Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile Strain”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

611 records · Page 34

Utilizing integrated neutron diffraction and elastoplastic self-consistent crystal plasticity model to quantitatively assess the strengthening mechanism in Al–12.5Ce and Al–12.5Ce–0.4Mg alloys

An integrated in-situ neutron diffraction and elastic plastic self-consistent crystal plasticity (EPSC-CP) modeling scheme is performed on a binary Al–12Ce alloy and a ternary Al–12Ce–0.4Mg alloys. Using this scheme, the constitutive parameters, i.e. elastic constants and slip system parameters of individual phases can be calibrated which can be used in microstructure-based CP models to predict materials performance. From this study, it is shown that the elastic constants of Al 11 Ce 3 intermetallics calculated from density function theory calculation in the literature are rather accurate. When applied to the EPSC-CP model, the lattice strains of both the binary and ternary alloys are correctly predicted as compared with experiments, and large lattice strain differences between Al (100) plane and Al 11 Ce 3 (010) plane are demonstrated. The slip system parameters calibrated by the scheme shows that the addition of 0.4 wt% Mg in the alloy has little influence on the critical resolved shear stress of initial dislocation glide in the Al matrix which caused plastic yield in the material. This can be explained by the very dilute Mg solute content in the Al solid solution, causing large spacing of Al–Mg lattice misfit sites and little impact on resistance of dislocation glide at initial yield. The 0.4 wt% Mg addition, on the other hand, has a large influence on the hardening term in the slip system parameters, indicating those Al–Mg misfit sites do help dislocation accumulation during the deformation. The impact of dilute Mg addition on the Al slip system parameters is also reflected in the flow behavior of the ternary alloy: little impact on the yield stress, but a large impact on working hardening and tensile strength of the materials which is consistent with the literature.

36 MATERIALS SCIENCE↗

Effect of laminae count and manufacturing methods on mechanical properties of thin‐ply woven composites

Abstract Thin‐ply woven composites exhibit exceptional mechanical performance by delaying the onset of damage, making them suitable for high‐performance structural applications. This study outlines the impact of manufacturing techniques (vacuum bagging and hot pressing), ply count, and fiber waviness on the mechanical properties of aromatic thermosetting copolyester/carbon‐fiber (ATSP/CF) composites. The analysis encompasses several different ply counts, evaluating their effects on the in‐plane elastic modulus (0°–90°) and tensile strength. Results demonstrate that reducing the waviness (or crimp) ratio significantly enhances the in‐plane elastic modulus, with improvements up to 188%, highlighting the importance of fiber alignment. Vacuum bagging produced ply thicknesses from 128 to 58 μm for 1–36 plies, with in‐plane elastic moduli from 30.3 to 87.2 GPa, and 4‐ and 8‐ply samples showed approximately 40% higher stiffness than those made by hot pressing. ATSP resin with high thermal stability (up to 400°C) and recyclability was used. Furthermore, this study highlights the microstructural enhancements achieved through vacuum bagging, as revealed by scanning electron and optical microscopy, and micro‐computed tomography imaging. This paper provides insights into damage mitigation and achieving enhanced mechanical properties by controlling fiber waviness using vacuum bagging and higher ply count in thin‐ply ATSP/CF composites. Highlights Crimp ratio reduction enhances elastic in‐plane elastic modulus up to 188%. Vacuum bagging increases modulus over the hot pressing manufacturing method by 40%. Lowering thickness‐per‐ply increases failure strain from 0.8% to 1.2%. Explored the performance of a novel ATSP matrix with high recyclability and thermal stability.

Kushwaha, Shashank [The Grainger College of Engine↗

Synthesis and characterization of biobased copolyesters based on pentanediol: (1) Poly(pentylene dodecanoate–co–furandicarboxylate)

A series of biobased aliphatic-aromatic copolyesters, poly(pentylene dodecanoate-co-furandicarboxylates) (PPeDFs) were synthesized via an esterification and polycondensation melt process. The copolyesters were characterized using gel permeation chromatography, Fourier transform infrared spectroscopy, 1 H NMR spectroscopy, differential scanning calorimetry, thermogravimetric analysis, wide angle x-ray scattering, and tensile testing. The thermal transition behavior was strongly dependent on composition, with the melting and glass transition temperatures reaching a minimum at approximately equimolar ratio of D to F. All copolyesters were stable below 300°C with their R 600 (the weight of material remaining at 600°C) values increasing with F fraction. PPeD to PPeDF30 (e.g., mole ratio D/F = 7:3) show sharp PPeD crystalline reflections only while broad PPeF reflections are shown in PPeF and PPeDF90. PPeDF40 to PPeDF80 showed both crystal structures. The fractional crystallinity for the PPeD was much higher than PPeF and the fractional crystallinity of the copolymers showed a minimum at D/F ratios closer to the latter. Here, the stress at break and modulus both exhibited maxima at D/F ratios that were either high or low, but somewhat surprisingly a strong maximum in percent elongation at break of over 600% occurs at PPeDF40. For this composition, a typical plastic behavior curve was found including a yield point, high elongation at break, and strain hardening.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Robust Dissimilar Metal Friction Welded Spool for Enhanced Capability for Steam Power Components (Final Program Report)

This project successfully demonstrated the feasibility and advantages of producing durable, friction-welded dissimilar-metal spools, both with and without transition pieces, as well as the use of advanced oxidation-protective coatings for steam power applications. The work encompassed the optimization and full-scale production of NFA tubing, overcoming manufacturing and processing challenges to achieve enhanced strength, creep, and fatigue properties validated by extensive microstructural characterization. Optimized welding techniques were developed and refined for joining dissimilar materials, resulting in defect-free welds optimized for both low- and high-pressure boiler circuits. Systematic evaluation of welding parameters, coupled with heat treatments, ensured reliable performance and minimized weld defects such as banding and cracking. Comprehensive mechanical and non-destructive testing, including tensile, bend, fatigue, and CT scanning, confirmed the superior integrity and durability of the friction-welded joints under representative service conditions. To address oxidation-related degradation, a range of protective alloy coatings—such as IN625, APMT, Duplex 2507, and FeCrAlY—were selected and evaluated for their ability to counteract oxide notch formation at dissimilar metal interfaces. These coatings demonstrated improved oxidation resistance and long-term stability under thermal cycling, thereby extending weld service life. Thermal cyclic testing and long-term studies captured the phase stability and diffusion behavior of coated and uncoated configurations. Validated models for low-cycle fatigue (LCF), creep, and thermal mechanical fatigue (TMF) were developed to predict component life and failure modes. These models confirmed that friction-welded configurations exhibited significantly enhanced performance compared to conventional gas-tungsten arc welding (GTAW), with up to 7× improvement in creep resistance and at least 2× enhancement in fatigue properties. The introduction of a tailored transition piece further reduced thermally induced strains, enhancing fatigue life. The results demonstrate a robust pathway for retrofitting existing steam fleet components and upgrading future equipment to deliver substantially improved cold-start cycling behavior and reduction of unplanned outages due to premature weld failures.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Design of a V–Ti–Ni alloy with superelastic nano-precipitates

Stress-induced martensitic transformations enable metastable alloys to exhibit enhanced strain hardening capacity, leading to improved formability and toughness. As is well-known from transformation-induced plasticity (TRIP) steels, however, the resulting martensite can limit ductility and fatigue life due to its intrinsic brittleness. In this work, we explore an alloy design strategy that utilizes stress-induced martensitic transformations but does not retain the martensite phase. This strategy is based on the introduction of superelastic nano-precipitates, which exhibit reverse transformation after initial stress-induced forward transformation. To this end, utilizing ab-initio simulations and thermodynamic calculations we designed and produced a V 45 Ti 30 Ni 25 (at%) alloy. In this alloy, TiNi is present as nano-precipitates uniformly distributed within a ductile V-rich base-centered cubic (bcc) β matrix, as well as being present as a larger matrix phase. We characterized the microstructure of the produced alloy using various scanning electron microscopy (SEM) and transmission electron microscopy (TEM) methods. Furthermore, the bulk mechanical properties of the alloy are demonstrated through tensile tests, and the reversible transformation in each of the TiNi morphologies were confirmed by in-situ TEM micro-pillar compression experiments, in-situ high-energy diffraction synchrotron cyclic tensile tests, indentation experiments, and differential scanning calorimetry experiments. The observed transformation pathways and variables impacting phase stability are critically discussed.

59 BASIC BIOLOGICAL SCIENCES↗

Correlating dislocation structures to basal and prismatic slip bands near grain boundaries in tensile-tested Mg–4Al using a multiscale electron microscopy approach

Dislocation structures where basal and prismatic slip bands meet grain boundaries in tensile-tested Mg with 4 wt% Al (Mg–4Al) were studied using a multiscale electron microscopy approach to explore the assumptions made for the dislocation pileup theory: a) slip bands consist of dislocation arrays piling up near grain boundaries, and b) stress concentration in the adjacent grain is solely caused by dislocation pileup. After post-testing electron backscatter diffraction (EBSD) scans, focused-ion-beam (FIB) lift-out specimens were prepared from regions of interest so that the specimen plane is parallel to the bulk sample surface to allow for direct correlation between mesoscale and microscale characterization. High dislocation density and the dislocation arrays in the slip bands corroborated with the first assumption. Evidence of plastic deformation in all grains, however, showed that the second assumption was false. Additionally, dislocation structures including crystal rotation boundaries and dislocations dissociating to the basal plane provide additional stress relief mechanisms near grain boundaries that are not accounted for in many crystal plasticity models, which requires auxiliary models to more accurately predict the stress and strain distribution in a microstructure.

36 MATERIALS SCIENCE↗

Experimental investigation of the dependence of void nucleation and growth on initial microstructure in high-purity titanium under tension

An experimental investigation of failure mechanisms in relation to the initial microstructure in high-purity titanium samples is presented. The initial microstructure of the specimens was measured in 3D using diffraction-contrast tomography (DCT). Ex-situ X-ray computed tomography (XCT) was used to visualize voids in specimens at various levels of deformation attained by interrupted tensile testing. Electron backscatter diffraction (EBSD) mapping was used to characterize the deformed microstructures per specimen. The investigation showed that the location of failures was unrelated to the formation of the first voids, but rather the nucleation and growth of cracks were from heavily deformed surface regions. The areas surrounding the failure-causing cracks had the highest propensity for void development of any area in the specimen. This facilitated crack propagation through the specimen via “linking up”. The failure of the specimens by microvoid coalescence was bolstered by “dimpled” fracture surfaces. Paint composed of gallium embedded in rubber was used to track the displacement of points along the loading direction of the specimens, to relate the location of failure to the material's initial microstructure. However, the correlation proved difficult, due to complex microstructural evolution involving voids, grain fragmentations, and profuse twinning. Nevertheless, it was shown that necking occurred near the largest grain in the gauge section of the specimens. This is likely caused by the decrease in strength of larger grains, causing strain to concentrate in their vicinity. Here, a comprehensive picture of the failure processes in high-purity titanium under axial loading is presented and discussed in the paper.

36 MATERIALS SCIENCE↗

A study on texture stability and the biaxial creep behavior of as-hydrided CWSR Zircaloy-4 cladding at the effective stresses from 55 MPa to 65 MPa and temperatures from 300°C to 400°C

The creep rupture of high burnup used nuclear fuel (> 45 GWD/MTU) cladding is regarded as one of the failure mechanisms during long-term dry storage. A high amount of zirconium hydride in the cladding matrix would degrade the mechanical properties of the cladding especially leading to delayed hydride cracking. To better understand the influence of zirconium hydride on the biaxial thermal creep performance and the crystalline texture stability of Zircaloy-4 cladding, the pressurized tube technique is applied to test the durability of the as-hydrided material. Tests were performed on as-received Zircaloy-4 tubular specimens as well as-hydrided ones with targeted 300 wt parts per million (wppm) or 750 wppm hydrogen. The biaxial creep experiments were conducted at temperatures from 300 degrees C to 400 degrees C and at equivalent stresses at mid-wall from 55 MPa to 65 MPa. The hydridation process prior to creep tests induces the formation of FCC delta-hydride platelets along the circumferential direction of the tube. This alignment and phase structure of hydride show no significant change after biaxial creep tests. The creep strain-rate negatively depends on the hydrogen content. The synchrotron wide-angle X-ray diffraction (WAXD) technique and electron backscatter diffraction (EBSD) analysis were applied for the study of the crystallographic orientation relationship. zirconium-to-hydride grain orientation follows Shoji-Nishiyama crystallographic relationship. This relationship is stable before and after creep deformation. These results of creep performance and texture stability of Zircaloy-4 claddings can help support the design basis of interim and long-term dry storage facilities.

creep↗

Nanoscale structural evolution and phase transformation of geopolymers: In situ SAXS/WAXS investigation under uniaxial tension at elevated temperatures

This investigation delves into the degradation mechanisms of high-density polyethylene geomembranes (PE GMXs) under a spectrum of conditions, replicating real-world scenarios within a rigorously controlled laboratory setting. The treatment protocols applied induced a notable increase in the crystallinity of the treated specimens relative to the untreated controls. Small-angle x-ray scattering (SAXS) analysis identified an initial long period (interlamellar distance) of 16.9 nm for the untreated polymer, which expanded by 19.5% at a strain of 16.7 percent. Conversely, the treated PE GMXs exhibited a more gradual elongation of the long period, with an increase of merely 10.6% at a strain of 23.3 percent. At an elevated temperature of 65°C, both samples exhibited pronounced strain hardening, with the treated PE GMXs demonstrating superior stability even at a strain of 150 percent. Wide-angle x-ray scattering (WAXS) experiments corroborated these observations, revealing that the diffraction patterns of the untreated PE remained stable up to a strain of 16.7%, whereas those of the treated PE remained distinct up to a strain of 46.1 percent. Scanning electron microscopy (SEM) images substantiated the formation of a shish–kebab structure in the treated samples. The study concludes that the geopolymer underwent oxidation and material degradation as a result of the chemical and mechanical treatments, transitioning to a more crystalline state and concomitantly losing its initial elasticity.

36 MATERIALS SCIENCE↗

Imaging Bragg Edge Analysis TooLs for Engineering Structures (iBeatles)

The Spallation Neutron Source (SNS) at Oak Ridge National Laboratory (ORNL) provides pulsed neutrons with energies varying from epithermal to cold. In preparation for VENUS, the neutron imaging beamline to be located at beam port 10, we have performed a series of experiments focused on wavelength-dependent radiography and computed tomography for a broad range of applications, from materials science to biological tissues.One of the time-of-flight (TOF) techniques that is of interest to the scientific community is the 2-dimensional mapping of phases and average crystalline plane orientation in samples both ex-situ and during applied stresses such as tensile loading and heating. This technique is known as Bragg edgeimaging and relies on the identification of changes of transmission values, fitting of the edge to measure its displacement, and thus identify the shift in lattice parameter due to stresses. One of the challenges of TOF imaging measurements is the amount of data and the inability to observe Bragg edge shifts in real time during an experiment. Thus, we have been focusing on creating a Python-based interface that allows fast data processing and instantaneous mapping and fitting of the Bragg edges, and their evolution through time. Python libraries and Jupyter notebooks have been implemented to facilitate decision making during an experiment. The advantage of the notebooks is the possibility to guide an experiment as they can quickly process and display Bragg edge data. These notebooks can be used independently, or can be combined in a Python Graphical User Interface (GUI) tool called iBeatles. This interface permits visualization and fitting of the Bragg edges, and ultimately back-projects the fitting results onto the radiographs to display a strain map. Assuming data collection has sufficient statistics, the strain mapping analysis can be performed on a pixel-by-pixel basis. This development is a step forward toward a better user experience at the future VENUS beamline in terms of live feedback and productivity. Analysis that used to take days of switching between different applications can now be done in minutes within the

Bilheux, JeanChristophe [Oak Ridge National Labora↗

Exceptional fracture toughness of CrCoNi-based medium- and high-entropy alloys at 20 kelvin

Medium- and high-entropy alloys based on the CrCoNi-system have been shown to display outstanding strength, tensile ductility and fracture toughness (damage-tolerance properties), especially at cryogenic temperatures. Here we examine the J Ic and (back-calculated) K JIc fracture toughness values of the face-centered cubic, equiatomic CrCoNi and CrMnFeCoNi alloys at 20 K. At flow stress values of ~1.5 GPa, crack-initiation K JIc toughnesses were found to be exceptionally high, respectively 235 and 415 MPa√m for CrMnFeCoNi and CrCoNi, with the latter displaying a crack-growth toughness K ss exceeding 540 MPa√m after 2.25 mm of stable cracking, which to our knowledge is the highest such value ever reported. Characterization of the crack-tip regions in CrCoNi by scanning electron and transmission electron microscopy reveal deformation structures at 20 K that are quite distinct from those at higher temperatures and involve heterogeneous nucleation, but restricted growth, of stacking faults and fine nanotwins, together with transformation to the hexagonal closed-packed phase. The coherent interfaces of these features can promote both the arrest and transmission of dislocations to generate respectively strength and ductility which strongly contributes to sustained strain hardening. Indeed, we believe that these nominally single-phase, concentrated solid-solution alloys develop their fracture resistance through a progressive synergy of deformation mechanisms, including dislocation glide, stacking-fault formation, nano-twinning and eventually in situ phase transformation, all of which serve to extend continuous strain hardening which simultaneously elevates strength and ductility (by delaying plastic instability), leading to truly exceptional resistance to fracture.

36 MATERIALS SCIENCE↗

Revealing Deformation Mechanisms in Polymer-Grafted Thermoplastic Elastomers via In Situ Small-Angle X-ray Scattering

The tunable properties of thermoplastic elastomers (TPEs), through polymer chemistry manipulations, enable these technologically critical materials to be employed in a broad range of applications. The need to “dial-in” the mechanical properties and responses of TPEs generally requires the design and synthesis of new macromolecules. In these designs, TPEs with nonlinear macromolecular architectures outperform the mechanical properties of their linear copolymer counterparts, but the differences in the deformation mechanism providing enhanced performance are unknown. Here, in situ small-angle X-ray scattering (SAXS) measurements during uniaxial extension reveal distinct deformation mechanisms between a commercially available linear poly(styrene)–poly(butadiene)–poly(styrene) (SBS) triblock copolymer and the grafted SBS version containing grafted poly(styrene) (PS) chains from the poly(butadiene) (PBD) midblock. The neat SBS (φ SBS = 100%) sample deforms congruently with the macroscopic dimensions, with the domain spacing between spheres increasing and decreasing along and transverse to the stretch direction, respectively. At high extensions, end segment pullout from the PS-rich domains is detected, which is indicated by a disordering of SBS. Conversely, the PS-grafted SBS that is 30 vol % SBS and 70% styrene (φ SBS = 30%) exhibits a lamellar morphology, and in situ SAXS measurements reveal an unexpected deformation mechanism. During deformation, there are two simultaneous processes: significant lamellar domain rearrangement to preferentially orient the lamellae planes parallel to the stretch direction and crazing. The samples whiten at high strains as expected for crazing, which corresponds with the emergence of features in the 2D SAXS pattern during stretching consistent with fibril-like structures that bridge the voids in crazes. The significant domain rearrangement in the grafted copolymers is attributed to the new junctions formed across multiple PS domains by the grafting of a single chain. In conclusion, the in situ SAXS measurements provide insights into the enhanced mechanical properties of grafted copolymers that arise through improved physical cross-linking that leads to nanostructure domain reorientation for self-reinforcement and craze formation where fibrils help to strengthen the polymer.

36 MATERIALS SCIENCE↗

Hydrogen-Aided Microstructural Engineering of Additively Manufactured Ti–6Al–4V

Electron beam melting (EBM) additive manufacturing of Ti–6Al–4V subjects the material to complex thermal cycles, resulting in a columnar morphology of the prior β grains (PBGs). While the columnar PBGs of EBM-processed Ti–6Al–4V can be transformed to an equiaxed morphology through a super-transus (i.e., above the β -transus temperature) heat treatment, this also leads to the formation of a coarse lamellar two-phase microstructure. Such a microstructure is prone to strain localization and premature fracture. In this study, we present a thermohydrogen post-process treatment that achieves equiaxed PBG morphology in EBM-processed Ti–6Al–4V without sacrificing mechanical properties. Our results show that a three-step thermohydrogen post-process treatment can transform the columnar PBG morphology to an equiaxed morphology with fine microstructure, and strength and ductility levels comparable to those of the most optimum as-fabricated samples. This three-step thermohydrogen post-process treatment involves hydrogenation and phase transformation treatment in a hydrogen atmosphere, and subsequent dehydrogenation treatment in vacuum. Notably, all these treatments are carried out at temperatures well below the β -transus temperature of hydrogen-free Ti–6Al–4V.

36 MATERIALS SCIENCE↗

Thermal shock resistance of lightweight cements developed for geothermal conditions

Cements are a critical component in well construction, as they act to prevent well fluid and gas escape, prevent corrosion of the casing, and strengthen the wellbore to prevent deformation. Under the high temperature/pressure conditions common in geothermal systems, the injection of cold water for energy production is expected to induce cyclic damage to the borehole cement through the rapid temperature fluctuations. These “thermal shocks” are expected to cause casing shrinkage, annulus formation, and cement tensile stresses. To understand the effect of cold water injection on the wellbore environment, a set of rock-cement-steel samples were created to simulate the structure of a geothermal well. Lightweight thermally-insulating cement blends were tested under thermal shock conditions in this study. In each test, the samples were pressurized to an effective pressure of ~3.5 MPa and placed at high temperatures. Thermal shocks were performed by injecting cold water (~10-15 °C) through the samples at a constant rate while keeping the samples at high temperatures until the sample temperature stopped decreasing and deformation ceased. Eight thermal shock tests were conducted with each sample – two at 100 °C and six at 200 °C. Post-tests analysis was then conducted by cutting open each sample to examine the damage in each component of the simulated wellbore. Experimental results suggest that all samples experienced similar degrees of axial and lateral contraction during cold water injection, but for the most part this contraction is recoverable when injection halts. Post-test analysis revealed that fly ash cenosphere pre-treatment had the best effect on improving thermal shock resistance in the cement blends. Thermomechanical modeling of likely stress paths experienced by the cements during heating/cooling cycles shows that elasto-plastic cement constitutive behavior results in most plastic strain occurring during the initial heating steps, with mostly elastic strain occurring during the thermal shock cycles. In conclusion, this agrees with experimental evidence, suggesting that cement damage from shocking occurs via other mechanisms such as chemical alteration, corrosion, and fatigue.

36 MATERIALS SCIENCE↗

Grain boundary slip – twin transmission in titanium

Here, using a combination of mechanical testing, scanning electron microscopy, and a unified crystal plasticity framework for discrete intragranular shear localization, we investigate intense, localized slip bands on prismatic planes and {10$\bar{1}$2} $\langle$$\bar{1}$011$\rangle$ tensile twins, and their transmission across the grain boundaries (GBs) in commercially pure titanium. The analyses show that the orientation and curvature of the GB influence the local stress fields at the GBs, and consequently, the slip/twin transmission across the boundary. In addition to host grain properties, neighboring grain properties, such as active slip systems and instances of heterogeneity like slip bands and twins, heavily affect the deformation mechanisms in each grain. Finally, the applicability of geometric factors to predict the transmission in the experimentally observed co-located pairs is discussed. The local stress field calculated by the discrete slip and twin band model is shown to be capable of determining whether a transmission has occurred in an observed co-located pair, and also the direction of the transmission.

36 MATERIALS SCIENCE↗

Mechanical properties, strain hardening, and fracture behavior of ultrasonic additively manufactured Zircaloy-4 after low-temperature neutron irradiation

Ultrasonic additive manufacturing (UAM) is a solid-state, layer-by-layer advanced manufacturing process that has the potential to create custom spatially controlled composites with embedded wires and sensors for nuclear component manufacture. For this work, to assess the feasibility of using UAM for nuclear-relevant materials research, the technique was used to produce a 3.5-mm-thick Zircaloy-4 plate for irradiation testing. The UAM Zircaloy-4 specimens were irradiated in the High Flux Isotope Reactor at a target irradiation temperature of 117 °C to 2.9 displacements per atom (dpa) to assess differences in irradiation-hardening behavior as a function of alloy processing path. The UAM and reference baseplate (BP) materials increased in yield strength by 372±27 MPa and 346±21 MPa, respectively, and both suffered significant reductions in uniform and total elongation attributed to irradiation hardening at low-temperature. Although the materials had similar nanoscale defect structures, including nanoscale black dot/loop features and strain-induced dislocation channels, the UAM material’s processing-related defects resulted in accelerated strain localization and failure as demonstrated by lower post-irradiation uniform elongation of UAM specimens (0.5 %) compared to BP (1.5 %) material. The UAM material also showed considerable anisotropy in mechanical response due to crack propagation along weld boundaries, resulting in differences in strength & ductility when tested parallel and perpendicular to the prior UAM build orientation. Therefore, although the fundamental irradiation response of UAM-processed Zircaloy-4 was phenomenologically comparable to that of BP reference material, additional optimization of the UAM processing is needed to produce irradiation-resistant and nuclear-relevant materials.

Digital image correlation↗

High tensile alloy of copper to mitigate current collector deformation in silicon electrodes for lithium-ion batteries

The volumetric changes of silicon electrodes, along with the strong adhesive properties of certain binders, can lead to plastic deformation of the current collector and create damage in the electrode coating. Here, in this study, we report a detailed study of silicon coatings on a high-tensile alloy (HTA) foil of copper with strength over twice that of conventional copper foils. The HTA current collectors with high mechanical strength can mitigate plastic deformation upon continuous cycling. At moderate areal capacities (2.5–3 mAh cm −2 ), conventional copper foils show significant wrinkling after only a few electrochemical cycles, whereas the HTA foils remain intact. We demonstrate viability of the HTA foils in large format xx6395 pouch cells, in which the HTA current collectors remain intact even at an areal capacity of 4.5 mAh cm −2 ; in contrast, wrinkles form in conventional copper current collectors increasing the likelihood of lithium plating. Computational studies show that stresses generated during cycling of silicon electrodes are very high in the current collector and at the current collector-coating interface, explaining the wrinkling of conventional Cu foils. Our studies highlight importance of current collector to solve the electrochemical and chemo-mechanical performance challenges associated with high-loading silicon electrodes.

Chemo-mechanical degradation↗