Tantalum strength at extreme strain rates from impact-driven Richtmyer-Meshkov instabilities
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
In this paper, we present results from an experimental technique used to estimate the strength of Ta at extreme pressures (150 GPa) and strain rates (10 7 s -1 ). A graded-density impactor (GDI) was fabricated using sputter deposition to produce an approximately 40-μm-thick film containing alternating layers of Al and Cu. The thicknesses of the respective layers are adjusted to give an effective density gradient through the film. The GDIs were launched with a 2-stage light gas gun, and shock-ramp-release velocity profiles were measured over timescales of ~10 ns. Results are presented for the direct impact of the film onto LiF windows, which allows for a dynamic characterization of the GDI, as well as from impact onto thin (~40μm) sputtered Ta samples backed by a LiF window. The measurements were coupled with mesoscale numerical simulations to infer the strength of Ta, and the results agree well with other high-pressure platforms, particularly when strain-rate, microstructural, and thermodynamic-path differences are considered.
Here, this paper presents a comprehensive review of existing research examining the effects of supplementary cementitious materials on age-dependent concrete properties with the most profound implications for precast concrete production. The review covers the physical and chemical properties of selected types of supplementary cementitious materials, concrete mixture proportions, concrete curing methods, testing procedures, and test results related to the fresh properties and strengths of a range of concrete mixtures. Although the use of supplementary cementitious materials in precast concrete products is common, the detailed information provided in this paper may facilitate more widespread use of these materials to enhance concrete properties and comply with sustainability initiatives.
Diamond is used extensively as a component in high-energy-density experiments, but existing equation of state (EOS) models do not capture its observed response to dynamic loading. In particular, in contrast with first-principles theoretical models of equilibrium multiphase EOS, no solid-solid phase changes have been detected, and no general-purpose EOS models match the measured ambient isotherm. We have performed density functional theory (DFT) calculations of the diamond phase to ~10 TPa, well beyond its predicted range of thermodynamic stability, and used these results as the basis of a Mie-Grüneisen EOS. We also performed DFT calculations of the elastic moduli, and calibrated an algebraic elasticity model for use in simulations. We then estimated the flow stress of diamond by comparison with the stress-density relation measured experimentally in ramp-loading experiments. Furthermore, the resulting constitutive model allows us to place a constraint on the Taylor-Quinney factor (the fraction of plastic work converted to heat) from the observation that diamond does not melt on ramp compression.
The internal architecture of an AlSi12CuMgNi piston alloy, revealed by synchrotron tomography, consists of three dimensional interconnected hybrid networks of Cu-rich aluminides, Mg-rich aluminides and eutectic/primary Si embedded in an α-Al matrix. The strength at room temperature and at 300°C is studied as a function of solution treatment time at 490°C and compared with results previously reported for an AlSi12Ni alloy. The addition of 1 wt% Cu and 1 wt% Mg to AlSi12CuMgNi increases the room temperature strength by precipitation hardening while the strength at 300°C is similar for both alloys in as-cast condition. The strength of AlSi12CuMgNi decreases with solution treatment time and stabilizes at 4 h solution treatment. The effect of solution treatment time on the strength of the AlSi12CuMgNi alloy is less pronounced than for the AlSi12Ni alloy both at room temperature and at 300°C. - Highlights: • The 3D microstructure of AlSi12CuMgNi is revealed by synchrotron tomography. • An imaging analysis procedure to segment phases with similar contrasts is presented. • 1 wt% Cu and Mg results in the formation of 3D networks of rigid phases. • AlSi12CuMgNi is stronger than AlSi12Ni owing to the stability of the 3D networks.
This work reports two independent experimental estimations of the dynamic strength of the body-centered tetragonal (bct) 𝛾 phase of tin, which occurs at pressures above about 9 GPa and transforms promptly back to the ambient 𝛽 phase upon pressure release. Measuring strength in such a transient high-pressure phase is challenging. One measurement used free-surface Richtmyer-Meshkov instabilities generated with gas gun impact. Another set of measurements used ramp-release loading in a pulsed-power facility. Strength estimations came from comparison to simulations using a comprehensive multiphase modeling framework that includes equation of state, shear moduli, and strength separately for each phase, and treats mixed-phase regions. Both experimental methods found the 𝛾-phase strength to be very low, within experimental uncertainty of zero. The existing literature on other materials, by contrast, almost universally reports higher strength in transient high-pressure phases compared with ambient phases. Recent Molecular-Dynamics simulations on tin in the literature showed almost zero deviatoric strength during a deformation-induced bct → bct transformation in which one of the 𝛾-phase 𝑎 axes “flips” to the 𝑐 axis. This reorientation currently provides the most plausible explanation for the low observed strength in 𝛾-phase tin.
An ultrafine/nano-grained AZ31 magnesium alloy was processed through multipass accumulative back extrusion at 280 and 380 °C. Texture analysis was conducted to determine preferred crystallographic orientations developed during multipass deformation. The anisotropy in mechanical properties of the processed materials was studied by compressive and tensile testing. The results implied that the accumulative back extrusion effectively reduces the anisotropy of yield strength, ultimate strength and strain-to-fracture during compressive and tensile loading. The operations of different twinning/slip systems during compressive and tensile deformation were discussed using Schmid factors measurements. A decrease in twinning-related anisotropy, as well as the contribution of different slip systems in strain accommodation, could reduce the mechanical anisotropy of ultrafine/nano-grained AZ31 alloy. The compressive strength of the two-pass processed material was lower along extrusion direction than transverse direction; however, the result was reverse after four passes. The tensile behavior implied that the contribution of basal slip might accommodate strain along length as well as the thickness of the specimen, while prismatic slip may assist in narrowing the width of the specimen and elongating the length.
When materials are deformed at extreme strain rates, >10 6 s -1 , a counterintuitive mechanical response is seen where the strength and hardness of pure metals increases with increasing temperature. This anti-thermal hardening is due to dislocations meeting resistance to their motion from phonons in the crystal lattice. However, here, using optically-driven microballistic impact testing to measure dynamic strength and hardness, we show that when the composition is systematically varied away from high purity, the mechanical response of metals transitions from phonon drag of dislocations back to thermally activated pinning of dislocations, even at the highest strain rates. This boundary from “hotter-is-stronger” to “hotter-is-softer” is observed and mapped for nickel, titanium and gold. Furthermore, the ability to tune between deformation mechanisms with very different temperature dependencies speaks to new directions for alloy design in extreme conditions.
Magnesium alloys have been increasingly used in automotive and electronic industries because of their excellent strength to weight ratio and EMI shielding properties. However, magnesium alloys have low formability at room temperature due to their unique mechanical behavior (twinning and untwining), prompting for forming at an elevated temperature. In this study, a temperature dependent constitutive model for magnesium alloy (AZ31B) sheet is developed. A hardening law based on non linear kinematic hardening model is used to consider Bauschinger effect properly. Material parameters are determined from a series of uni-axial cyclic experiments (T-C-T or C-T-C) with the temperature ranging 150-250 deg. C. The influence of temperature on the constitutive equation is introduced by the material parameters assumed to be functions of temperature. Fitting process of the assumed model to measured data is presented and the results are compared.
Abstract This study investigates the mechanical properties and in vitro cytotoxicity of one‐ and two‐dimensional boron nitride nanomaterials‐reinforced biodegradable polymeric nanocomposites. Poly(propylene fumarate) (PPF) nanocomposites were fabricated using crosslinking agent N ‐vinyl pyrrolidone and inorganic nanomaterials: boron nitride nanotubes (BNNTs) and boron nitride nanoplatelets (BNNPs) dispersed at 0.2 wt % in the polymeric matrix. The incorporation of BNNPs and BNNTs resulted in a ∼38 and ∼15% increase in compressive (Young's) modulus, and ∼31 and ∼6% increase in compressive yield strength compared to PPF control, respectively. The nanocomposites showed a time‐dependent increased protein adsorption for collagen I protein. The cytotoxicity evaluation of aqueous BNNT and BNNP dispersions (at 1–100 μg/mL concentrations) using murine MC3T3 preosteoblast cells showed ∼73–99% viability. The cytotoxicity evaluation of media extracts of nanocomposites before crosslinking, after crosslinking, and upon degradation (using 1×–100× dilutions) showed dose‐dependent cytotoxicity responses. Crosslinked nanocomposites showed excellent (∼79–100%) cell viability, cellular attachment (∼57–67%), and spreading similar to cells grown on the surface of tissue culture polystyrene control. The media extracts of degradation products showed a dose‐dependent cytotoxicity. The favorable cytocompatibility results in combination with improved mechanical properties of BNNT and BNNP nanocomposites opens new avenues for further in vitro and in vivo safety and efficacy studies towards bone tissue engineering applications. © 2015 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 105B: 406–419, 2017.
Deformation mechanisms found at the pore scale are responsible for producing large strains in porous rocks. Furthermore, they include cataclastic flow, dislocation creep, dynamic recrystallization, diffusive mass transfer, and grain boundary sliding, among others. Here, we focus on two dominant pore-scale mechanisms resulting from purely mechanical, isothermal loading: crystal plasticity and micro-fracturing. We examine the contributions of each mechanism to the overall behavior at a scale larger than the grains but smaller than the specimen, which is commonly referred to as the mesoscale. Crystal plasticity is assumed to occur as dislocations along the many crystallographic slip planes, whereas micro-fracturing entails slip and frictional sliding on microcracks. It is observed that under combined shear and tensile loading, micro-fracturing generates a softer response compared to crystal plasticity alone, which is attributed to slip weakening where the shear stress drops to a residual level determined by the frictional strength. For compressive loading, however, micro-fracturing produces a stiffer response than crystal plasticity due to the presence of frictional resistance on the slip surface. Behaviors under tensile, compressive, and shear loading invariably show that porosity plays a critical role in the initiation of the deformation mechanisms. Both crystal plasticity and micro-fracturing are observed to initiate at the peripheries of the pores, consistent with results of experimental studies.
In this work, Fe{sub 3}Al-based composites reinforced with carbon nanotubes were fabricated by a hot-press sintering process under various sintering pressures. The effects of sintering pressure and additives (alumina and lanthanum) on both the physical and the mechanical properties were systematically investigated. Results showed that with the sintering pressure of 15 MPa and incorporation of carbon nanotubes (CNTs), the microhardness of Fe{sub 3}Al composite exhibited a peak value at 1038.1 HV, which was ~ 60% higher than those without the addition of carbon nanotubes (644.9 HV). Also, both the compressive yield strength and the thermal conductivity of Fe{sub 3}Al composite were also significantly improved. Results of wear test showed the Fe{sub 3}Al composite exhibited a low wearing rate (10{sup −6}-10{sup −5} order of magnitude) and a friction coefficient (0.53-0.67).
In the present study, a homogeneous ultrafine grain structure composite consisting of metallic glass particles reinforcements was developed by equal-channel angular pressing (ECAP) process. The microstructure of composite was characterized using x-ray diffraction (XRD), transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD) techniques. The uniaxial compression test was used to determine the mechanical properties. The mechanisms of grain refinement during ECAP process were discussed based on the microstructural evolutions. A composite was successfully produced after four passes of ECAP, having an average grain size of 610 nm and compressive yield strength of 242 MPa. Also, the yield strength of composite after each pass was quantitatively estimated by considering all the effective strengthening mechanism. The findings showed that the dislocations strengthening mechanism with contribution of more than 50% plays a major role in strengthening the composite. There was a negligible gap between the experimental and theoretical values of yield strength for all ECAP pass numbers.
Al{sub 0.4}FeCrNiCo{sub x} (x = 0, 0.25, 0.5, 1.0 mol) high-entropy alloys are developed by arc melting route to investigate the effect of cobalt content on thermal, mechanical, and microstructural properties. The phase, microstructure, and chemical composition are analyzed using x-ray diffraction, transmission electron microscope, and scanning electron microscope with attached energy-dispersive x-ray spectrometer. The obtained results have shown that the Al{sub 0.4}FeCrNiCo{sub x} (x = 0-0.5 mol) high-entropy alloys form a simple FCC + BCC-type solid solution and Al{sub 0.4}FeCrNiCo{sub x=1} HEA forms a single-phase FCC structure. The compressive yield strength, microhardness, and thermal conductivity are observed to decrease from 965.22 to 233.37 MPa, 253.6 to 155.6 HV, and from 4.87 to 2.674 W/mK, respectively, whereas the electrical resistivity is observed to increase from 150.30 to 273.74 µΩ-cm with the addition of cobalt from x = 0-1 mol. Differential scanning calorimetry analysis has indicated that the Al{sub 0.4}FeCrNiCo{sub x} (x = 0, 0.25, 0.5, 1.0 mol) high-entropy alloys are thermally stable up to 1000 °C.
Binding and particle phases are the two important parameters influencing materials properties. In this study, a series of novel W-4.9Ni-2.1Fe-xY{sub 2}O{sub 3} (in weight%) alloys with different Y{sub 2}O{sub 3} contents are prepared by secondary ball milling and spark plasma sintering (SPS) techniques to obtain uniformly distributed γ-(Ni, Fe) binding phases and finer grains. The microstructure, mechanical, wear resistance, and corrosion behavior of the sintered bodies with different Y{sub 2}O{sub 3} were obtained by x-ray diffraction, scanning electron microscopy, Rockwell hardness tester, friction wear tester, and three-dimensional profile instruments. The results showed that a certain addition of Y{sub 2}O{sub 3} led to refined grains and uniformed microstructures; but, if excessive, a weak grain refinement would be appeared. Moreover, the grain size tends to be stable with enhancing of the Y{sub 2}O{sub 3} content. Considering properties such as density, hardness, compression yield strength, grain size, and uniform distribution of tungsten hard phase and γ-(Ni, Fe) binding phase, the comprehensive optimal amount of 0.7 wt.% of Y{sub 2}O{sub 3} was attained for the alloy. Meanwhile, the SPS sintered body also exhibited the best friction, wear behavior, and corrosion resistance in 3.5% of NaCl solution.
An iron-rich high entropy alloy Al 0.65 CoCrFe 2 Ni comprising of both FCC and BCC phases was designed and fabricated using induction melting at a large industrial scale and suction casting at a small lab scale. Spinodally decomposed interdendritic regions were uniformly distributed in the industrially melted alloy, and a finer dendritic structure with smaller sized spinodal structures was observed in the alloy suction cast at lab scale. The suction cast alloy fabricated at the lab scale exhibited significantly higher compressive yield strength compared to the industrially cast alloy. The relative strengthening contributions in the alloys due to solid solution, grain boundary, dislocation interactions and interphase boundary were analyzed. Dislocation hardening was the major contributor responsible for the higher strength of the SC alloy. The deformation behavior in the alloys was examined with the help of orientation image mapping. Finally, intense slip band formation at large strains in the industrially melted alloy indicates that cold working can be an effective technique to enhance the strength of the dual-phase high entropy alloy processed at a large scale.
Photocatalytic activity of TiO{sub 2} was studied in two types of calcium aluminate cement (CAC) under two different curing regimes. The effect of the TiO{sub 2} addition on the setting time, consistency and mechanical properties of the CACs was evaluated. The abatement of gaseous pollutants (NO{sub x}) under UV irradiation was also assessed. These cementitious matrices were found to successfully retain NO{sub 2}: more abundant presence of aluminates in white cement (w-CAC, iron-lean) helped to better adsorb NO{sub 2}, thus improving the conversion performance of the catalyst resulting in a larger NO{sub x} removal under UV irradiation. As evidenced by XRD, SEM, EDAX and zeta potential analyses, the presence of ferrite in dark cement (d-CAC, iron-reach) induced a certain chemical interaction with TiO{sub 2}. The experimental findings suggest the formation of new iron titanate phases, namely pseudobrookite. The reduced band-gap energy of these compounds compared with that of TiO{sub 2} accounts for the photocatalytic activity of these samples.
This paper reports strategies to design the binder phase of ultra-high performance concretes (UHPC) from commonly available cement replacement (fly ash, slag, microsilica, metakaolin) and fine filler (limestone) materials. A packing algorithm is used to extract the number density, mean centroidal distance, and coordination number of the microstructure. Similarly, rheological studies on the pastes provide yield stress, plastic viscosity, and min-slump spread. The selection criteria involves using the three microstructural and three rheological parameters individually or in combination to define packing and flow coefficients. The selection criteria is flexible enough to allow users modify the constraints depending on the application. In this study, only ternary and quaternary blends, with a total cement replacement of 30% by mass are selected for further characterization. The highly efficient microstructural packing in these mixtures and better workability that facilitated dispersion of particles to enhance the reactivity results in beneficial pore structure and mechanical properties.