Structure refinement and dielectric relaxation of M-type Ba, Sr, Ba-Sr, and Ba-Pb hexaferrites
M-type hexaferrites with compositions BaFe{sub 12}O{sub 19} (BFO), SrFe{sub 12}O{sub 19} (SFO), Ba{sub 0.5}Sr{sub 0.5}Fe{sub 12}O{sub 19} (BSFO), and Ba{sub 0.5}Pb{sub 0.5}Fe{sub 12}O{sub 19} (BPFO) were synthesized by commercial solid state reaction method. The Rietveld refinement of x-ray powder diffraction revealed a single hexagonal phase with space group P6{sub 3}/mmc for BFO, SFO, and BSFO samples, whereas BPFO sample contains hematite ({alpha}-Fe{sub 2}O{sub 3}) phase with space group R3c along with the M-type main phase. All the samples show dispersion in dielectric constant ({epsilon} Prime ) and dielectric loss (tan {delta}) values with frequency. The values of {epsilon} Prime and tan {delta} increase with increase in temperature due to increase in the number of charge carriers and their mobilities, which are thermally activated. The reciprocal temperature dependence of conductivity ({sigma}{sub ac}) and the most probable relaxation time ({tau}{sub M Double-Prime }) satisfies the Arrhenius relation. A perfect overlapping of the normalized plots of modulus isotherms on a single 'super curve' for all the studied temperatures reveals a temperature independence of dynamic processes involved in conduction and for relaxation. Further, the complex plots of M{sup *} (M Double-Prime vs M Prime ) indicate that dc conductivity dominates in the region below the M Double-Prime {sub max} point. Above M Double-Prime {sub max}, the variations follow Jonscher power law ({sigma} = A{omega}{sup s}) implying that ac conductivity is dominating in this region. Among the prepared samples, SFO hexaferrite has lowest values of {sigma}{sub ac}, {epsilon} Prime , and tan {delta} making it suitable for use in microwave devices.