-C implantation. Projected range of the implanted elements is up to 20 nm with the implantation energy 20 keV that was obtained with XPS depth profiling.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Probing spectroscopic like information using resonant scattering

Resonant x-ray scattering can combine layer sensitivity of reflectivity technique with short-range structural sensitivity of absorption technique due to element specificity and contrast variation mechanism of resonant effect. We demonstrated the idea through depth profile study of chemical composition of multi-element thin film system at soft x-ray spectral range near boron K-absorption edge.

36 MATERIALS SCIENCE↗

A novel method for effective sodium ion implantation into silicon

Although sodium ion implantation is useful to the surface modification of biomaterials and nano-electronic materials, it is a challenging to conduct effective sodium implantation by traditional implantation methods due to its high chemical reactivity. In this paper, we present a novel method by coupling a Na dispenser with plasma immersion ion implantation and radio frequency discharge. X-ray photoelectron spectroscopy (XPS) depth profiling reveals that sodium is effectively implanted into a silicon wafer using this apparatus. The Na 1s XPS spectra disclose Na{sub 2}O-SiO{sub 2} bonds and the implantation effects are confirmed by tapping mode atomic force microscopy. Our setup provides a feasible way to conduct sodium ion implantation effectively.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

As-grown deep-level defects in n-GaN grown by metal-organic chemical vapor deposition on freestanding GaN

Traps of energy levels E{sub c}-0.26 and E{sub c}-0.61 eV have been identified as as-grown traps in n-GaN grown by metal-organic chemical vapor deposition by using deep level transient spectroscopy of the Schottky contacts fabricated by resistive evaporation. The additional traps of E{sub c}-0.13 and E{sub c}-0.65 eV have been observed in samples whose contacts are deposited by electron-beam evaporation. An increase in concentration of the E{sub c}-0.13 and E{sub c}-0.65 eV traps when approaching the interface between the contact and the GaN film supports our argument that these traps are induced by electron-beam irradiation. Conversely, the depth profiles of as-grown traps show different profiles between several samples with increased or uniform distribution in the near surface below 50 nm. Similar profiles are observed in GaN grown on a sapphire substrate. We conclude that the growth process causes these large concentrations of as-grown traps in the near-surface region. It is speculated that the finishing step in the growth process should be an essential issue in the investigation of the surface state of GaN.

36 MATERIALS SCIENCE↗

New beam line for time-of-flight medium energy ion scattering with large area position sensitive detector

A new beam line for medium energy ion mass scattering (MEIS) has been designed and set up at the Angstroem laboratory, Uppsala University, Sweden. This MEIS system is based on a time-of-flight (ToF) concept and the electronics for beam chopping relies on a 4 MHz function generator. Repetition rates can be varied between 1 MHz and 63 kHz and pulse widths below 1 ns are typically obtained by including beam bunching. A 6-axis goniometer is used at the target station. Scattering angle and energy of backscattered ions are extracted from a time-resolved and position-sensitive detector. Examples of the performance are given for three kinds of probing ions, {sup 1}H{sup +}, {sup 4}He{sup +}, and {sup 11}B{sup +}. Depth resolution is in the nanometer range and 1 and 2 nm thick Pt layers can easily be resolved. Mass resolution between nearby isotopes can be obtained as illustrated by Ga isotopes in GaAs. Taking advantage of the large size detector, a direct imaging (blocking pattern) of crystal channels are shown for hexagonal, 4H-SiC. The ToF-MEIS system described in this paper is intended for use in semiconductor and thin film areas. For example, depth profiling in the sub nanometer range for device development of contacts and dielectric interfaces. In addition to applied projects, fundamental studies of stopping cross sections in this medium energy range will also be conducted.

43 PARTICLE ACCELERATORS↗

On the interplay of point defects and Cd in non-polar ZnCdO films

Non-polar ZnCdO films, grown over m- and r-sapphire with a Cd concentration ranging between 0.8% and 5%, have been studied by means of slow positron annihilation spectroscopy (PAS) combined with chemical depth profiling by secondary ion mass spectroscopy and Rutherford back-scattering. Vacancy clusters and Zn vacancies with concentrations up to 10{sup 17} cm{sup -3} and 10{sup 18} cm{sup -3}, respectively, have been measured inside the films. Secondary ion mass spectroscopy results show that most Cd stays inside the ZnCdO film but the diffused atoms can penetrate up to 1.3 {mu}m inside the ZnO buffer. PAS results give an insight to the structure of the meta-stable ZnCdO above the thermodynamical solubility limit of 2%. A correlation between the concentration of vacancy clusters and Cd has been measured. The concentration of Zn vacancies is one order of magnitude larger than in as-grown non-polar ZnO films and the vacancy cluster are, at least partly, created by the aggregation of smaller Zn vacancy related defects. The Zn vacancy related defects and the vacancy clusters accumulate around the Cd atoms as a way to release the strain induced by the substitutional Cd{sub Zn} in the ZnO crystal.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗