Positive Charge in SOS Heterostructures with Interlayer Silicon Oxide
The continuous transfer of (001)Si layers 0.2–1.7 μm thick by implanted hydrogen to the c-sapphire surface during direct bonding at high temperatures of 300–500°C is demonstrated for the first time. The formation of an intermediate silicon-oxide layer SiO{sub x} during subsequent heat treatments at 800–1100°C, whose increase in thickness (up to 3 nm) correlates with an increase in the positive charge Q{sub i} at the heterointerface to ~1.5 × 10{sup 12} cm{sup –2} in contrast to the negative charge at the SiO{sub x}/Al{sub 2}O{sub 3} ALD heterointerface. During silicon-layer transfer to sapphire with a thermal silicon-dioxide layer, Q{sub i} decreases by more than an order of magnitude to 5 × 10{sup 10} cm{sup –2} with an increase in the SiO{sub 2} thickness from 50 to 400 nm, while the electron and hole mobilities barely differ from the values in bulk silicon. Based on these results, a qualitative model of the formation of positively charged oxygen vacancies in a 5-nm sapphire layer near the bonding interface is proposed.