Search NASA⌕ Search

SEARCH · Search NASA

Results for “Pit”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 577 records · Page 32

Web Growth Used to Confine Screw Dislocations to Predetermined Lateral Positions in 4H-SiC Epilayers

Silicon-carbide- (SiC-) based power devices could enable substantial aerospace electronics benefits over today's silicon-based electronics. However, present-day SiC wafers contain electrically harmful dislocations (including micropipes) that are unpredictably distributed in high densities across all commercial 4H- and 6H-SiC wafers. The NASA Glenn Research Center recently demonstrated a crystal growth process that moves SiC wafer dislocations to predetermined lateral positions in epitaxial layers so that they can be reproducibly avoided during subsequent SiC electronic device fabrication. The process starts by reactive ion etching mesa patterns with enclosed trench regions into commercial on-axis (0001) 4H- or 6H-SiC substrates. An example of a pregrowth mesa geometry with six enclosed triangular-shaped trench regions is shown. After the etch mask is stripped, homoepitaxial growth is carried out in pure stepflow conditions that enable thin cantilevers to grow laterally from the tops of mesas whose pregrowth top surfaces are not threaded by substrate screw dislocations. The image in the bottom figure shows the postgrowth structure that forms after the lateral cantilevers expand to coalesce and completely roof over each of the six triangular trench regions. Atomic force microscope (AFM) measurements of the roof revealed that three elementary screw dislocation growth spirals, each shown in the AFM insets of the bottom image on the previous page, formed in the film roof at three respective points of cantilever film coalescence. The image above shows the structure following an etch in molten potassium hydroxide (KOH) that produced surface etch pits at the dislocation defects. The larger KOH etch pits--S1, S2, and S3--shown in this image correspond to screw dislocations relocated to the final points of cantilever coalescence. The smaller KOH etch pits are consistent with epilayer threading edge dislocations from the pregrowth substrate mesa (P1, P3, and P4) and a final cantilever coalescence point (P2). No defects (i.e., no etch pits) are observed in other cantilevered portions of the film surface. On the basis of the principle of dislocation Burgers vector conservation, we hypothesize that all vertically propagating substrate dislocations in an enclosed trench region become combined into a single dislocation in the webbed film roof at the point of final roof coalescence. The point of final roof coalescence, and therefore the lateral location of a webbed roof dislocation, can be designed into the pregrowth mesa pattern. Screw dislocations with predetermined lateral positions can then be used to provide the new growth steps necessary for growing a 4H/6H-SiC epilayer with a lower dislocation density than the substrate. Devices fabricated on top of such films can be positioned to avoid the preplaced dislocations.

Powell, J. Anthony↗

Surface Textures and Features Indicative of Endogenous Growth at the McCartys Flow Field, NM, as an Analog to Martian Volcanic Plains

Basaltic lavas typically form channels or tubes, which are recognized on the Earth and Mars. Although largely unrecognized in the planetary community, terrestrial inflated sheet flows also display morphologies that share many commonalities with lava plains on Mars. The McCartys lava flow field is among the youngest (approx.3000 yrs) basaltic flows in the continental United States. The southwest sections of the flow displays smooth, flat-topped plateaus with irregularly shaped pits and hummocky inter-plateau units that form a polygonal surface. Plateaus are typically elongate in map view, up to 20 m high and display lineations within the glassy crust. Lineated surfaces occasionally display small < 1m diameter lava coils. Lineations are generally straight and parallel each other, sometimes for over 100 meters. The boundaries between plateaus and depressions are also lineated and tilted to angles sometimes approaching vertical. Plateau-parallel cracks, sometimes containing squeeze-ups, mark the boundary between tilted crust and plateau. Some plateau depressions display level floors with hummocky surfaces, while some are bowl shaped with floors covered in broken lava slabs. The lower walls of pits sometimes display lateral, sagged lava wedges. Infrequently, pit floors display the upper portion of a tumulus from an older flow. In some places the surface crust has been disrupted forming a slabby texture. Slabs are typically on the scale of a meter or less across and no less than 7-10 cm thick. The slabs preserve the lineated textures of the undisturbed plateau crust. It appears that this style of terrain represents the emplacement of an extensive sheet that experiences inflation episodes within preferred regions where lateral spreading of the sheet is inhibited, thereby forming plateaus. Rough surfaces represent inflation-related disruption of pahoehoe lava and not a a lava. Depressions are often the result of non-inflation and can be clearly identified by lateral squeeze-outs along the pit walls that form when the rising crust exposes the still liquid core of the sheet. The plains of Tharsis and Elysium, Mars, display many analogous features

Bleacher, Jacob E.↗

Low and High-Power Inductive Pulsed Plasma Thruster Development Testing at NASA-MSFC

The inductive pulsed plasma thruster (IPPT) is an electromagnetic plasma accelerator that has been identified in NASA roadmaps as an enabling propulsion technology for some niche low-power missions and for high-power in-space propulsion needs. The IPPT is an electrodeless space propulsion device where a capacitor is charged to an initial voltage and then discharged producing a high current pulse through a coil. The field produced by this pulse ionizes propellant, inductively driving current in a plasma located near the face of the coil. Once the plasma is formed it can be accelerated and expelled at a high exhaust velocity by the electromagnetic Lorentz body force arising from the interaction of the induced plasma current and the magnetic field produced by the current in the coil. Thrusters of this type possess many demonstrated and potential benefits that make them worthy of continued investigation. The electrodeless nature of these thrusters eliminates the lifetime and contamination issues associated with electrode erosion in conventional electric thrusters. Also, a wider variety of propellants are accessible when compatibility with metallic electrodes in no longer an issue. IPPTs have been successfully operated using propellants like ammonia, hydrazine, and CO2, and there is no fundamental reason why they would not operate on other in situ propellants like H2O. It is well-known that pulsed accelerators can maintain constant specific impulse (I(sub sp)) and thrust efficiency (eta(sub t)) over a wide range of input power levels by adjusting the pulse rate to hold the discharge energy per pulse constant. It has also been demonstrated that an inductive pulsed plasma thruster can operate in a regime where eta(sub t) is relatively constant over a wide range of I(sub sp) values (3000-8000 s). Finally, thrusters in this class have operated in single-pulse mode at high energy per pulse, and by increasing the pulse rate they offer the potential to process very high levels of power using a single thruster. There has been significant previous research on IPPTs designed around a planar-coil (flat-plate) geometry. The most notable of these was the Pulsed Inductive Thruster (PIT), with the PIT MkV presently representing the state-of- the-art in pulsed high-power IPPT technological development. In this paper, we focus on two planar-geometry devices that operate at significantly different power levels. Most work performed at NASA-Marshall Space Flight Center (MSFC) has, to date, focused on lower power thruster operation (approx. = 10s to 100s of J/pulse, up to 2-2.5 kW average power throughput) and previously described. The most recent work aimed to assemble a device that could be tested in cyclic mode on a thrust-stand, and which could augment the existing data set for IPPTs. In addition, the thruster was designed to serve as a test-bed for solid state switching circuitry and pulsed gas valves, with the modular design of the device allowing for variation in or upgrades to test configuration. Recently, MSFC obtained on loan from the Georgia Institute of Technology (Atlanta, GA) the PIT MkVI, successor to the PIT MkV. The MkV and MkVI are similar in design with much of the hardware from the former, specifically the capacitors and spark-gap switches, being reused in the latter. The coil is similar in geometry but has bent copper rods used in the latest iteration in place of the Litz wire windings found in the MkV. The MkVI master switch for the spark gaps is located in the vacuum chamber contained within a sealed, pressurized vessel fastened to the back of the thruster. This is different from the MkV where many capacitor charging lines and spark gap-triggering delay lines ran to the thruster from a master trigger located outside the vacuum chamber. The MkVI was damaged during testing soon after its fabrication was completed. The thruster arrived at MSFC still-damaged and mostly disassembled into many individual pieces. The device has been repaired, with a few additional design changes implemented after discussions with the late Prof. Lovberg regarding the initial testing results and issues encountered. In the present work, we present results from testing of both the small IPPT and the larger MkVI thruster. The smaller device (Fig. 1) is tested on a thrust stand on multiple gases to demonstrate its capability to operate in a repetition-rate mode and serve as a IPPT technology-development testbed. The larger MkVI (Fig. 2) is operated for the first time in its newly reconstituted state, demonstrating full-power pulsed operation and, for the first time, repetition-rate operation of a high-power IPPT. The additional upgrades required for synchronous operation of all the pulsed systems in single-pulse and repetition-rate mode are described in detail.

Polzin, Kurt A.↗

Inductive Pulsed Plasma Thruster Development Testing at NASA-MSFC

The inductive pulsed plasma thruster (IPPT) is an electromagnetic plasma accelerator that has been identified in NASA roadmaps as an enabling propulsion technology for some niche low-power missions and for high-power in-space propulsion needs. The IPPT is an electrodeless space propulsion device where a capacitor is charged to an initial voltage and then discharged producing a high current pulse through a coil. The field produced by this pulse ionizes propellant, inductively driving current in a plasma located near the face of the coil. Once the plasma is formed it can be accelerated and expelled at a high exhaust velocity by the electromagnetic Lorentz body force arising from the interaction of the induced plasma current and the magnetic field produced by the current in the coil. Thrusters of this type possess many demonstrated and potential benefits that make them worthy of continued investigation. The electrodeless nature of these thrusters eliminates the lifetime and contamination issues associated with electrode erosion in conventional electric thrusters. Also, a wider variety of propellants are accessible when compatibility with metallic electrodes in no longer an issue. IPPTs have been successfully operated using propellants like ammonia, hydrazine, and CO2, and there is no fundamental reason why they would not operate on other in situ propellants like H2O. It is well-known that pulsed accelerators can maintain constant specific impulse (I(sub sp)) and thrust efficiency (η(sub t)) over a wide range of input power levels by adjusting the pulse rate to hold the discharge energy per pulse constant. It has also been demonstrated that an inductive pulsed plasma thruster can operate in a regime where η(sub t) is relatively constant over a wide range of I(sub sp) values (3000-8000 s). Finally, thrusters in this class have operated in single-pulse mode at high energy per pulse, and by increasing the pulse rate they offer the potential to process very high levels of power using a single thruster. There has been significant previous research on IPPTs designed around a planar-coil (flat-plate) geometry. The most notable of these was the Pulsed Inductive Thruster (PIT), with the PIT MkV presently representing the state of- the-art in pulsed high-power IPPT technological development. In this paper, we focus on two planar-geometry devices that operate at significantly different power levels. Most work performed at NASA-Marshall Space Flight Center (MSFC) has, to date, focused on lower power thruster operation (≈ 10s to 100s of J/pulse, up to 2-2.5 kW average power throughput) and previously described in Refs. [5,6]. The most recent work aimed to assemble a device that could be tested in cyclic mode on a thrust-stand, and which could augment the existing data set for IPPTs. In addition, the thruster was designed to serve as a test-bed for solid state switching circuitry and pulsed gas valves, with the modular design of the device allowing for variation in or upgrades to test configuration. Recently, MSFC obtained on loan from the Georgia Institute of Technology (Atlanta, GA) the PIT MkVI, successor to the PIT MkV. The MkV and MkVI are similar in design with much of the hardware from the former, specifically the capacitors and spark-gap switches, being reused in the latter. The coil is simliar in geometry but has bent copper rods used in the latest iteration in place of the Litz wire windings found in the MkV. The MkVI master switch for the spark gaps is located in the vacuum chamber contained within a sealed, pressurized vessel fastened to the back of the thruster. This is different from the MkV where many capacitor charging lines and spark gap-triggering delay lines ran to the thruster from a master trigger located outside the vacuum chamber. The MkVI was damaged during testing soon after its fabrication was completed. The thruster arrived at MSFC still-damaged and mostly disassembled into many individual pieces. The device has been repaired, with a few additional design changes implemented after discussions with the late Prof. Lovberg regarding the initial testing results and issues encountered.

Polzin, Kurt A.↗

Determining Drying Conditions to Mitigate Hanford Transfer Line Corrosion

Radioactive waste is stored in underground, carbon-steel double-shell tanks at the Department of Energy Hanford site.1,2,3 The underground transfer lines are used to transfer the waste between the tanks and other assets at the Hanford tank farm facilities. The transfer lines constructed before 1990 are pipe-in-pipe design with most of the lines having carbon steel carrier pipe and carbon steel encasements. The lines constructed after 1990 have a stainless-steel carrier with a carbon steel encasement. The carrier lines, which are in contact with the waste, provide a critical confinement function, while the encasements provide secondary containment to reduce the risk of a release and contamination to the environment. In 2022, a visual inspection of the annulus between the encasement and the carrier for one of the pre-1990 transfer lines revealed standing liquid in contact with the carrier pipe. Additionally, a significant build-up of corrosion products on the exterior of the carrier pipe and the interior of the encasement pipe was observed. To assess the extent of condition, borescope inspections were performed in the encasement space of additional transfer lines in the facility to provide a baseline. The inspection revealed that of the lines inspected, 29 had either moisture present or evidence that moisture had been present in the past (e.g., waterline corrosion where the pipe had been exposed to standing water). Additional inspections indicated several instances of pitting corrosion on the interior of the encasement and exterior the carrier transfer lines. An image of the carrier pipe with several pits is presented in Figure 1(a) and the profiled image of the transfer line section along with the pit depths are presented Figure 1(b). As seen in the figure, the deepest pit was 73 mils on the pipe section. These lines were designated as “do-not-use” until further compensatory actions are implemented to return the lines to service.

Shukla, Pavan K. [Savannah River National Laborato↗

Composite Lithium Metal Structure to Mitigate Pulverization and Enable Long‐Life Batteries

In lithium metal batteries, non‐uniform stripping of lithium results in pit formation, which promotes subsequent non‐uniform, dendritic deposition. This viscous cycle leads to pulverization of lithium which promotes cell shorting or capacity degradation, symptoms further exaggerated by high electrode areal loading and lean electrolytes. Here, to address this challenge, a composite lithium metal anode is engineered that contains uniformly distributed, nanometer‐sized carbon particles. This composite lithium is shown to strip more uniformly since the growth of non‐uniform pits is intercepted by the carbon particles. This mechanism is corroborated by a continuum electrochemical model. Subsequent lithium deposition on carbon particles is also found to be more uniform than on the surface with irregular pits. Notably, the pulverization rate of composite lithium is 26 times slower than that of commercial lithium. Moreover, in a Li‐S battery with sulfurized polyacrylonitrile cathode, the use of the composite anode extends the cycle life by three times when the areal capacity is 8 mAh cm −2 . The approach of using an engineered lithium composite structure to address challenges during both stripping and plating can inform future designs of lithium metal anodes for high areal capacity operations.

high areal capacity↗

Microstructure and Corrosion Properties of Laser-Welded SAF 2507 Super Duplex Stainless Steel Joints

SAF 2507 super duplex stainless steel has been welded using laser beam (LB) welding and laser/gas metal arc hybrid (LGH) welding processes. The pitting and intergranular corrosion properties of the welding joints have been tested using electrochemical testing and microstructure observations. The volume fraction of the ferrite phase reaches 70% in the weld zone of the LB welding joint, while the volume fraction of the ferrite phase is 60% for the welding joint of LGH due to the introduction of Ni from welding wire. The pitting corrosion resistance of the welding joint for LB is better than that of LGH. The pitting corrosion is easily conceived in the heat-affected zone (HAZ) because of the formation of Cr{sub 2}N in the HAZ during welding.

36 MATERIALS SCIENCE↗

Corrosion Inhibition Study of Mg-Nd-Y High Strength Magnesium Alloy Using Organic Inhibitor

A study on corrosion inhibition mechanism has been performed on rare earth containing WE43 magnesium alloy in 3.5 wt.% NaCl containing 8-hydroxyquinoline (HQ). After an initial increase in corrosion rate due to the formation of sparingly soluble MgQ{sub 2} complex, it was found to decrease owing to inhibition effect of the complex. Scanning electrochemical microscopic analysis showed a decrease in corrosion currents and enhanced resistance to pitting corrosion was observed for WE43 samples in the presence of HQ after an exposure of 48 h. With time, the MgQ{sub 2} thus generated formed a protective layer on the Mg alloy surface to prevent further corrosion. The corrosion rate of WE43 samples decreased by ~ 50% in HQ containing medium after a constant exposure of 28 days (from ~ 0.22 mg/cm{sup 2} day in no HQ to ~ 0.11 mg/cm{sup 2} day in HQ). For the WE43 samples in the presence of HQ, formation of MgO and MgQ{sub 2} was detected by x-ray photoelectron spectroscopy and x-ray diffraction. Shallower and smaller pits appeared on the magnesium alloy with HQ in the solution as compared to deeper and larger pits on the samples with no HQ in the solution. The significance of metal-complexing organic agent, hydroxyquinoline, in initial acceleration and subsequent prevention of Mg corrosion via protective MgQ{sub 2} complex layer formation is demonstrated.

36 MATERIALS SCIENCE↗

The Electrochemical Corrosion Behavior of Plasma Electrolytic Oxidation Coatings Fabricated on Aluminum in Silicate Electrolyte

Plasma electrolytic oxidation (PEO) coatings were fabricated on the aluminum in silicate electrolyte. Microstructures and elemental compositions of these PEO coatings were examined by scanning electron microscopy (SEM) equipped with an energy-dispersive x-ray spectroscopy (EDS). Corrosion resistances of the coated samples were evaluated using the measurements of open-circuit potential (OCP), repetitive polarization and electrochemical impedance spectroscopy (EIS) in 3.5 wt.% NaCl solution. The results indicated that the PEO coatings not only act as a physical shield limiting the penetration of corrosive solution, but also establish an anodic location with high concentration of H{sup +} ions and other product ions as pitting corrosion begins. With the development of pitting corrosion, the accumulation of corrosion products inside the pits and pores of the coatings decreases the corrosion process effectively.

36 MATERIALS SCIENCE↗

Effect of Cobalt on the Microstructure and Corrosion Behavior of Martensitic Age-Hardened Stainless Steel

To evaluate the influence of cobalt on the microstructure and pitting behavior of martensitic age-hardened stainless steel (MASS), the microstructures and electrochemical behaviors were characterized by optical microscopy, scanning electron microscopy, transmission electron microscopy, x-ray photoelectron spectroscopy, potentiodynamic curve, electrochemical impedance spectroscopy, and Mott–Schottky analysis. Results indicated that adding cobalt reduced the grain size of the original austenite, refined the lath martensite, inhibited the precipitation of Cu-rich phases, and increased the content of reversed austenite. Compared with the cobalt-free steel, the cobalt-containing steel has a higher pitting potential, lower corrosion current density, and higher pitting resistance. The primary components of the passive film grown on the cobalt-free steel included (Cr, Fe) oxides, such as Cr{sub 2}O{sub 3}, Cr(OH){sub 3}, FeOOH, and Fe{sub 2}O{sub 3}. The cobalt-containing steel included the aforementioned components as well as Co, which was attributed to the formation of the passive film in the forms of CoFe{sub 2}O{sub 4}, Co(OH){sub 2}, and CoO. In addition, the synergy of the refined lath martensite and the precipitation of the Cu-rich phase induced an increase in corrosion resistance in MASS containing cobalt.

36 MATERIALS SCIENCE↗

Aqueous Corrosion Behavior of Cast CoCrFeMnNi Alloy

CoCrFeMnNi high-entropy alloy demonstrates good mechanical properties and can be further strengthened by thermomechanical processes. A sample alloy prepared by vacuum casting in a graphite mold was further investigated for its corrosion resistance. One-millimeter thin strips of cast alloy were used to investigate its corrosion behavior at room temperature. Linear potentiodynamic tests of the alloy in sodium chloride solution confirmed uniform corrosion property comparable to stainless steel AISI 304. However, a positive cyclic hysteresis loop indicated susceptibility to pitting corrosion. In sodium hydroxide solution, metastable pit formation was observed, while sulfuric acid solution passivated the alloy. In both cases, the alloy did not show any spontaneous pitting tendency.

36 MATERIALS SCIENCE↗

The corrosion pattern of reinforcement and its influence on serviceability of reinforced concrete members in chloride environment

This paper deals with two corroded reinforcement concrete beams, which have been stored under sustained load in a chloride environment for 14 and 23 years respectively. The evolution of corrosion pattern of reinforcement and its influence on serviceability are studied. In chloride-induced corrosion process, corrosion cracking affects significantly the corrosion pattern. During the corrosion cracking initiation period, only local pitting corrosion occurs. At early stage of cracking propagation, localized pitting corrosion is still predominant as cracks widths are very small and cracks are not interconnected, but a general corrosion slowly develops as the cracks widen. At late cracking stage, interconnected cracking with wide width develops along large parts of the beam leading to a general corrosion pattern. Macrocells and microcells concepts are used for the interpretation of the results. Mechanical experiments and corrosion simulation tests are performed to clarify the influence of this corrosion pattern evolution on the serviceability of the beams (deflection increase). Experimental results show that, when the corrosion is localized (early cracking stage), the steel-concrete bond loss is the main factor affecting the beams serviceability. The local cross-section loss resulting from pitting attack does not significantly influence the deflection of the beam. When corrosion is generalized (late cracking stage), as the steel-concrete bond is already lost, the generalized steel cross-section reduction becomes the main factor affecting the beams serviceability. But, at this stage, the deflection increase is slower due to the low general corrosion rate.

36 MATERIALS SCIENCE↗

In-situ visualization of corrosion behavior of Al CoCrFeNi high-entropy alloys during electrochemical polarization

In this study, the corrosion behavior of the Al x CoCrFeNi (x = 0.3, 0.5, 0.7) high-entropy alloys (HEAs) is investigated by an in-situ visualization system. Surface morphology changes on both micro-spatial and temporal scales are monitored in the 3.5 wt% NaCl solution during the potentiodynamic polarization. The microstructures of the Al x CoCrFeNi HEAs are characterized by SEM, EBSD, and EDS. The results show that the microstructure evolves from singe face-centered cubic (FCC) phase to multi-phases by increasing the Al content. The in-situ observations directly reveal the different localized corrosion processes in the AlxCoCrFeNi HEAs. In the single FCC phase Al 0.3 CoCrFeNi HEA, localized corrosion shows in the form of pitting. In the Al 0.5 CoCrFeNi and Al 0.7 CoCrFeNi alloys, which possess FCC and body-centered cubic (BCC) phases, the localized corrosion initiates and propagates in the Cr-depleted BCC phase. In addition, the in-situ visualization uncovers the evolution of current serration, which represents the propagation and repassivation of metastable pit during the polarization. The frequent occurrence of metastable pits indicates distinct repassivation ability of the Al 0.3 CoCrFeNi HEA.

36 MATERIALS SCIENCE↗

Observations of Atmospheric Corrosion Testing on Heated Austenitic Stainless Steel Surfaces: Exploring the Role of Inert Dust Particulates and Seawater

Relevant atmospheric corrosion laboratory testing environments were developed to explore the influence of inert dust and seawater on the corrosion susceptibility of stainless steel in spent nuclear fuel dry storage conditions. Measurements from dust collected on in-service dry storage canisters were applied to develop exposure conditions. Three atmospheric exposure conditions, two static and one cyclic, were examined with three different surface coverages: co-deposited large dust and seawater, co-deposited small dust and seawater, and solely seawater. Stainless steel coupons representative of spent nuclear fuel dry storage canister material were subjected to the various corrosion environments, with the results from exposures up to 1 year presented here. Post exposure, corrosion damage was analyzed using optical microscopy, scanning electron microscopy, and energy dispersive X-ray spectroscopy. Initial observations are presented herein, and potential implications with respect to the influence of inert dust particles on corrosion susceptibility are summarized. In general, the co-deposition of dust and salt resulted in larger pits and exhibited mixed modes of corrosion that were not observed in the no-dust conditions (i.e., crevicing, filiform, and pits within pits). The presence of the inert dust may influence brine spreading and/or act as crevice formers, leading to enhanced corrosion. This study highlights the significance of incorporating dust particulate(s) beyond the deliquescent chemistries to fully evaluate atmospheric corrosion severity.

Sea salt↗

An intermetallic powder-in-tube approach to increased flux-pinning in Nb 3 Sn by internal oxidation of Zr

We report on the development of multifilamentary Nb 3 Sn superconductors by a versatile powder-in-tube technique (PIT) that demonstrates a simple pathway to a strand with a higher density of flux-pinning sites that has the potential to increase critical current density beyond present levels. The approach uses internal oxidation of Zr-alloyed Nb tubes to produce Zr oxide particles within the Nb 3 Sn layer that act as a dispersion of artificial pinning centres (APCs). In this design, SnO 2 powder is mixed with Cu 5 Sn 4 powder within the PIT core that supplies the Sn for the A15 reaction with Nb1Zr filament tubes. Initial results show an average grain size of ~38 nm in the A15 layer, compared to the 90–130 nm of typical APC-free high-J c strands made by conventional PIT or Internal Sn processing. Furthermore, there is a shift in the peak of the pinning force curve from H/H irr of ~0.2 to ~0.3 and the pinning force curves can be deconvoluted into grain boundary and point-pinning components, the point-pinning contribution dominating for the APC Nb-1wt%Zr strands.

36 MATERIALS SCIENCE↗

PROBABILITY BASED CORROSION CONTROL FOR LIQUID WASTE TANKS - PART III

The liquid waste chemistry control program is designed to reduce the pitting corrosion occurrence on tank walls. The chemistry control program has been implemented, in part, by applying engineering judgment safety factors to experimental data. However, the simple application of a general safety factor can result in use of excessive corrosion inhibiting agents. The required use of excess corrosion inhibitors can be costly for tank maintenance, waste processing, and in future tank closure. It is proposed that a probability-based approach can be used to quantify the risk associated with the chemistry control program. This approach can lead to the application of tank-specific chemistry control programs reducing overall costs associated with overly conservative use of inhibitor. Furthermore, when using nitrite as an inhibitor, the current chemistry control program is based on a linear model of increased aggressive species requiring increased protective species. This linear model was primarily supported by experimental data obtained from dilute solutions with nitrate concentrations less than 0.6 M, but is used to produce the current chemistry control program up to 1.0 M nitrate. Therefore, in the nitrate space between 0.6 and 1.0 M, the current control limit is based on assumptions that the linear model developed from data in the <0.6 M region is applicable in the 0.6-1.0 M region. Due to this assumption, further investigation of the nitrate region of 0.6 M to 1.0 M has potential for significant inhibitor reduction, while maintaining the same level of corrosion risk associated with the current chemistry control program. Ongoing studies have been conducted in FY07, FY08, FY09 and FY10 to evaluate the corrosion controls at the SRS tank farm and to assess the minimum nitrite concentrations to inhibit pitting in ASTM A537 carbon steel below 1.0 molar nitrate. The experimentation from FY08 suggested a non-linear model known as the mixture/amount model could be used to predict the probability of corrosion in ASTM A537 in varying solutions as shown in Figure 1. The mixture/amount model takes into account not only the ratio (or mixture) of inhibitors and aggressive species, but also the total concentration (or amount) of species in a solution. Historically, the ratio was the only factor taken into consideration in the development of the current chemistry control program. During FY09, an experimental program was undertaken to refine the mixture/amount model by further investigating the risk associated with reducing the minimum molar nitrite concentration required to confidently inhibit pitting in dilute solutions. The results of FY09, as shown in Figure 2, quantified the probability for a corrosion free outcome for combinations of nitrate and nitrite. The FY09 data predict probabilities up to 70%. Additional experimental data are needed to increase the probability to an acceptable percentage.

36 MATERIALS SCIENCE↗

Hanford double shell waste tank corrosion studies - final report FY2014

SRNL tasks for FY14 included studies to evaluate the susceptibility of carbon steel to vapor space corrosion (VSC), liquid-air interface (LAI) corrosion, and pitting corrosion. Additionally, SRNL evaluated the susceptibility of carbon steel to pitting corrosion under buffered waste conditions, with the objective of determining the adequate amount of inhibitor (e.g., nitrite) necessary to mitigate pitting corrosion. Other CPP experiments were performed in historical waste simulants and the results were compared to previously gathered results. The results of these activities were utilized to assess the robustness of the standardized CPP protocol

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Experimental Studies of Engineered Barrier Systems Conducted at Los Alamos National Laboratory (FY16)

Over the past five years the Used Fuel Campaign has investigated Engineered Barrier Systems (EBS) at higher heat loads (up to 300°C) and pressure (150 bar). This past year experimental work was hindered due to a revamping of the hydrothermal lab. Regardless, two experiments were run this past year, EBS-18 and EBS-19. EBS-18 was run using Low Carbon Steel (LCS) and opalinus clay in addition to the bentonite and opalinus brine. Many of the past results were confirmed in EBS-18, such as the restriction of illite formation due to the bulk chemistry, pyrite degradation, and zeolite formation dependent on the bentonite and opalinus clay. The LCS show vast amounts of pit corrosion (over 100μm of corrosion in six weeks), leading a corrosion rate of 1083 μm/year. In addition, a mineral goethite, an iron-bearing hydroxide, formed in the pits of the LCS. Preliminary results from EBS-19 water chemistry are included but SEM imaging, micro probe and XRD are still needed for further results. Copper corrosion was investigated further and over 850 measurements were taken. It was concluded that pitting and pyrite degradation drastically increase the corrosion rate from 0.12 to 0.39 μm/day. However, the growth of a layer of the mineral chalcocite is thought to subdue the corrosion rate to 0.024 μm/day as observed in the EBS-13, a sixth month experiment. This document presents the findings of this past year.