Corrosion Behavior of Fe-7Cr-1Mo-12Zr Metal Waste Form Alloy in Simulated Repository Environment

Metal waste forms (MWF) are solid metallic waste categorized as high-level radioactive waste generated during pyro-reprocessing of spent metallic fuels and geologically disposed off. This waste form generated requires an excellent corrosion resistance in a geological repository environment. In the present work, Fe-7Cr-1Mo-12Zr MWF alloy was developed by casting in an arc melting furnace. The x-ray diffraction analysis revealed the formation of stable phases of α-Fe solid solution and the intermetallic phases of Fe{sub 2}Zr and Fe{sub 23}Zr{sub 6}. The corrosion behavior of Fe-7Cr-1Mo-12Zr alloy was investigated using electrochemical techniques in aggressive (highly acidic with Cl{sup −}) and nominal repository pH environment. Cyclic potentiodynamic polarization studies indicated the shift in corrosion potential toward cathodic potential in highly acidic solution with Cl{sup −}. The corrosion mechanism of pitting is associated with acidified pH medium with more Cl{sup −}, whereas uniform corrosion or transpassive dissolution is resultant of mild acidity or mild alkaline medium. The passive region is wider in pH 5 and 8 when compared to pH 1 and 3. Electrochemical impedance spectroscopic (EIS) analysis revealed the lowering of passive film stability in the highly acidic medium in the presence of Cl{sup −}. The role of passive oxide layers on the corrosion resistance of the Fe-7Cr-1Mo-12Zr MWF alloy is discussed.

36 MATERIALS SCIENCE↗

Basalt-CO2-H2O Interactions and Variability in Carbonate Mineralization Rates

Flood basalts are receiving increasing attention as possible host formations for geologic sequestration of anthropogenic CO2, with studies underway in the U.S., India, Iceland, and Canada. Our previous laboratory studies with Columbia River basalts showed relative quick precipitation of carbonate minerals compared to other siliclastic rocks when batch reacted with water and supercritical CO2. In this study, our prior work with Columbia River basalt was extended to tests with basalts from the eastern U.S., India, and Africa. The basalts are all similar in bulk chemistry and share common minerals such as plagioclase, augite, and a glassy mesostasis. Single pass flow through dissolution experiments under dilute solution and mildly acidic conditions indicate similar cation release behavior among the basalt samples tested. Despite similar bulk chemistry and apparent dissolution kinetics, long-term static experiments with CO2 saturated water show significant differences in rates of mineralization as well as precipitate chemistry and morphology. For example, basalt from the Newark Basin in the U.S. is by far the most reactive of any basalt tested to date. Carbonate reaction products for the Newark Basin basalt were globular in form and contained significantly more Fe than the secondary carbonates that precipitated on the other basalt samples. Calcite grains with classic “dogtooth spar” morphology and trace cation substitution (Mg and Mn) were observed in post-reacted samples associated with the Columbia River basalts. Other basalts produced solid precipitates with compositions that varied chemically throughout the entire testing period. Polished cross sections of the reacted grains show precipitate overgrowths with irregular regions outlined by dark and bright layers indicative of zonations of different compositions. For example, SEM-EDX analysis across carbonate precipitates, which resulted from 854 days of reaction of the Central Atlantic Mafic Province (CAMP) basalt with CO2 saturated water showed distinct chemical regions. Composition of dark colored regions was dominated by a CaCO3 end-member composition, whereas the bright regions were chemically closer to an FeCO3. Chemical differences in the precipitates indicate changes in fluid chemistry unique to the dissolution behavior of each basalt sample reacted with CO2 saturated water.

54 ENVIRONMENTAL SCIENCES↗

Interaction of CuS and sulfur in Li-S battery system

Lithium-Sulfur (Li-S) battery has been a subject of intensive research in recent years due to its potential to provide much higher energy density and lower cost than the current state of the art lithiumion battery technology. In this work, we have investigated Cupric Sulfide (CuS) as a capacitycontributing conductive additive to the sulfur electrode in a Li-S battery. Galvanostatic charge/discharge cycling has been used to compare the performance of both sulfur electrodes and S:CuS hybrid electrodes with various ratios. We found that the conductive CuS additive enhanced the utilization of the sulfur cathode under a 1C rate discharge. However, under a C/10 discharge rate, S:CuS hybrid electrodes exhibited lower sulfur utilization in the first discharge and faster capacity decay in later cycles than a pure sulfur electrode due to the dissolution of CuS. The CuS dissolution is found to be the result of strong interaction between the soluble low order polysulfide Li 2 S 3 and CuS. As a result, we identified the presence of conductive copper-containing sulfides at the cycled lithium anode surface, which may degrade the effectiveness of the passivation function of the solid-electrolyte-interphase (SEI) layer, accounting for the poor cycling performance of the S:CuS hybrid cells at low rate.

25 ENERGY STORAGE↗

Development and evaluation of die and container materials. Low cost silicon solar array project

Specific compositions of high purity silicon aluminum oxynitride (Sialon) and silicon beryllium oxynitride (Sibeon) solid solutions were shown to be promising refractory materials for handling and manipulating solar grade silicon into silicon ribbon. Evaulation of the interaction of these materials in contact with molten silicon indicated that solid solutions based upon beta-Si3N4 were more stable than those based on Si2N2O. Sibeon was more resistant to molten silicon attack than Sialon. Both materials should preferably be used in an inert atmosphere rather than under vacuum conditions because removal of oxygen from the silicon melt occurs as SiO enhances the dissolution of aluminum and beryllium. The wetting angles of these materials were low enough for these materials to be considered as both die and container materials.

Wills, R. R.↗

Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment

Highlights: • Microstructural characterization of SLM AlSi10Mg alloy and comparison with cast and powder AlSi10Mg • Effect of solution heat treatment and aging on the hardness change of SLM AlSi10Mg alloy • Evolution of strengthening precipitates and Fe-rich intermetallics in SLM AlSi10Mg during heat treatment - Abstract: The microstructure and precipitates within selectively laser melted (SLM) AlSi10Mg alloys in the as-built state and after T6 heat treatment were examined and correlated to the hardness evolution. The as-built alloy exhibited columnar patterns perpendicular to the build-direction and fish-scale pattern along the build-direction originating from the melt pool. The microstructure consisted of fine Al cells and eutectic structure with up to 4 μm in size. Tiny needle-like Si particles with highly faulted structure were identified within the Al cells and formed semi-coherent interface with the matrix. Nanoscale Si particles and π-Al{sub 8}Si{sub 6}Mg{sub 3}Fe phase were observed to segregate along the cell and grain boundary. Solution heat treatment (SHT) at 520 °C resulted in the dissolution of Al cellular microstructure. Precipitation and coarsening of the Si particles occurred, while the aspect ratio of Si particles remained nearly constant. The π-Al{sub 8}Si{sub 6}Mg{sub 3}Fe phase decomposed into plate-shaped β-Al{sub 5}SiFe. The artificial aging (AA) at 160 °C did not alter the microstructure but led to the formation of metastable Mg{sub 2}Si precipitates. The GP zones and β″ were identified through transmission electron microscopy after AA of 6 h, and β″ existed up to AA of 24 h. The hardness decreased after SHT due to the coarsening of the microstructure and reduced solid solution hardening. Hardness reached maximum magnitude after AA of 6–10 h due to the precipitation hardening, and remained relatively unchanged up to AA of 24 h. Microstructure and/or hardness of gas atomized powders and bulk cast AlSi10Mg alloys were also examined as references.

36 MATERIALS SCIENCE↗

Bio-processing of solid wastes and secondary resources for metal extraction - A review

Highlights: Black-Right-Pointing-Pointer Review focuses on bio-extraction of metals from solid wastes of industries and consumer goods. Black-Right-Pointing-Pointer Bio-processing of certain effluents/wastewaters with metals is also included in brief. Black-Right-Pointing-Pointer Quantity/composition of wastes are assessed, and microbes used and leaching conditions included. Black-Right-Pointing-Pointer Bio-recovery using bacteria, fungi and archaea is highlighted for resource recycling. Black-Right-Pointing-Pointer Process methodology/mechanism, R and D direction and scope of large scale use are briefly included. - Abstract: Metal containing wastes/byproducts of various industries, used consumer goods, and municipal waste are potential pollutants, if not treated properly. They may also be important secondary resources if processed in eco-friendly manner for secured supply of contained metals/materials. Bio-extraction of metals from such resources with microbes such as bacteria, fungi and archaea is being increasingly explored to meet the twin objectives of resource recycling and pollution mitigation. This review focuses on the bio-processing of solid wastes/byproducts of metallurgical and manufacturing industries, chemical/petrochemical plants, electroplating and tanning units, besides sewage sludge and fly ash of municipal incinerators, electronic wastes (e-wastes/PCBs), used batteries, etc. An assessment has been made to quantify the wastes generated and its compositions, microbes used, metal leaching efficiency etc. Processing of certain effluents and wastewaters comprising of metals is also included in brief. Future directions of research are highlighted.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Evaluation of Resin Dissolution Using an Advanced Oxidation Process - 13241

The ion-exchange resin is widely used in nuclear reactors, in cooling water purification and removing radioactive elements. Because of the long periods of time inside the reactor system, the resin becomes radioactive. When the useful life of them is over, its re-utilization becomes inappropriate, and for this reason, the resin is considered radioactive waste. The most common method of treatment is the immobilization of spent ion exchange resin in cement in order to form a solid monolithic matrix, which reduces the radionuclides release into the environment. However, the characteristic of contraction and expansion of the resin limits its incorporation in 10%, resulting in high cost in its direct immobilization. Therefore, it is recommended the utilization of a pre-treatment, capable of reducing the volume and degrading the resin, which would increase the load capacity in the immobilization. This work aims to develop a method of degradation of ion spent resins from the nuclear research reactor of Nuclear and Energy Research Institute (IPEN/CNEN-SP), Brazil, using the Advanced Oxidative Process (AOP) with Fenton's reagent (hydrogen peroxide and ferrous sulphate as catalyst). The resin evaluated was a mixture of cationic (IR 120P) and anionic (IRA 410) resins. The reactions were conducted by varying the concentration of the catalyst (25, 50, 100 e 150 mM) and the volume of the hydrogen peroxide, at three different temperatures, 50, 60 and 70 deg. C. The time of reaction was three hours. Total organic carbon content was determined periodically in order to evaluate the degradation as a function of time. The concentration of 50 mM of catalyst was the most effective in degrading approximately 99%, using up to 330 mL of hydrogen peroxide. The most effective temperature was about 60 deg. C, because of the decomposition of hydrogen peroxide in higher temperatures. TOC content was influenced by the concentration of the catalyst, interfering in the beginning of the degradation process. It was possible to correlate it with the final amount of non-degraded resins. These results show that these conditions were favorable to destroy the resins, indicating to be the AOP an effective technique to reduce the volume of the waste. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Note: High-speed Z tip scanner with screw cantilever holding mechanism for atomic-resolution atomic force microscopy in liquid

High-speed atomic force microscopy has attracted much attention due to its unique capability of visualizing nanoscale dynamic processes at a solid/liquid interface. However, its usability and resolution have yet to be improved. As one of the solutions for this issue, here we present a design of a high-speed Z-tip scanner with screw holding mechanism. We perform detailed comparison between designs with different actuator size and screw arrangement by finite element analysis. Based on the design giving the best performance, we have developed a Z tip scanner and measured its performance. The measured frequency response of the scanner shows a flat response up to ∼10 kHz. This high frequency response allows us to achieve wideband tip-sample distance regulation. We demonstrate the applicability of the scanner to high-speed atomic-resolution imaging by visualizing atomic-scale calcite crystal dissolution process in water at 2 s/frame.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Removal of Tc-99, Zr-95, and Nb-95, From Solutions Obtained After Dissolution of Irradiated Mo Targets

Decontamination of 99 Tc, Nb, and Zr impurities in dissolved irradiated Mo disks can be accomplished using Fe(II) precipitation. Here, we report bench-scale experiments and large-scale demonstrations on removal of 99 Tc (0.1 mM), 95 Nb, and 95 Zr from dissolved Mo disk simulant solutions. Tc removal is accomplished through the reduction and simultaneous immobilization of Tc(VII) by Fe(II), producing an insoluble, Tcincorporated Fe(II)-Fe(III) solid that is removed by filtration. Large-scale testing showed that Tc (97.6% ± 1.7%) is removed without affecting 99 Mo yields. Other important side reaction product impurities in irradiated Mo targets, namely various isotopes of Nb and Zr, are also removed (>99%) in this process. The effects of metal (Fe, Tc, Mo) concentrations, Fe(II)/Fe(III) ratio, pH, temperature, Fe addition method, and hydrogen peroxide addition were tested. The minimum amount of Fe(II) needed to remove up to 99% Tc is 10 mM and the optimal pH value for simultaneous removal of Tc, Nb, and Zr impurities is pH 13.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The high-pressure lithium–palladium and lithium–palladium–hydrogen systems

Abstract The lithium–palladium and lithium–palladium–hydrogen systems are investigated at high pressures at and above room temperature. Two novel lithium–palladium compounds are found below $${18.7}\,{\mathrm{GPa}}$$ 18.7 GPa . An ambient temperature phase is tentatively assigned as $$F{\bar{4}}3m\,\hbox {Li}_{17}\hbox {Pd}_{4}$$ F 4 ¯ 3 m Li 17 Pd 4 , with $$a = 17.661(1)$$ a = 17.661 ( 1 ) Å at 8.64 GPa, isostructural with $$\hbox {Li}_{17}\hbox {Sn}_{4}$$ Li 17 Sn 4 . The other phase occurs at high-temperature and is $$I{\bar{4}}3m\, \hbox {Li}_{11}\hbox {Pd}_{2}$$ I 4 ¯ 3 m Li 11 Pd 2 , $$a = 9.218(1)$$ a = 9.218 ( 1 ) Å at 3.88 GPa and 200 $$^\circ {\mathrm{C}}$$ ∘ C , similar to $$\hbox {Li}_{11}\hbox {Pt}_{2}$$ Li 11 Pt 2 , which is also known at high pressure. The presence of hydrogen in the system results in an $$I{\bar{4}}3m$$ I 4 ¯ 3 m structure with $$a = 8.856(1)$$ a = 8.856 ( 1 ) Å at 9.74 GPa. This persists up to $${13.3}\,\mathrm{GPa}$$ 13.3 GPa , the highest pressure studied. Below $${2}\,{\mathrm{GPa}}$$ 2 GPa an fcc phase with a large unit cell, $$a = 19.324(1)$$ a = 19.324 ( 1 ) Å at 0.39 GPa, is also observed in the presence of hydrogen. On heating the hydrogen containing system at 4 GPa the $$I{\bar{4}}3m$$ I 4 ¯ 3 m phases persists to the melting point of lithium. In both systems melting the lithium results in the loss of crystalline diffraction from palladium containing phases. This is attributed to dissolution of the palladium in the molten lithium, and on cooling the palladium remains dispersed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Integrated Simulation Framework for Additively Manufactured Ti-6Al-4V: Melt Pool Dynamics, Microstructure, Solid-State Phase Transformation, and Microelastic Response

In this work, to accelerate the establishment of fundamental understanding of the additive manufacturing (AM) process and its influence on microstructural evolution and related properties, we develop a multiphysics and multiscale modeling framework that integrates: (1) a high-fidelity powder-scale three-dimensional simulation of transient heat transfer and melt flow dynamics, (2) cellular automaton simulation of solidification grain structure and texture, (3) phase-field modeling of precipitation and dissolution of second-phase precipitate during repeated thermal cycles, and (4) microstructure-based micro- and mesoscopic elastic response calculation. Using Ti-6Al-4V as a model system, we demonstrate the application of the integrated framework to simulate complex microstructure evolution during a single-track laser powder bed fusion process and the associated mechanical response. Our modeling framework successfully captures the solidification β grain structure as a function of laser power and scanning speed, α precipitation upon subsequent cooling with different rates, and elastic response of the resulting (α + β) two-phase microstructure. The key features of solidification and second-phase precipitate microstructures, and their dependence on processing parameters, agree well with existing experimental observations. Finally, the established modeling framework is generally applicable to other metallic materials fabricated by AM.

36 MATERIALS SCIENCE↗

The effect of Ca-Fe-As coatings on microbial leaching of metals in arsenic bearing mine waste

Globally arsenic (As) is a ubiquitous trace element derived from the natural weathering of As-bearing rock. With the onset of reducing conditions, the prevalence of aqueous As(III) may be intensified through biotic and abiotic processes. Here we evaluate the stability of arsenic bearing Ca-Fe hydroxide phases collected from exposed tailings at Ketza River mine, Yukon, Canada, during the reductive dissolution of both acid treated and untreated samples by Shewanella putrefaciens 200R and Shewanella sp. ANA-3. Samples were acid treated in order to remove Ca-Fe oxide coatings and evaluate the influence of these coatings on the rates of microbial Fe(III) and As(V) reduction. Environmental scanning electron microscope (ESEM) micrographs of the solid phase show significant differences in the chemistry and physical morphology of the material by the bacteria over time and are especially evident in the acid treated samples. Moreover, while solution chemistry showed similar As(III) respiration rates of the inoculated acid treated samples for both ANA3 and 200R at {approx}1.1 x 10{sup -6} {micro}M {center_dot} s{sup -1} {center_dot} m{sup -2}, the Fe(II) respiration rates differed at 1.4 x 10{sup -7} and 9.5 x 10{sup -8} {micro}M {center_dot} s{sup -1} {center_dot} m{sup -2} respectively, thus suggesting strain specific metal reduction metabolic pathways Additionally, the enhanced metal reduction observed in the acid treated inoculated samples suggests that the presence of the Ca-Fe hydroxide phase in the untreated samples acted as a barrier, inhibiting the bacteria from accessing the metals. This has implications for increased mobilization of metals by metal reducing bacteria within areas of increased acidity, such as acid mine drainage sites and industrial tailings ponds that can come into contact with surface and ground water sources.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Vitrification of Hanford Tank Waste 241-AP-107 in a Continuous Laboratory-Scale Melter

Low-activity waste (LAW) stored in underground tanks on the Hanford Site in Washington State is planned to be filtered for solids removal and processed through ion exchange columns for cesium removal. These pretreatment steps will allow the waste to be transferred to the Hanford Tank Waste Treatment and Immobilization Plant’s LAW Facility for immobilization into glass. The liquid waste will be combined with glass-forming chemicals (GFCs) to form a waste feed slurry that can be fed to electric melters for vitrification. The process of continuously converting the aqueous feed slurry into a melt is dynamic and includes multiple reactions, degassing, and dissolution processes that depend on heat from the melt below. In this conversion process, waste components are partitioned into one of two streams: glass and off-gas. Washington River Protection Solutions has requested processing information and chemical information associated with these waste products for actual waste from Hanford tank 241-AP-107 (referred to herein as AP-107). To acquire this type of information, a small-scale melter system was designed that would not require high volumes of input waste or the large resource commitment of a full-scale melter system, while also providing dynamic information that would be difficult to determine from batch reactions in a crucible system. A continuous laboratory-scale melter (CLSM) has been designed to operate with a continuous feeding process while periodically pouring glass product and collecting off-gas. The CLSM vessel has been sized to collect the relevant process and chemical information from obtainable volumes of AP-107 waste samples. A total 8.6 L of actual AP-107 tank waste were received after filtering for solids removal and ion exchange for cesium removal. This volume of AP-107 waste was mixed with GFCs to form an estimated 11.8 L of melter feed slurry. A mass of 7.01 kg of glass product were poured from the CLSM vessel during 10.07 hours of charging the AP-107 melter feed, indicating that about 15.0 kg of melter feed was vitrified into glass. The CLSM system was also designed with the capability to fully divert the flow of off-gas produced in the CLSM vessel to a sampling line that could capture the volatile species of interest, such as technetium-99 ( 99 Tc). This novel sampling system avoided the difficulties of slipstream sampling and could be activated once the feeding reached a steady state within the CLSM vessel. Off-gas product samples captured via high-efficiency particulate air (HEPA) filters using this method, as well as selected glass product samples were sent to an analytical lab for chemical analysis.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Quantifying dry supercritical CO 2 -induced changes of the Utica Shale

Traditionally, shale formations have been studied as sealing layers that prevent vertical migration of hydrocarbons and CO2 due to their low permeability and fracture porosity. Recent research has focused on storing CO2 in hydrocarbon-bearing shale formations that have already undergone depletion through primary production and using CO2 as a potential fracturing agent for unconventional reservoirs. The injected CO2 will interact with shale components (i.e. clays, organic matter) and affect rock properties through chemical alteration, matrix swelling/shrinkage, and related geomechanical effects. As changes in rock properties will impact both anthropogenic CO2 storage and hydraulic fracturing, it is imperative to increase our understanding of the CO2-shale interactions. In-situ Fourier Transform infrared (FT-IR) spectroscopy coupled with high temperature and pressure capability was used to examine the interaction of dry CO2 on Utica Shale, clay, and kerogen samples at the molecular scale and characterize vibrational changes of sorption bands sensitive to the gas-solid environment. The Utica Shale was also analyzed for micro and macro-scale chemical and physical changes before and after exposure to dry CO2 at subsurface storage conditions using surface relocation techniques via high-resolution field-emission scanning electron microscopy (FE-SEM). Brunauer-Emmett-Teller (BET) surface area/pore size analysis and quantitative adsorption isotherms were applied to understand changes in surface area, pore volumes, and understand the storage potential of CO2 in the Utica Shale sample. FT-IR and feature relocation via FE-SEM indicate carbonate formation and dissolution occurs in shale exposed to dry CO2. Results indicate that etching and pitting occur, with minor calcite precipitation along the surface of the shale sample. Quantitative isotherm results indicate that shales with a higher content of kerogen and illite-smectite clays would be expected to have the highest CO2 storage capacity provided these constituents were accessible for interaction.

04 OIL SHALES AND TAR SANDS↗

Delamination recycling of multilayer plastic films: Solvent-assisted separation pathways and recovery of solid polyolefins

Multilayer plastic films are excellent packaging materials due to the bound layers of multiple polymers, with each different polymer contributing to the film properties. Desirable properties lead to continuously growing demand for multilayer films. Multilayer plastic films are typically single-use and, as such, their increased production and disposal have led to waste management problems. Multilayer films are not currently recyclable primarily due to the multiple bound polymers. This work advances delamination as a recycling process to separate and sequester valuable polymers from multilayer films, facilitating the incorporation of these polymers into the circular economy. We effect delamination in a physical process that preserves targeted polymers as solid film, hence retaining their embodied energy. This work documents three different pathways of inducing delamination of multilayer films, with appropriate solvents disrupting adhesion between adjacent layers or dissolving a minor component of the film in less than an hour and at temperatures below 90°C, and where all initial polyethylene is maintained in its solid form throughout the process and is recovered at high purity. Solvent-based delamination is exemplified on commercial multilayer films with majority polyethylene (PE), and polyethylene terephthalate (PET) or ethylene vinyl alcohol copolymer (EVOH) or nylon also present. Solvent-based delamination is an energy-efficient and environmentally friendly recycling process that improves upon dissolution-precipitation recycling, since delamination involves very little dissolution and no precipitation, and is superior to pyrolysis which breaks down the polymers, while delamination keeps polymer chains intact. Furthermore, delamination recycling can contribute to the sustainable use of multilayer films as they continue to protect our food and medicine.

Chemical Recycling↗

Ternary metal fluorides as high-energy cathodes with low cycling hysteresis

In this study, transition metal fluorides are an appealing alternative to conventional intercalation compounds for use as cathodes in next-generation lithium batteries due to their extremely high capacity (3–4 times greater than the current state-of-the-art). However, issues related to reversibility, energy efficiency and kinetics prevent their practical application. Here we report on the synthesis, structural and electrochemical properties of ternary metal fluorides (M 1 y M 2 1-y F x : M 1 , M 2 = Fe, Cu), which may overcome these issues. By substituting Cu into the Fe lattice, forming the solid–solution Cu y Fe 1-y F 2 , reversible Cu and Fe redox reactions are achieved with surprisingly small hysteresis (<150 mV). This finding indicates that cation substitution may provide a new avenue for tailoring key electrochemical properties of conversion electrodes. In conclusion, although the reversible capacity of Cu conversion fades rapidly, likely due to Cu + dissolution, the low hysteresis and high energy suggest that a Cu-based fluoride cathode remains an intriguing candidate for rechargeable lithium batteries.

36 MATERIALS SCIENCE↗

Phase diagram of KHF2 and non-equilibrium effects

The equilibrium diagram for the KHF2-H2O system was constructed from cooling and heating curves for the compositions between 5 wt% and 40 wt% KHF2 and the results are shown. The phase diagrams shown is typical of that of a two component system with miscible liquid phases and whole solid phases consist of pure components. A eutectic point was found at approximately 15% KHF2 which remains completely liquid down to a temperature of -9.0 C. No hydrate formation was observed and no anomalous behavior such as the occurrence of solid transitions or metastable states was observed. The effect of rapid freezing on the equilibrium diagram did not appear, and cooling curves exhibited only one halt. Also, at rapid freezing rates, the supercooling of the solutions was smaller than those observed at the slow cooling rates. The existence of a eutectic composition and the slow rate of dissolution of the salt are used to interpret heat absorption behavior in practical applications of the KHF2-H2O system.

Hobson, M. C.↗

Passivation of a Corrosion Resistant High Entropy Alloy in Non-oxidizing Sulfate Solutions

The passivation behavior of a novel high entropy alloy (HEA) of composition 38Ni-21Cr-20Fe-13Ru-6Mo-2W at.% (33Ni-16Cr-17Fe-19Ru-9Mo-6W wt.%) was investigated in sulfate solutions of various pH levels. The HEA was compared to a commercially available Ni-Cr-Mo-W-Fe alloy, C-22. Experiments were conducted using in-situ electrochemical and ex-situ surface-sensitive methods to probe the growth and dissolution of the passive layer. The HEA exhibited excellent corrosion resistance in highly acidic and highly alkaline solutions, maintaining passivity through a broad range of potentials below the Cr transpassivity range. Extremely rapid and efficient oxide formation and lower quasi-steady passive current densities were observed during oxide growth in the passive range compared to commercial alloy C-22. Ex-situ characterization of the passive film by atom probe tomography and X-ray photoelectron spectroscopy provided insight into the oxide composition, thickness, and elemental valence states of potentiostatically-grown and air-formed oxides. All elements in the alloy were oxidized following potentiostatic oxide growth. Instead of distinct stoichiometric and phase-distinct oxides, a disordered solid solution oxide was observed with significant enrichment in Cr and Ru with the latter depending sensitively on potential, as well as depletion of Fe and Ni. Enrichment of Cr was modeled with a modified surface enrichment model. The oxide thickness was estimated to be 3-4 nm thick. The connection between the enrichment of Cr in the passive layer, Mo and W presence, and excellent passivity is discussed.

corrosion, High entropy alloys, XPS, atom probe to↗