Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscatter diffraction (EBSD)”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

Relationships Between the Phase Transformation Kinetics, Texture Evolution, and Microstructure Development in a 304L Stainless Steel Under Biaxial Loading Conditions: Synchrotron X-ray and Electron Backscatter Diffraction Studies

The relationships between the martensitic phase transformation kinetics, texture evolution, and the microstructure development in the parent austenite phase were studied for a 304L stainless steel that exhibits the transformation-induced plasticity effect under biaxial loading conditions at ambient temperature. The applied loading paths included: pure torsion, simultaneous biaxial torsion/tension, simultaneous biaxial torsion/compression, and stepwise loading of tension followed by torsion (i.e., first loading by uniaxial tension and then by pure torsion in sequence). Synchrotron X-ray and electron backscatter diffraction techniques were used to measure the evolution of the phase fractions, textures, and microstructures as a function of the applied strains. The influence of loading character and path on the changes in martensitic phase transformation kinetics is discussed in the context of (1) texture-transformation relationship and the preferred transformation of grains belonging to certain texture components over the others, (2) effects of axial strains on shear band evolutions, and (3) volume changes associated with martensitic transformation.

Complex Loading↗

Effect of Nd:YAG laser welding on microstructure and hardness of an Al-Li based alloy

Butt joints of 3.0 mm thick sheets of an Al-Li based alloy have been produced using Nd:YAG laser welding without filler metals. The hardness distribution and microstructure of the alloy and welded joints were investigated. The changes in the grain shapes, grain orientations, microtexture, and precipitates of the fusion zone were analyzed using optical microscope, electron back scattered diffraction (EBSD) and transmission electron microscopy (TEM). The results show that Nd:YAG laser welding leads to a change of the microhardness, grain shape, grain orientations, and a disappearance of the microtexture and precipitates. A narrow band of EQZ along the fusion boundary and a predominantly equiaxed dendritic structure are developed in the fusion zone. The formation of the predominately equiaxed dendritic grains is due to a heterogeneous nucleation mechanism aided by equilibrium A1{sub 3}Zr phases as well as the growth of pre-existing nuclei created by dendrite fragmentation, or by grain detachment resulted from Nd:YAG laser welding processes. In addition, Nd:YAG laser welding produces lower Vickers hardness than that of the base metal due to the decrease in the in quantity of {delta} Prime precipitates in the fusion zone. - Graphical Abstract: The grain shapes, grain orientations, microtexture, and precipitates of the solidified fusion zone were investigated and compared with the base metal using optical microscope, electron back scattered diffraction (EBSD) and transmission electron microscope (TEM). EBSD orientation map of laser welded joint in 5A90 alloys is presented in Fig. 3. It clearly shows that a narrow band EQZ along the fusion boundary and the predominantly equiaxed grains have been developed in the fusion zone of 5A90 alloys. Also, it is clear that the microstructure of the base metal is characterized by laminated grains with preferred orientations, whereas the fusion zone is predominately equiaxed grains in different colors having random orientations. Highlights: Black-Right-Pointing-Pointer The predominantly equiaxed dendritic structure is developed in the fusion zone. Black-Right-Pointing-Pointer The fusion zone with equiaxed grains shows random orientations and microtexture. Black-Right-Pointing-Pointer The loss in hardness in the fusion zone is due to the decrease in {delta} Prime precipitates. Black-Right-Pointing-Pointer The non-epitaxial growth occurs at fusion boundary. Black-Right-Pointing-Pointer The equilibrium A1{sub 3}Zr phases maybe the nuclei of new grains in the fusion zone.

36 MATERIALS SCIENCE↗

Effects of Changing Hot Rolling Direction on Microstructure, Texture and Mechanical Properties of Cu-2.7Be Sheets

A hot rolling scheme (cross-rolling and unidirectional rolling) was adopted to process Cu-2.7Be sheets used as multiplier dynodes in photomultiplier. The effects of changing rolling direction on microstructure, texture and mechanical properties were studied by a combination of XRD, EBSD and TEM. It was found that higher copper-type texture and lower brass texture intensity were obtained in the ultimately cross-rolling (CR) sheet compared with the unidirectional rolling (UR) sheet.The EBSD results indicated that the grain orientation from mainly 〈101〉 for UR sample turns to random for CR sample. Great enhancements in YS and UTS after unidirectional rolling were attributed to the massive and polygonal γ precipitates. The CR sample exhibited lower anisotropy, because of the increase of S and γ precipitates with spherical and tiny shape.

36 MATERIALS SCIENCE↗

Microstructure evolution and a new mechanism of B2 phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy prepared by hot isostatic pressing

Highlights: • The microstructure evolution of Ti-47Al-2Cr-2Nb alolly was investigated in detail. • The foramtion of B{sub 2} phase can be adjusted in Ti-47Al-2Cr-2Nb alloy. • A new mechanism of B{sub 2} phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy was proposed. - Abstract: The formation of B{sub 2} phase was adjusted via various hot isostatic pressing processes in Ti-47Al-2Cr-2Nb alloy. The microstructure evolution and a new mechanism of B{sub 2} phase on room temperature mechanical properties was investigated by BSE, EBSD and TEM in detail. The result shows that the formation of B{sub 2} phase leads to Cr element content decrease in γ matrix phase, which results in lattice parameter increase, namely the c/a ratio of γ matrix phase. Finally, at room temperature the mechanical properties of Ti-47Al-2Cr-2Nb alloy deteriorates.

36 MATERIALS SCIENCE↗

Mechanical behavior and texture development of over-aged and solution treated Al-Cu-Mg alloy during multi-directional forging

The effects of initial heat treatments, i.e. solution treating and over ageing, on deformation behavior of an age hardenable Al-Cu-Mg alloy, including mechanical properties and texture evolution, during multi-directional forging (MDF) are investigated. Hardness measurements, electron back scatter diffraction (EBSD) maps, and differential scanning calorimetry (DSC) are carried out. Mechanical behaviors of the alloy in terms of compressive stress and hardness test after MDF are investigated. In both solution treated and over-aged alloys, the compressive stress during MDF shows an increase up to the second pass, and by further straining the flow stress is decreased. However, shear and deformation bands are formed in both solution treated and over-aged alloys, the density of these instabilities in the solution treated alloy is higher than that in over-aged alloy. In the solution treated alloy, not only large particles induce deformation bands, but also the dynamically formed GPB zones/Cu-Mg co-clusters. Texture analysis shows that the shear component of C {001}<110> (Φ{sub 1} = 90°, Φ = 0°, Φ{sub 2} = 45°) is developed with 18 mrd during MDF of the over-aged alloy. In the solution treated alloy, due to the high density of deformation bands and different microchemistry of the matrix in comparison with that of the over-aged alloy, the Copper type texture component {112}<111> (Φ{sub 1} = 90°, Φ = 35°, Φ{sub 2} = 45°) is developed with 11 mrd.

36 MATERIALS SCIENCE↗

Cold rolling texture evolution of TiB2 particle reinforced Al-based composites by Neutron Diffraction and EBSD analysis

Highlights: • Texture development of in-situ TiB{sub 2} particle reinforced Al matrix composites after cold rolling were characterized. • The sum of rolling texture volume fractions has been significantly reduced by the weak texture in particle deformation zone. • Recrystallization nuclei with the Cube and Rotated-Cube orientations were observed in the particle deformation zones. • Small TiB{sub 2} particles within Al grains kept the parallel relationship with surrounding matrix during the deformation. - Abstract: Texture development of particle-reinforced metal matrix materials (P-MMCs) has not been understood well, especially the effects of second-phase particles during the deformation. In this work, we have investigated the texture evolution of TiB{sub 2}/Al composites during cold rolling by Neutron Diffraction and EBSD analysis. Two forms of TiB{sub 2} particles influenced the texture evolution in different ways. The particle-clusters aggregated along grain boundaries led to a reduction of texture volume fraction; recrystallization nuclei with weak texture appeared around these particle-clusters. Small non-shearable TiB{sub 2} particles dispersed inside Al matrix contributed to strong Copper texture component at high strains; the individual particles rotated together with Al matrix during the deformation. These revealed effects of particles on the texture development in TiB{sub 2}/Al composites provide a reference for the texture control of P-MMCs.

36 MATERIALS SCIENCE↗

Effect of carbon content on solidification behaviors and morphological characteristics of the constituent phases in Cr-Fe-C alloys

A combination of transmission electron microscopy, electron backscatter diffraction and wavelength dispersive spectrum has been used to identify crystal structure, grain boundary characteristic and chemical composition of the constituent phases in Cr-Fe-C alloys with three different carbon concentrations. Depending on the three different carbon concentrations, the solidification structures are found to consist of primary {alpha}-phase and [{alpha} + (Cr,Fe){sub 23} C{sub 6}] eutectic in Cr-18.4Fe-2.3 C alloy; primary (Cr,Fe){sub 23} C{sub 6} and [{alpha} + (Cr,Fe){sub 23} C{sub 6}] eutectic in Cr-24.5Fe-3.8 C alloy and primary (Cr,Fe){sub 7} C{sub 3} and [{alpha} + (Cr,Fe){sub 7} C{sub 3}] eutectic in Cr-21.1Fe-5.9 C alloy, respectively. The grain boundary analysis is useful to understand growth mechanism of the primary phase. The morphologies of primary (Cr,Fe){sub 23} C{sub 6} and (Cr,Fe){sub 7} C{sub 3} carbides are faceted structures with polygonal shapes, different from primary {alpha}-phase with dendritic shape. The primary (Cr,Fe){sub 23} C{sub 6} and (Cr,Fe){sub 7} C{sub 3} carbides with strong texture exist a single crystal structure and contain a slight low angle boundary, resulting in the polygonal growth mechanism. Nevertheless, the primary {alpha}-phase with relative random orientation exhibits a polycrystalline structure and comprises a massive high-angle boundary, caused by the dendritic growth mechanism. - Highlights: Black-Right-Pointing-Pointer Microstructures of the as-clad Cr-based alloys are characterized by TEM. Black-Right-Pointing-Pointer EBSD technique has been use to characterize the grain boundary of primary phases. Black-Right-Pointing-Pointer We examine transitions in morphology about the primary phases. Black-Right-Pointing-Pointer Morphologies of primary carbides are polygonal different from primary {alpha}-phase. Black-Right-Pointing-Pointer Solidification structures rely on C concentrations in Cr-Fe-C alloy.

36 MATERIALS SCIENCE↗

Microstructure evolution and properties of graphene nanoplatelets reinforced aluminum matrix composites

Highlights: • Lamellar structure of GNPs fibers and Al matrix was obtained in the rolling direction. • Stacking faults were observed in Al grains due to greatly increased GNPs/Al interfaces. • Strength of Al-0.2 wt% GNPs increased 36.8% with negligible electrical conductivity loss. - Abstract: Aluminum matrix composites reinforced with graphene nanoplatelets (GNPs) were prepared by continuous casting and subsequent rolling. Al-GNPs master alloy, prepared by ball milling and cold pressing, was added into Al melts to fabricate the composites. Microstructure evolution of the composites were observed using scanning electron microscopy (SEM), transmission electron microscopy (TEM) and electron back scattered diffraction (EBSD). GNPs distributed uniformly in the as-cast specimen and then transformed into fibers in the rolling direction after deformation and finally a lamellar structure formed in the composites. Raman spectra showed that the structural damage of GNPs mainly came from ball milling. The interface between GNPs and Al was well combined in general while a few microcracks were observed, which reduced the ductility of the composites and no adverse aluminum carbide (Al{sub 4}C{sub 3}) was detected at the interface. Stacking faults were observed interior of the aluminum grain, which may due to the existence of plentiful interface introduced by GNPs. Fracture observation revealed that the load transferred from Al matrix to GNPs. The ultimate tensile strength of Al-0.2 wt% GNPs composites was about 36.8% higher than that of pure Al with the same casting and rolling process, which should result from the lamellar structure and load transfer, while the conductivity of the composites decreased slightly, indicating that interface scattering between Al and GNPs is very limited. The investigation results show that Al-GNPs composite is potential for high strength and high conductivity application.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Surface working of 304L stainless steel: Impact on microstructure, electrochemical behavior and SCC resistance

The effect of surface working operations on the microstructure, electrochemical behavior and stress corrosion cracking resistance of 304L stainless steel (SS) was investigated in this study. The material was subjected to (a) solution annealing (b) machining and (c) grinding operations. Microstructural characterization was done using stereo microscopy and electron back scattered diffraction (EBSD) technique. The electrochemical nature of the surfaces in machined, ground and solution annealed condition were studied using potentiodynamic polarization and scanning electrochemical microscopy (SECM) in borate buffer solution. The stress corrosion cracking resistance of 304L SS in different conditions was studied by exposing the samples to boiling MgCl{sub 2} environment. Results revealed that the heavy plastic deformation and residual stresses present near the surface due to machining and grinding operations make 304L SS electrochemically more active and susceptible to stress corrosion cracking. Ground sample showed highest magnitude of current density in the passive potential range followed by machined and solution annealed 304L SS. Micro-electrochemical studies established that surface working promotes localized corrosion along the surface asperities which could lead to crack initiation. - Highlights: Black-Right-Pointing-Pointer Machining/grinding produce extensive grain fragmentation near the surface of 304L SS. Black-Right-Pointing-Pointer Machining/grinding result in martensitic transformation near the surface of 304L SS. Black-Right-Pointing-Pointer Machining/grinding drastically reduce the SCC resistance of 304L SS in chloride. Black-Right-Pointing-Pointer Machining/grinding make the surface of 304L SS electrochemically much more active. Black-Right-Pointing-Pointer SECM study reveal that preferential dissolution takes place along surface asperities.

36 MATERIALS SCIENCE↗

Microstructural variation through weld thickness and mechanical properties of peened friction stir welded 6061 aluminum alloy joints

The current study examined the effect of microstructure variation on the development of mechanical properties in friction stir welded joints of 6061-T6 aluminum alloy, which were subsequently processed by shot peening (SP). Following to FSW, fatigue specimens were extracted perpendicularly to the welding direction. Surface Skimming to 0.5 mm from crown and root sides of the joint was made and SP was later applied on the two sides using ceramic shots of two different Almen intensities of 0.18 mmA and 0.24 mmA. Microstructural examination by electron back scattered diffraction (EBSD) indicated variation in the grain refinement of the weld zone, with coarsest grains (5 μm) at the crown side and finest grains (2 μm) at the root side. Reduction of microhardness to 60 HV occurred in the weld zone for samples in FSW condition. Application of SP promoted significant strain hardening at the crown side, with Almen intensities of 0.24 mmA providing maximum increase in microhardness to 120 HV. On the contrary, only a maximum microhardness of 75 HV was obtained at the root side. The difference in strain hardening capability at the two sides was strongly dependent on grain size. The two Almen intensities produced similar distribution of compressive residual stresses in the subsurface regions that led to enhance the fatigue strength to the level of base metal for N ≥ 10{sup 5} cycles. Yet, the increase in fatigue strength was more pronounced with increasing Almen intensity to 0.24 mmA, demonstrating further enhancement by strain hardening. - Highlights: • Grain refinement was observed after friction stir welding of AA 6061-T6. • Reduction in microhardness and fatigue strength were obtained after welding. • Variation in grain refinement led to different hardening behavior after peening. • Shot peening induced beneficial compressive residual stresses. • Shot peening and surface skimming markedly improved the fatigue performance.

36 MATERIALS SCIENCE↗

Advanced processing of EBSD data to distinguish the complex microstructure evolution of a Cu-Ni-Si alloy induced by fatigue

Highlights: • Microstructure investigation of the fatigue behaviour of a Cu-Ni-Si alloy • Use of ECCI and EBSD to investigate the microstructure evolution related to fatigue dislocations structures • Characterisation of local plastic accommodation through EBSD misorientation criteria - Abstract: The present work aims at identifying the evolution of the microstructure of a Cu-Ni-Si (Corson alloy) alloy after low cycle fatigue by means of advanced electron microscopy analysis techniques (SEM-ECCI, Orientation Imaging Microscopy by means of SEM-EBSD and TEM). Deep attention is paid on the material subjected to high cyclic strains where a transient cellular dislocation structure transformed into precipitate free bands. It is shown that the formation of dislocation cells leads to a high GROD and high GOSaera value and its standard deviation. However, the presence of precipitate free bands results in the low GOSarea level and its low standard deviation.

36 MATERIALS SCIENCE↗

Fabrication and characterization of microstructure of stainless steel matrix composites containing up to 25 vol% NbC

AISI 440 stainless steels reinforced with various volume fractions of niobium carbide (NbC) particles of up to 25 vol% were fabricated in-situ using an argon arc furnace and then heat-treated to produce a martensitic matrix. Optical and scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDS) and electron back-scatter diffraction (EBSD) techniques were used to analyze the microstructure, phases and composition of these composites. Interestingly, it was found that Chinese-script NbC could nucleate on existing primary NbC particles creating NbC clusters with complex microstructures. Additionally, hardness tests were used to evaluate viability in mining and mineral processing applications. The increase in NbC content resulted in an overall increase in the hardness of the composites while causing a marginal decrease in the amount of Cr in solid solution with the matrix, which could be a concern for corrosion resistance. The latter was due to the fact that the NbC lattice could dissolve a minor amount of Cr. Thermodynamic simulations also attributed this to a slight increase in M{sub 7}C{sub 3} precipitation. Nonetheless, these novel composites show great promise for applications in wear and corrosive environments. - Highlights: •Stainless steels reinforced with NbC particles of up to 25 vol% were fabricated. •NbC was formed in-situ in the steels using an arc melter. •Martensitic transformation of the matrix of each sample was achieved. •NbC reinforcements increased the bulk hardness values of the steels. •Dissolved Cr in the matrix of each sample was sufficient for passivity in theory.

36 MATERIALS SCIENCE↗

Crystallographic orientation variation of isothermal pearlite under high magnetic field

Crystallographic orientation (CO) variation of magnetic-induced pearlite (MIP) during its microstructure evolution in 19.8 T was investigated by electron back-scatter diffraction (EBSD). It is closely related to the isothermal temperatures (ITs) and the applied magnetic time (MT) during the process of MIP formation. The <100> easy magnetization direction in MIP colonies is strengthened with the MT within the certain transformed fraction of MIP (f{sub MIP}) at the relatively lower IT (983 K) above the eutectoid temperature but below the magnetically shifted upward eutectoid temperature, while this special CO tends to be weakened at a relatively higher IT (995 K). For the same MT, the higher the IT, the relatively larger is the proportion in <100> orientation for MIP colonies at the early growth stage. These results have demonstrated that the change of <100> orientation of MIP is closely related to the growth rate of pearlite ferrite (PF), and strengthened mainly at early transformation stage. When f{sub MIP} reaches some value, the growth rate of MIP at other COs, such as <110>, even at the hard magnetization direction, turns to present speed-up. - Highlights: • HMF can induce pearlite with different fractions above the eutectoid temperature. • CO is closely related to isothermal temperatures and applied magnetic time. • <100> direction is related to the growth rate of PF, and strengthened at early stage. • When f{sub MIP} reaches some value, the growth rate at other COs turns to present speed-up.

36 MATERIALS SCIENCE↗

Examining the microtexture evolution in a hole-edge punched into 780 MPa grade hot-rolled steel

The deformation behavior in the hole-edge of 780 MPa grade hot-rolled steel during the punching process was investigated via microstructure characterization and computational simulation. Microstructure characterization was conducted to observe the edges of punched holes through the thickness direction, and electron back-scattered diffraction (EBSD) was used to analyze the heterogeneity of the deformation. Finite element analysis (FEA) that could account for a ductile fracture criterion was conducted to simulate the deformation and fracture behaviors of 780 MPa grade hot-rolled steel during the punching process. Calculation of rotation rate fields at the edges of the punched holes during the punching process revealed that metastable orientations in Euler space were confined to specific orientation groups. Rotation-rate fields effectively explained the stability of the initial texture components in the hole-edge region during the punching process. A visco-plastic self-consistent (VPSC) polycrystal model was used to calculate the microtexture evolution in the hole-edge region during the punching process. FEA revealed that the heterogeneous effective strain was closely related to the heterogeneity of the Kernel average misorientation (KAM) distribution in the hole-edge region. A simulation of the deformation microtexture evolution in the hole-edge region using a VPSC model was in good agreement with the experimental results. - Highlights: •We analyzed the microstructure in a hole-edge punched in HR 780HB steel. •Rotation rate fields revealed the stability of the initial texture components. •Heterogeneous effective stain was closely related to the KAM distribution. •VPSC model successfully simulated the deformation microtexture evolution.

36 MATERIALS SCIENCE↗

Three-dimensional characterization of bainitic microstructures in low-carbon high-strength low-alloy steel studied by electron backscatter diffraction

We investigated the microstructural evolution of high strength low alloy steel, Fe–2.0Mn–0.15Si–0.05C (wt.%), by varying the continuous cooling rates from 1 K/s to 50 K/s using three-dimensional electron backscatter diffraction and transmission electron microscopy. Granular bainitic microstructure was prevalent under a slow cooling rate of 1–10 K/s, while lath-type bainite was dominant at a high cooling rate of 50 K/s. The acicular ferrite that was the major microstructure under the intermediate ranges of cooling rates between 10 K/s and 30 K/s was tangled with each other, leading to a three-dimensional interwoven structure with highly misoriented grains. Because of the formation of three-dimensional structures, we propose that the terms “acicular ferrite” and “bainitic ferrite,” which are currently used in steel, be replaced by the terms “interwoven acicular bainite” and “lath bainite,” respectively. Moreover, we also confirmed that the cooling rate is an important factor in determining whether bainitic microstructures occur in the form of granular bainite, interwoven bainite, or lath bainite. - Highlights: • The morphology of bainitic grains was characterized by 3D-EBSD. • The ‘interwoven bainite’ and ‘lath bainite’ were suggested. • Interwoven bainite consisted of lenticular plates that were interlinked in 3D regime. • The packets of lath bainite were aligned in a specific direction.

36 MATERIALS SCIENCE↗

Characterization of complex carbide–silicide precipitates in a Ni–Cr–Mo–Fe–Si alloy modified by welding

Nickel based alloys of the type Hastelloy-N™ are ideal candidate materials for molten salt reactors, as well as for applications such as pressure vessels, due to their excellent resistance to creep, oxidation and corrosion. In this work, the authors have attempted to understand the effects of welding on the morphology, chemistry and crystal structure of the precipitates in the heat affected zone (HAZ) and the weld zone of a Ni–Cr–Mo–Fe–Si alloy similar to Hastelloy-N™ in composition, by using characterization techniques such as scanning and transmission electron microscopy. Two plates of a Ni–Cr–Mo–Fe–Si alloy GH-3535 were welded together using a TiG welding process without filler material to achieve a joint with a curved molten zone with dendritic structure. It is evident that the primary precipitates have melted in the HAZ and re-solidified in a eutectic-like morphology, with a chemistry and crystal structure only slightly different from the pre-existing precipitates, while the surrounding matrix grains remained unmelted, except for the zones immediately adjacent to the precipitates. In the molten zone, the primary precipitates were fully melted and dissolved in the matrix, and there was enrichment of Mo and Si in the dendrite boundaries after solidification, and re-precipitation of the complex carbides/silicides at some grain boundaries and triple points. The nature of the precipitates in the molten zone varied according to the local chemical composition. - Graphical abstract: Display Omitted - Highlights: • Ni-based alloy with Cr, Mo, Si, Fe and C was welded, examined with SEM, EBSD, and TEM. • Original Ni{sub 2}(Mo,Cr){sub 4}(Si,C) carbides changed from equiaxed to lamellar shape in HAZ. • Composition and crystal structure remained almost unchanged in HAZ. • Original carbides changed to lamellar Ni{sub 3}(Mo,Cr){sub 3}(Si,C) in some cases in weld metal. • Precipitates were mostly incoherent, but semi-coherent in some cases in weld metal.

36 MATERIALS SCIENCE↗

Cesium incorporation in hollandite-rich multiphasic ceramic waste forms

Hollandite-rich multiphase waste form compositions processed by melt-solidification and spark plasma sintering (SPS) were characterized, compared, and validated for nuclear waste incorporation. Phase identification by x-ray diffraction (XRD) and electron back-scattered diffraction (EBSD) confirmed hollandite as the major phase present in these samples along with perovskite, pyrochlore and zirconolite. Distribution of selected elements observed by wavelength dispersive spectroscopy (WDS) maps indicated that Cs formed a secondary phase during SPS processing, which was considered undesirable. On the other hand, Cs partitioned into the hollandite phase in melt-processed samples. Further analysis of hollandite structure in melt-processed composition by selected area electron diffraction (SAED) revealed ordered arrangement of tunnel ions (Ba/Cs) and vacancies, suggesting efficient Cs incorporation into the lattice.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Correlation Between Structural Parameters and Mechanical Properties of Al5083 Sheets Processed by ECAR

In the paper, structural parameters and mechanical properties of Al5083 alloy sheet during equal channel angular rolling (ECAR) process and their relationship are studied. In order to evaluate the effect of ECAR process, Al5083 strips were subjected to the ECAR process for 1, 2, and 3 passes through the die channel angles 110°, 120°, and 130° at two routes. The effect of the process on the microstructural evolution of samples was investigated by means of x-ray diffraction and EBSD techniques. X-ray pattern has been analyzed using Rietveld method to compute structural parameters, including microstrain, average crystallite size, and dislocation density. The results showed that the dislocation density and microstrain were increased, and crystallite size was decreased during ECAR process. It was found that the behavior of variations in mechanical properties was in accordance with the dislocation density changes. This paper revealed that the increase in the strength of ECARed samples could be attributed to reduction in high-angle grain boundaries and the increase in dislocation density. Moreover, the yield strength estimated from Taylor equation was found in accordance very well with the experimentally measured yield strength of the samples.

36 MATERIALS SCIENCE↗