Selectivity in the emission of material from solid binary alloys during pulse discharges in air
Selectivity in material emission from solid binary copper-zinc alloys during electric discharge in air - electrode erosion
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Selectivity in material emission from solid binary copper-zinc alloys during electric discharge in air - electrode erosion
An algorithm is outlined for simulating the contact surface erosion for impact problems. The algorithm dynamically relocates the contact surface as projectile and target materials exceed their failure criterion. Example computations of axisymmetric and oblique impacts are compared with experimental data.
A high intensity (greater than 10(exp 15) ions/sq cm) low energy (down to 5 eV) mass selected ion beam (MSIB) facility was used to study the effects of ATOX on two polymers commonly used for space applications (Kapton H and Teflon FEP). The polymers were exposed to O(+) and Ne(+) fluences on 10(exp 15) - 10(exp 19) ions/sq cm, using 30eV ions. A variety of analytical methods were used to analyze the eroded surfaces including: (1) atomic force microscopy (AFM) for morphology measurements; (2) total mass loss measurements using a microbalance; (3) surface chemical composition using x-ray photoelectron spectroscopy (XPS), and (4) residual gas analysis (RGA) of the released gases during bombardment. The relative significance of the collisional and chemical degradation processes was evaluated by comparing the effects of Ne(+) and O(+) bombardment. For 30 eV ions it was found that the Kapton is eroded via chemical mechanisms while Teflon FEP is eroded via collisional mechanisms. AFM analysis was found very powerful in revealing the evolution of the damage from its initial atomic scale (roughness of approx. 1 nm) to its final microscopic scale (roughness greater than 1 micron). Both the surface morphology and the average roughness of the bombarded surfaces (averaged over 1 micron x 1 micron images by the system's computer) were determined for each sample. For 30 eV a non linear increase of the Kapton roughness with the O(+) fluence was discovered (a slow increase rate for fluences phi less than 5 x 10(exp 17) O(+)/sq cm, and a rapid increase rate for phi greater than 5 x 10(exp 17) O(+)/sq cm). Comparative studies on the same materials exposed to RF and DC oxygen plasmas indicate that the specific details of the erosion depend on the simulation facility emphasizing the advantages of the ion beam facility.
Sojourner rover showing Lewis' wheel abrasion experiment. The Mars Pathfinder spacecraft soft-landed on Mars on July 4, 1997. Among the many experiments on its small Sojourner rover are three technology experiments from the NASA Lewis Research Center, including the Wheel Abrasion Experiment (WAE). The WAE was designed, built, delivered, and operated on Mars by a team of engineers and scientists from Lewis' Photovoltaics and Space Environments Branch. This experiment collected data to assess wheel surface wear on the Sojourner. It used a specially designed rover wheel, with thin films (200 to 1000 angstroms) of aluminum, nickel, and platinum deposited on black, anodized aluminum strips attached to the rover's right center wheel. As the wheel spun in the Martian soil, a photovoltaic sensor monitored changes in film reflectivity. These changes indicated abrasion of the metal films by Martian surface material. Rolling wear data were accumulated by the WAE. Also, at frequent intervals, all the rover wheels, except the WAE test wheel, were locked to hold the rover stationary while the test wheel alone was spun and dug into the Martian regolith. These tests created wear conditions more severe than simple rolling. The WAE will contribute substantially to our knowledge of Martian surface characteristics. Marked abrasion would indicate a surface composed of hard, possibly sharply edged grains, whereas lack of abrasion would suggest a somewhat softer surface. WAE results will be correlated with ground simulations to determine which terrestrial materials behave most like those on Mars. This knowledge will enable a deeper understanding of erosion processes on Mars and the role they play in Martian surface evolution. Preliminary results show that electrostatic charging of the rover wheels sometimes caused dust to accumulate on the WAE wheel, making interpretation of the reflectance data problematic. If electrostatic charging is the mechanism for dust attraction, this indicates that the Martian dust has a size somewhat smaller than 40 microns in diameter. The WAE experiment has detected electrostatic charging in the Martian environment for the first time; however, under conditions when the wheel is relatively clean of Martian dust, flight data now indicate that abrasion has also been detected. Crude limits so far place the hardness of the Martian dust at harder than aluminum but softer than nickel, and place the grain size at somewhat smaller than 40 microns.
This viewgraph presentation describes a very detailed reconstruction plan and failure analysis of The Space Shuttle Columbia accident. The contents include: 1) STS-107 Timeline; 2) Foam Impact; 3) Recovery; 4) Reconstruction; 5) Reconstruction Plan; 6) Reconstruction Hanger; 7) Pathfinders; 8) Aluminum Pathfinder; 9) Early Analysis - Left MLG Door Area; 10) Emphasis Switched to Left Hand Wing Leading Edge; 11) Wing Leading Edge Subsystem (LESS); 12) 3D Reconstruction of Left WLE; 13) Left Wing Tile Table; 14) LESS Observations; 15) Left Hand Wing Debris Points to RCC 8/9 - Slumped Tile; 16) Reconstructed View of LC/P 9 tile with I/B Tile; 17) Reconstructed View of Lower C/P 9 Tile; 18) Carrier Panel 8 - Upper; 19) Left Hand Wing Debris Points to RCC 8/9 - Erosion and RCC with attach hole intact; 20) Erosion on Panel 8 Upper Outboard Rib; 21) RCC Panels 8 & 9 Erosion Features; 22) Slumping Source for Carrier Panel 9 Tile was Revealed; 23) Debris Indicated Highest Probability Initiation Site; 24) Left Hand Wing Debris Points to RCC 8/9- Metallic Deposits; 25) Relative Metallic Deposition on L/H Wing Materials; 26) Metallic Deposit Example, LH RCC 8; 27) High Level Questions; 28) Analysis Plan Challenges; 29) Analysis Techniques; 30) Analysis Approach; 31) RCC Panel 8 Erosion Features; 32) Radiographic Features; 33) Radiography WLE LH Panel 8; 34) LH RCC 8 Upper Apex; 35) LH RCC 8 - Deposit Feature: Thick Tear Shaped; 36) LH RCC 8 - Deposit Feature: Thick Globules; 37) LH RCC 8 - Deposit Feature: Spheroids; 38) LH RCC 8 - Deposit Feature: Uniform Deposit; 39) Significant Findings - Sampling All Other panels; 40) Proposed Breach Location and Plasma Flow; 41) Corroborating Information - RCC Panel Debris Locations; 42) Corroborating Information - LH OMS Pod Analysis; 43) Corroborating Information - Impact Testing; and 44) Overall Forensic Conclusions.
Cavitation-induced erosion damage in different Spallation Neutron Source (SNS) target designs are simulated using explicit finite element–based techniques and compared with observations of erosion in targets after operation. The efficacy of the previously developed method, called saturation time, was evaluated using erosion-damaged samples from new target designs. A new metric called maximum bubble size was implemented under the rationale that larger cavitation bubbles will collapse more intensely. The maximum cavitation bubble size over 1 ms of simulated time was calculated based on the Rayleigh–Plesset equation for each element integration point and presented as a contour map at the vessel surface for assessing with erosion observations. SNS targets are now operated with helium gas injection to reduce cavitation damage. A simulation method using a material model for the mixture of mercury and gas bubbles was recently developed and used to account for the effect of small gas bubbles on the structural response of the target vessel. Furthermore, this work compares the new method's results with observed cavitation damage. Maps of the calculated maximum bubble size for targets operated with and without gas injection were compared with photographs of erosion damage observed in SNS targets. The patterns in maximum bubble size maps correlated well with observations of erosion patterns in target vessels after service. Advantages and challenges of the maximum bubble size simulation technique are provided, and differences between results from the previous and the newly proposed metric are discussed.
Triton atomic Oxygen Resistant polymers TOR(TM), were developed by Chelmsford, Massachusetts-based Triton Systems, Inc., through a Small Business Innovation Research (SBIR) contract from NASA's Langley Research Center. The new family of polymers comes from a Langley-developed polymer technology, which marks a new class of aerospace materials that resist the extreme effects of low Earth orbit (LEO). When applied to spacecraft surfaces, TOR polymers protect against erosion caused by the atomic oxygen and radiation present in space. Other polymers, such as Teflon(R) and Kapton(R), are subject to degradation from atomic oxygen and ultraviolet radiation, but TOR polymers use atomic oxygen to their advantage. A long-lasting protective barrier means major savings in the cost of spacecraft maintenance and the time spent performing repairs. While the obvious application of this material lies with the aerospace industry, an underlying benefit is found in the field of electronics. TOR polymers can be made electrically conductive, and then utilized in the creation of sensors that react to the presence of chemical and biological agents by exhibiting a detectable change in electrical conductivity. These sensors have applications in the defense, medical, and industrial sectors.
Thermal analyses were conducted to evaluate the thermal response of various individual materials and multi-layer configurations for an in-space heat shield exposed to a rocket plume during stage separation. Frequently used, readily available thermal protection materials consisting of cork, carbon cloth phenolic (CCP), and silica cloth phenolic (SCP) were selected for an initial screening analysis. SCP was chosen as the primary material for further evaluation using an updated thermal environment calculated using computational fluid dynamics (CFD) results. A multi-layer configuration consisting of SCP providing erosion resistance and a Nomex honeycomb providing thermal protection was then evaluated as a solution for more mass-efficient performance. Pyrolysis depth, bondline temperature, back-side temperature, and a thermal factor of safety were used to define the necessary material thickness profile. Adhesives were included in the analyses with considerations for maximum temperature and application method. One dimensional thermal analyses at several stations along the heat shield surface were performed for the initial screening and follow-on analyses. The methodology used standard processes and computer programs applicable to solid rocket motor internal insulation and nozzle thermal analysis such as Chemical Equilibrium and Applications (CEA), Aerotherm Chemical Equilibrium (ACE), Momentum/Energy Integral Technique (MEIT), and Insulation Thermal Response and Ablation Code (ITRAC). The baseline SCP/Nomex honeycomb multi-layer configuration thermal performance predictions satisfied the objectives with an acceptable mass estimate for the design maturity. The EA9673 film adhesive and SCP resin were the best performing bonding agents considered for the SCP/Nomex honeycomb and Nomex honeycomb/structural substrate interfaces. The baseline mass estimate was lowest when the resin was the bonding agent due to the higher maximum service temperature. These thermal analyses evaluated typical internal and external nozzle materials using a calculated thermal environment and heat loads that were lower than a typical rocket motor internal environment but greater than standard external aeroheating.
Polymer-matrix composites have considerable potential for use in the construction of orbiting structures such as the space station and space antennas because of their light weight, high strength, and low thermal expansion. However, they can suffer surface erosion by interaction with atomic oxygen in low-Earth orbit and degradation and/or embrittlement by electrons and ultraviolet radiation especially in geosynchronous orbit. Thus, a study of the effect of these environmental hazards on polymeric materials is an important step in the assessment of such materials for future use in space.
A pulsed high flux source of nearly monoenergetic atomic oxygen was designed, built, and successfully demonstrated. Molecular oxygen at several atmospheres pressure is introduced into an evacuated supersonic expansion nozzle through a pulsed molecular beam valve. An 18 J pulsed CO2 TEA laser is focused to intensities greater than 10(9) W/sq cm in the nozzle throat to generate a laser-induced breakdown. The resulting plasma is heated in excess of 20,000 K by a laser supported detonation wave, and then rapidly expands and cools. Nozzle geometry confines the expansion to provide rapid electron-ion recombination into atomic oxygen. Average O atom beam velocities from 5 to 13 km/s were measured at estimated fluxes to 10(18) atoms per pulse. Preliminary materials testing has produced the same surface oxygen enrichment in polyethylene samples as obtained on the STS-8 mission. Scanning electron microscope examinations of irradiated polymer surfaces reveal an erosion morphology similar to that obtained in low Earth orbit, with an estimated mass removal rate of approx. 10(-24) cu cm/atom. The characteristics of the O atom source and the results of some preliminary materials testing studies are reviewed.
Diamond offers good optical properties and hosts bright color centers with long spin coherence times. Recent advances in angled-etching of diamond, specifically with reactive ion beam angled etching (RIBAE), have led to successful demonstration of quantum photonic devices operating at visible wavelengths. However, larger devices operating at telecommunication wavelengths have been difficult to fabricate due to the increased mask erosion, arising from the increased size of devices requiring longer etch times. We evaluated different mask materials for RIBAE of diamond photonic crystal nanobeams and waveguides, and how their thickness, selectivity, aspect ratio and sidewall smoothness affected the resultant etch profiles and optical performance. We found that a thick hydrogen silesquioxane (HSQ) layer on a thin alumina adhesion layer provided the best etch profile and optical performance. The techniques explored in this work can also be adapted to other bulk materials that are not available heteroepitaxially or as thin films-on-insulator.
The solar wind is described and its effects on surfaces are reviewed. Experimental results are given for materials subjected to simulated solar-wind bombardment. Among the effects discussed are sputtering-type erosion, chemical reaction with paint vehicles and reduction of oxide pigments, and production of lunar-surface optical characteristics in a basalt powder.
The plasma sprayed graded layered yittria stabilized zirconia (ZrO2)/metal(CoCrAlY) seal system for gas turbine blade tip applications up to 1589 K (2400 F) seal temperatures was studied. Abradability, erosion, and thermal fatigue characteristics of the graded layered system were evaluated by rig tests. Satisfactory abradability and erosion resistance was demonstrated. Encouraging thermal fatigue tolerance was shown. Initial properties for the plasma sprayed materials in the graded, layered seal system was obtained, and thermal stress analyses were performed. Sprayed residual stresses were determined. Thermal stability of the sprayed layer materials was evaluated at estimated maximum operating temperatures in each layer. Anisotropic behavior in the layer thickness direction was demonstrated by all layers. Residual stresses and thermal stability effects were not included in the analyses. Analytical results correlated reasonably well with results of the thermal fatigue tests. Analytical application of the seal system to a typical gas turbine engine application predicted performance similar to rig specimen thermal fatigue performance. A model for predicting crack propagation in the sprayed ZrO2/CoCrAlY seal system was proposed, and recommendations for improving thermal fatigue resistance were made. Seal system layer thicknesses were analytically optimized to minimize thermal stresses in the abradability specimen during thermal fatigue testing. Rig tests on the optimized seal configuration demonstrated some improvement in thermal fatigue characteristics.
In the present computation of the evolution of grain size distribution in a turbulent disk for turbulent solar nebula models, using realistic collisional outcomes and strengths of grain aggregates, the half space above the central plane of the disk is divided into a series of levels. At each level, the size distribution is represented by the population of a series of discrete size bins, each spanning an order of magnitude in mass. Coagulation, erosion, or disruption, occur for various combinations of relative particle sizes and velocities, together with assumed material strength, based on experimental impact data. The calculation is one-dimensional, in that it is performed at a single radial location in the disk.
A projected fringe profilometry system was applied to surface contour measurements of an accelerator electrode from an ion thrustor. The system permitted noncontact, nondestructive evaluation of the fine and gross structure of the electrode. A 3-D surface map of a dished electrode was generated without altering the electrode surface. The same system was used to examine charge exchange erosion pits near the periphery of the electrode to determine the depth, location, and volume of material lost. This electro-optical measurement system allowed rapid, nondestructive, digital data acquisition coupled with automated computer data processing. In addition, variable sensitivity allowed both coarse and fine measurements of objects having various surface finishes.
A novel projected fringe profilometry system was applied to surface contour measurements of an accelerator electrode from an ion thruster. The system permitted noncontact, nondestructive evaluation of the fine and gross structure of the electrode. A 3D surface map of a dished electrode was generated without altering the electrode surface. The same system was used to examine charge exchange erosion pits near the periphery of the electrode to determine the depth, location, and volume of material lost. This electro-optical measurement system allowed rapid nondestructive digital data acquisition coupled with automated computer data-processing. In addition, variable sensitivity allowed both coarse and fine measurements of objects having various surface finishes.
The performance and lifetime expectations of 30 cm xenon ion thruster technology at low values of specific impulse were evaluated, with emphasis on 1000-2500 s operation. Power levels of up to 2.0 kW, appropriate for auxiliary and orbit maneuvering propulsion, were processed at thrust-to-power ratios up to 57 mN/kW. These tests were conducted using a derated 30 cm ion thruster with high-perveance design two-grid ion optics with xenon propellent. Lifetime projections were made based on a simple analysis of critical component erosion rates, and it was found that a strong correlation exists with the ratio of the specific impulse-to-input power. Under all operating conditions for which the projected thruster lifetime is less than 10,000 hrs, the life-limiting component of this technology is erosion of the accelerator grid due to charge-exchange ions. The use of alternative grid materials such as carbon is estimated to increase useful thruster lifetimes by as much as an order of magnitude and may enable long-life high thrust-density, sub-2500 s Isp operation. The performance and life of the derated thruster appears similar to that of the Russian SPT-100 thruster in the 1.0-2.0 kW, 1600-2000 s operational envelope.
With the U.S. about to embark on a new space age, the effects of the space environment on a spacecraft during its mission lifetime become more relevant. Included among these potential effects are degradation and erosion due to micrometeoroid and debris impacts, atomic oxygen and ultraviolet light exposure as well as material alteration from thermal cycling, and electron and proton exposure. This paper focuses on the effects caused by micrometeoroid and debris impacts on several LDEF aluminum plates from four different bay locations: C-12, C-10, C-01, and E-09. Each plate was coated with either a white, black, or gray thermal paint. Since the plates were located at different orientations on the satellite, their responses to the hypervelocity impacts varied. Crater morphologies range from a series of craters, spall zones, domes, spaces, and rings to simple craters with little or no spall zones. In addition, each of these crater morphologies is associated with varying damage areas, which appear to be related to their respective bay locations and thus exposure angles. More than 5% of the exposed surface area examined was damaged by impact cratering and its coincident effects (i.e., spallation, delamination and blow-off). Thus, results from this analysis may be significant for mission and spacecraft planners and designers.