Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 595 records · Page 33

Room Temperature Creep Of SiC/SiC Composites

During a recent experimental study, time dependent deformation was observed for a damaged Hi-Nicalon reinforced, BN interphase, chemically vapor infiltrated SiC matrix composites subjected to static loading at room temperature. The static load curves resembled primary creep curves. In addition, acoustic emission was monitored during the test and significant AE activity was recorded while maintaining a constant load, which suggested matrix cracking or interfacial sliding. For similar composites with carbon interphases, little or no time dependent deformation was observed. Evidently, exposure of the BN interphase to the ambient environment resulted in a reduction in the interfacial mechanical properties, i.e. interfacial shear strength and/or debond energy. These results were in qualitative agreement with observations made by Eldridge of a reduction in interfacial shear stress with time at room temperature as measured by fiber push-in experiments.

Morscher, Gregory N.↗

Constituent Effects on the Stress-Strain Behavior of Woven Melt-Infiltrated SiC Composites

The stress-strain behavior of 2D woven SiC fiber reinforced, melt-infiltrated SiC matrix composites with BN interphases were studied for composites fabricated with different fiber tow ends per unit length, different composite thickness, and different numbers of plies. In general, the stress-strain behavior, i.e., the 'knee' in the curve and the final slope of the stress-strain curve, was controlled by the volume fraction of fibers. Some of the composites exhibited debonding and sliding in between the interphase and the matrix rather than the more common debonding and sliding interface between the fiber and the interphase. Composites that exhibited this 'outside debonding' interface, in general, had lower elastic moduli and higher ultimate strains as well as longer pull-out lengths compared to the 'inside debonding' interface composites. Stress-strain curves were modeled where matrix crack formation as a function of stress was approximated from the acoustic emission activity and the measured crack density from the failed specimens. Interfacial shear strength measurements from individual fiber push-in tests were in good agreement with the interfacial shear strength values used to model the stress-strain curves.

Morscher, Gregory N.↗

Intermediate Temperature Strength Degradation in SiC/SiC Composites

Woven silicon carbide fiber-reinforced, silicon carbide matrix composites are leading candidate materials for an advanced jet engine combustor liner application. Although the use temperature in the hot region for this application is expected to exceed 1200 C, a potential life-limiting concern for this composite system exists at intermediate temperatures (800 +/- 200 C), where significant time-dependent strength degradation has been observed under stress-rupture loading. A number of factors control the degree of stress-rupture strength degradation, the major factor being the nature of the interphase separating the fiber and the matrix. BN interphases are superior to carbon interphases due to the slower oxidation kinetics of BN. A model for the intermediate temperature stress-rupture of SiC/BN/SiC composites is presented based on the observed mechanistic process that leads to strength degradation for the simple case of through-thickness matrix cracks. The approach taken has much in common with that used by Curtin and coworkers, for two different composite systems. The predictions of the model are in good agreement with the rupture data for stress-rupture of both precracked and as-produced composites. Also, three approaches that dramatically improve the intermediate temperature stress-rupture properties are described: Si-doped BN, fiber spreading, and 'outside debonding'.

Morscher, Gregory N.↗

Effect of Adventitious Carbon on the Environmental Degradation of SiC/BN/SiC Composites

Pesting remains a major obstacle to the application of SiC/SiC composites in engine service and selective degradation of the boron nitride interphase at intermediate temperatures is of primary concern. However, significant progress has been made on interphase improvement recently and we now know more about the phenomenon and ways to suppress it. By screening SiC/BN/SiC materials through characterization of strength and microstructures after exposure in a burner rig, some factors that control pesting in these composites have been determined. A key precaution is careful control of elemental carbon presence in the interphase region.

Ogbuji, L. U. J. T.↗

Organic-Inorganic Hybrids Using Novel Phenylethynyl Imide Silanes

In this presentation, polyimide-silica hybrids using novel phenylethynyl imide silanes are reported. The phenylethynyl group is present in the organic precursor as either a pendent or an end group to bond chemically with the polyimide adhesive containing phenylethynyl groups during processing, while the silane group of the organic precursor would chemically react with the inorganic precursor through oxane bond formation. The chemical compositions of these novel hybrids were examined using X-ray mapping modes of scanning electron microscopy (SEM), which revealed a silicon gradient interphase between the high surface energy substrate and the polyimide adhesive. Novel aromatic phenylethynyl imide silanes (APEISs) and pendent phenylethynyl imide oligomeric disilanes (PPEIDSs) have been synthesized, and sol-gel solutions containing the new silanes, a phenylethynyl terminated imide oligomer (PETI-5), and an inorganic precursor were formulated to develop a gradient hybrid interphase between a titanium alloy and the adhesive. Two different sol-gel systems were investigated to develop organic-inorganic hybrids. Hybrid I was composed of an organic precursor containing both phenylethynyl and silane groups (PPEIDS) and an inorganic precursor. Functional group concentrations were controlled by the variation of the molecular weight of the imide backbone of PPEIDS. Hybrid II was composed of organic and inorganic precursors and a coupling agent containing both phenylethynyl and silane groups. Morphology and chemical composition of the hybrid interphase between the inorganic substrate and the adhesive were investigated, and the bond strength and durability were evaluated using lap shear tests at various conditions. The assessment of how the bonding at an interface is affected by various sol-gel solution compositions and environments is reported.

Park, C.↗

Rejoining and misrejoining of radiation-induced chromatin breaks. III. Hypertonic treatment

It has been shown that treatment in anisotonic medium modifies rejoining of radiation-induced breaks in interphase chromosomes. In previous work, we have demonstrated that formation of exchanges in human lymphocytes has a slow component (half-time of 1-2 h), but a fraction of exchanges are also observed in samples assayed soon after exposure. In this paper we studied the effect of hypertonic treatment on rejoining and misrejoining of radiation-induced breaks using fluorescence in situ hybridization of prematurely condensed chromosomes in human lymphocytes. Isolated lymphocytes were irradiated with 7 Gy gamma rays, fused to mitotic hamster cells and incubated in hypertonic solution (0.5 M NaCl) for the period normally allowed for interphase chromosome condensation to occur. The data from hypertonic treatment experiments indicate the presence of a class of interphase chromosome breaks that rejoin and misrejoin very quickly (half-time of 5-6 min). The fast misrejoining of these lesions is considered to be responsible for the initial level of exchanges which we reported previously. No significant effect of hypertonic treatment on the yield of chromosome aberrations scored at the first postirradiation mitosis was detected.

NASA Discipline Radiation Health↗

Mechanical continuity and reversible chromosome disassembly within intact genomes removed from living cells

Chromatin is thought to be structurally discontinuous because it is packaged into morphologically distinct chromosomes that appear physically isolated from one another in metaphase preparations used for cytogenetic studies. However, analysis of chromosome positioning and movement suggest that different chromosomes often behave as if they were physically connected in interphase as well as mitosis. To address this paradox directly, we used a microsurgical technique to physically remove nucleoplasm or chromosomes from living cells under isotonic conditions. Using this approach, we found that pulling a single nucleolus or chromosome out from interphase or mitotic cells resulted in sequential removal of the remaining nucleoli and chromosomes, interconnected by a continuous elastic thread. Enzymatic treatments of interphase nucleoplasm and chromosome chains held under tension revealed that mechanical continuity within the chromatin was mediated by elements sensitive to DNase or micrococcal nuclease, but not RNases, formamide at high temperature, or proteases. In contrast, mechanical coupling between mitotic chromosomes and the surrounding cytoplasm appeared to be mediated by gelsolin-sensitive microfilaments. Furthermore, when ion concentrations were raised and lowered, both the chromosomes and the interconnecting strands underwent multiple rounds of decondensation and recondensation. As a result of these dynamic structural alterations, the mitotic chains also became sensitive to disruption by restriction enzymes. Ion-induced chromosome decondensation could be blocked by treatment with DNA binding dyes, agents that reduce protein disulfide linkages within nuclear matrix, or an antibody directed against histones. Fully decondensed chromatin strands also could be induced to recondense into chromosomes with pre-existing size, shape, number, and position by adding anti-histone antibodies. Conversely, removal of histones by proteolysis or heparin treatment produced chromosome decondensation which could be reversed by addition of histone H1, but not histones H2b or H3. These data suggest that DNA, its associated protein scaffolds, and surrounding cytoskeletal networks function as a structurally-unified system. Mechanical coupling within the nucleoplasm may coordinate dynamic alterations in chromatin structure, guide chromosome movement, and ensure fidelity of mitosis.

NASA Discipline Cell Biology↗

DC Electrical Conductivity of Silicon Carbide Ceramics and Composites for Flow Channel Insert Applications

High purity chemically vapor-deposited silicon carbide (SiC) and 2D continuous SiC fiber, chemically vapor-infiltrated SiC matrix composites with pyrocarbon interphases were examined for temperature dependent (RT to 800 C) electrical conductivity and the influence of neutron irradiation on it. In the 2D composites, trans-thickness electrical conductivity was dominated by bypass conduction via interphase network at relatively low temperatures, whereas conduction through SiC constituents dominated at higher temperatures. The Influence of neutron irradiation on electrical properties appeared very strong for SiC, resulting typically in by orders lower ambient conductivity and steeper temperature dependency. Through-thickness electrical conductivity of neutron-irradiated 2D SiC composites with thin PyC interphase will likely in the order of 10 S/m in the typical operating temperature range for flow channel inserts. Mechanisms of electrical conduction in the composites and irradiation-induced modification of electrical conductivity of the composites and their constituents are discussed.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Polysulfide-incompatible additive suppresses spatial reaction heterogeneity of Li-S batteries

Rational electrolyte engineering for practical pouch cells remains elusive because the correlation between the cathode/solid-electrolyte interphase layer and cell-level reaction behavior is poorly understood. Here, by combining multiscale characterization and computational modeling, we show that—counter to the conventional perception of polysulfide-incompatible additives—the spontaneous reaction of sparingly solvated polysulfides with Lewis acid additives (LAAs) can induce in situ formation of a homogeneous interphase on thick and tortuous S cathode. Multiscale synchrotron X-ray characterization consistently affirms that such interface design could effectively eliminate the notorious problems of polysulfide shuttle and lithium corrosion and, more importantly, provide an interconnected “ion transport highway” to alleviate the uneven ion transport within the tortuous S cathode. Hence, this design dramatically reduces the reaction heterogeneity of lithium-sulfur (Li-S) pouch cells under lean electrolyte conditions. Further, this work resolves controversy around the role of polysulfide-incompatible additives in high-energy Li-S pouch cells and highlights the importance of suppressing reaction heterogeneity for practical batteries.

36 MATERIALS SCIENCE↗

F and N Rich Solid Electrolyte for Stable All-Solid-State Battery

We report the instability of sulfide solid electrolytes to Li anode and high-voltage LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes limits the cyclic performance of all-solid-state lithium battery (ASSLB). Herein, the stability of Li 6 PS 5 Cl against Li anode is enhanced by mixing a small amount (0.32 wt%) of CuF 2 -LiNO 3 (CL) into Li 6 PS 5 Cl electrolyte layer to in-situ form a mixed-conductive-lithiophobic and self-healing LiF-Li 3 N-Cu solid electrolyte interphase (SEI) at Li 6 PS 5 Cl-CL/Li interface. The critical current density (CCD) of Li 6 PS 5 Cl-CuF 2 -LiNO 3 increases to 1.4 mA cm –2 /1.4 mAh cm –2 at room temperature, which is much higher than that of pristine Li 6 PS 5 Cl (0.4 mA cm –2 /0.4 mAh cm –2 ) even though mixing 0.32 wt% CL into Li 6 PS 5 Cl slightly reduces the ionic conductivity from 2.9 × 10 –3 to 1.5 × 10 –3 S cm –1 . The compatibility of Li 6 PS 5 Cl-CL electrolyte to single-crystalline NMC811 (S-NMC811) is further enhanced by adding a small amount (0.02 wt%) of AlF 3 into Li 6 PS 5 Cl-CL forming Li 6 PS 5 Cl-CuF 2- LiNO 3 -AlF 3 (Li 6 >PS 5 Cl-CLA) as a cathode electrolyte and by doing Cl – on S-NMC811 (Cl@S-NMC811) surface. The Cl@S-NMC811-Li 6 PS 5 Cl-CLA|Li 6 PS 5 Cl-CL|Li cells with areal capacity of 2.55 mAh cm -2 achieve a capacity retention of 69.4% after 100 cycles at 1C (1C = 200 mAh g -1 ). Adding a small amount of SEI and cathode/electrolyte interphase (CEI) former into the sulfide electrolytes with minimal reduction (48.3%) of ionic conductivity is an effective method to enhance the performance of ASSLB.

36 MATERIALS SCIENCE↗

Effects of Propylene Carbonate Content in CsPF 6 -Containing Electrolytes on the Enhanced Performances of Graphite Electrode for Lithium-Ion Batteries

The effects Of propylene carbonate (PC) content in CsPF6-containing electrolytes on the performances of graphite electrode in lithium half cells and in graphite parallel to LiNi0.80Co0.15Al0.05O2 (NCA) full cells are investigated. It is found that the performance of graphite electrode is significantly-affected by PC content in the CsPF6-containing electrolytes. An optimal PC content of 20% by weight in the solvent mixtures is identified. The enhanced electrochemical performance of graphite electrode can be attributed to the synergistic effects of the PC solvent and the Cs+ additive. The synergistic effects of Cs+ additive and appropriate amount of PC enable the formation of a robust, ultrathin, and compact solid electrolyte interphase (SEI) layer on the surface of graphite electrode, which is only permeable for desolvated Li+ ions and allows fast Li+ ion transport through it. Therefore, this SEI layer effectively suppresses the PC cointercalation and largely alleviates the Li dendrite formation on graphite electrode during lithiation even at relatively high current densities. The presence of low-melting-point PC solvent improves the sustainable operation of graphite parallel to NCA full cells under a wide temperature range. The fundamental findings also shed light On the importance of manipulating/maintaining the electrode/electrolyte interphasial stability in various energy-storage devices.

25 ENERGY STORAGE↗

Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System

Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, in this work, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.

Si anode↗

In Situ Cyclized Polyacrylonitrile Coating: Key to Stabilizing Porous High-Entropy Oxide Anodes for High-Performance Lithium-Ion Batteries

High-entropy oxides (HEOs) composed of multiple metal elements have attracted great attention as anode materials for lithium-ion batteries (LIBs) due to the synergistic effects of various metal species. However, the practical applications of HEOs are still plagued by poor conductivity, unstable solid electrolyte interphase (SEI) and poor cycling stability. In this work, nanosized (FeCoNiCrMn) 3 O 4 HEO (NHEO) is prepared successfully by the NaCl-assisted mechanical ball-milling strategy. Novelly, polyacrylonitrile (PAN) is used as the binder and then in situ thermochemically cyclized to construct a cyclized PAN (cPAN) outer layer onto NHEO (NHEO-cPAN). The in situ formed cPAN coating not only improves the electrical conductivity, but also reinforces the structural and interfacial stability, and thereby, the resulted NHEO-cPAN electrode exhibits significantly enhanced rate and cyclic performance. Specifically, NHEO-PAN500 electrode delivers a high reversible capacity of 560 mAh g –1 at 5 A g –1 and a high-capacity retention of 83% over 800 cycles at 3 A g –1 . Furthermore, the structural evolution and electrochemical behavior of NHEO-PAN electrode during discharge/charge is systematically investigated by operando X-ray diffraction, in situ impedance spectroscopy and ex situ high-resolution transmission electron microscopy. Therefore, this work provides new insights into the engineering of electrode and interphase for high-performance HEO electrode materials, potentially enlightening the practical applications of HEO-based LIBs.

25 ENERGY STORAGE↗

Unveiling the Stabilities of Nickel–Based Layered Oxide Cathodes at an Identical Degree of Delithiation in Lithium–Based Batteries

Bulk, surface, and interfacial instabilities that impact the cycle and thermal performances are the major challenges with high-energy-density LiNi 1–x–y Mn x Co y O 2 (NMC) cathodes with high nickel contents. It is generally believed that the instabilities and performance losses become exponentially aggravated as the nickel content increases. Disparate from this prevailing belief, it is herein demonstrated that NMC cathodes with higher Ni contents may imply better overall stability than “lower-Ni” cathodes under an identical degree of delithiation (charging) conditions. With two representative cathodes, LiNi 0.8 Mn 0.1 Co 0.1 O 2 and LiNiO 2 , a systematic investigation into their stabilities with control of the degree of delithiation is presented. Electrochemical tests indicate that LiNiO 2 displays better cyclability than LiNi 0.8 Mn 0.1 Co 0.1 O 2 at the same delithiation state. Comprehensive structural and interphase investigations unveil that the inferior cyclability of LiNi 0.8 Mn 0.1 Co 0.1 O 2 predominantly results from aggravated parasitic reactions, and the interphase stability may be more critical than lattice stability in dictating cyclability. Also, LiNiO 2 delivers similar or better thermal behavior than LiNi 0.8 Mn 0.1 Co 0.1 O 2 . Finally, the findings demonstrate a strong correlation of the stability of NMC cathodes to the degree of delithiation state rather than the Ni content itself, highlighting the importance of reassessing the true implications of Ni content and structural and interphasial tuning on the stabilities of NMC cathodes.

25 ENERGY STORAGE↗

Designing Electrolytes With Controlled Solvation Structure for Fast‐Charging Lithium‐Ion Batteries

Recharging battery-powered electric vehicles (EVs) in a similar timeframe as those used for refueling gas-powered internal combustion vehicles is highly desirable for rapid penetration of the EV market. It is well known that the electrolyte in a battery plays a critical role in fast-charging capability of the battery because it determines the rate of ion transport together with its derived electrode/electrolyte interphases on both cathode and anode of the battery. In this study, the effects of contents of salt, coordinating solvent, and noncoordinating diluent on salt dissociation degree and electrolyte ionic conductivity are investigated, and a controlled solvation structure electrolyte is developed to improve the lithium ion mobility and conductivity in the electrolyte and to enhance the kinetics and stability of the electrode/electrolyte interphases in the battery. This electrolyte enables fast-charging capability of high energy density lithium-ion batteries (LIBs) at up to 5 C rate (12-min charging), which significantly outperforms the state-of-the-art electrolyte. The controlled solvation structure sheds light on the future electrolyte design for fast-charging LIBs.

25 ENERGY STORAGE↗

A Systematic Study on the Effects of Solvating Solvents and Additives in Localized High‐Concentration Electrolytes over Electrochemical Performance of Lithium‐Ion Batteries

Abstract Localized high‐concentration electrolytes (LHCEs) based on five different types of solvents were systematically studied and compared in lithium (Li)‐ion batteries (LIBs). The unique solvation structure of LHCEs promotes the participation of Li salt in forming solid electrolyte interphase (SEI) on graphite (Gr) anode, which enables solvents previously considered incompatible with Gr to achieve reversible lithiation/delithiation. However, the long cyclability of LIBs is still subject to the intrinsic properties of the solvent species in LHCEs. Such issue can be readily resolved by introducing a small amount of additive into LHCEs. The synergetic decompositions of Li salt, solvating solvent and additive yield effective SEIs and cathode electrolyte interphases (CEIs) in most of the studied LHCEs. This study reveals that both the structure and the composition of solvation sheaths in LHCEs have significant effect on SEI and CEI, and consequently, the cycle life of energetically dense LIBs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synergetic Dual‐Additive Electrolyte Enables Highly Stable Performance in Sodium Metal Batteries

Sodium (Na)-metal batteries (SMBs) are considered one of the most promising candidates for the large-scale energy storage market owing to their high theoretical capacity (1,166 mAh g -1 ) and the abundance of Na raw material. However, the limited stability of electrolytes still hindered the application of SMBs. Herein, sulfolane (Sul) and vinylene carbonate (VC) are identified as effective dual additives that can largely stabilize propylene carbonate (PC)-based electrolytes, prevent dendrite growth, and extend the cycle life of SMBs. The cycling stability of the Na/NaNi 0.68 Mn 0.22 Co 0.1 O 2 (NaNMC) cell with this dual-additive electrolyte is remarkably enhanced, with a capacity retention of 94% and a Coulombic efficiency (CE) of 99.9% over 600 cycles at a 5 C (750 mA g -1 ) rate. The superior cycling performance of the cells can be attributed to the homogenous, dense, and thin hybrid solid electrolyte interphase consisting of F- and S-containing species on the surface of both the Na metal anode and the NaNMC cathode by adding dual additives. Such unique interphases can effectively facilitate Na-ion transport kinetics and avoid electrolyte depletion during repeated cycling at a very high rate of 5 C. This electrolyte design is believed to result in further improvements in the performance of SMBs.

25 ENERGY STORAGE↗