Time at Temperature Experiments on Neutron Irradiated Zircaloy-2 using Conventional & Flash DSC

Dryout events in Boiling Water Reactors (BWRs) are currently treated by NRC regulations as automatic disqualification for continued fuel rod operation, even though this criterion does not account for the rate or duration of power increases, associated changes in material behavior, or the possibility of rewetting. Operational history from Anticipated Operational Occurrences (AOOs) shows that short, transient power excursions often demand only modest heat removal, and industry experience suggests that fuel can briefly enter dryout yet return to safe, stable operation. The lack of detailed understanding of the material response during such events motivates the present series of experiments. This study uses unique and innovative methods to investigate microstructural evolution in irradiated Zircaloy-2 exposed to high temperatures in inert environments. Differential Scanning Calorimetry (DSC) and FlashDSC are combined to build a comprehensive experimental framework capable of identifying the a–ß phase transformation in zirconium and examining defect annealing under steep thermal gradients. FlashDSC enables rapid heating and cooling of Focused Ion Beam (FIB)–prepared large-area lift-outs (LALOs) of irradiated Zircaloy-2 at rates of 1,000 K/s to peak temperatures of 600°C, 750°C, and 900°C. The goal is to determine whether these conditions produce measurable microstructural changes that could influence cladding performance in typical BWR environments. Microstructural characterization includes quantifying dislocation density and assessing secondary phase particle (SPP) size and distribution using Transmission Electron Microscopy (TEM). Ongoing analysis, such as diffraction pattern indexing and 4D STEM processing, will further refine these observations.

36 - MATERIALS SCIENCE↗

Phase formation, structural and microstructural characterization of novel oxynitride-perovskites synthesized by thermal ammonolysis of (Ca,Ba)MoO{sub 4} and (Ca,Ba)MoO{sub 3}

Reactions of AMoO{sub 4} and AMoO{sub 3} (A=Ca{sup 2+}, Ba{sup 2+}) with ammonia were investigated at 873 K<T<1123 K with the particular intention to synthesize novel oxynitride-perovskites of the general composition AMo(O,N){sub 3} and to study their crystal structure. CaMo(O,N){sub 3} and BaMo(O,N){sub 3} were prepared by thermal ammonolysis of the corresponding CaMoO{sub 3} and BaMoO{sub 3} precursors at T=898 and 998 K, respectively. The structural parameters of the oxynitrides were obtained from Rietveld refinements of X-ray and neutron powder diffraction data. CaMo(O,N){sub 3} crystallizes in the GdFeO{sub 3} distorted perovskite structure with orthorhombic space group Pbnm and a=5.5029(1) A, b=5.5546(1) A, c=7.8248(1) A as determined by X-ray powder diffraction. Its O/N content refined from the neutron diffraction data corresponds to the composition CaMoO{sub 1.7(1)}N{sub 1.3(1)}. BaMo(O,N){sub 3} crystallizes in the cubic perovskite structure with space group Pm3-bar m and a=4.0657(1) A as determined by X-ray powder diffraction. Transmission electron microscopy reveals a complex microstructure for both CaMoO{sub 3} and CaMoO{sub 1.7(1)}N{sub 1.3(1)} represented by twin domains of different orientation. - Graphical abstract: Reactions of AMoO{sub 4} and AMoO{sub 3} (A=Ca{sup 2+}, Ba{sup 2+}) oxides with ammonia have been studied at T=873-1123 K. Orthorhombic CaMoO{sub 1.7(1)}N{sub 1.3(1)} (Pbnm) and cubic BaMo(O,N){sub 3} (Pm3-bar m) were prepared by thermal ammonolysis of the corresponding CaMoO{sub 3} and BaMoO{sub 3} precursors at T=898 and 998 K, respectively. Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improving precipitation hardening behavior of Mg−Zn based alloys with Ce−Ca microalloying additions

The precipitation hardening behavior of newly developed Mg−Zn−Ca−Ce alloys, with modified texture and improved ductility, is studied to delineate the microstructural characteristics that lead to effective hardening upon ageing treatments. Advanced electron microscopy and atom probe techniques are used to analyze the structural characteristics in relevance to the hardening potential. It has been found that the formation of a new basal precipitate phase, which evolves from a single atomic layer GP zone, and is finely distributed in both under-aged and peak-aged microstructures, has a significant impact in the improvement of the hardening response compared with the base Mg−Zn alloys. It has also been found that the β′{sub 1} rod precipitates, commonly formed during ageing treatments of Mg−Zn alloys, have their size and distribution significantly refined in the Ca−Ce containing alloys. The role of alloy chemistry in the formation of the fine basal plate GP zones and the refinement in β′{sub 1} precipitation and their relationships to the hardening behavior are discussed. It is proposed that Ca microalloying governs the formation of the GP zones and the enhancement of hardening, particularly in the under-aged conditions, but that this is aided by a beneficial effect from Ce. - Highlights: • Ce−Ca microalloying additions improve hardening in Mg−Zn, over Ce or Ca alone. • Improved hardening is due to refined β′{sub 1} rods, and fine basal plate precipitates. • Atom probe tomography identifies Ca in both β′{sub 1} and the fine basal plates. • The fine basal plates originate as ordered monolayer GP zones with 1:1 Zn:Ca (at.%). • With ageing GP zones become more Zn-rich and transform to the fine basal plates.

36 MATERIALS SCIENCE↗

Structure, microstructure and infrared studies of Ba{sub 0.06}(Na{sub 1/2}Bi{sub 1/2}){sub 0.94}TiO{sub 3}-NaNbO{sub 3} ceramics

Lead-free solid solutions (1-x)Ba{sub 0.06}(Na{sub 1/2}Bi{sub 1/2}){sub 0.94}TiO{sub 3}-xNaNbO{sub 3} (0 ≤ x ≤ 1.0) were prepared by conventional ceramic fabrication technique. X-ray diffraction and Rietveld refinement analyses of these ceramics were carried out using X’Pert HighScore Plus software to determine the crystal symmetry, space group and unit cell dimensions. Rietveld refinement revealed that NaNbO{sub 3} with orthorhombic structure was completely diffused into Ba{sub 0.06}(Na{sub 1/2}Bi{sub 1/2}){sub 0.94}TiO{sub 3} lattice having the rhombohedral-tetragonal symmetry. EDS and SEM studies were carried out in order to evaluate the quality and purity of the compounds. SEM images showed a change in grain shape with the increase of NaNbO{sub 3} content. FTIR spectra confirmed the formation of solid solution.

36 MATERIALS SCIENCE↗

Structural, Morphological, Raman, and Mössbauer Studies on (La{sub 0.8}Ca{sub 0.2}){sub 1−x}Bi{sub x}FeO{sub 3} (x = 0.0, 0.1, and 0.2) Compounds

(La{sub 0.8}Ca{sub 0.2}){sub 1−x}Bi{sub x}FeO{sub 3} (x = 0.0, 0.1, and 0.2) compounds were prepared by the sol-gel method, using the citric acid route. Structural and microstructural characteristics of the samples were studied by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and Raman spectroscopy. Mössbauer spectroscopy was also used for magnetic characterization and structural confirmation of X-ray data. Refinement of XRD patterns indicated that the compounds crystallize in an orthorhombic structure, Pnma space group. The SEM measurements showed that the morphology of the samples is characterized by the existence of large agglomerates, while TEM confirmed the fine particle size. Raman spectra revealed that, when increasing temperature, the level of oxygen species adsorbed at the surface of the particles increases progressively. Room temperature Mössbauer spectroscopy data revealed the existence of two octahedral magnetic sites in the structure of the compounds, which is compatible with XRD data, and a small percentage of a paramagnetic phase in the samples, which increases with Bi-content.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure and Electromagnetic Shielding Properties of Mg-Zn-Ce-Y-Zr Alloys

Microstructure and electromagnetic interference shielding properties of extruded Mg-Zn-Ce-Y-Zr alloys were systematically investigated. A bimodal grain structure of fine recrystallized grains and deformed grains was observed in the alloys. Yttrium (Y) and cerium (Ce) refined the recrystallized grains. Mg-Zn-Ce phase, Mg{sub 3}Zn{sub 3}Y{sub 2} phase and a few precipitates containing Zn and Zr were observed. Y and Ce additions changed the texture of the alloys. When the total rare earth content reached 4 wt.%, the texture was remarkably weaker than other studied alloys. The shielding capacity increased first and then decreased with Y contents. The value of shielding effectiveness for the extruded Mg-5Zn-1Ce-2Y-0.6Zr alloys reached 79-118 dB in the frequency range of 30 MHz-1.5 GHz, which was significantly higher than that of some aluminum alloys. The addition of Y and Ce is effective in improving the shielding capacity in Mg alloys. The electrical conductivity and second phases in the alloys were important in enhancing shielding effectiveness. The texture and precipitation exerted significant effect on electrical conductivity. In addition, subsequently aging treatment evidently improved shielding effectiveness.

36 MATERIALS SCIENCE↗

Stress Corrosion Cracking of AZ91 + xCe Alloy Using Proof Ring Test in ASTM D1384 and NaCl-K{sub 2}CrO{sub 4} Solutions

The effect of cerium addition on AZ91 magnesium alloy and its influence on stress corrosion cracking (SCC) were studied using constant load proof ring testing NaCl-K{sub 2}CrO{sub 4} and ASTM D1384 solutions at 70 and 80% of yield stress, respectively. The investigation revealed that the optimum grain refinement of desired phases occurred with 0.5% addition of cerium. The addition levels of cerium above 1.5 wt.% to AZ91 alloy resulted in premature failures due to poor SCC resistance in both solutions (K{sub 2}CrO{sub 4} and ASTM D1384 solutions). The microstructural studies of the experimental alloys were characterized by using optical and scanning electron microscopy. The elemental compositions of cerium-added AZ91 magnesium alloys were studied by energy-dispersive spectroscopy. The results indicate that the mode of SCC failure was found to be transgranular in nature along with secondary cracks containing cleavages which resulted from the hydrogen embrittlement and anodic dissolution phenomena. The AZ91 alloy with 0.5 wt.% cerium exhibits better mechanical properties and high stress corrosion resistance.

36 MATERIALS SCIENCE↗

Quantitative examination of carbide and sulphide precipitates in chemically complex steels processed by direct strip casting

A high strength low alloy steel composition has been melted and processed by two different routes: simulated direct strip casting and slow cooled ingot casting. The microstructures were examined with scanning and transmission electron microscopy, atom probe tomography and small angle neutron scattering (SANS). The formation of cementite (Fe{sub 3}C), manganese sulphides (MnS) and niobium carbo-nitrides (Nb(C,N)) was investigated in both casting conditions. The sulphides were found to be significantly refined by the higher cooling rate, and developed an average diameter of only 100 nm for the fast cooled sample, and a diameter too large to be measured with SANS in the slow cooled condition (> 1.1 μm). Slow cooling resulted in the development of classical Nb(C,N) precipitation, with an average diameter of 7.2 nm. However, after rapid cooling both the SANS and atom probe tomography data indicated that the Nb was retained in the matrix as a random solid solution. There was also some evidence that O, N and S are also retained in solid solution in levels not found during conventional processing. - Highlights: • The influence of cooling rate on microstructure is investigated in a HSLA steel. • SANS, TEM and APT are used to characterise the sulphides and Nb(C,N) precipitates. • The slow cooling rate result in the formation of Nb(C,N) precipitates. • The fast cooling rate results in a microstructure supersaturated in Nb, C and N. • The sulphides are 100 nm in the fast cooled sample and > 1 μm in the slow cooled one.

36 MATERIALS SCIENCE↗

Electrochemical Behavior of Mg-Al-Zn-Ga Alloy as Anode Materials in 3.5 wt.% NaCl Solution

The microstructure and electrochemical behaviors of Mg-Al-Zn and Mg-Al-Zn-Ga alloys as anode materials were investigated by morphology observation, composition analysis, phase identification, and electrochemical tests. The experimental results suggest that Ga alloying can refine the grains of the Mg-Al-Zn alloy by promoting second-phase segregation, which comprises Mg{sub 17}Al{sub 12} and GaMg{sub 2}. The comparison of discharge tests indicates that adding Ga to the Mg-Al-Zn alloy can negatively shift the discharge potential, provide a high current density, promote the formation of tiny and thin products, and improve the utilization efficiency. Meanwhile, the addition of Ga can increase the corrosion resistance of Mg-Al-Zn alloy because the Ga alloying promotes the segregation of the intermetallic phases in the Mg matrix. The intermetallic phases disperse in isolate states in the Mg matrix, resulting in their falling off from the substrate once their adjacent Mg is exhausted and subsequently ceasing the micro-galvanic corrosion. The Mg-Al-Zn-Ga alloy with higher corrosion resistance performs better discharge activity than that of Mg-Al-Zn alloy in 3.5 wt.% NaCl solution, implying that the Mg-Al-Zn-Ga alloy is a promising anode material for seawater-activated battery.

36 MATERIALS SCIENCE↗

Synergistic Tuning of Microstructure and Morphology in Carbon Molecular Sieve Hollow Fibers for Propylene/Propane Separation

Abstract Asymmetric carbon molecular sieve (CMS) hollow fiber membranes with tunable micro‐ and macro‐structural morphologies for energy efficient propylene‐propane separation are reported here. A sub‐glass transition temperature (sub‐Tg) thermal oxidative crosslinking strategy enables simultaneous optimization of the intrinsic molecular sieving properties while also reducing the thickness of the CMS “skin” derived from the 6FDA : BPDA/DAM polyimide precursors. Such synergistic tuning of CMS microstructure and macroscopic morphology of CMS hollow fibers enables significantly increased propylene permeance (reaching 186.5 GPU) while maintaining an appealing propylene/propane selectivity of 13.3 for 50/50 propylene/propane mixed gas feeds. Our findings reveal a more refined and versatile tool than available with previous O 2 ‐doping pretreatments. The advanced approach here should be broadly useful to other polyimide precursors and diverse gas pairs.

Liu, Zhongyun [School of Chemical &amp, Biomolecul↗

Synergistic Tuning of Microstructure and Morphology in Carbon Molecular Sieve Hollow Fibers for Propylene/Propane Separation

Abstract Asymmetric carbon molecular sieve (CMS) hollow fiber membranes with tunable micro‐ and macro‐structural morphologies for energy efficient propylene‐propane separation are reported here. A sub‐glass transition temperature (sub‐Tg) thermal oxidative crosslinking strategy enables simultaneous optimization of the intrinsic molecular sieving properties while also reducing the thickness of the CMS “skin” derived from the 6FDA : BPDA/DAM polyimide precursors. Such synergistic tuning of CMS microstructure and macroscopic morphology of CMS hollow fibers enables significantly increased propylene permeance (reaching 186.5 GPU) while maintaining an appealing propylene/propane selectivity of 13.3 for 50/50 propylene/propane mixed gas feeds. Our findings reveal a more refined and versatile tool than available with previous O 2 ‐doping pretreatments. The advanced approach here should be broadly useful to other polyimide precursors and diverse gas pairs.

Liu, Zhongyun↗

Influences of Gd on the microstructure and strength of Mg-4.5Zn alloy

Microstructure and mechanical properties of peak-aged Mg-4.5Zn-xGd (x 0, 0.5, 1.0 and 1.5 wt.%) alloys have been investigated. The results showed that the grain size of the alloys was refined gradually with increasing Gd. Mg{sub 5}Gd and Mg{sub 3}Gd{sub 2}Zn{sub 3} phases were found in the Gd-containing alloys. The strengths were greatly improved with Gd additions, and the highest strength level was obtained in the Mg-4.5Zn-1.5Gd alloy, in which the ultimate tensile strength and yield strength were 231 MPa and 113 MPa, respectively. Through comparing with the Mg-4.5Zn alloy, the increments of ultimate tensile strength and yield strength were 22 MPa and 56 MPa, respectively. The improved strength was mainly correlated to the grain refining effect, the strengthening effect of the Mg{sub 5}Gd and Mg{sub 3}Gd{sub 2}Zn{sub 3} phases and also the hardening effect of the solutioned Gd atoms.

36 MATERIALS SCIENCE↗

Effect of gadolinium addition on microstructural evolution and solidification characteristics of Al-15%Mg2Si in-situ composite

Highlights: • The Al{sub 3}Gd is the heterogeneous nucleation of primary Mg{sub 2}Si in Al-15%Mg{sub 2}Si composite. • Addition of Gd to Al-15%Mg{sub 2}Si resulted in the formation of Al{sub 2}Si{sub 2}Gd and AlSiGd intermetallic compounds. • Absorption of Gd atoms preferentially on {100} facets of Mg{sub 2}Si crystals changed its growth manners. • Primary Mg{sub 2}Si transformed from coarse-dendritic to perfect truncated octahedral shape after treating with 1.0 wt% Gd. • Gd addition increased the nucleation and growth temperatures of primary Mg{sub 2}Si. - Abstract: The current study investigated the effects of gadolinium (Gd) addition (0, 0.3, 0.5, 1.0, and 2.0 wt%) on microstructural development and solidification characteristics of hypereutectic Al-15%Mg{sub 2}Si in-situ composite. Microstructural examinations were carried out via optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM), and electron backscattered diffraction (EBSD). The results showed that an addition of 1.0 wt% Gd, changed the morphology of primary Mg{sub 2}Si from coarse dendritic to fine truncated octahedral shape. Furthermore, the average size of primary Mg{sub 2}Si particles decreased from 40 μm to 20 μm and density increased from 495 to 1167 particles/mm{sup 2}. Besides that, cooling curve thermal analysis (CCTA) technique revealed that Gd addition increased nucleation and growth temperatures of primary Mg{sub 2}Si phase. It is proposed that modification and refinement mechanism of Gd addition are mainly attributed to formation of tiny Al{sub 3}Gd particles as the heterogeneous nucleation substrates for primary Mg{sub 2}Si, which results in a refined distribution of these particles and poisoning effect by adsorbing Gd atoms, preferentially on {100} facets of Mg{sub 2}Si crystals. Moreover, it is believed that formation of Gd intermetallic compounds is responsible for refinement of primary Mg{sub 2}Si particles.

36 MATERIALS SCIENCE↗

Microstructural, optical and electrical properties of LaFe{sub 0.5}Cr{sub 0.5}O{sub 3} perovskite nanostructures

Perovskite nanocrystalline powder of LaFe{sub 0.5}Cr{sub 0.5}O{sub 3} was synthesized by sol-gel combustion route and characterized by x-ray diffractometer (XRD), scanning electron microscopy (SEM) equipped with EDS, UV-visible and LCR meter at room temperature Rietveld refinement of the XRD data confirms that the sample is in single phase-rhombohedral structure with space group R-3C. SEM micrograph shows clear nanostructure of the sample and EDS ensures the presence of all elements in good stoichiometric. The optical absorption indicates the maximum absorption at 315 nm and optical band gap of 2.94 eV was estimated using Tauc’s relation. Dielectric constant (ε’) and loss were found to decrease with increase in frequencies. The dielectric behavior was explained on the basis of Maxwell-Wagner’s two layer model.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Structure, microstructure, and size dependent catalytic properties of nanostructured ruthenium dioxide

Nanostructured powders of ruthenium dioxide RuO{sub 2} were synthesized via a sol gel route involving acidic solutions with pH varying between 0.4 and 4.5. The RuO{sub 2} nanopowders were characterized by X-ray diffraction, scanning and transmission electron microscopy (SEM and TEM). Rietveld refinement of mean crystal structure was performed on RuO{sub 2} nanopowders and crystallized standard RuO{sub 2} sample. Crystallite sizes measured from X-ray diffraction profiles and TEM analysis varied in the range of 4-10 nm, with a minimum of crystallite dimension for pH=1.5. A good agreement between crystallite sizes calculated from Williamson Hall approach of X-ray data and from direct TEM observations was obtained. The tetragonal crystal cell parameter (a) and cell volumes of nanostructured samples were characterized by values greater than the values of standard RuO{sub 2} sample. In addition, the [Ru-O{sub 6}] oxygen octahedrons of rutile structure also depended on crystal size. Catalytic conversion of methane by these RuO{sub 2} nanostructured catalysts was studied as a function of pH, catalytic interaction time, air methane composition, and catalysis temperature, by the way of Fourier transform infrared (FTIR) spectroscopy coupled to homemade catalytic cell. The catalytic efficiency defined as FTIR absorption band intensities I(CO{sub 2}) was maximum for sample prepared at pH=1.5, and mainly correlated to crystallite dimensions. No significant catalytic effect was observed from sintered RuO{sub 2} samples. - Graphical abstract: Nanosized crystals of RuO{sub 2} prepared by sol gel route, at pH=0.4 and 1.5. Mean size values <D>, respectively, 10 and 8 nm.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Microstructure, Tensile Properties, and Corrosion Behavior of Die-Cast Mg-7Al-1Ca-xSn Alloys

The microstructure, tensile properties, and corrosion behavior of die-cast Mg-7Al-1Ca-xSn (x = 0, 0.5, 1.0, and 2.0 wt.%) alloys were studied using OM, SEM/EDS, tensile test, weight loss test, and electrochemical test. The experimental results showed that Sn addition effectively refined grains and intermetallic phases and increased the amount of intermetallic phases. Meanwhile, Sn addition to the alloys suppressed the formation of the (Mg,Al){sub 2}Ca phase and resulted in the formation of the ternary CaMgSn phase and the binary Mg{sub 2}Sn phase. The Mg-7Al-1Ca-0.5Sn alloy exhibited best tensile properties at room temperature, while Mg-7Al-1Ca-1.0Sn alloy exhibited best tensile properties at elevated temperature. The corrosion resistance of studied alloys was improved by the Sn addition, and the Mg-7Al-1Ca-0.5Sn alloy presented the best corrosion resistance.

36 MATERIALS SCIENCE↗

Microstructural, Magnetic, and Nanoindentation Studies of the Ball-Milled Ti80Ni20 Alloy

Nanostructured Ti{sub 80}Ni{sub 20} material was elaborated by mechanical alloying from pure Ti and Ni powders in a planetary ball-mill P7 under argon atmosphere at ambient temperature. Morphological, microstructural, magnetic, and nanoindentation properties were studied using scanning electron microscopy, X-ray diffraction, magnetic measurements, and nanoindentation test. The morphological observations show the predominance of the welding phenomenon during the milling process. The Rietveld refinement of the X-ray diffraction pattern reveals, after 4 h of milling, the formation of the disordered hcp-Ti (Ni) solid solution in addition to elemental hcp-Ti and fcc-Ni. On further milling (20 h), the interdiffusion between Ti and Ni atoms is evidenced by the formation of disordered hcp-Ti (Ni) and fcc-Ni (Ti) solid solutions. The saturation magnetization and coercivity values are about of 159.8 emu/g and 80.79 Oe, respectively, after 20 h of milling. M{sub r}/M{sub s} ratio indicates the existence of small magnetic particles which are typically single domains (M{sub r}/M{sub s} 0.1–0.5) and/or multidomain (M{sub r}/M{sub s} < 0.1). Nanohardness values of the sintered powders fluctuates between 1.53 and 5.98 GPa while those of the elastic modulus varies in the range 130.73 to 164.53 GPa.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Characterization and Strain-Hardening Behavior of Friction Stir-Welded Ferritic Stainless Steel

In this study, friction stir-welded joint of 3-mm-thick plates of 409 ferritic stainless steel (FSS) was characterized in light of microstructure, x-ray diffraction analysis, hardness, tensile strength, ductility, corrosion and work hardening properties. The FSW joint made of ferritic stainless steel comprises of three distinct regions including the base metal. In stir zone highly refined ferrite grains with martensite and some carbide precipitates at the grain boundaries were observed. X-ray diffraction analysis also revealed precipitation of Cr{sub 23}C{sub 6} and martensite formation in heat-affected zone and stir zone. In tensile testing of the transverse weld samples, the failure eventuated within the gauge length of the specimen from the base metal region having tensile properties overmatched to the as-received base metal. The tensile strength and elongation of the longitudinal (all weld) sample were found to be 1014 MPa and 9.47%, respectively. However, in potentiodynamic polarization test, the corrosion current density of the stir zone was highest among all the three zones. The strain-hardening exponent for base metal, transverse and longitudinal (all weld) weld samples was calculated using various equations. Both the transverse and longitudinal weld samples exhibited higher strain-hardening exponents as compared to the as-received base metal. In Kocks–Mecking plots for the base metal and weld samples at least two stages of strain hardening were observed.

36 MATERIALS SCIENCE↗