At least 613 records · Page 34

Rapid Adhesive Bonding of Composites

Strong bonds created in less time and with less power than use of conventional bonding methods. Rapid adhesive bonding (RAB) technique for composites uses high-frequency induction heating toroids to quickly heat metallic susceptor impregnated with thermoplastic adhesive or sandwiched between thermoset or thermoplastic adhesive cloths or films. Susceptor steel screen or perforated steel foil.

Stein, B. A.↗

Recent developments in polyimide and bismaleimide adhesives

Research on high temperature resin systems has intensified. In the Aerospace Industry, the motivation for this increased activity has been to replace heat resistant alloys of aluminum, stainless steel and titanium by lighter weight glass and carbon fiber reinforced composites. Applications for these structures include: (1) engine nacelles involving long time exposure (thousands of hours) to temperatures in the 150 to 300 C range, (2) supersonic military aircraft involving moderately long exposure (hundreds of hours) to temperatures of 150 to 200 C, and (3) missile applications involving only brief exposure (seconds or minutes) to temperatures up to 500 C and above. Because of fatigue considerations, whenever possible, it is preferable to bond rather than mechanically fasten composite structures. For this reason, the increased usage of high temperature resin matrix systems for composites has necessitated the devlopment of compatible and equally heat stable adhesive systems. The performance of high temperature epoxy, epoxy phenolic and condensation polyimide adhesives is reviewed. This is followed by a discussion of three recently developed types of adhesives: (1) condensation reaction polyimides having improved processing characteristics; (2) addition reaction polyimides; and (3) bismaleimides.

Politi, R. E.↗

Adhesive evaluation of thin films of LARC-TPI and LARC-TPI with 5 mol % ODA

A commercially available LARC-TPI film and an experimentally prepared film of LARC-TPI with 5 mol % of 4,4'-oxydianiline (ODA), designated as LARC-TPI/ODA in the report, supplied by Mitsui Toatsu Chemicals, Incorporated (MTCI), Japan, were evaluated as thermoplastic adhesive films for bonding Ti-6Al-4V. The LARC-TPI/ODA had been shown by MTCI to possess more flow than thermoplastic LARC-TPI and was, therefore, evaluated and compared to the LARC-TPI. Lap shear strength was used to evaluate the materials as adhesives. They were characterized after fracture by determining the glass transition temperature, Tg. The mode of failure was also reported. Thermal exposure at 204C for 500 and 1000 hrs and a 72-hour water-boil were conducted on lap shear specimens prepared with the two adhesive films. Lap shear tests were conducted at RT, 177C, 204C, and 232C before and after exposures.

Progar, D. J.↗

Evaluation of high temperature structural adhesives for extended service

The preliminary evaluation of crosslinked polyphenyl quinoxaline (X-PPQ), LARC-TPI, ethyl terminated polysulfone (ETPS), and crosslinked polyimide (X-PI) as adhesives is presented. Lap shear strength stability under thermal, combined thermal/humidity, and stressed and unstressed Skydrol exposure was determined. The X-PPQ, LARC-TPI, and X-PI exhibited good adhesive performance at 505K (450 F) after 1000 hours at 505K. These three polymers also performed well after exposure to combined elevated temperature/high humidity, as well as, to Skydrol while under stress. The ETPS exhibited good ambient temperature adhesive properties, but performed poorly under all other exposure conditions, presumably due to inadequate chain extension and crosslinking.

Hendricks, C. L.↗

Ceramic Adhesive for High Temperatures

Fused-silica/magnesium-phosphate adhesive resists high temperatures and vibrations. New adhesive unaffected by extreme temperatures and vibrations. Assuring direct bonding of gap filters to tile sidewalls, adhesive obviates expensive and time-consuming task of removal, treatment, and replacement of tiles.

Stevens, Everett G.↗

Adhesion, friction, and deformation of ion-beam-deposited boron nitride films

The tribological properties and mechanical strength of boron nitride films were investigated. The BN films were predominantly amorphous and nonstoichiometric and contained small amounts of oxides and carbides. It was found that the yield pressure at full plasticity, the critical load to fracture, and the shear strength of interfacial adhesive bonds (considered as adhesion) depended on the type of metallic substrate on which the BN was deposited. The harder the substrate, the greater the critical load and the adhesion. The yield pressures of the BN film were 12 GPa for the 440C stainless steel substrate, 4.1 GPa for the 304 stainless steel substrate, and 3.3 GPa for the titanium substrate.

Miyoshi, Kazuhisa↗

Adhesive evaluation of new polyimides

During the past 10 to 15 years, the Materials Division at NASA Langley Research Center (LaRC) has developed several novel high temperature polyimide adhesives for anticipated needs of the aerospace industry. These developments have resulted from fundamental studies of structure-property relationships in polyimides. Recent research at LaRC has involved the synthesis and evaluation of copolyimides which incorporate both flexibilizing bridging groups and meta-linked benzene rings. The purpose was to develop systems based on low cost, readily available monomers. Two of these copolyimides evaluated as adhesives for bonding titanium alloy, Ti(6Al-4V), are identified as LARC-STPI and STPI-LARC-2. Lap shear strength (LSS) measurements were used to determine the strength and durability of the adhesive materials. LSS results are presented for LARC-TPI and LARC-STPI lap shear specimens thermally exposed in air at 232 C for up to 5000 hrs. LARC-TPI was shown to perform better than the copolymer LARC-STPI which exhibited poor thermooxidative performance possibly due to the amines used which would tend to oxidize easier than the benzophenone system in LARC-TPI.

Stclair, Terry L.↗

Interfacial adhesion of carbon fibers

Relative adhesion strengths between AS4, AS1, and XAS carbon fibers and thermoplastic polymers were determined using the embedded single filament test. Polymers studied included polycarbonate, polyphenylene oxide, polyetherimide, polysulfone, polyphenylene oxide blends with polystyrene, and polycarbonate blends with a polycarbonate polysiloxane block copolymer. Fiber surface treatments and sizings improved adhesion somewhat, but adhesion remained well below levels obtained with epoxy matrices. An explanation for the differences between the Hercules and Grafil fibers was sought using X ray photon spectroscopy, wetting, scanning electron microscopy and thermal desorption analysis.

Bascom, Willard D.↗

The effects of molecular weight on the single lap shear creep and constant strain rate behavior of thermoplastic polyimidesulfone adhesive

The bonded shear creep and constant strain rate behaviors of zero, one, and three percent endcapped thermoplastic polyimidesulfone adhesive were examined at room and elevated temperatures. Endcapping was accomplished by the addition of phthalic anhydrides. The primary objective was to determine the effects of molecular weight on the mechanical properties of the adhesive. Viscoelastic and nonlinear elastic constitutive equations were utilized to model the adhesive. Ludwik's and Crochet's relations were used to describe the experimental failure data. The effects of molecular weight changes on the above mentioned mechanical behavior were assessed. The viscoelastic Chase-Goldsmith and elastic nonlinear relations gave a good fit to the experimental stress strain behavior. Crochet's relations based on Maxwell and Chase-Goldsmith models were fit to delayed failure data. Ludwik's equations revealed negligible rate dependence. Ultimate stress levels and the safe levels for creep stresses were found to decrease as molecular weight was reduced.

Dembosky, Stanley K.↗

Surface characterization in composite and titanium bonding: Carbon fiber surface treatments for improved adhesion to thermoplastic polymers

The effect of anodization in NaOH, H2SO4, and amine salts on the surface chemistry of carbon fibers was examined by X-ray photoelectron spectroscopy (XPS). The surfaces of carbon fibers after anodization in NaOH and H2SO4 were examined by scanning transmission electron microscopy (STEM), angular dependent XPS, UV absorption spectroscopy of the anodization bath, secondary ion mass spectrometry, and polar/dispersive surface energy analysis. Hercules AS-4, Dexter Hysol XAS, and Union Carbide T-300 fibers were examined by STEM, angular dependent XPS, and breaking strength measurement before and after commercial surface treatment. Oxygen and nitrogen were added to the fiber surfaces by anodization in amine salts. Analysis of the plasmon peak in the carbon 1s signal indicated that H2SO4 anodization affected the morphological structure of the carbon fiber surface. The work of adhesion of carbon fibers to thermoplastic resins was calculated using the geometric mean relationship. A correlation was observed between the dispersive component of the work of adhesion and the interfacial adhesion.

Devilbiss, T. A.↗

Nondestructive evaluation of adhesive bond strength using the stress wave factor technique

Acousto-ultrasonic nondestructive evaluation has been conducted to evaluate the adhesive bond strength between rubber and steel plates using the stress wave factor (SWF) measurement technique. Specimens with different bond strength were manufactured and tested using the SWF technique. Two approaches were used to define the SWF. One approach defines the SWF as the signal energy and the other approach defines the SWF as the square root of the zero moment of the frequency spectrum of the received signal. The strength of the rubber-steel adhesive joint was then evaluated using the destructive peel strength test method. It was observed that in both approaches higher values of the SWF measurements correspond to higher values of the peel strength test data. Therefore, these results show that the stress wave factor technique has the potential of being used in quality assurance of the adhesive bond strength between rubber and steel substrates.

Dos Reis, Henrique L. M.↗

Adhesion, friction and deformation of ion-beam-deposited boron nitride films

The tribological properties and mechanical strength of boron nitride films were investigated. The BN films were predominantly amorphous and nonstoichiometric and contained small amounts of oxides and carbides. It was found that the yield pressure at full plasticity, the critical load to fracture, and the shear strength of interfacial adhesive bonds (considered as adhesion) depended on the type of metallic substrate on which the BN was deposited. The harder the substrate, the greater the critical load and the adhesion. The yield pressures of the BN film were 12 GPa for the 440C stainless steel substrate, 4.1 GPa for the 304 stainless steel substrate, and 3.3 GPa for the titanium substrate.

Miyoshi, K.↗

Interfacial adhesion: Theory and experiment

Adhesion, the binding of different materials at an interface, is of general interest to many branches of technology, e.g., microelectronics, tribology, manufacturing, construction, etc. However, there is a lack of fundamental understanding of such diverse interfaces. In addition, experimental techniques generally have practical objectives, such as the achievement of sufficient strength to sustain mechanical or thermal effects and/or have the proper electronic properties. In addition, the theoretical description of binding at interfaces is quite limited, and a proper data base for such theoretical analysis does not exist. This presentation will review both experimental and theoretical aspects of adhesion in nonpolymer materials. The objective will be to delineate the critical parameters needed, governing adhesion testing along with an outline of testing objectives. A distinction will be made between practical and fundamental objectives. Examples are given where interfacial bonding may govern experimental consideration. The present status of theory is presented along wiith recommendations for future progress and needs.

Ferrante, John↗

Initial adhesive screening of novel polyamide-imides and their copolymers

Continued interest by the research community in thermally stable, tough, high temperature adhesives has resulted in the investigation by Langley Research Center of two linear aromatic polyamide-imide (PAI) homopolymers and two linear aromatic PAI copolymers. The homopolymers were made with either 3,3'=DABA or 4,4'-DABA and BTDA. The two polymers were prepared with a monomer ratio of 0.75 DABP:0.25 DABA:1.00 BTDA. These aromatic PAIs possess high thermal stability because of intermolecular hydrogen bonding and chain stiffness. Lap shear strength (LSS) was the main criteria used to evaluate the polymers as adhesives. LSS of bonded Ti-6Al-4V was determined at room temperature (RT), 177, 204 and 232 C. The glass transition temperature and the type of bond failure were also determined. The best LSS values of the four adhesive systems investigated were obtained with the PAI copolymer identified in the report as LARC-TPI (25 percent 3,3'-DABA); however, it did not produce LSSs nearly as high as LARC-TPI. The poor flow properties observed appear to be due to a combination of high molecular weight and the increased interchain electronic interactions associated with the amide group.

Donald J Progar↗

Reducing adhesion and agglomeration within a cloud of combustible particles

The study of combustible particle clouds inside flame tubes is of fundamental scientific interest as well as a practical concern. Only the suspended concentration is important to the combustion process, so that assurances must be provided that a minimum of particles adheres to the tube wall. This paper demonstrates experimentally the ability to minimize adhesion and agglomeration of acoustically-mixed lycopodium particles within a 5-cm diameter lexan flame tube. The area density of particles (ADP) adhering to the wall of bare lexan tubes was measured at greater than 100 particles/sq mm. The nature of adhesion was found to be clearly electrostatic, with the ADP level aggravated by increased mixing time, vigor, and the concentration of particles. Increases in the conductivity of the air and the tube wall did not affect ADP levels substantially. However, the observed adhesion was reduced to less than 10 p/sq mm when the air was ionized by use of an alpha emitter mounted on the inner walls of the flame tube.

Ross, Howard D.↗

Evaluation of polyimide films as adhesives

A commercially available LARC-TPI film and an experimentally prepared film of LARC-TPI with 5 mol pct of 4,4-prime-oxydianiline (ODA), designated as LARC-TPI/ODA, were evaluated as thermoplastic adhesive films for bonding Ti-6Al-4V. Lap shear strength was used to evaluate the materials as adhesives. They were characterized after fracture by determining the glass transition temperature, T(g). The mode of failure is also reported. Thermal exposure at 240 C for 500 and 1000 h and a 72-h water-boil were conducted on lap shear specimens prepared with the two adhesive films. Lap shear tests were conducted at room temperature, 177 C, 204 C, and 232 C before and after exposures.

Progar, Donald J.↗

Effect of adhesive interleaving and discontinuous plies on failure of composite laminates subject to transverse normal loads

Results of a series of tests to determine the effects of adhesive interleaving and discontinuous plies (plies with end-to-end gaps) on the displacements, failure loads and failure modes of graphite-epoxy laminates subjected to transverse normal loads are presented. Adhesive interleaving can be used to contain local damage within a group of plies, i.e., to arrest crack propagation on the interlaminate level, and it can increase the amount of normal displacement the laminate can withstand before failure. However, the addition of adhesive interleaving to a laminate does not significantly increase its load carrying capability. A few discontinuous plies in a laminate can reduce the normal displacement and load at failure by 10 to 40 percent compared to a laminate with no discontinuous plies, but the presence of the ply discontinuities does not generally change the failure location or the failure mode of the laminate.

Jegley, Dawn C.↗